Mrunali Sona
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Mrunali Sona has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Kotekar Narayan Prabhu
Department of Metallurgical and Materials Engineering, National Institute of Technology Karnataka, Surathkal, Mangalore, India
7 shared publications K. Narayan Prabhu
C Department of Metallurgical & Materials Engineering , National Institute of Technology Karnataka , Surathkal , India
2 shared publications- Nidambur Vasudev Ballal
Department of Conservative Dentistry and Endodontics, Manipal College of Dental Sciences, Manipal Manipal Academy of Higher Education Manipal Karnataka India
2 shared publications - Sanjay Tikale
National Institute of Technology Karnataka
2 shared publications - Bronwyn Louise Fox
Factory of the Future, Swinburne University of Technology, Hawthorn, Australia
1 shared publication Carmen Maria Ferrer-Luque
B Department of Stomatology, School of Dentistry , University of Granada , Granada , Spain
1 shared publication
Latest Publications
- 10 November 2017
- Published by Medical Journals Sweden AB in Acta Odontologica Scandinavica
- Vol. 76 (3) , 199-203
Evaluation of final irrigation regimens with maleic acid for smear layer removal and wettability of root canal sealer
Objective: To evaluate the smear layer removal and wettability of AH Plus sealer on root canal dentin treated with MA (maleic acid), MA + CTR (cetrimide) and MA + CTR + CHX (chlorhexidine) as final irrigating regimens. Material and methods: For smear layer removal, 40 teeth were instrumented to size F4 and divided into four groups: (1) 7% MA, (2) 7% MA + 0.2% CTR, (3) 7% MA + 0.2% CTR + 2% CHX, (4) distilled water (control). After irrigation, teeth were subjected to SEM analysis. For contact angle analysis, 20 teeth were split longitudinally and divided into four groups similar to smear layer analysis. AH plus sealer was placed on each specimen and contact angle was analysed. Results: In both smear layer (p = .393) and contact angle analysis (p = .961), there was no significant difference between the groups MA and MA + CTR. However, MA + CTR + CHX removed smear layer less effectively (p = .023) and increased the contact angle of the sealer (p = .005). In smear layer analysis, specimens in negative control group were heavily smeared. In case of contact angle analysis, samples in the control group had least contact angle. Conclusion: MA alone or in combination with CTR removed smear layer effectively and increased the wettability of AH plus sealer to root canal dentin.
- 10 November 2017
- Published by Medical Journals Sweden AB in Acta Odontologica Scandinavica
- Vol. 76 (3) , 199-203
Evaluation of final irrigation regimens with maleic acid for smear layer removal and wettability of root canal sealer
Objective: To evaluate the smear layer removal and wettability of AH Plus sealer on root canal dentin treated with MA (maleic acid), MA + CTR (cetrimide) and MA + CTR + CHX (chlorhexidine) as final irrigating regimens. Material and methods: For smear layer removal, 40 teeth were instrumented to size F4 and divided into four groups: (1) 7% MA, (2) 7% MA + 0.2% CTR, (3) 7% MA + 0.2% CTR + 2% CHX, (4) distilled water (control). After irrigation, teeth were subjected to SEM analysis. For contact angle analysis, 20 teeth were split longitudinally and divided into four groups similar to smear layer analysis. AH plus sealer was placed on each specimen and contact angle was analysed. Results: In both smear layer (p = .393) and contact angle analysis (p = .961), there was no significant difference between the groups MA and MA + CTR. However, MA + CTR + CHX removed smear layer less effectively (p = .023) and increased the contact angle of the sealer (p = .005). In smear layer analysis, specimens in negative control group were heavily smeared. In case of contact angle analysis, samples in the control group had least contact angle. Conclusion: MA alone or in combination with CTR removed smear layer effectively and increased the wettability of AH plus sealer to root canal dentin.
- 1 November 2017
- Published by Elsevier in Journal of Dentistry
- Vol. 66, 32-36
Effects of smear layer removal agents on the physical properties and microstructure of mineral trioxide aggregate cement
- 1 November 2017
- Published by Elsevier in Journal of Dentistry
- Vol. 66, 32-36
Effects of smear layer removal agents on the physical properties and microstructure of mineral trioxide aggregate cement
- 16 August 2017
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 26 (9) , 4177-4187
The Effect of Wetting Gravity Regime on Shear Strength of SAC and Sn-Pb Solder Lap Joints
- 16 August 2017
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 26 (9) , 4177-4187
The Effect of Wetting Gravity Regime on Shear Strength of SAC and Sn-Pb Solder Lap Joints
- 21 February 2017
- Published by ASTM International in Materials Performance and Characterization
- Vol. 6 (1) , 46-54
Effect of Cooling Rate on Joint Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Reliability of the solder joint largely depends on mechanical strength, fatigue resistance, coefficient of thermal expansion, and intermetallic compound formation. Cooling rate significantly affects the physical properties of an alloy and influences the mechanical behavior of solder joints. In the present study, Sn-9Zn lead-free solder alloy was solidified on Cu substrate under furnace cooling (0.04°C/s), air cooling (0.16°C/s), and water cooling (94°C/s) conditions. The effect of varying cooling rates on the intermetallic compound (IMC) formation at the interface and the resulting joint shear strength was studied. A microstructure study revealed the presence of Cu5Zn8 and CuZn5 intermetallic compounds at the solder-substrate interface. The IMC layer thickness at the interface increased with a decrease in the cooling rate. The joint shear strength increased with an increase in the cooling rate. The air and furnace cooling resulted in the formation of a thick IMC layer. The IMC obtained from the furnace cooling was associated with micro-cracks leading to a decrease in the joint shear strength.
- 21 February 2017
- Published by ASTM International in Materials Performance and Characterization
- Vol. 6 (1) , 46-54
Effect of Cooling Rate on Joint Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Reliability of the solder joint largely depends on mechanical strength, fatigue resistance, coefficient of thermal expansion, and intermetallic compound formation. Cooling rate significantly affects the physical properties of an alloy and influences the mechanical behavior of solder joints. In the present study, Sn-9Zn lead-free solder alloy was solidified on Cu substrate under furnace cooling (0.04°C/s), air cooling (0.16°C/s), and water cooling (94°C/s) conditions. The effect of varying cooling rates on the intermetallic compound (IMC) formation at the interface and the resulting joint shear strength was studied. A microstructure study revealed the presence of Cu5Zn8 and CuZn5 intermetallic compounds at the solder-substrate interface. The IMC layer thickness at the interface increased with a decrease in the cooling rate. The joint shear strength increased with an increase in the cooling rate. The air and furnace cooling resulted in the formation of a thick IMC layer. The IMC obtained from the furnace cooling was associated with micro-cracks leading to a decrease in the joint shear strength.
- 12 April 2016
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 45 (7) , 3744-3758
Effect of Reflow Time on Wetting Behavior, Microstructure Evolution, and Joint Strength of Sn-2.5Ag-0.5Cu Solder on Bare and Nickel-Coated Copper Substrates
- 12 April 2016
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 45 (7) , 3744-3758
Effect of Reflow Time on Wetting Behavior, Microstructure Evolution, and Joint Strength of Sn-2.5Ag-0.5Cu Solder on Bare and Nickel-Coated Copper Substrates
- 11 September 2015
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 68 (6) , 1027-1031
Spreading Behaviour and Joint Reliability of Sn–0.3Ag–0.7Cu Lead-Free Solder Alloy on Nickel Coated Copper Substrate as a Function of Reflow Time
- 11 September 2015
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 68 (6) , 1027-1031
Spreading Behaviour and Joint Reliability of Sn–0.3Ag–0.7Cu Lead-Free Solder Alloy on Nickel Coated Copper Substrate as a Function of Reflow Time
- 3 September 2015
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 830-831, 215-218
Wettability and Bond Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Lead-free solders are environment friendly and are in great demand for microelectronic applications. In the present study, Sn-9Zn lead free solder alloy was solidified on Cu substrate for different reflow times from 10 to 1000s. The influence of reflow time on wetting, formation of intermetallic compounds (IMCs) and bond shear strength was studied using dynamic contact angle analyzer, bond tester and scanning electron microscopy. The results indicate that, the wettability of the solder alloy increased with increase in reflow time. Microstructure study revealed the presence of Cu5Zn8 and CuZn5 IMCs at the interface. The thickness of an IMC increased with increase in the reflow time. The mean thickness of about 11μm for Cu5Zn8 IMC layer was observed for the reflow time of 1000s. The thickness of CuZn5 layer increased up to a reflow time of 100s and decreases thereafter. The bond shear strength increased up to 100s and decreased with increase in reflow time. The decrement in shear strength at higher reflow time is mainly due to excessive thickness of Cu5Zn8 IMC layer and diffusion of Sn from bulk solder towards the substrate. The excessive thick IMC layer exhibited pre micro-cracks led to the brittle failure of bond under the influence of shear stress.
- 3 September 2015
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 830-831, 215-218
Wettability and Bond Shear Strength of Sn-9Zn Lead-Free Solder Alloy Reflowed on Copper Substrate
Lead-free solders are environment friendly and are in great demand for microelectronic applications. In the present study, Sn-9Zn lead free solder alloy was solidified on Cu substrate for different reflow times from 10 to 1000s. The influence of reflow time on wetting, formation of intermetallic compounds (IMCs) and bond shear strength was studied using dynamic contact angle analyzer, bond tester and scanning electron microscopy. The results indicate that, the wettability of the solder alloy increased with increase in reflow time. Microstructure study revealed the presence of Cu5Zn8 and CuZn5 IMCs at the interface. The thickness of an IMC increased with increase in the reflow time. The mean thickness of about 11μm for Cu5Zn8 IMC layer was observed for the reflow time of 1000s. The thickness of CuZn5 layer increased up to a reflow time of 100s and decreases thereafter. The bond shear strength increased up to 100s and decreased with increase in reflow time. The decrement in shear strength at higher reflow time is mainly due to excessive thickness of Cu5Zn8 IMC layer and diffusion of Sn from bulk solder towards the substrate. The excessive thick IMC layer exhibited pre micro-cracks led to the brittle failure of bond under the influence of shear stress.
- 3 September 2015
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 830-831, 286-289
Wetting Kinetics and Joint Strength of Sn-0.3Ag-0.7Cu Lead-Free Solder Alloy on Copper Substrate as a Function of Reflow Time
Solder plays a vital role in the interconnection of electronic devices in electronic assemblies. As an interconnection material, the solder joint executes electrical, mechanical and thermal functions. The use of lead bearing solders in electronic products is banned due to the toxicity and environmental risks coupled with lead. In the present study, wetting kinetics, interfacial reactions and the formation of intermetallic compounds (IMCs) during solidification of Sn-0.3Ag-0.7Cu solder alloy on Cu substrate and the corresponding joint strength were studied as a function of reflow time. Experiments were carried out at various reflow times of 10, 100, 300 and 500s. The reflow temperature was maintained at 270°C. The solder alloy showed enhanced wettability on the substrate at longer reflow times. The thickness of IMC layer formed during a reflow time of 10s was 1.67μm and the thickness increased to 2.20μm, 2.85μm, 2.91μm during 100s, 300s and 500s of reflow time respectively. The joint shear test was performed to assess the integrity of Sn-0.3Ag-0.7Cu solder solidified on Cu substrates using Nordson DAGE 4000 Plus bond tester. The joint strength increased with the increase in reflow time up to 300s and the maximum joint strength was observed for samples reflowed for 300s. Although the samples reflowed for 500s samples showed good wettability, they exhibited lowest joint strength.
- 3 September 2015
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 830-831, 286-289
Wetting Kinetics and Joint Strength of Sn-0.3Ag-0.7Cu Lead-Free Solder Alloy on Copper Substrate as a Function of Reflow Time
Solder plays a vital role in the interconnection of electronic devices in electronic assemblies. As an interconnection material, the solder joint executes electrical, mechanical and thermal functions. The use of lead bearing solders in electronic products is banned due to the toxicity and environmental risks coupled with lead. In the present study, wetting kinetics, interfacial reactions and the formation of intermetallic compounds (IMCs) during solidification of Sn-0.3Ag-0.7Cu solder alloy on Cu substrate and the corresponding joint strength were studied as a function of reflow time. Experiments were carried out at various reflow times of 10, 100, 300 and 500s. The reflow temperature was maintained at 270°C. The solder alloy showed enhanced wettability on the substrate at longer reflow times. The thickness of IMC layer formed during a reflow time of 10s was 1.67μm and the thickness increased to 2.20μm, 2.85μm, 2.91μm during 100s, 300s and 500s of reflow time respectively. The joint shear test was performed to assess the integrity of Sn-0.3Ag-0.7Cu solder solidified on Cu substrates using Nordson DAGE 4000 Plus bond tester. The joint strength increased with the increase in reflow time up to 300s and the maximum joint strength was observed for samples reflowed for 300s. Although the samples reflowed for 500s samples showed good wettability, they exhibited lowest joint strength.
- 17 July 2015
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 69 (4) , 941-947
Assessment of Joint Reliability of Sn–2.5Ag–0.5Cu Solder/Cu as a Function of Reflow Time
- 17 July 2015
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 69 (4) , 941-947
Assessment of Joint Reliability of Sn–2.5Ag–0.5Cu Solder/Cu as a Function of Reflow Time
- 29 January 2014
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 25 (3) , 1446-1455
The effect of reflow time on reactive wetting, evolution of interfacial IMCs and shear strength of eutectic Sn–Cu solder alloy
- 29 January 2014
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 25 (3) , 1446-1455
The effect of reflow time on reactive wetting, evolution of interfacial IMCs and shear strength of eutectic Sn–Cu solder alloy