Narayana Dilip Raja
Narayana Dilip Raja has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Naren Shankar Radha Krishnan
Department of Aeronautical Engineering , Vel Tech Rangarajan Dr. Sagunthala R&D Institute of Science and Technology , Chennai , India
3 shared publications A.T. Ravichandran
Department of Mechanical Engineering, Vel Tech Rangarajan Dr. Sagunthala R & D Institute of Science and Technology, Chennai, India
1 shared publication- Hussein Mohamed Abdelmoneam Hussein
Mechanical Engineering Department, Faculty of Engineering and Technology, Future University in Egypt, New Cairo 11835, Egypt
1 shared publication - Jee Joe Michael
Department of Energy and Environmental engineering, SIMATS University Chennai Tamil Nadu India
1 shared publication K V A Kumar
Department of Mechanical Engineering, Vel Tech Rangarajan Dr. Sagunthala R&D Institute of Science and Technology, Avadi, Chennai-600062, Tamil Nadu, India
1 shared publicationK. Palani Kumar
Sairam College Road
1 shared publication
Latest Publications
- Open Access
- 29 May 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (2) , 155-161
The Effects of Deep Cryogenic Treatment on Heat transfer of Aluminium Heat Sink
Thermal management is critical for achieving peak performance and extending the life of electronic equipment. Heat sinks are the most effective thermal control tools. Copper and aluminium are the most used materials for heat sinks. Aluminium, in particular, attracts a lot of attention due to its lightweight and recyclability, which assures sustainability. Because of its robustness, malleability, and good thermal conductivity, the aluminium 6000 series is ideal for use in heat sink manufacturing. In this research, raw material consisting of Al6060 is turned into a square pin fin heat sink with 25 pin fins using a CNC milling machine. The natural convection heat transfer efficiency of the heat sink was identified with a specially constructed experimental setup. Four different heat inputs (15 W, 25 W, 35 W, and 45 W) were analyzed. The novelty of this work is that the heat sink undergoes deep cryogenic treatment (DCT). The soaking duration in liquid nitrogen is set at 24 hours. The heat transfer efficiency of DCT treated aluminium heat sink is compared with the bare aluminium heat sink. The testing findings revealed that when the heat input was 15W, the DCT treated square pin fin heat sink had a charging cycle that was up to 77.78 % longer than the untreated heat sink. At 25W, 35 W, and 45 W heat input, the charging cycle was 48 %, 39 %, and 28 % longer, respectively. Analyzing the discharge cycle revealed that only the 15 W heat input had an ideal discharge cycle, which was 20 % shorter than the untreated heat sink. The results are compared with the results of heat sink coupled with phase change materials (PCM) from the literature. The analysis revealed that for the DCT treated heat sink, heat input in the range of 15 W increased performance equivalent to that of PCM coupled heat sink.
- 29 May 2025
- Published by Kaunas University of Technology (KTU) in Materials Science
- Vol. 31 (2) , 155-161
Open AccessThe Effects of Deep Cryogenic Treatment on Heat transfer of Aluminium Heat Sink
Thermal management is critical for achieving peak performance and extending the life of electronic equipment. Heat sinks are the most effective thermal control tools. Copper and aluminium are the most used materials for heat sinks. Aluminium, in particular, attracts a lot of attention due to its lightweight and recyclability, which assures sustainability. Because of its robustness, malleability, and good thermal conductivity, the aluminium 6000 series is ideal for use in heat sink manufacturing. In this research, raw material consisting of Al6060 is turned into a square pin fin heat sink with 25 pin fins using a CNC milling machine. The natural convection heat transfer efficiency of the heat sink was identified with a specially constructed experimental setup. Four different heat inputs (15 W, 25 W, 35 W, and 45 W) were analyzed. The novelty of this work is that the heat sink undergoes deep cryogenic treatment (DCT). The soaking duration in liquid nitrogen is set at 24 hours. The heat transfer efficiency of DCT treated aluminium heat sink is compared with the bare aluminium heat sink. The testing findings revealed that when the heat input was 15W, the DCT treated square pin fin heat sink had a charging cycle that was up to 77.78 % longer than the untreated heat sink. At 25W, 35 W, and 45 W heat input, the charging cycle was 48 %, 39 %, and 28 % longer, respectively. Analyzing the discharge cycle revealed that only the 15 W heat input had an ideal discharge cycle, which was 20 % shorter than the untreated heat sink. The results are compared with the results of heat sink coupled with phase change materials (PCM) from the literature. The analysis revealed that for the DCT treated heat sink, heat input in the range of 15 W increased performance equivalent to that of PCM coupled heat sink.
- Open Access
- 6 May 2023
- Published by MDPI AG in Journal of Composites Science
- Vol. 7 (5) , 187
Investigation of Water Absorption Properties of 2D Interwoven Kevlar–Jute Reinforced Hybrid Laminates
The hygroscopic properties of natural fibers tend to degrade the mechanical properties of composite materials. It is essential to investigate the influence of water absorption behavior on the mechanical properties of hybrid composite materials. In this study, hybrid laminate materials consisting of two different reinforcement materials, i.e., Kevlar fibers and jute fibers in the same layer, are considered. Hybrid laminates that have four different weaving patterns: plain weave, basket weave, twill weave, and the satin weave, are tested for their water absorption characteristics. The jute fiber is a naturally extracted fiber that is subjected to chemical treatment. A comparison of mechanical properties before and after treatment of the jute fibers is carried out. Mechanical properties such as tensile strength, compressive strength, flexural strength, impact strength, and hardness are tested. It is found that the mechanical properties improved after the treatment of the jute fibers. The twill weave pattern exhibited negligible defects compared to its counterparts. Chemical treatment of the jute fibers enabled less water being absorbed into the hybrid laminate materials. Mechanical properties improved after using chemically treated jute fibers as the reinforcement material in the hybrid laminate materials. It is concluded that the twill weave pattern and chemical treatment of the natural fibers improved the mechanical properties of the hybrid laminate materials.
- 6 May 2023
- Published by MDPI AG in Journal of Composites Science
- Vol. 7 (5) , 187
Open AccessInvestigation of Water Absorption Properties of 2D Interwoven Kevlar–Jute Reinforced Hybrid Laminates
The hygroscopic properties of natural fibers tend to degrade the mechanical properties of composite materials. It is essential to investigate the influence of water absorption behavior on the mechanical properties of hybrid composite materials. In this study, hybrid laminate materials consisting of two different reinforcement materials, i.e., Kevlar fibers and jute fibers in the same layer, are considered. Hybrid laminates that have four different weaving patterns: plain weave, basket weave, twill weave, and the satin weave, are tested for their water absorption characteristics. The jute fiber is a naturally extracted fiber that is subjected to chemical treatment. A comparison of mechanical properties before and after treatment of the jute fibers is carried out. Mechanical properties such as tensile strength, compressive strength, flexural strength, impact strength, and hardness are tested. It is found that the mechanical properties improved after the treatment of the jute fibers. The twill weave pattern exhibited negligible defects compared to its counterparts. Chemical treatment of the jute fibers enabled less water being absorbed into the hybrid laminate materials. Mechanical properties improved after using chemically treated jute fibers as the reinforcement material in the hybrid laminate materials. It is concluded that the twill weave pattern and chemical treatment of the natural fibers improved the mechanical properties of the hybrid laminate materials.
- 18 September 2022
- Published by Taylor & Francis in Energy Sources, Part A: Recovery, Utilization, and Environmental Effects
- Vol. 44 (4) , 8679-8693
Evaluation of efficiency of double slope solar still and drinking water yield using silver nanoparticle mixed with phase change material
This study shows the contribution of silver nanoparticles mixed with macro-encapsulated phase change material (PCM) in a double slope solar still. Experiments are carried out in three different depths and settings, first using simple double slope solar still, then by addition of PCM, and finally using PCM mixed with silver nanoparticles. Results obtained are compared during the sunshine period and also after sunset. The study shows that the silver nanoparticles in PCM results in reducing the yield and efficiency of the double slope solar still by 7.64% and 5.26% during the charging period. However, it continues to deliver potable water even after sunset due to the stored latent heat in the PCM. The higher thermal capacity of the PCM and the higher thermal conductivity of the silver nanoparticles resulted in a 16% increase in drinking water yield and a 62.53% rise in the thermal efficiency of the double slope solar still. The final cost per liter of the potable water generated using the double slope solar still was reduced to 3.80 INR and the payback time is 2 years which can be reduced further using PCM and nano-enhanced PCM inside the solar still.
- 18 September 2022
- Published by Taylor & Francis in Energy Sources, Part A: Recovery, Utilization, and Environmental Effects
- Vol. 44 (4) , 8679-8693
Evaluation of efficiency of double slope solar still and drinking water yield using silver nanoparticle mixed with phase change material
This study shows the contribution of silver nanoparticles mixed with macro-encapsulated phase change material (PCM) in a double slope solar still. Experiments are carried out in three different depths and settings, first using simple double slope solar still, then by addition of PCM, and finally using PCM mixed with silver nanoparticles. Results obtained are compared during the sunshine period and also after sunset. The study shows that the silver nanoparticles in PCM results in reducing the yield and efficiency of the double slope solar still by 7.64% and 5.26% during the charging period. However, it continues to deliver potable water even after sunset due to the stored latent heat in the PCM. The higher thermal capacity of the PCM and the higher thermal conductivity of the silver nanoparticles resulted in a 16% increase in drinking water yield and a 62.53% rise in the thermal efficiency of the double slope solar still. The final cost per liter of the potable water generated using the double slope solar still was reduced to 3.80 INR and the payback time is 2 years which can be reduced further using PCM and nano-enhanced PCM inside the solar still.
- 11 June 2022
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 19 (16) , 13076-13087
Effect of Weaving Pattern on the Mechanical Properties of 2D Interwoven Kevlar-Jute Hybrid Laminates
Hybrid laminates were produced using epoxy resin and interwoven fibers of kevlar and jute. In this study, different weaving patterns, i.e.,, plain weave, basket weave, twill weave, and satin weave were considered. Mechanical properties like hardness, tensile strength, flexural strength, compressive strength, and impact strength were experimentally measured. The hybrid laminate having the plain weave and basket weave patterns were observed to have equally spaced pockets of matrix element, which facilitated the isotropic distribution of applied load during the testing of the mechanical properties. The twill weave pattern in the reinforcement exhibited augmented mechanical properties as well as superior elasticity. Its elongation percentage was 32%, while the satin weave pattern exhibited only 21.5%. The satin weave pattern revealed microcracks within the matrix, whereas the twill weave pattern exhibited superior bonding between the matrix and the reinforcement fibers. The twill weave pattern showed anisotropic load transfer during the mechanical test. Thus, the applied load was distributed along the warp direction that contained kevlar fibers. Hence, it exhibited the tensile strength of 6.77 GPa, the flexural strength of 3.4 GPa, the compressive strength of 105.6 MPa, an absorbed maximum impact load of 89 J, and shore-D hardness of 72.2, respectively.
- 11 June 2022
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 19 (16) , 13076-13087
Effect of Weaving Pattern on the Mechanical Properties of 2D Interwoven Kevlar-Jute Hybrid Laminates
Hybrid laminates were produced using epoxy resin and interwoven fibers of kevlar and jute. In this study, different weaving patterns, i.e.,, plain weave, basket weave, twill weave, and satin weave were considered. Mechanical properties like hardness, tensile strength, flexural strength, compressive strength, and impact strength were experimentally measured. The hybrid laminate having the plain weave and basket weave patterns were observed to have equally spaced pockets of matrix element, which facilitated the isotropic distribution of applied load during the testing of the mechanical properties. The twill weave pattern in the reinforcement exhibited augmented mechanical properties as well as superior elasticity. Its elongation percentage was 32%, while the satin weave pattern exhibited only 21.5%. The satin weave pattern revealed microcracks within the matrix, whereas the twill weave pattern exhibited superior bonding between the matrix and the reinforcement fibers. The twill weave pattern showed anisotropic load transfer during the mechanical test. Thus, the applied load was distributed along the warp direction that contained kevlar fibers. Hence, it exhibited the tensile strength of 6.77 GPa, the flexural strength of 3.4 GPa, the compressive strength of 105.6 MPa, an absorbed maximum impact load of 89 J, and shore-D hardness of 72.2, respectively.
- Open Access
- 29 October 2021
- Published by EDP Sciences in International Journal for Simulation and Multidisciplinary Design Optimization
- Vol. 12, 28
Optimization of friction STIR welded AA6061 + SiCp metal matrix composite to increase joint tensile strength and reduce defects
Friction stir welding has been used in automobiles, locomotive, and aircraft structures. This metal joining process exhibits defects like kissing bonds, micropores, and tunnels. Factors like the joining material, joint thickness, tool geometry, and operating parameters control the defects in friction stir welding. The parameters like tool rotation, tool pass speed, and tool force have a greater influence on the joint quality. In this study, these parameters are considered to augment the strength of the joint and minimize defects. The metal matrix composite consisting of AA6061 matrix and 10 wt. % SiCp reinforcement is joined used FSW. The weld parameters were varied between 731 and 1068 rpm tool rotation speed, 0.33 and 1.17 mm/s tool pass speed, and 11 and 28 MPa tool force. The joint strength varied from 165 MPa to 244 MPa. The numerical analysis using ANOVA revealed that compared between the three parameters, the tool force had greater control over the tensile strength of the joint. After optimization, the joint was made at a tool rotation speed of 910 rpm, tool pass speed of 0.77 mm/s, and tool force of 22.33 MPa. The tensile strength increased to 249 MPa after using the optimized weld parameters. The number of defects in the joint was reduced after using the optimized weld parameters.
- 29 October 2021
- Published by EDP Sciences in International Journal for Simulation and Multidisciplinary Design Optimization
- Vol. 12, 28
Open AccessOptimization of friction STIR welded AA6061 + SiCp metal matrix composite to increase joint tensile strength and reduce defects
Friction stir welding has been used in automobiles, locomotive, and aircraft structures. This metal joining process exhibits defects like kissing bonds, micropores, and tunnels. Factors like the joining material, joint thickness, tool geometry, and operating parameters control the defects in friction stir welding. The parameters like tool rotation, tool pass speed, and tool force have a greater influence on the joint quality. In this study, these parameters are considered to augment the strength of the joint and minimize defects. The metal matrix composite consisting of AA6061 matrix and 10 wt. % SiCp reinforcement is joined used FSW. The weld parameters were varied between 731 and 1068 rpm tool rotation speed, 0.33 and 1.17 mm/s tool pass speed, and 11 and 28 MPa tool force. The joint strength varied from 165 MPa to 244 MPa. The numerical analysis using ANOVA revealed that compared between the three parameters, the tool force had greater control over the tensile strength of the joint. After optimization, the joint was made at a tool rotation speed of 910 rpm, tool pass speed of 0.77 mm/s, and tool force of 22.33 MPa. The tensile strength increased to 249 MPa after using the optimized weld parameters. The number of defects in the joint was reduced after using the optimized weld parameters.
- 15 July 2021
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 19 (13) , 7229-7240
Effect of stacking sequence on mechanical and moisture absorption properties of abaca-kenaf-carbon fiber reinforced hybrid composites
Hybrid composite materials containing natural fibers are replacing conventional materials for automobile, aerospace and sports goods structural applications. Fiber extracted from plants and man-made fibers reinforced with polymer matrix find many applications because of improved characteristics, such as light weight and high strength. In this work, fabricated hybrid composites using chemically treated abaca, kenaf and carbon fiber reinforced with epoxy and teta hardener are studied. Hybrid composites have four stacking sequences and five layer composites made up of hand laid up then compression molding. Produced hybrid composites are subjected to various loads to determine the mechanical strength. Moisture absorption measured in the distilled water was used as the medium during water absorption test. Experimental results showed that the treated fiber hybrid composite provided higher mechanical strength and absorbed less moisture. The morphology of fractured surfaces was analyzed by electron microscopy.
- 15 July 2021
- Published by Taylor & Francis in Journal of Natural Fibers
- Vol. 19 (13) , 7229-7240
Effect of stacking sequence on mechanical and moisture absorption properties of abaca-kenaf-carbon fiber reinforced hybrid composites
Hybrid composite materials containing natural fibers are replacing conventional materials for automobile, aerospace and sports goods structural applications. Fiber extracted from plants and man-made fibers reinforced with polymer matrix find many applications because of improved characteristics, such as light weight and high strength. In this work, fabricated hybrid composites using chemically treated abaca, kenaf and carbon fiber reinforced with epoxy and teta hardener are studied. Hybrid composites have four stacking sequences and five layer composites made up of hand laid up then compression molding. Produced hybrid composites are subjected to various loads to determine the mechanical strength. Moisture absorption measured in the distilled water was used as the medium during water absorption test. Experimental results showed that the treated fiber hybrid composite provided higher mechanical strength and absorbed less moisture. The morphology of fractured surfaces was analyzed by electron microscopy.
- 1 January 2021
- Published by Elsevier in Materials Today: Proceedings
- Vol. 46, 3712-3715
Investigation of tensile strength, hardness and wear of titanium diboride reinforced AA6061 composite
- 1 January 2021
- Published by Elsevier in Materials Today: Proceedings
- Vol. 46, 3712-3715
Investigation of tensile strength, hardness and wear of titanium diboride reinforced AA6061 composite
- Open Access
- 1 December 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 988 (1) , 012103
Estimation of Tensile and Compression Properties of 2D Woven Jute and Kevlar Hybrid Laminate
In this study, the mechanical properties of a 2D woven novel hybrid laminate containing jute in the warp direction and Kevlar in the weft direction as reinforcement material is compared with four different weaving patterns. The hybrid laminates were tested for its tensile strength, elongation percentage and compressive strength. The results show that under the condition of identical composition of the matrix element, similarity in the thickness of the laminates and same stacking sequences, the weaving patterns exhibit profound influence on the tensile and compressive properties. The plain weaving pattern exhibited lowest tensile strength and compressive strength while the highest values for the two properties was observed from the hybrid laminate having twill weave pattern.
- 1 December 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 988 (1) , 012103
Open AccessEstimation of Tensile and Compression Properties of 2D Woven Jute and Kevlar Hybrid Laminate
In this study, the mechanical properties of a 2D woven novel hybrid laminate containing jute in the warp direction and Kevlar in the weft direction as reinforcement material is compared with four different weaving patterns. The hybrid laminates were tested for its tensile strength, elongation percentage and compressive strength. The results show that under the condition of identical composition of the matrix element, similarity in the thickness of the laminates and same stacking sequences, the weaving patterns exhibit profound influence on the tensile and compressive properties. The plain weaving pattern exhibited lowest tensile strength and compressive strength while the highest values for the two properties was observed from the hybrid laminate having twill weave pattern.
- Open Access
- 17 January 2020
- Published by FapUNIFESP (SciELO) in Journal of Aerospace Technology and Management
- Vol. 12 (12)
Novel Characteristics of Subsonic Coflowing Jets With Varying Lip Thickness
Effect of Mach number on coflowing jet at lip thickness of 0.2 Dp, 1.0 Dp and 1.5 Dp (where Dp is primary nozzle exit diameter, 10 mm) at Mach numbers 1.0, 0.8 and 0.6 were studied experimentally. It was found that an increase in Mach number does not have any profound effect on axial total and static pressure variation for 0.2 Dp. Decreasing the mean diameter is due to the geometrical constraints. In this study, the primary nozzle dimension and secondary duct is maintained constant for comparison. For the case of 0.2 Dp, static pressure is almost equal to atmospheric pressure for all Mach numbers. Whereas for other two lip thickness, increase in Mach number marginally influences axial total pressure and profoundly varies static pressure. It is noted that it varies considerably up to 11.1% in the axial direction and up to 17% in the radial direction for Mach number 1.0. For lower Mach numbers, such variation is not observed. Increase in Mach number increases static pressure variation in the coflowing jet flow field with lip thickness 1.0 Dp and 1.5 Dp.
- 17 January 2020
- Published by FapUNIFESP (SciELO) in Journal of Aerospace Technology and Management
- Vol. 12 (12)
Open AccessNovel Characteristics of Subsonic Coflowing Jets With Varying Lip Thickness
Effect of Mach number on coflowing jet at lip thickness of 0.2 Dp, 1.0 Dp and 1.5 Dp (where Dp is primary nozzle exit diameter, 10 mm) at Mach numbers 1.0, 0.8 and 0.6 were studied experimentally. It was found that an increase in Mach number does not have any profound effect on axial total and static pressure variation for 0.2 Dp. Decreasing the mean diameter is due to the geometrical constraints. In this study, the primary nozzle dimension and secondary duct is maintained constant for comparison. For the case of 0.2 Dp, static pressure is almost equal to atmospheric pressure for all Mach numbers. Whereas for other two lip thickness, increase in Mach number marginally influences axial total pressure and profoundly varies static pressure. It is noted that it varies considerably up to 11.1% in the axial direction and up to 17% in the radial direction for Mach number 1.0. For lower Mach numbers, such variation is not observed. Increase in Mach number increases static pressure variation in the coflowing jet flow field with lip thickness 1.0 Dp and 1.5 Dp.
- 8 June 2015
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 766-767, 276-280
The Comparative Analysis of Mechanical Properties on MMC (AA6061 + SiCp 10% wt) before and after Age Hardening
Discontinuously reinforced SiCp/Al composites were extensively used in space applications including joints and attachment fittings for truss structures, electronic packages, thermal planes, mechanism housing and bushing. In this research work, the metal matrix composite of AA6061+ SiCp 10% were produced by stir casting method with an aim to predict the mechanical properties of a Metal Matrix Composite (MMC) subjected to age hardening. The Ultimate tensile test and Vickers hardness test was carried on the both condition of produced MMC and Age hardened (HMMC). A comparative study of the mechanical properties of the MMC before and after age hardening has been reported.
- 8 June 2015
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 766-767, 276-280
The Comparative Analysis of Mechanical Properties on MMC (AA6061 + SiCp 10% wt) before and after Age Hardening
Discontinuously reinforced SiCp/Al composites were extensively used in space applications including joints and attachment fittings for truss structures, electronic packages, thermal planes, mechanism housing and bushing. In this research work, the metal matrix composite of AA6061+ SiCp 10% were produced by stir casting method with an aim to predict the mechanical properties of a Metal Matrix Composite (MMC) subjected to age hardening. The Ultimate tensile test and Vickers hardness test was carried on the both condition of produced MMC and Age hardened (HMMC). A comparative study of the mechanical properties of the MMC before and after age hardening has been reported.