Devendra Kumar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Devendra Kumar has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- C. J. Dileep Kumar
TRL Krosaki Refractories Limited Belpahar India
1 shared publication - In-Ho Jung
Department of Materials Science and Engineering Seoul National University Seoul South Korea
1 shared publication Komal Syed
Department of Materials Science and Engineering University of California Irvine CA USA
1 shared publicationMarie‐Aline Van Ende
Department of Materials Science and Engineering Research Institute of Advanced Materials Seoul National University Seoul South Korea
1 shared publication- Sarah Finkeldei
Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
1 shared publication - Somnath Mandal
Materials Science and Engineering University of Alabama at Birmingham Birmingham Alabama USA
1 shared publication
Latest Publications
- 7 August 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (12) , 7095-7114
Designing environment‐friendly chromium‐free Spinel‐Periclase‐Zirconia refractories for Ruhrstahl Heraeus degasser
Ruhrstahl Heraeus (RH) degassers are globally used to manufacture vacuum‐treated steel for automotive and railroad applications. The state‐of‐the‐art environment‐friendly chromium‐free alternatives for direct‐bonded magnesia‐chrome refractories used in RH degassers are expensive, and the scientific literature lacks direct correlation between materials chemistry, processing, and functional properties. We have designed a novel spinel‐periclase‐15 wt% ZrO 2 composition containing 14 wt% in situ spinel which exhibited 7.2 MPa hot modulus of rupture (1500℃), exceeding all reported Cr‐free refractories for RH degasser applications. Investigation with scanning electron microscopy coupled with energy dispersive spectroscopy (SEM‐EDS) attributed this improvement to a reduction in interparticle Ca and Si content which forms low‐melting phases, as supported by FactSage thermodynamic simulations. The spinel‐periclase composition SP exhibited superior thermal shock resistance because thermal shock‐induced cracks were stopped by fracture porosity around MgO particles, formed due to thermal expansion mismatch. SEM‐EDS analysis of the SP composition corroded by RH slag at 1650°C revealed that Fe is the most corrosive element followed by Ca and Si. Contradicting the consensus, it was observed that corrosion resistance of fused MgO was better than that of ZrO 2 . The cubic ZrO 2 phase reduced FeO x penetration locally by incorporating CaO from the RH slag into a solid solution and forming a CaZrO 3 phase creating a “slag barrier”. Lastly, pore size was found to greatly exacerbate slag penetration following the Washburn percolation model.
- 7 August 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (12) , 7095-7114
Designing environment‐friendly chromium‐free Spinel‐Periclase‐Zirconia refractories for Ruhrstahl Heraeus degasser
Ruhrstahl Heraeus (RH) degassers are globally used to manufacture vacuum‐treated steel for automotive and railroad applications. The state‐of‐the‐art environment‐friendly chromium‐free alternatives for direct‐bonded magnesia‐chrome refractories used in RH degassers are expensive, and the scientific literature lacks direct correlation between materials chemistry, processing, and functional properties. We have designed a novel spinel‐periclase‐15 wt% ZrO 2 composition containing 14 wt% in situ spinel which exhibited 7.2 MPa hot modulus of rupture (1500℃), exceeding all reported Cr‐free refractories for RH degasser applications. Investigation with scanning electron microscopy coupled with energy dispersive spectroscopy (SEM‐EDS) attributed this improvement to a reduction in interparticle Ca and Si content which forms low‐melting phases, as supported by FactSage thermodynamic simulations. The spinel‐periclase composition SP exhibited superior thermal shock resistance because thermal shock‐induced cracks were stopped by fracture porosity around MgO particles, formed due to thermal expansion mismatch. SEM‐EDS analysis of the SP composition corroded by RH slag at 1650°C revealed that Fe is the most corrosive element followed by Ca and Si. Contradicting the consensus, it was observed that corrosion resistance of fused MgO was better than that of ZrO 2 . The cubic ZrO 2 phase reduced FeO x penetration locally by incorporating CaO from the RH slag into a solid solution and forming a CaZrO 3 phase creating a “slag barrier”. Lastly, pore size was found to greatly exacerbate slag penetration following the Washburn percolation model.