Miftakhur Rohmah
Miftakhur Rohmah has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
Dedi Irawan
Research Center for Metallurgy, National Research and Innovation Agency, KST BJ Habibie, South Tangerang, Banten, 15314, Indonesia
3 shared publications- Efendi Mabruri
Department of Materials, Physics and Energy Engineering, Graduate School of Engineering, Nagoya University
3 shared publications Dedi Pria Utama
Research Center for Metallurgy, National Research and Innovation Agency
2 shared publications- Dedi Pria Utama
Research Center for Metallurgy, National Research and Innovation Agency (BRIN), South Tangerang 15314, Indonesia
2 shared publications - Rahadian Roberto
Research Center for Metallurgy, National Research and Innovation Agency (BRIN), South Tangerang 15314, Indonesia
2 shared publications - Sigit Dwi Yudanto
National Research and Innovation Agency, Indonesia
2 shared publications
Latest Publications
- 1 December 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (12) , 125917
Mechanical properties and corrosion resistance of tungsten-containing FeNiCoCr high-entropy alloys
Face-centered cubic (FCC) high entropy alloys (HEAs) have attracted research interest due to their superior strength, flexibility, and irradiation resistance. However, FCC HEAs have low yield strength, limiting their practical applications. Adding W to HEAs is expected to improve their mechanical properties. Tungsten enhances many strengthening mechanisms, including solid solution, precipitation ( μ , σ phases), and grain refinement. In addition to improving mechanical properties, the addition of W improves corrosion resistance by forming a dense WO 3 film layer on the alloy surface. This study examined the effects of W addition in FeNiCoCrW x ( x = 0, 0.3, 0.6, 1 at.%) FCC HEAs from three perspectives: microstructure, mechanical properties, and corrosion resistance. Increased W in as-cast FeNiCoCrW x alloys resulted in rounded dendritic grains with increased interdendritic areas due to W atom segregation during solidification. The ultimate tensile strength of FeNiCoCrW 0.6 (1171 MPa) was lower than that of FeNiCoCrW 1 (1714.62 MPa) without loss of elasticity (40.8%). The open circuit potential (OCP) values of FeNiCoCr and FeNiCoCrW 0.3 are 66.36 and 66.32 mV, respectively. These values are lower than those of the other alloys, indicating better corrosion resistance.
- 1 December 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (12) , 125917
Mechanical properties and corrosion resistance of tungsten-containing FeNiCoCr high-entropy alloys
Face-centered cubic (FCC) high entropy alloys (HEAs) have attracted research interest due to their superior strength, flexibility, and irradiation resistance. However, FCC HEAs have low yield strength, limiting their practical applications. Adding W to HEAs is expected to improve their mechanical properties. Tungsten enhances many strengthening mechanisms, including solid solution, precipitation ( μ , σ phases), and grain refinement. In addition to improving mechanical properties, the addition of W improves corrosion resistance by forming a dense WO 3 film layer on the alloy surface. This study examined the effects of W addition in FeNiCoCrW x ( x = 0, 0.3, 0.6, 1 at.%) FCC HEAs from three perspectives: microstructure, mechanical properties, and corrosion resistance. Increased W in as-cast FeNiCoCrW x alloys resulted in rounded dendritic grains with increased interdendritic areas due to W atom segregation during solidification. The ultimate tensile strength of FeNiCoCrW 0.6 (1171 MPa) was lower than that of FeNiCoCrW 1 (1714.62 MPa) without loss of elasticity (40.8%). The open circuit potential (OCP) values of FeNiCoCr and FeNiCoCrW 0.3 are 66.36 and 66.32 mV, respectively. These values are lower than those of the other alloys, indicating better corrosion resistance.
- 1 November 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (11) , 115939
The influence of carbon level on mechanical properties, microstructure, and shape memory effect of Fe-14Mn-4Si-8Ni-10Cr-xC steel at large pre-strain
The chemical composition of Fe-Mn-Si shape memory steel continues to be optimized by researchers since Sato and colleagues first reported its shape memory effect in 1982. This work aimed to elucidate the effect of carbon content on the shape memory effect of Fe-14Mn-4Si-8Ni-10Cr steel subjected to a large pre-strain. The shape memory steels were prepared through a process involving melting, hot rolling, cold drawing, and subsequent solution treatment. The recovery strain was measured in solution-treated steels after a large pre-strain of 36% applied via tensile testing, followed by recovery heating at 600 °C. The results indicated that adding carbon up to approximately 0.22 wt% has a beneficial effect on shape recovery strain; further carbon addition to 0.39 wt% degraded the shape memory effect. The maximum recovery strain of 5.72% was exhibited by the steel containing 0.22 wt% carbon. Notably, the recovery strain of the Fe-14Mn-4Si-8Ni-10Cr-xC shape memory steel tested at a large pre-strain of 36% showed values comparable to those tested at lower pre-strains up to 17% for similar steels reported in the literature.
- 1 November 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (11) , 115939
The influence of carbon level on mechanical properties, microstructure, and shape memory effect of Fe-14Mn-4Si-8Ni-10Cr-xC steel at large pre-strain
The chemical composition of Fe-Mn-Si shape memory steel continues to be optimized by researchers since Sato and colleagues first reported its shape memory effect in 1982. This work aimed to elucidate the effect of carbon content on the shape memory effect of Fe-14Mn-4Si-8Ni-10Cr steel subjected to a large pre-strain. The shape memory steels were prepared through a process involving melting, hot rolling, cold drawing, and subsequent solution treatment. The recovery strain was measured in solution-treated steels after a large pre-strain of 36% applied via tensile testing, followed by recovery heating at 600 °C. The results indicated that adding carbon up to approximately 0.22 wt% has a beneficial effect on shape recovery strain; further carbon addition to 0.39 wt% degraded the shape memory effect. The maximum recovery strain of 5.72% was exhibited by the steel containing 0.22 wt% carbon. Notably, the recovery strain of the Fe-14Mn-4Si-8Ni-10Cr-xC shape memory steel tested at a large pre-strain of 36% showed values comparable to those tested at lower pre-strains up to 17% for similar steels reported in the literature.
- Open Access
- 9 October 2023
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 38 (2) , 57-64
EFFECT OF HOT ROLLING AND SOLUTION TREATMENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FE-MN-SI-CR-NI SHAPE MEMORY ALLOY
Fe-14Mn-4Si-8Ni-11Cr SMA (shape memory alloy) was designed as a smart material because of its specific properties, which can memorize the original shape, so it has the potential to dampen vibration in seismic structures. Memory effect is triggered by SIM (stress-induced martensitic) transformation from γ-austenite to ε-martensite (hexagonal close-packed / HCP) structure, and it is recovered by heating after unloading. This study investigated the effect of hot rolling and solution treatment on the microstructure and its relationship with hardness and SME (shape memory effect) properties. The as cast of Fe-14Mn-4Si-8Ni-11Cr was hot rolled (900 and 1000 ℃) and solution treated (1000 and 1100 ℃). After the thermomechanical process, all microstructures consist of γ-FCC (face-centered cubic), the annealing twins, and a fine band of ε-martensite. The grain size of the γ-phase is 29.43, 41.96, 42.44, and 45.57 μm for samples B, C, D, and E, respectively. The higher the temperature of hot rolling and solution treatment applied, the larger the grain size obtained, indirectly reducing the hardness to 299.93 BHN and 286.52 BHN for samples D and E. The coarsened austenite grain, a lower number of annealing twins, and the pre-existing line band of ε-martensite are favorable to obtain the enormous recovery strain, up to 8.26% for sample E.
- 9 October 2023
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 38 (2) , 57-64
Open AccessEFFECT OF HOT ROLLING AND SOLUTION TREATMENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FE-MN-SI-CR-NI SHAPE MEMORY ALLOY
Fe-14Mn-4Si-8Ni-11Cr SMA (shape memory alloy) was designed as a smart material because of its specific properties, which can memorize the original shape, so it has the potential to dampen vibration in seismic structures. Memory effect is triggered by SIM (stress-induced martensitic) transformation from γ-austenite to ε-martensite (hexagonal close-packed / HCP) structure, and it is recovered by heating after unloading. This study investigated the effect of hot rolling and solution treatment on the microstructure and its relationship with hardness and SME (shape memory effect) properties. The as cast of Fe-14Mn-4Si-8Ni-11Cr was hot rolled (900 and 1000 ℃) and solution treated (1000 and 1100 ℃). After the thermomechanical process, all microstructures consist of γ-FCC (face-centered cubic), the annealing twins, and a fine band of ε-martensite. The grain size of the γ-phase is 29.43, 41.96, 42.44, and 45.57 μm for samples B, C, D, and E, respectively. The higher the temperature of hot rolling and solution treatment applied, the larger the grain size obtained, indirectly reducing the hardness to 299.93 BHN and 286.52 BHN for samples D and E. The coarsened austenite grain, a lower number of annealing twins, and the pre-existing line band of ε-martensite are favorable to obtain the enormous recovery strain, up to 8.26% for sample E.
- Open Access
- 30 December 2022
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 37 (3)
EFFECT NICKEL AND QUENCH-TEMPER PROCESS ON MECHANICAL AND CORROSION PROPERTIES OF ASTM A588 WAETHERING STEEL
The mechanical improvement and "self-protection" properties are mainly needed to develop weather-resistant steel materials. In this study, A588 steel was given thermomechanical treatment (hot-rolling) followed by a quench-tempering process. The A588 is modified by adding 1, 2, and 3 wt% nickel to the primary alloy. Steel is made using a hot rolling process at 750 ℃ for 1 hour with 70% thickness reduction. The sample is heat-treated at 850 ℃ for 1 hour and quenched in water, oil, and open air. The tempering process is conducted at 400 ℃ for 30 minutes. Metallography test is confirmed final microstructural and compared with CCT simulation result. The fast cooling (water and oil quenchant) produces tempered martensite, ferrite, and pearlite, while the air-cooled forms a ferrite-pearlite. The cooling rate significantly affects strength and hardness and the nickel addition on hardness, and both factors have no significant on ductility. The sample owns the highest tensile strength value (~1226 MPa) with 1 %Ni, and the highest ductility value (around 17.1–27.43%) is obtained by air cooling. With 3% Ni, the corrosion rate decreases to 0072 mpy with -432.5 mV for corrosion potential and 0.12µA/cm-2 for current density.
- 30 December 2022
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 37 (3)
Open AccessEFFECT NICKEL AND QUENCH-TEMPER PROCESS ON MECHANICAL AND CORROSION PROPERTIES OF ASTM A588 WAETHERING STEEL
The mechanical improvement and "self-protection" properties are mainly needed to develop weather-resistant steel materials. In this study, A588 steel was given thermomechanical treatment (hot-rolling) followed by a quench-tempering process. The A588 is modified by adding 1, 2, and 3 wt% nickel to the primary alloy. Steel is made using a hot rolling process at 750 ℃ for 1 hour with 70% thickness reduction. The sample is heat-treated at 850 ℃ for 1 hour and quenched in water, oil, and open air. The tempering process is conducted at 400 ℃ for 30 minutes. Metallography test is confirmed final microstructural and compared with CCT simulation result. The fast cooling (water and oil quenchant) produces tempered martensite, ferrite, and pearlite, while the air-cooled forms a ferrite-pearlite. The cooling rate significantly affects strength and hardness and the nickel addition on hardness, and both factors have no significant on ductility. The sample owns the highest tensile strength value (~1226 MPa) with 1 %Ni, and the highest ductility value (around 17.1–27.43%) is obtained by air cooling. With 3% Ni, the corrosion rate decreases to 0072 mpy with -432.5 mV for corrosion potential and 0.12µA/cm-2 for current density.
- Open Access
- 16 September 2021
- Published by Institute of Research and Community Services Diponegoro University (LPPM UNDIP) in Jurnal Kimia Sains dan Aplikasi
- Vol. 24 (7) , 236-243
Effectiveness and Isotherm Models of Lewatit Monoplus S-108 on Lithium Adsorption Process from Bledug Kuwu Brine with Continuous Flow
Sorption of a series of alkali metals (Ca, Mg, Li, and K) from Bledug Kuwu’s Brine into Lewatit MonoPlus S-108 resins has been studied. Bledug Kuwu’s Brine comprised 15.11 ppm Li, 179.91 ppm K, 72.01 ppm Ca, and 29.76 ppm Mg. The adsorption was carried out by varying pH of brine (4, 6, 8, and 10) and contact time (1, 2, and 4 hours) with continuous flow in column test at room temperature. The result showed the quantity adsorbate in outer resin: K>Li>Ca>Mg in all conditions, which is 0.038–0.043 mmol/g lithium, 0.087–0.09 mmol/g potassium, 0.031–0.035 mmol/g calcium, and 0.023–0.024 mmol/g magnesium into outer resin surface. The selectivity factor to lithium followed Mg/Li > K/Li> Ca/Li in all conditions. Contact time variable provided high lithium separation after the adsorption process for 2–3 hours, while pH had little effect. FTIR results affirm that resin was changed at new peaks M-O-M at low wavenumber with polystyrene crosslinked-divinylbenzene matrix and contains the sulfonic type. The results obtained from ICP were fitted to isotherm models in ion exchange, as follows: Langmuir, Freundlich, Temkin, and Dubinin-Radushkevic models. The best model of lithium adsorption into Lewatit S-108 is represented by Freundlich and Temkin Model (R2 ≥ 0.82) with 1.0056 mg/g of adsorption capacity (Kf) and 64.885 J/mol of heat process of sorption.
- 16 September 2021
- Published by Institute of Research and Community Services Diponegoro University (LPPM UNDIP) in Jurnal Kimia Sains dan Aplikasi
- Vol. 24 (7) , 236-243
Open AccessEffectiveness and Isotherm Models of Lewatit Monoplus S-108 on Lithium Adsorption Process from Bledug Kuwu Brine with Continuous Flow
Sorption of a series of alkali metals (Ca, Mg, Li, and K) from Bledug Kuwu’s Brine into Lewatit MonoPlus S-108 resins has been studied. Bledug Kuwu’s Brine comprised 15.11 ppm Li, 179.91 ppm K, 72.01 ppm Ca, and 29.76 ppm Mg. The adsorption was carried out by varying pH of brine (4, 6, 8, and 10) and contact time (1, 2, and 4 hours) with continuous flow in column test at room temperature. The result showed the quantity adsorbate in outer resin: K>Li>Ca>Mg in all conditions, which is 0.038–0.043 mmol/g lithium, 0.087–0.09 mmol/g potassium, 0.031–0.035 mmol/g calcium, and 0.023–0.024 mmol/g magnesium into outer resin surface. The selectivity factor to lithium followed Mg/Li > K/Li> Ca/Li in all conditions. Contact time variable provided high lithium separation after the adsorption process for 2–3 hours, while pH had little effect. FTIR results affirm that resin was changed at new peaks M-O-M at low wavenumber with polystyrene crosslinked-divinylbenzene matrix and contains the sulfonic type. The results obtained from ICP were fitted to isotherm models in ion exchange, as follows: Langmuir, Freundlich, Temkin, and Dubinin-Radushkevic models. The best model of lithium adsorption into Lewatit S-108 is represented by Freundlich and Temkin Model (R2 ≥ 0.82) with 1.0056 mg/g of adsorption capacity (Kf) and 64.885 J/mol of heat process of sorption.
- Open Access
- 10 July 2021
- Published by Institute of Research and Community Services Diponegoro University (LPPM UNDIP) in Teknik
- Vol. 42 (2) , 149-159
The development of a588 modified laterite steel using thermomechanical and low-temperature tempering process for weather resistant steel
Laterite Steel A-588 has the potential to be a high strength low alloy for Corten steel application. Laterite steel A-588 is developed through a thermomechanical process followed by a tempering process to obtain high strength and corrosion resistance. This study aims to determine the correlation between the addition of nickel content, the variation of the cooling rate during heat treatment to the mechanical properties, and the corrosion resistance of A-588 laterite steel. The Cu, Cr, Ni, P, and Si elements significantly impact microstructure transformation. Laterite Steel A-588 with nickel and thermo-mechanical process variation has been focused on in this research. Laterite steel with 0,42%, 1%, 2%, and 3% nickel varied was homogenized, hot rolled, and heat treated with three cooling variations by water, oil, and air. They are processed with 150 C tempering. Low tempering temperature caused fine carbide precipitation and phase transition of martensite to bainite. This resulted in bainite as the final microstructure, lath tempered martensite, carbide, and ferrite. 3% Ni with a fast cooling rate increased the tempered martensite and bainite phase formation. It allowed the strength and hardness to increase relatively, followed by decreased elongation and corrosion resistance caused by the galvanic reaction. Most optimal of mechanical properties determined at a sample with 2% nickel in a water medium (strength 1203 MPa, elongation 10%, hardness 404 BHN, corrosion rate 1,306 mpy).
- 10 July 2021
- Published by Institute of Research and Community Services Diponegoro University (LPPM UNDIP) in Teknik
- Vol. 42 (2) , 149-159
Open AccessThe development of a588 modified laterite steel using thermomechanical and low-temperature tempering process for weather resistant steel
Laterite Steel A-588 has the potential to be a high strength low alloy for Corten steel application. Laterite steel A-588 is developed through a thermomechanical process followed by a tempering process to obtain high strength and corrosion resistance. This study aims to determine the correlation between the addition of nickel content, the variation of the cooling rate during heat treatment to the mechanical properties, and the corrosion resistance of A-588 laterite steel. The Cu, Cr, Ni, P, and Si elements significantly impact microstructure transformation. Laterite Steel A-588 with nickel and thermo-mechanical process variation has been focused on in this research. Laterite steel with 0,42%, 1%, 2%, and 3% nickel varied was homogenized, hot rolled, and heat treated with three cooling variations by water, oil, and air. They are processed with 150 C tempering. Low tempering temperature caused fine carbide precipitation and phase transition of martensite to bainite. This resulted in bainite as the final microstructure, lath tempered martensite, carbide, and ferrite. 3% Ni with a fast cooling rate increased the tempered martensite and bainite phase formation. It allowed the strength and hardness to increase relatively, followed by decreased elongation and corrosion resistance caused by the galvanic reaction. Most optimal of mechanical properties determined at a sample with 2% nickel in a water medium (strength 1203 MPa, elongation 10%, hardness 404 BHN, corrosion rate 1,306 mpy).
- Open Access
- 29 April 2021
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 36 (1) , 33-42
PENGARUH PENEMPAAN DAN PERLAKUAN PANAS TERHADAP SIFAT MEKANIK DAN KETAHANAN KOROSI PADA MODIFIKASI BAJA LATERIT A-588
High strength low alloy (HSLA) yang diaplikasikan menjadi baja tahan cuaca merupakan terobosan terbaru untuk menghasilkan sifat mekanik dan ketahanan korosi yang tinggi. Modifikasi Baja Laterit dengan penambahan kadar nikel yang diterapkan proses termomekanikal (TMCP) berupa kombinasi proses penempaan panas dan perlakuan panas menjadi fokusan penelitian ini. Sampel yang digunakan merupakan Baja Laterit A-588 hasil investment casting yang telah ditambahkan kadar nikel sebesar 1, 2, dan 3% kemudian diproses penempaan panas dengan pembebanan 100 ton pada temperatur 1050 ℃. Nikel berfungsi sebagai penstabil austenit. Variabel perlakuan panas yang digunakan yakni (1) langsung pendinginan udara, (2) dilanjutkan proses pemanasan pada temperatur 750 ℃ yang diikuti pendinginan cepat. Karakterisasi material menggunakan uji metalografi, uji keras, uji tarik, dan uji polarisasi. Pada sampel tempa panas+pendinginan udara, pertambahan kadar nikel hingga 3% mempengaruhi nilai fraksi fasa ferrit-perlit yang terbentuk, pertambahan ukuran butir hingga ±0,1 mm, penurunan kekerasan hingga 185,22 BHN, penurunan kekuatan hingga 554 MPa, dan pertambahkan elongasi sebesar 29.1%. Sedangkan pada sampel tempa panas+perlakuan panas dengan pendinginan air, pertambahan nikel hingga 3% menyebabkan terbentuknya fasa dislokasi lath martensit+ferrit+retained austenite, penurunan kekerasan hingga 236,18 BHN, penurunan kekuatan hingga 852 MPa, penurunan elongasi hingga 24,7%. Fasa retained austenite memiliki efek merusak pada sifat mekanis.
- 29 April 2021
- Published by National Research and Innovation Agency in Metalurgi
- Vol. 36 (1) , 33-42
Open AccessPENGARUH PENEMPAAN DAN PERLAKUAN PANAS TERHADAP SIFAT MEKANIK DAN KETAHANAN KOROSI PADA MODIFIKASI BAJA LATERIT A-588
High strength low alloy (HSLA) yang diaplikasikan menjadi baja tahan cuaca merupakan terobosan terbaru untuk menghasilkan sifat mekanik dan ketahanan korosi yang tinggi. Modifikasi Baja Laterit dengan penambahan kadar nikel yang diterapkan proses termomekanikal (TMCP) berupa kombinasi proses penempaan panas dan perlakuan panas menjadi fokusan penelitian ini. Sampel yang digunakan merupakan Baja Laterit A-588 hasil investment casting yang telah ditambahkan kadar nikel sebesar 1, 2, dan 3% kemudian diproses penempaan panas dengan pembebanan 100 ton pada temperatur 1050 ℃. Nikel berfungsi sebagai penstabil austenit. Variabel perlakuan panas yang digunakan yakni (1) langsung pendinginan udara, (2) dilanjutkan proses pemanasan pada temperatur 750 ℃ yang diikuti pendinginan cepat. Karakterisasi material menggunakan uji metalografi, uji keras, uji tarik, dan uji polarisasi. Pada sampel tempa panas+pendinginan udara, pertambahan kadar nikel hingga 3% mempengaruhi nilai fraksi fasa ferrit-perlit yang terbentuk, pertambahan ukuran butir hingga ±0,1 mm, penurunan kekerasan hingga 185,22 BHN, penurunan kekuatan hingga 554 MPa, dan pertambahkan elongasi sebesar 29.1%. Sedangkan pada sampel tempa panas+perlakuan panas dengan pendinginan air, pertambahan nikel hingga 3% menyebabkan terbentuknya fasa dislokasi lath martensit+ferrit+retained austenite, penurunan kekerasan hingga 236,18 BHN, penurunan kekuatan hingga 852 MPa, penurunan elongasi hingga 24,7%. Fasa retained austenite memiliki efek merusak pada sifat mekanis.