Yinge Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yinge Li has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
Lisheng Zhong
State Key Laboratory of Electrical Insulation and Power Equipment, Xi'an Jiaotong University, Xi'an, Shannxi, China
5 shared publicationsJinghui Gao
State Key Laboratory of Electrical Insulation and Power Equipment, Xi'an Jiaotong University, Xi'an, Shannxi, China
3 shared publications- Wei Zhao
State Key Laboratory of Electrical Insulation and Power Equipment, Xi'an Jiaotong University, Xi'an, 710049, China
3 shared publications Haiyang Ren
State Key Laboratory of Electrical Insulation and Power Equipment, Xi'an Jiaotong University, Xi'an, 710049, China
2 shared publicationsLiang Cao
State Key Laboratory of Electrical Insulation and Power Equipment, Xi'an Jiaotong University, Xi'an, Shannxi, China
2 shared publicationsQinxue Yu
State Key Laboratory of Electrical Insulation and Power Equipment, Xi'an Jiaotong University, 710049, China
2 shared publications
Latest Publications
- 14 December 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Dielectrics and Electrical Insulation
- Vol. 27 (6) , 2064-2070
Temperature Stability of DC Conductivity and Breakdown of Crosslinked LLDPE
In this paper, a way to improve the temperature stability of DC conductivity and breakdown characteristics of polyethylene (PE) is proposed using a crosslinked linear low density polyethylene (LLDPE). The ratio of DC conductivity, as well as breakdown strength values under 90 to 30°C is used to determine the temperature stability of DC properties. The closer it is to 1, the better the performance of temperature stability. The results show that when using crosslinked-LLDPE material, the ratio of DC conductivity under 90 to 30°C is 10.5, while it is 461.6 for crosslinked-LDPE samples with the same DCP content. And the ratio of DC breakdown strength is 0.97 for crosslinked-LLDPE, while it is 0.32 for crosslinked-LDPE. The gel permeation chromatography (GPC) method, hot-set test, differential scanning calorimetry (DSC) analysis and scanning electron microscopy (SEM) images show that the fine arrangement and smaller molecular weight between crosslinks of molecular and morphology structure that LLDPE owns contribute to the improvement in comparison with LDPE. The findings may contribute a solution to the development of HVDC power cable insulation materials.
- 14 December 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Dielectrics and Electrical Insulation
- Vol. 27 (6) , 2064-2070
Temperature Stability of DC Conductivity and Breakdown of Crosslinked LLDPE
In this paper, a way to improve the temperature stability of DC conductivity and breakdown characteristics of polyethylene (PE) is proposed using a crosslinked linear low density polyethylene (LLDPE). The ratio of DC conductivity, as well as breakdown strength values under 90 to 30°C is used to determine the temperature stability of DC properties. The closer it is to 1, the better the performance of temperature stability. The results show that when using crosslinked-LLDPE material, the ratio of DC conductivity under 90 to 30°C is 10.5, while it is 461.6 for crosslinked-LDPE samples with the same DCP content. And the ratio of DC breakdown strength is 0.97 for crosslinked-LLDPE, while it is 0.32 for crosslinked-LDPE. The gel permeation chromatography (GPC) method, hot-set test, differential scanning calorimetry (DSC) analysis and scanning electron microscopy (SEM) images show that the fine arrangement and smaller molecular weight between crosslinks of molecular and morphology structure that LLDPE owns contribute to the improvement in comparison with LDPE. The findings may contribute a solution to the development of HVDC power cable insulation materials.
- Open Access
Enhanced High-Temperature DC Dielectric Performance of Crosslinked Polyethylene with a Polystyrene Pinning Structure
In this paper, we propose a method on improving direct current (DC) dielectric performance by designing a polystyrene (PS) pinning crosslinked polyethylene (XLPE) for the application of insulation materials on high voltage direct current (HVDC) extruded cable. Electrical experimental results show that the addition of PS (1–5 phr, parts per hundreds of resin) can significantly reduce DC conductivity and increase DC breakdown strength of XLPE in the test temperature range of 30–90 °C. Microstructure investigation shows PS distributed as particles could participate in the formation of a crosslinking network with the help of a crosslinking agent, thus forming a polymer pinning structure at the interface between XLPE and PS. It is believed that such a special design strengthens the structure of XLPE, which leads to the improved DC dielectric performance at elevated temperatures. Our findings may contribute a new solution for developing HVDC cable insulation materials.
Open AccessEnhanced High-Temperature DC Dielectric Performance of Crosslinked Polyethylene with a Polystyrene Pinning Structure
In this paper, we propose a method on improving direct current (DC) dielectric performance by designing a polystyrene (PS) pinning crosslinked polyethylene (XLPE) for the application of insulation materials on high voltage direct current (HVDC) extruded cable. Electrical experimental results show that the addition of PS (1–5 phr, parts per hundreds of resin) can significantly reduce DC conductivity and increase DC breakdown strength of XLPE in the test temperature range of 30–90 °C. Microstructure investigation shows PS distributed as particles could participate in the formation of a crosslinking network with the help of a crosslinking agent, thus forming a polymer pinning structure at the interface between XLPE and PS. It is believed that such a special design strengthens the structure of XLPE, which leads to the improved DC dielectric performance at elevated temperatures. Our findings may contribute a new solution for developing HVDC cable insulation materials.
- 1 September 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-5
Effects of Revulcanization on XLPE Crystalline Morphology and AC Breakdown Performance
The extruded insulation submarine cable of large length employs a number of factory joints for connection in sea-crossing transmission projects. The vulcanization process of factory joint will inevitably involve reheating the cable insulation near the joint position, which may cause change of the crystalline morphology and dielectric properties of crosslinked polyethylene (XLPE). This phenomenon is especially obvious in cable with large insulation thickness since the required heating time is longer than others. This paper reports the influence of factory joint vulcanization process on crystalline morphology and AC breakdown performance of XLPE from cable near joint. XLPE of cable bulk and cable near joint were divided into inner, middle and outer parts due to their distinct thermal history in practical situation. Then the crosslinking degree, crystalline morphology and breakdown field strength at power frequency in each insulation position were measured. The results show that there is a revulcanization in cable near joint, which leads to the slight increase on the crosslinking degree, while the corresponding crystallinity reduces and the spacing of crystal plane as well as the crystal integrality increases compared with cable bulk. Moreover, the divergence of crosslinking degree and crystalline morphology between cable bulk and cable near joint exhibit more evidently in inner insulation, and AC breakdown field strength of cable near joint at power frequency is slightly lower.
- 1 September 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-5
Effects of Revulcanization on XLPE Crystalline Morphology and AC Breakdown Performance
The extruded insulation submarine cable of large length employs a number of factory joints for connection in sea-crossing transmission projects. The vulcanization process of factory joint will inevitably involve reheating the cable insulation near the joint position, which may cause change of the crystalline morphology and dielectric properties of crosslinked polyethylene (XLPE). This phenomenon is especially obvious in cable with large insulation thickness since the required heating time is longer than others. This paper reports the influence of factory joint vulcanization process on crystalline morphology and AC breakdown performance of XLPE from cable near joint. XLPE of cable bulk and cable near joint were divided into inner, middle and outer parts due to their distinct thermal history in practical situation. Then the crosslinking degree, crystalline morphology and breakdown field strength at power frequency in each insulation position were measured. The results show that there is a revulcanization in cable near joint, which leads to the slight increase on the crosslinking degree, while the corresponding crystallinity reduces and the spacing of crystal plane as well as the crystal integrality increases compared with cable bulk. Moreover, the divergence of crosslinking degree and crystalline morphology between cable bulk and cable near joint exhibit more evidently in inner insulation, and AC breakdown field strength of cable near joint at power frequency is slightly lower.
- 1 September 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-4
DC Breakdown Characteristics of LLDPE-based XLPE with Different Crosslinking Degrees
Temperature stability is one of the most determinant factor in the design of HVDC cable insulation, since the conductivity and correlated field strength distribution are temperature-dependent. Low density polyethylene (LDPE)-based cross-linked polyethylene (XLPE) material is the prevailing material system in HVDC cable insulation. Here, we report a method on improving the temperature stability for the DC performance of XLPE by changing the starting material into linear low density polyethylene (LLDPE). In order to understand the role of crosslinking agent-dicumyl peroxide (DCP), we investigate DC breakdown characteristics of LLDPE-based materials with different crosslinking degrees under different temperatures. The results show that DC breakdown strength for LLDPE-based materials varies smaller compared with LDPE-based materials. Further differential Scanning Calorimetry (DSC) results suggest that the temperature-stable DC performance for LLDPE material stems from its higher crystallinity as well as melting point than LDPE samples. And the optimal DCP content for LLDPE-based materials has been further discussed.
- 1 September 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-4
DC Breakdown Characteristics of LLDPE-based XLPE with Different Crosslinking Degrees
Temperature stability is one of the most determinant factor in the design of HVDC cable insulation, since the conductivity and correlated field strength distribution are temperature-dependent. Low density polyethylene (LDPE)-based cross-linked polyethylene (XLPE) material is the prevailing material system in HVDC cable insulation. Here, we report a method on improving the temperature stability for the DC performance of XLPE by changing the starting material into linear low density polyethylene (LLDPE). In order to understand the role of crosslinking agent-dicumyl peroxide (DCP), we investigate DC breakdown characteristics of LLDPE-based materials with different crosslinking degrees under different temperatures. The results show that DC breakdown strength for LLDPE-based materials varies smaller compared with LDPE-based materials. Further differential Scanning Calorimetry (DSC) results suggest that the temperature-stable DC performance for LLDPE material stems from its higher crystallinity as well as melting point than LDPE samples. And the optimal DCP content for LLDPE-based materials has been further discussed.
- 1 May 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 324-327
Effects of degassing duration on crosslinking byproducts of HVDC cable insulation
With the rapid development of power engineering and electronic technology, high voltage direct current (HVDC) extruded cable with low loss, long lifespan, high reliability has become a rising concern, especially in China. Whereas HVDC cable holds insulation with greater thickness and longer distance than other cables, crosslinking condition of crosslinking polyethylene (XLPE) in cable extrusion and the variation of crosslinking byproducts including α-methyl styrene, acetophenone and cumyl alcohol, which have effects on the dielectric properties of cable insulation, are still in need of further research. The temperature and duration in factory degassing of HVDC cable have been handled in accordance to experience so far. In this paper, the effect of duration in factory degassing on crystallinity and crosslinking byproducts of HVDC cable insulation is studied. During the degassing, small grains are taken crystallization in outer insulation. No obvious change of crosslinking degree has taken place in HVDC cable after degassing treatment, as well as α-methyl styrene and cumyl alcohol content, while the relative content of acetophenone in crosslinking byproduct has varied significantly. And there is a variety of relative content of acetophenone in radial direction.
- 1 May 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 324-327
Effects of degassing duration on crosslinking byproducts of HVDC cable insulation
With the rapid development of power engineering and electronic technology, high voltage direct current (HVDC) extruded cable with low loss, long lifespan, high reliability has become a rising concern, especially in China. Whereas HVDC cable holds insulation with greater thickness and longer distance than other cables, crosslinking condition of crosslinking polyethylene (XLPE) in cable extrusion and the variation of crosslinking byproducts including α-methyl styrene, acetophenone and cumyl alcohol, which have effects on the dielectric properties of cable insulation, are still in need of further research. The temperature and duration in factory degassing of HVDC cable have been handled in accordance to experience so far. In this paper, the effect of duration in factory degassing on crystallinity and crosslinking byproducts of HVDC cable insulation is studied. During the degassing, small grains are taken crystallization in outer insulation. No obvious change of crosslinking degree has taken place in HVDC cable after degassing treatment, as well as α-methyl styrene and cumyl alcohol content, while the relative content of acetophenone in crosslinking byproduct has varied significantly. And there is a variety of relative content of acetophenone in radial direction.
- 29 June 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Dielectrics and Electrical Insulation
- Vol. 24 (3) , 1476-1484
DC electrical breakdown dependence on the radial position of specimens within HVDc XLPE cable insulation
Because of temperature gradients and inhomogeneous cooling rates after extrusion, the performances of HVDC XLPE cable insulation at radial position are not uniformly distributed. DC breakdown strength measurements of HVDC XLPE cable insulation specimens in inner insulation (near conductor shield), middle insulation and outer insulation (near insulation shield) have been carried out and show that DC breakdown strength of specimens in middle insulation is relatively lower than that of in inner and outer insulation at 30, 50 and 70 °C. At 90 °C, there is no significant difference of DC breakdown strength of specimens at radial position. Thus the micro performances of XLPE specimens at different radial position have been studied by FTIR, DSC, SEM and XRD. FTIR measurements show that cross-linked by-products (benzyl alcohol and acetophenone) content in middle insulation is higher; DSC measurements shows that crystallinity of specimens in middle insulation is slightly higher; SEM measurements show that the grains of specimens in middle insulation are unevenly distributed and their sizes have obvious difference; the results of XRD measurements show a higher content of by-products, a higher crystallinity and a larger crystalline interplanar spacing (a larger grain size) of specimens in middle insulation, which are consistent with FTIR, DSC and SEM analysis. Therefore, cross-linked by-products, crystallinity and crystal morphology together make DC breakdown strength of specimens in middle insulation lower.
- 29 June 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Dielectrics and Electrical Insulation
- Vol. 24 (3) , 1476-1484
DC electrical breakdown dependence on the radial position of specimens within HVDc XLPE cable insulation
Because of temperature gradients and inhomogeneous cooling rates after extrusion, the performances of HVDC XLPE cable insulation at radial position are not uniformly distributed. DC breakdown strength measurements of HVDC XLPE cable insulation specimens in inner insulation (near conductor shield), middle insulation and outer insulation (near insulation shield) have been carried out and show that DC breakdown strength of specimens in middle insulation is relatively lower than that of in inner and outer insulation at 30, 50 and 70 °C. At 90 °C, there is no significant difference of DC breakdown strength of specimens at radial position. Thus the micro performances of XLPE specimens at different radial position have been studied by FTIR, DSC, SEM and XRD. FTIR measurements show that cross-linked by-products (benzyl alcohol and acetophenone) content in middle insulation is higher; DSC measurements shows that crystallinity of specimens in middle insulation is slightly higher; SEM measurements show that the grains of specimens in middle insulation are unevenly distributed and their sizes have obvious difference; the results of XRD measurements show a higher content of by-products, a higher crystallinity and a larger crystalline interplanar spacing (a larger grain size) of specimens in middle insulation, which are consistent with FTIR, DSC and SEM analysis. Therefore, cross-linked by-products, crystallinity and crystal morphology together make DC breakdown strength of specimens in middle insulation lower.