P. Ravi Teja
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
P. Ravi Teja has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Raja Annamalai Arunjunai Rajan
Centre for Innovative Manufacturing Research, Vellore Institute of Technology, Vellore 632014, Tamil Nadu, India
2 shared publications A. Muthuchamy
1 shared publication- Chun-Ping Jen
Department of Mechanical Engineering and Advanced Institute of Manufacturing for High-Tech Innovations, National Chung Cheng University, Chiayi 62102, Taiwan
1 shared publication Dinesh K. Agrawal
1 shared publication- Dinesh K. Agrawal
Materials Research Institute, The Pennsylvania State University, University Park, PA 16802, USA
1 shared publication - Gecil Evangeline T.
School of Mechanical Engineering, Vellore Institute of Technology, Vellore 632014, India
1 shared publication
Latest Publications
- Open Access
Effect of Heating Modes on Reactive Sintering of Ca3Co4O9 Ceramics
The traditional solid-state reaction method was employed to synthesize bulk calcium cobaltite (Ca349/Ca3Co4O9) ceramics via ball milling the precursor mixture. The samples were compacted using conventional sintering (CS) and spark plasma sintering (SPS) at 850, 900, and 950 °C. The X-ray diffraction (XRD) pattern indicates the presence of the Ca349 phase for samples sintered at 850 and 900 °C. In addition, SPS fosters higher densification (81.18%) than conventional sintering (50.76%) at elevated sintering temperatures. The thermo-gravimetric analysis (TGA) and differential thermal analysis (DTA) performed on the precursor mixture reported a weight loss of ~25.23% at a temperature range of 600–820 °C. This current work aims to analyze the electrical properties (Seebeck coefficient (s), electrical resistivity (ρ), and power factor) of sintered samples as a function of temperature (35–500 °C). It demonstrates that the change in sintering temperature (conventional sintering) did not evince any significant change in the Seebeck coefficient (113–142 μV/K). However, it reported a low resistivity of 153–132 μΩ-m and a better power factor (82–146.4 μW/mK2) at 900 °C. On the contrary, the SPS sintered samples recorded a higher Seebeck coefficient of 121–181 μV/K at 900 °C. Correspondingly, the samples sintered at 950 °C delineated a low resistivity of 145–158 μΩ-m and a better power factor (97–152 μW/mK2).
Open AccessEffect of Heating Modes on Reactive Sintering of Ca3Co4O9 Ceramics
The traditional solid-state reaction method was employed to synthesize bulk calcium cobaltite (Ca349/Ca3Co4O9) ceramics via ball milling the precursor mixture. The samples were compacted using conventional sintering (CS) and spark plasma sintering (SPS) at 850, 900, and 950 °C. The X-ray diffraction (XRD) pattern indicates the presence of the Ca349 phase for samples sintered at 850 and 900 °C. In addition, SPS fosters higher densification (81.18%) than conventional sintering (50.76%) at elevated sintering temperatures. The thermo-gravimetric analysis (TGA) and differential thermal analysis (DTA) performed on the precursor mixture reported a weight loss of ~25.23% at a temperature range of 600–820 °C. This current work aims to analyze the electrical properties (Seebeck coefficient (s), electrical resistivity (ρ), and power factor) of sintered samples as a function of temperature (35–500 °C). It demonstrates that the change in sintering temperature (conventional sintering) did not evince any significant change in the Seebeck coefficient (113–142 μV/K). However, it reported a low resistivity of 153–132 μΩ-m and a better power factor (82–146.4 μW/mK2) at 900 °C. On the contrary, the SPS sintered samples recorded a higher Seebeck coefficient of 121–181 μV/K at 900 °C. Correspondingly, the samples sintered at 950 °C delineated a low resistivity of 145–158 μΩ-m and a better power factor (97–152 μW/mK2).
- 1 August 2020
- Published by Elsevier in Ceramics International
- Vol. 46 (11) , 17951-17956
Microwave heating synthesis and thermoelectric property characterization of highly dense Ca3Co4O9 bulk
- 1 August 2020
- Published by Elsevier in Ceramics International
- Vol. 46 (11) , 17951-17956
Microwave heating synthesis and thermoelectric property characterization of highly dense Ca3Co4O9 bulk