JFJianqing Feng

Jianqing Feng

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Jianqing Feng has a total of 28 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Influences of Precursors Phase Composition on the Phase Evolution Dynamics of Bi-2223 Superconducting Tapes

    by Shengnan Zhang, Botao Shao, Wen Zhang, Xiaobo Ma, Jixing Liu, Xueqian Liu, Jianqing Feng, Qingyang Wang, Chengshan Li, Pingxiang Zhang

    Bi 2 Sr 2 Ca 2 Cu 3 O 10+δ (Bi-2223) precursors for the fabrication of high temperature superconducting tapes were prepared by spray pyrolysis technique followed by a calcination process. The influences of precursor powder phase composition on the phase evolution dynamics and final current capacity of Bi-2223 superconducting tapes were systematically studied. It was interesting to notice that slight increase of Cu content in chemical composition could cause obvious variations of both the phase composition and the morphology of CuO particles in precursors. Therefore, the Bi-2223 phase formation process during the sintering process of tapes could be affected, and the current capacity changed accordingly. On the other hand, during the calcination temperature optimization process, the Bi-2223 phase content in precursors changed accordingly, thus the Bi-2223 phase formation dynamics were also studied. More Bi-2223 nuclei were formed due to the pre-existed Bi-2223 grains, which worked as inhomogeneous nuclei centers. Thus, although the final Bi-2223 phase contents were similar in all the tapes, the particle size and texture structure of Bi-2223 varied greatly, which caused a dramatic decrease of critical current in Bi-2223 tapes with the formation of Bi-2223 in precursors. Therefore, it could be concluded that both the morphology of CuO particles and the Bi-2223 phase content in precursors were the factors controlling the phase evolution dynamics during Bi-2223 tape sintering process.


  • Annealing Effect of FeSe Superconducting Polycrystalline Bulks in Low Oxygen Atmosphere

    by Botao Shao, Tianzi Yang, Shengnan Zhang, Jixing Liu, Wen Zhang, Hao Cao, Jianqing Feng, Chengshan Li, Pingxiang Zhang

    FeSe superconducting bulks with different Fe contents were prepared by high energy ball milling aided sintering process followed by a post annealing process in low oxygen atmosphere. The influences of Fe content, annealing temperature and oxygen partial pressure have been systematically studied. It was found that both the critical temperature and superconducting phase volume ratio have been obviously improved with annealing. However, the effect of oxygen annealing process on FeSe polycrystalline bulks was different with that on FeSe single crystals. In polycrystalline bulks, the annealing process could further promote the phase transition from nonsuperconducting hexagonal -FeSe phase to superconducting tetragonal -FeSe phase. Meanwhile, the chemical composition uniformity has also been enhanced with no obvious FeO phase detected by X-Ray Diffraction. With optimized annealing process under the oxygen partial pressure of 5% at 400 oC for 10 h, FeSe superconducting bulks have reached the critical temperature of 9.1 K.

  • Fabrication of Bi-2223 High Temperature Superconducting Tapes With Groove Rolling Process

    by Shengnan Zhang, Chengshan Li, Xiaobo Ma, Jianqing Feng, Botao Shao, Xueqian Liu, Pingxiang Zhang

    ${\text{Bi}_{1.76}\text{Pb}_{0.34}\text{Sr}_{1.93}\text{Ca}_{2.02}\text{Cu}_{3.06}O_{10+\delta}}$ (Bi-2223) high temperature superconducting tapes were fabricated with Powder in tube (PIT) process. The traditional drawing process was partially replaced by groove rolling. The influences of cold working method on the filament density, the phase evolution mechanism as well as superconducting properties has been systematically studied. The groove rolling process could obviously enhance the filament density of Bi-2223 green wires, which thus led to the change of Bi-2223 formation rate. Meanwhile, although the heat treatment process has not been thoroughly optimized and the residual secondary phase content was still high, the critical current has been improved for more than 20% with groove rolling process, which should be attributed to the improved intergrain connections. On the other hand, the groove rolling process was also effective on the fabrication with Bi-2223 tapes with larger filament number, such as 85 or 121 to maintain the uniformity of filament deformation.


  • Improving Transport Properties of Bi-2223 Superconducting Tapes With the Optimization of Packing Atmosphere

    by Shengnan Zhang, Xiaobo Ma, Lijun Cui, Guoqing Liu, Huiling Zheng, Yingjian Huang, Jianqing Feng, Chengshan Li, Pingxiang Zhang

    Multi-filamentary $\text{Bi}_2 \text{Sr}_2 \text{Ca}_2 \text{Cu}_3 \text{O}_{10 + \delta}$ (Bi-2223) high temperature superconducting tapes were fabricated by powder in tube process (PIT). During the precursor powder packing process, environment atmosphere was changed from pure oxygen to dry air and 7.5% $\text{O}_2$ balanced with $\text{N}_2$ , with the oxygen partial pressure decreasing from 100% to 25% and 7.5 %, respectively. The change of packing atmosphere obviously influenced the phase assemblage in the early stage of Bi-2223 phase formation process. Therefore, the chemical composition of obtained Bi-2223 phase as well as the content and distribution of secondary phases changed accordingly. Meanwhile, the changes of intergrain connections and the flux pinning properties were investigated based on the in-field critical current, $I_{\text{c}}$ -B measurements. Finally, attributed to the decreased oxygen partial pressure in packing atmosphere, the $I_{\text{c}}$ improvements of 25% at self field and 0.6 T were obtained comparing with the tapes packed under pure oxygen. With further optimization of sintering process, the final $I_{\text{c}}$ of 116 A was achieved, which corresponded to the critical current density, $J_{\text{c}}$ of ~21 $\text{kAcm}^{-2}$ .

  • Optimization of High-Energy Ball-Milling Time for Fe1.1Se0.5Te0.5 Polycrystalline Superconductors

    by Jixing Liu, Chengshan Li, Shengnan Zhang, Meng Li, Jianqing Feng, Pingxiang Zhang, Lian Zhou

    The $Fe_{1.1}Se_{0.5}Te_{0.5}$ polycrystalline superconductors were prepared by a high energy ball milling (HEBM) technique. The different ball milling time of 0, 2, 4, 6 and 8 h was adopted to optimize this technique. The influences of ball milling time on the phase distributions of milled powders and sintered bulks, the morphology of ball milled powders and superconducting properties of final sintered bulks were systematically studied. It was found that with increasing ball milling time, the ball milled powders changed from crystal to non-crystalline then to alloy. At the same time, the main phases in ball milled powders changed from original mixed powders of Fe, Se and Te to (Se, Te) solid solution then to the two phases of β-Fe(Se, Te) and δ-Fe(Se, Te), accordingly. Due to the reduction of diffusion length, it was more likely for HEBM powders forming FeSeTe ternary alloys. Thus, the obtained Fe(Se, Te) bulk with HEBM time of 4 h exhibited the highest Tc of 14.3 K and the largest content of superconducting phase. However, in the samples achieved by longer HEBM time, phase segregation and oxidation were observed. Therefore, the HEBM time of 4 h is the most suitable for the fabrication of high-quality precursor powders according to the experiments.


  • Optimization of FeSe Superconducting Tapes with Different Sheath Materials and Precursor Powders

    by Shengnan Zhang, Jixing Liu, Jianqing Feng, Botao Shao, Chengshan Li, Pingxiang Zhang