I. C. Lavos-Valereto has a total of 12 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Electrochemical impedance spectroscopy characterization of passive film formed on implant Ti–6Al–7Nb alloy in Hank's solution

    by I. C. Lavos-Valereto, S. Wolynec, I. Ramires, A. C. Guastaldi, I. Costa

    The influence of potential on electrochemical behavior of Ti–6Al–7Nb alloy under simulated physiological conditions was investigated by electrochemical impedance spectroscopy (EIS). The experimental results were compared with those obtained by potentiodynamic polarization curves. All measurements were carried out in Hank's aerated solution at 25 °C, at pH 7.8 and at different potentials (corrosion potential, 0 mV(SCE), 1000 mV(SCE), and 2000 mV(SCE)). The EIS spectra exhibited a two-step or a two-time constant system, suggesting the formation of a two-layer oxide film on the metal surface. The high corrosion resistance, displayed by this alloy in electrochemical polarization tests, is due to the dense inner layer, while its osseointegration ability can be ascribed to the presence of the outer porous layer.


  • Evaluation of the Titanium Ti‐6Al‐7Nb Alloy With and Without Plasma‐Sprayed Hydroxyapatite Coating on Growth and Viability of Cultured Osteoblast‐Like Cells

    by Ivone de C. Lavos‐Valereto, Maria Cristina Z. Deboni, Nilton Azambuja, Márcia M. Marques

    Background: Osseointegrated dental implants are currently recognized as a standard treatment method in dentistry. Titanium (Ti) and its alloys are the metals of choice for endosseous parts of currently available dental implants. Ti‐6Al‐4V is the most used Ti alloy, however; an improved version, Ti‐6Al‐7Nb, has been recently developed.Methods: Rat osteoblast‐like cells (osteo‐1 culture) were used to analyze the biocompatibility of Ti‐6Al‐7Nb alloy with and without hydroxyapatite (HA) coating. The cells were grown on culture Petri dishes on the top of either plain Ti‐6Al‐7Nb or HAcoated Ti‐6Al‐7Nb disks. Osteo‐1 cells grown on plain culture dishes were used as controls. Growth and cell viability curves were obtained by scanning electron microscopy. For the growth and viability curves, 104 cells were seeded on 35 mm dishes. Cells from each group were counted, in triplicate at 3, 7, 11, and 15 days after seeding using the Trypan blue dye exclusion assay.Results: The cells grew as multiple layers on both Ti‐6Al‐7Nb substrates, showing extracellular matrix only when grown on HA‐coated Ti‐6Al‐7Nb disks. The cells grown on HA‐coated Ti‐6Al‐7Nb grew more slowly than the other 2 groups, with significantly smaller cell numbers than control cultures at the end of the experimental time. Additionally, the HA coated Ti‐6Al‐7Nb group presented smaller percentage of cell viability when compared to the control group. However, no significant differences were observed between the Ti groups.Conclusions: The presence of HA on the Ti‐6Al‐7Nb surface impaired the cell growth and viability of osteo‐1 cells. However, this coating improved the extracellular matrix formation. Thus, our cell viability and structural studies showed that Ti‐6Al‐7Nb with or without HA coating has relevant physical and biological properties as an implant material. J Periodontol 2002;73:900‐905.


  • The electrochemical behavior of Ti‐6Al‐7Nb alloy with and without plasma‐sprayed hydroxyapatite coating in Hank's solution

    by I. C. Lavos‐Valereto, I. Costa, S. Wolynec

    The electrochemical behavior of Ti‐6Al‐7Nb alloy with and without plasma‐sprayed hydroxyapatite (HA) coating was investigated in Hank's balanced salt solution at 37 °C. This behavior was evaluated by analyzing both corrosion potential variation with time curves and potentiodynamic polarization curves. The polarization curves were determined both in aerated and deaerated solutions. It was found that the corrosion potential of uncoated sample is always more noble than that of coated one. In aerated solutions the polarization curve of a coating‐free alloy presents a typical passive/transpassive behavior, which is absent in the HA‐coated alloy and in deaerated solution for both coated and uncoated conditions. In the latter polarization curves, the current density continuously increases with the increase of the potential. The corrosion rate determined from polarization curves is higher for HA‐coated alloys, but it still can be considered negligible (less than 1 μA/cm2). © 2002 Wiley Periodicals, Inc. J Biomed Mater Res (Appl Biomater) 63: 664–670, 2002


  • A study of histological responses from Ti-6Al-7Nb alloy dental implants with and without plasma-sprayed hydroxyapatite coating in dogs

    by I. C. Lavos-Valereto, B. Ko¨nIg, C. Rossa, E. Marcantonio, A. C. Zavaglia

    Titanium alloys are hoped to be used much more for applications as implant materials in the medical and dental fields because of their basic properties, such as biocompatibility, corrosion resistance...


  • In vitro and in vivo biocompatibility testing of Ti‐6Al‐7Nb alloy with and without plasma‐sprayed hydroxyapatite coating

    by I. C. Lavos‐Valereto, S. Wolynec, M. C. Z. Deboni, B. König

    The Ti‐6Al‐7Nb alloy has been recently developed for biomedical use, particularly for orthopedics and dental applications. Osteosynthesis has been used to analyze biocompatibility and osseoconduction properties. The interaction of the implant with its biological environment, the formation of the implant material/tissue interface, and the long‐term success or failure of integration in the human body is strongly connected with the surface properties of the implant device. This study was undertaken to evaluate the processes involved in biological responses of the Ti‐6Al‐7Nb alloy with and without hydroxyapatite coatings with both in vitro and in vivo tests. The results were analyzed by scanning electron microscopy (SEM) and energy‐dispersive x‐ray (EDX) microanalysis. The morphology of the in vitro and in vivo testing results with hydroxyapatite coating was similar to those obtained on the uncoated samples. A mineralized extracellular matrix was formed on all materials. Observation of the interface between the cell layer and substrata showed the presence of calcium and phosphorous‐rich globular deposits associated with collagen fibers on all materials in vitro and in vivo. A higher density of these globular deposits was observed in all samples. © 2001 John Wiley & Sons, Inc. J Biomed Mater Res (Appl Biomater) 58: 727–733, 2001