Dedi Pria Utama
Research Subjects
Dedi Pria Utama has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
- Efendi Mabruri
Department of Materials, Physics and Energy Engineering, Graduate School of Engineering, Nagoya University
2 shared publications - Miftakhur Rohmah
Research Center for Metallurgy, National Research and Innovation Agency (BRIN), South Tangerang 15314, Indonesia
2 shared publications - Rahadian Roberto
Research Center for Metallurgy, National Research and Innovation Agency (BRIN), South Tangerang 15314, Indonesia
2 shared publications - Sigit Dwi Yudanto
National Research and Innovation Agency, Indonesia
2 shared publications Bintang Adjiantoro
Research Center for Metallurgy, National Research and Innovation Agency, KST BJ Habibie, South Tangerang, Banten, 15314, Indonesia
1 shared publicationDedi Irawan
Research Center for Metallurgy, National Research and Innovation Agency, KST BJ Habibie, South Tangerang, Banten, 15314, Indonesia
1 shared publication
Latest Publications
- 1 December 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (12) , 125917
Mechanical properties and corrosion resistance of tungsten-containing FeNiCoCr high-entropy alloys
Face-centered cubic (FCC) high entropy alloys (HEAs) have attracted research interest due to their superior strength, flexibility, and irradiation resistance. However, FCC HEAs have low yield strength, limiting their practical applications. Adding W to HEAs is expected to improve their mechanical properties. Tungsten enhances many strengthening mechanisms, including solid solution, precipitation ( μ , σ phases), and grain refinement. In addition to improving mechanical properties, the addition of W improves corrosion resistance by forming a dense WO 3 film layer on the alloy surface. This study examined the effects of W addition in FeNiCoCrW x ( x = 0, 0.3, 0.6, 1 at.%) FCC HEAs from three perspectives: microstructure, mechanical properties, and corrosion resistance. Increased W in as-cast FeNiCoCrW x alloys resulted in rounded dendritic grains with increased interdendritic areas due to W atom segregation during solidification. The ultimate tensile strength of FeNiCoCrW 0.6 (1171 MPa) was lower than that of FeNiCoCrW 1 (1714.62 MPa) without loss of elasticity (40.8%). The open circuit potential (OCP) values of FeNiCoCr and FeNiCoCrW 0.3 are 66.36 and 66.32 mV, respectively. These values are lower than those of the other alloys, indicating better corrosion resistance.
- 1 December 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (12) , 125917
Mechanical properties and corrosion resistance of tungsten-containing FeNiCoCr high-entropy alloys
Face-centered cubic (FCC) high entropy alloys (HEAs) have attracted research interest due to their superior strength, flexibility, and irradiation resistance. However, FCC HEAs have low yield strength, limiting their practical applications. Adding W to HEAs is expected to improve their mechanical properties. Tungsten enhances many strengthening mechanisms, including solid solution, precipitation ( μ , σ phases), and grain refinement. In addition to improving mechanical properties, the addition of W improves corrosion resistance by forming a dense WO 3 film layer on the alloy surface. This study examined the effects of W addition in FeNiCoCrW x ( x = 0, 0.3, 0.6, 1 at.%) FCC HEAs from three perspectives: microstructure, mechanical properties, and corrosion resistance. Increased W in as-cast FeNiCoCrW x alloys resulted in rounded dendritic grains with increased interdendritic areas due to W atom segregation during solidification. The ultimate tensile strength of FeNiCoCrW 0.6 (1171 MPa) was lower than that of FeNiCoCrW 1 (1714.62 MPa) without loss of elasticity (40.8%). The open circuit potential (OCP) values of FeNiCoCr and FeNiCoCrW 0.3 are 66.36 and 66.32 mV, respectively. These values are lower than those of the other alloys, indicating better corrosion resistance.
- 1 November 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (11) , 115939
The influence of carbon level on mechanical properties, microstructure, and shape memory effect of Fe-14Mn-4Si-8Ni-10Cr-xC steel at large pre-strain
The chemical composition of Fe-Mn-Si shape memory steel continues to be optimized by researchers since Sato and colleagues first reported its shape memory effect in 1982. This work aimed to elucidate the effect of carbon content on the shape memory effect of Fe-14Mn-4Si-8Ni-10Cr steel subjected to a large pre-strain. The shape memory steels were prepared through a process involving melting, hot rolling, cold drawing, and subsequent solution treatment. The recovery strain was measured in solution-treated steels after a large pre-strain of 36% applied via tensile testing, followed by recovery heating at 600 °C. The results indicated that adding carbon up to approximately 0.22 wt% has a beneficial effect on shape recovery strain; further carbon addition to 0.39 wt% degraded the shape memory effect. The maximum recovery strain of 5.72% was exhibited by the steel containing 0.22 wt% carbon. Notably, the recovery strain of the Fe-14Mn-4Si-8Ni-10Cr-xC shape memory steel tested at a large pre-strain of 36% showed values comparable to those tested at lower pre-strains up to 17% for similar steels reported in the literature.
- 1 November 2025
- Published by IOP Publishing in Physica Scripta
- Vol. 100 (11) , 115939
The influence of carbon level on mechanical properties, microstructure, and shape memory effect of Fe-14Mn-4Si-8Ni-10Cr-xC steel at large pre-strain
The chemical composition of Fe-Mn-Si shape memory steel continues to be optimized by researchers since Sato and colleagues first reported its shape memory effect in 1982. This work aimed to elucidate the effect of carbon content on the shape memory effect of Fe-14Mn-4Si-8Ni-10Cr steel subjected to a large pre-strain. The shape memory steels were prepared through a process involving melting, hot rolling, cold drawing, and subsequent solution treatment. The recovery strain was measured in solution-treated steels after a large pre-strain of 36% applied via tensile testing, followed by recovery heating at 600 °C. The results indicated that adding carbon up to approximately 0.22 wt% has a beneficial effect on shape recovery strain; further carbon addition to 0.39 wt% degraded the shape memory effect. The maximum recovery strain of 5.72% was exhibited by the steel containing 0.22 wt% carbon. Notably, the recovery strain of the Fe-14Mn-4Si-8Ni-10Cr-xC shape memory steel tested at a large pre-strain of 36% showed values comparable to those tested at lower pre-strains up to 17% for similar steels reported in the literature.