Ekrem Burak Toka
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ekrem Burak Toka has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Murat Olgun
Konya Teknik Üniversitesi
4 shared publications - Alican Şenkaya
Konya Teknik Üniversitesi
3 shared publications - Mustafa Abdalwahid Noori Noori
Konya Teknik Üniversitesi
2 shared publications - Gülsüm Yalçınyiğit1 shared publication
Murat Olgun
Professor, Dept. of Civil Engineering, Faculty of Engineering and Natural Sciences, Konya Technical Univ., Konya 42250, Turkey
1 shared publication- İbrahim Hakkı Erkan
Department of Civil Engineering, Konya Technical University, Konya (Turkey)
1 shared publication
Latest Publications
- Open Access
- 14 July 2026
- Published by Omer Halisdemir Universitesi in Ömer Halisdemir Üniversitesi Mühendislik Bilimleri Dergisi
- Vol. 17
Derin karıştırma kolonu dayanımının yanıt yüzey yöntemi esaslı modellenmesi ve karşılaştırmalı analitik ve metasezgisel optimizasyonu
Bu çalışmada, düşük plastisiteli killi zeminde oluşturulan laboratuvar ölçekli derin karıştırma kolonlarının (DKK) 28 günlük serbest basınç dayanımı (UCS), yanıt yüzey yöntemi (YYY) esaslı I-optimal yaklaşımla modellenmiş ve analitik/metasezgisel optimizasyon yöntemleriyle optimize edilmiştir. Laboratuvar ölçekli DKK’lerde çimento (%5–%20), silis dumanı (%0–%15), akışkanlaştırıcı katkı (%0–%5), su/bağlayıcı oranı (0.9–2.5) ve su muhtevası (%25–%33) etkileri 21 karışımla incelenmiştir. Karotların 28 günlük UCS değerleri 123.8–5037.7 kPa aralığında bulunmuş, varyans analizi (ANOVA) ile en etkili parametrelerin sırasıyla su/bağlayıcı oranı, çimento oranı ve silis dumanı oranı olduğu belirlenmiştir. Belirleme katsayısı (R²) = 0.945 olan regresyon modeli üzerinde Lagrange çarpanları 5089.7 kPa, parçacık sürü optimizasyonu (PSO) ve arılar algoritması ise 5154.2 kPa optimum UCS öngörmüş; optimum karışımla üretilen DKK’den alınan karotlardan ortalama 5218 kPa UCS ölçülerek tahminlerle %1.24–%2.52 aralığında uyum sağlanmıştır. Çalışma; DKK için I-optimal tasarımı, analitik/metasezgisel optimizasyonu ve laboratuvar ölçekli DKK boyutlarında doğrulamayı birleştirerek literatüre özgün bir katkı sunmaktadır.
- 14 July 2026
- Published by Omer Halisdemir Universitesi in Ömer Halisdemir Üniversitesi Mühendislik Bilimleri Dergisi
- Vol. 17
Open AccessDerin karıştırma kolonu dayanımının yanıt yüzey yöntemi esaslı modellenmesi ve karşılaştırmalı analitik ve metasezgisel optimizasyonu
Bu çalışmada, düşük plastisiteli killi zeminde oluşturulan laboratuvar ölçekli derin karıştırma kolonlarının (DKK) 28 günlük serbest basınç dayanımı (UCS), yanıt yüzey yöntemi (YYY) esaslı I-optimal yaklaşımla modellenmiş ve analitik/metasezgisel optimizasyon yöntemleriyle optimize edilmiştir. Laboratuvar ölçekli DKK’lerde çimento (%5–%20), silis dumanı (%0–%15), akışkanlaştırıcı katkı (%0–%5), su/bağlayıcı oranı (0.9–2.5) ve su muhtevası (%25–%33) etkileri 21 karışımla incelenmiştir. Karotların 28 günlük UCS değerleri 123.8–5037.7 kPa aralığında bulunmuş, varyans analizi (ANOVA) ile en etkili parametrelerin sırasıyla su/bağlayıcı oranı, çimento oranı ve silis dumanı oranı olduğu belirlenmiştir. Belirleme katsayısı (R²) = 0.945 olan regresyon modeli üzerinde Lagrange çarpanları 5089.7 kPa, parçacık sürü optimizasyonu (PSO) ve arılar algoritması ise 5154.2 kPa optimum UCS öngörmüş; optimum karışımla üretilen DKK’den alınan karotlardan ortalama 5218 kPa UCS ölçülerek tahminlerle %1.24–%2.52 aralığında uyum sağlanmıştır. Çalışma; DKK için I-optimal tasarımı, analitik/metasezgisel optimizasyonu ve laboratuvar ölçekli DKK boyutlarında doğrulamayı birleştirerek literatüre özgün bir katkı sunmaktadır.
- Open Access
- 24 June 2026
- Published by Tulpar Academic Publishing in Challenge Journal of Concrete Research Letters
- Vol. 17 (2) , 207-221
Behavior of GGBFS-modified DSM columns in clay soil: Strength–permeability characteristics and predictive laboratory modeling
This study investigated the influence of partially substituting cement with ground granulated blast furnace slag (GGBFS) on the unconfined compressive strength (UCS), splitting tensile strength (STS), and permeability coefficient (kDSM) of deep soil mixing (DSM) columns formed in clay soil. The water/binder ratio was kept constant at 1.0. Cast specimens were prepared using two binder contents, aw = 15% and 20% by dry soil mass, and five GGBFS substitution ratios of 0%, 10%, 20%, 35%, and 50%. Strength specimens were tested after 7, 28, and 56 days of curing, whereas permeability specimens were tested after 28 and 56 days. Four laboratory-scale DSM columns with a diameter of 300 mm and a length of 600 mm were formed for selected mixtures with aw = 20% and GGBFS ratios of 0%, 20%, 35%, and 50%; core samples were extracted after 28 days. UCS values ranged from 859 to 4939 kPa, STS from 182 to 830 kPa, and kDSM from 0.16×10⁻¹⁰ to 9.17×10⁻¹⁰ cm/s for cast specimens. GGBFS reduced early-age strength at 7 days, but improved strength and reduced permeability at later curing ages. The UCS and STS values of core samples were 45.26–69.79% and 63.00–77.58% of the corresponding cast specimen values, respectively, while permeability values of core samples were higher. SEM and XRD observations supported the formation of hydration and pozzolanic products.
- 24 June 2026
- Published by Tulpar Academic Publishing in Challenge Journal of Concrete Research Letters
- Vol. 17 (2) , 207-221
Open AccessBehavior of GGBFS-modified DSM columns in clay soil: Strength–permeability characteristics and predictive laboratory modeling
This study investigated the influence of partially substituting cement with ground granulated blast furnace slag (GGBFS) on the unconfined compressive strength (UCS), splitting tensile strength (STS), and permeability coefficient (kDSM) of deep soil mixing (DSM) columns formed in clay soil. The water/binder ratio was kept constant at 1.0. Cast specimens were prepared using two binder contents, aw = 15% and 20% by dry soil mass, and five GGBFS substitution ratios of 0%, 10%, 20%, 35%, and 50%. Strength specimens were tested after 7, 28, and 56 days of curing, whereas permeability specimens were tested after 28 and 56 days. Four laboratory-scale DSM columns with a diameter of 300 mm and a length of 600 mm were formed for selected mixtures with aw = 20% and GGBFS ratios of 0%, 20%, 35%, and 50%; core samples were extracted after 28 days. UCS values ranged from 859 to 4939 kPa, STS from 182 to 830 kPa, and kDSM from 0.16×10⁻¹⁰ to 9.17×10⁻¹⁰ cm/s for cast specimens. GGBFS reduced early-age strength at 7 days, but improved strength and reduced permeability at later curing ages. The UCS and STS values of core samples were 45.26–69.79% and 63.00–77.58% of the corresponding cast specimen values, respectively, while permeability values of core samples were higher. SEM and XRD observations supported the formation of hydration and pozzolanic products.
- 14 March 2022
- Published by Springer Nature in Arabian Journal for Science and Engineering
- Vol. 47 (10) , 13035-13047
Effects of Cement Grout Characteristics on Formation and Strength of Jet Grouting Columns
- 14 March 2022
- Published by Springer Nature in Arabian Journal for Science and Engineering
- Vol. 47 (10) , 13035-13047
Effects of Cement Grout Characteristics on Formation and Strength of Jet Grouting Columns
- 19 April 2021
- Published by Taylor & Francis in International Journal of Pavement Engineering
- Vol. 23 (11) , 3729-3742
Performance of granular road base and sub-base layers containing recycled concrete aggregate in different ratios
In this study, the usability and performance properties of recycled concrete aggregates (RCA) as granular road base (GRB) and granular road subbase (GRSB) material were investigated. A natural aggregate and the RCAs obtained from concretes with three different compressive strength and mixtures created by adding the RCAs to NA at the ratios of 25, 50 and 75% were used. Physical properties, modified Proctor, resilient modulus, permanent deformation, California bearing ratio (CBR), and permeability tests were carried out on all mixtures. Resilient modulus values (Mr) were obtained using three different resilient modulus models. The highest Mr value among pure RCAs was observed for RCA2 (average of 200 MPa). For the mixture samples, the highest Mr values were obtained in the mixtures containing RCA1 (average of 250 MPa). The minimum of permanent deformation value (ϵp) for the mixtures was obtained when the ratio of the RCA1 in the mixtures was 50% (ϵp = 0.238%). The obtained CBR values were not related to the Mr values, and the highest CBR values were found for the pure RCAs (average of 126%). High permeability coefficient values (average of 9.973×10−6 m/s) were obtained for the RCAs. As a result, it was more appropriate to blend the RCAs with the natural material rather than to use them in pure form. In general, it was appropriate to use 50% of RCAs in the mixtures. It was observed that if concrete compressive strength is as high as in RCA1 (18.5 MPa), RCA can be used even in the mixture at a ratio of 75%.
- 19 April 2021
- Published by Taylor & Francis in International Journal of Pavement Engineering
- Vol. 23 (11) , 3729-3742
Performance of granular road base and sub-base layers containing recycled concrete aggregate in different ratios
In this study, the usability and performance properties of recycled concrete aggregates (RCA) as granular road base (GRB) and granular road subbase (GRSB) material were investigated. A natural aggregate and the RCAs obtained from concretes with three different compressive strength and mixtures created by adding the RCAs to NA at the ratios of 25, 50 and 75% were used. Physical properties, modified Proctor, resilient modulus, permanent deformation, California bearing ratio (CBR), and permeability tests were carried out on all mixtures. Resilient modulus values (Mr) were obtained using three different resilient modulus models. The highest Mr value among pure RCAs was observed for RCA2 (average of 200 MPa). For the mixture samples, the highest Mr values were obtained in the mixtures containing RCA1 (average of 250 MPa). The minimum of permanent deformation value (ϵp) for the mixtures was obtained when the ratio of the RCA1 in the mixtures was 50% (ϵp = 0.238%). The obtained CBR values were not related to the Mr values, and the highest CBR values were found for the pure RCAs (average of 126%). High permeability coefficient values (average of 9.973×10−6 m/s) were obtained for the RCAs. As a result, it was more appropriate to blend the RCAs with the natural material rather than to use them in pure form. In general, it was appropriate to use 50% of RCAs in the mixtures. It was observed that if concrete compressive strength is as high as in RCA1 (18.5 MPa), RCA can be used even in the mixture at a ratio of 75%.