Sanjay Tikale
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Sanjay Tikale has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Kotekar Narayan Prabhu
Department of Metallurgical and Materials Engineering, National Institute of Technology Karnataka, Surathkal, Mangalore, India
7 shared publications - Mrunali Sona
National Institute of Technology Karnataka
2 shared publications Augustine Samuel
National Institute of Technology Karnataka
1 shared publicationK. Narayan Prabhu
Department of Metallurgical & Materials Engineering, National Institute of Technology 2 Karnataka, Surathkal, 575 025, IN
1 shared publicationK.N. Prabhu
National Institute of Technology Karnataka
1 shared publicationMrunali Sona
National Institute of Technology Karnataka
1 shared publication
Latest Publications
- 6 January 2021
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 32 (3) , 2865-2886
Bond shear strength of Al2O3 nanoparticles reinforced 2220-capacitor/SAC305 solder interconnects reflowed on bare and Ni-coated copper substrate
- 6 January 2021
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 32 (3) , 2865-2886
Bond shear strength of Al2O3 nanoparticles reinforced 2220-capacitor/SAC305 solder interconnects reflowed on bare and Ni-coated copper substrate
- 1 March 2019
- Published by ASTM International in Materials Performance and Characterization
- Vol. 8 (3) , 421-433
The Effect of Multi-Walled Carbon Nanotubes Reinforcement and Multiple Reflow Cycles on Shear Strength of SAC305 Lead-Free Solder Alloy
In this study, the effect of multi-walled carbon nanotubes (MWCNT) reinforcement on joint shear strength and microstructural development of tin-3.0silver-0.5copper (SAC305)/copper solder joint subjected to multiple reflow cycles was investigated. The MWCNT-reinforced SAC305 solder systems (SAC305-x MWCNT; x = 0.01, 0.05, 0.1, and 0.5 wt.%) were developed by a mechanical dispersion method. The microstructural, mechanical, and melting properties of SAC305 composite solders were evaluated as a function of different wt.% of MWCNT addition. The melting behavior of composite solders was analyzed using differential scanning calorimetry. The morphology and intermetallic compound growth at the solder joint interface were studied using scanning electron microscopy. The copper/solder/copper micro-lap-shear solder joint specimens reflowed for multiple reflow cycles were systematically characterized to evaluate the joint shear strength. The results showed that the reinforcement in the range of 0.01–0.05 wt.% of MWCNT resulted in the improvement of joint shear strength and better wettability compared to plain SAC305 solder alloy. Amongst all compositions analyzed, SAC305-0.05MWCNT nanocomposite suppressed the intermetallic compound layer growth effectively leading to improvement in the joint shear strength under multiple reflow cycles.
- 1 March 2019
- Published by ASTM International in Materials Performance and Characterization
- Vol. 8 (3) , 421-433
The Effect of Multi-Walled Carbon Nanotubes Reinforcement and Multiple Reflow Cycles on Shear Strength of SAC305 Lead-Free Solder Alloy
In this study, the effect of multi-walled carbon nanotubes (MWCNT) reinforcement on joint shear strength and microstructural development of tin-3.0silver-0.5copper (SAC305)/copper solder joint subjected to multiple reflow cycles was investigated. The MWCNT-reinforced SAC305 solder systems (SAC305-x MWCNT; x = 0.01, 0.05, 0.1, and 0.5 wt.%) were developed by a mechanical dispersion method. The microstructural, mechanical, and melting properties of SAC305 composite solders were evaluated as a function of different wt.% of MWCNT addition. The melting behavior of composite solders was analyzed using differential scanning calorimetry. The morphology and intermetallic compound growth at the solder joint interface were studied using scanning electron microscopy. The copper/solder/copper micro-lap-shear solder joint specimens reflowed for multiple reflow cycles were systematically characterized to evaluate the joint shear strength. The results showed that the reinforcement in the range of 0.01–0.05 wt.% of MWCNT resulted in the improvement of joint shear strength and better wettability compared to plain SAC305 solder alloy. Amongst all compositions analyzed, SAC305-0.05MWCNT nanocomposite suppressed the intermetallic compound layer growth effectively leading to improvement in the joint shear strength under multiple reflow cycles.
- 29 January 2019
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 72 (6) , 1579-1583
Wettability, Interfacial Intermetallic Growth and Joint Shear Strength of Eutectic Sn–Cu Solder Reflowed on Bare and Nickel-Coated Copper Substrates
- 29 January 2019
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 72 (6) , 1579-1583
Wettability, Interfacial Intermetallic Growth and Joint Shear Strength of Eutectic Sn–Cu Solder Reflowed on Bare and Nickel-Coated Copper Substrates
- 3 October 2018
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (11) , 2687-2691
Assessment of the Performance of Sn–3.5Ag/Cu Solder Joint Under Multiple Reflows, Thermal Cycling and Corrosive Environment
- 3 October 2018
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (11) , 2687-2691
Assessment of the Performance of Sn–3.5Ag/Cu Solder Joint Under Multiple Reflows, Thermal Cycling and Corrosive Environment
- 3 October 2018
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (11) , 2693-2698
Performance of MWCNT-Reinforced SAC0307/Cu Solder Joint Under Multiple Reflow Cycles
- 3 October 2018
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (11) , 2693-2698
Performance of MWCNT-Reinforced SAC0307/Cu Solder Joint Under Multiple Reflow Cycles
- 19 September 2018
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (11) , 2855-2859
Effect of Multiple Reflow Cycles on the Shear Strength of Nano-Al2O3 Particles Reinforced Sn3.6Ag Lead-Free Solder Alloy
- 19 September 2018
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 71 (11) , 2855-2859
Effect of Multiple Reflow Cycles on the Shear Strength of Nano-Al2O3 Particles Reinforced Sn3.6Ag Lead-Free Solder Alloy
- 4 May 2018
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 27 (6) , 3102-3111
Effect of Multiple Reflow Cycles and Al2O3 Nanoparticles Reinforcement on Performance of SAC305 Lead-Free Solder Alloy
- 4 May 2018
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 27 (6) , 3102-3111
Effect of Multiple Reflow Cycles and Al2O3 Nanoparticles Reinforcement on Performance of SAC305 Lead-Free Solder Alloy
- 21 February 2017
- Published by ASTM International in Materials Performance and Characterization
- Vol. 6 (1) , 46-54
Effect of Cooling Rate on Joint Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Reliability of the solder joint largely depends on mechanical strength, fatigue resistance, coefficient of thermal expansion, and intermetallic compound formation. Cooling rate significantly affects the physical properties of an alloy and influences the mechanical behavior of solder joints. In the present study, Sn-9Zn lead-free solder alloy was solidified on Cu substrate under furnace cooling (0.04°C/s), air cooling (0.16°C/s), and water cooling (94°C/s) conditions. The effect of varying cooling rates on the intermetallic compound (IMC) formation at the interface and the resulting joint shear strength was studied. A microstructure study revealed the presence of Cu5Zn8 and CuZn5 intermetallic compounds at the solder-substrate interface. The IMC layer thickness at the interface increased with a decrease in the cooling rate. The joint shear strength increased with an increase in the cooling rate. The air and furnace cooling resulted in the formation of a thick IMC layer. The IMC obtained from the furnace cooling was associated with micro-cracks leading to a decrease in the joint shear strength.
- 21 February 2017
- Published by ASTM International in Materials Performance and Characterization
- Vol. 6 (1) , 46-54
Effect of Cooling Rate on Joint Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Reliability of the solder joint largely depends on mechanical strength, fatigue resistance, coefficient of thermal expansion, and intermetallic compound formation. Cooling rate significantly affects the physical properties of an alloy and influences the mechanical behavior of solder joints. In the present study, Sn-9Zn lead-free solder alloy was solidified on Cu substrate under furnace cooling (0.04°C/s), air cooling (0.16°C/s), and water cooling (94°C/s) conditions. The effect of varying cooling rates on the intermetallic compound (IMC) formation at the interface and the resulting joint shear strength was studied. A microstructure study revealed the presence of Cu5Zn8 and CuZn5 intermetallic compounds at the solder-substrate interface. The IMC layer thickness at the interface increased with a decrease in the cooling rate. The joint shear strength increased with an increase in the cooling rate. The air and furnace cooling resulted in the formation of a thick IMC layer. The IMC obtained from the furnace cooling was associated with micro-cracks leading to a decrease in the joint shear strength.
- 3 September 2015
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 830-831, 215-218
Wettability and Bond Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Lead-free solders are environment friendly and are in great demand for microelectronic applications. In the present study, Sn-9Zn lead free solder alloy was solidified on Cu substrate for different reflow times from 10 to 1000s. The influence of reflow time on wetting, formation of intermetallic compounds (IMCs) and bond shear strength was studied using dynamic contact angle analyzer, bond tester and scanning electron microscopy. The results indicate that, the wettability of the solder alloy increased with increase in reflow time. Microstructure study revealed the presence of Cu5Zn8 and CuZn5 IMCs at the interface. The thickness of an IMC increased with increase in the reflow time. The mean thickness of about 11μm for Cu5Zn8 IMC layer was observed for the reflow time of 1000s. The thickness of CuZn5 layer increased up to a reflow time of 100s and decreases thereafter. The bond shear strength increased up to 100s and decreased with increase in reflow time. The decrement in shear strength at higher reflow time is mainly due to excessive thickness of Cu5Zn8 IMC layer and diffusion of Sn from bulk solder towards the substrate. The excessive thick IMC layer exhibited pre micro-cracks led to the brittle failure of bond under the influence of shear stress.
- 3 September 2015
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 830-831, 215-218
Wettability and Bond Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Lead-free solders are environment friendly and are in great demand for microelectronic applications. In the present study, Sn-9Zn lead free solder alloy was solidified on Cu substrate for different reflow times from 10 to 1000s. The influence of reflow time on wetting, formation of intermetallic compounds (IMCs) and bond shear strength was studied using dynamic contact angle analyzer, bond tester and scanning electron microscopy. The results indicate that, the wettability of the solder alloy increased with increase in reflow time. Microstructure study revealed the presence of Cu5Zn8 and CuZn5 IMCs at the interface. The thickness of an IMC increased with increase in the reflow time. The mean thickness of about 11μm for Cu5Zn8 IMC layer was observed for the reflow time of 1000s. The thickness of CuZn5 layer increased up to a reflow time of 100s and decreases thereafter. The bond shear strength increased up to 100s and decreased with increase in reflow time. The decrement in shear strength at higher reflow time is mainly due to excessive thickness of Cu5Zn8 IMC layer and diffusion of Sn from bulk solder towards the substrate. The excessive thick IMC layer exhibited pre micro-cracks led to the brittle failure of bond under the influence of shear stress.