Pavlo Barvitskyi
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Pavlo Barvitskyi has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
- Tatiana A. Prikhna
V. Bakul Institute for Superhard Materials of the National Academy of Sciences of Ukraine
3 shared publications - Anastasiia Lokatkina
V. Bakul Institute for Superhard Materials of National Academy of Sciences of Ukraine
2 shared publications - Leonid Devin
Bakul Institute for Superhard Materials, National Academy of Sciences of Ukraine, 04074, Kyiv, Ukraine
2 shared publications - Richard A. Haber
Department of Material Science and Engineering, Rutgers, The State University of New Jersey, Piscataway, NJ 08854, United States of America
2 shared publications - Viktor E. Moshchil
V. Bakul Institute for Superhard Materials, National Academy of Sciences of Ukraine, Kyiv, Ukraine
2 shared publications A.V. Maznaya
Institute for Problems in Material Science, NAS Ukraine, 3 Krzhizhanovsky Str., 03680 Kiev, Ukraine
1 shared publication
Latest Publications
- 28 September 2026
- Published by Trans Tech Publications, Ltd. in Advances in Science and Technology
- Vol. 182, 489-498
Composite Materials in the “Epoxy Resin – Magnetite” System for Protection against Microwave Radiation from Domestic and Industrial Sources
The article presents data on the use of epoxy resin as a matrix for creating composite materials with magnetite powder to protect against microwave radiation from domestic and industrial sources. It is shown that epoxy resin, with average reflection values at certain frequencies, contributes to a sharp decrease in reflection (up to -40 dB), and the real part of permeability lies within 2.7 units, the imaginary part is minimal, and magnetic permeability is absent. With a content of 15% and 45% magnetite in the composite material, the reflection of microwave radiation at points of wavelength and sample multiplicity decreases to -30...-20 dB, and the real part of the permeability is 3.25...4 units. With a magnetite powder content of 30% and 60%, sharp jumps in both dielectric and magnetic permeability we observed, which are associated with the uneven distribution of the filler throughout the matrix volume. The values of the real and imaginary parts of the dielectric permeability after approximation are more or less acceptable, but the value of the magnetic permeability they cannot processed mathematically and the microwave radiation reflection is within the range of -27...-22 dB.
- 28 September 2026
- Published by Trans Tech Publications, Ltd. in Advances in Science and Technology
- Vol. 182, 489-498
Composite Materials in the “Epoxy Resin – Magnetite” System for Protection against Microwave Radiation from Domestic and Industrial Sources
The article presents data on the use of epoxy resin as a matrix for creating composite materials with magnetite powder to protect against microwave radiation from domestic and industrial sources. It is shown that epoxy resin, with average reflection values at certain frequencies, contributes to a sharp decrease in reflection (up to -40 dB), and the real part of permeability lies within 2.7 units, the imaginary part is minimal, and magnetic permeability is absent. With a content of 15% and 45% magnetite in the composite material, the reflection of microwave radiation at points of wavelength and sample multiplicity decreases to -30...-20 dB, and the real part of the permeability is 3.25...4 units. With a magnetite powder content of 30% and 60%, sharp jumps in both dielectric and magnetic permeability we observed, which are associated with the uneven distribution of the filler throughout the matrix volume. The values of the real and imaginary parts of the dielectric permeability after approximation are more or less acceptable, but the value of the magnetic permeability they cannot processed mathematically and the microwave radiation reflection is within the range of -27...-22 dB.
- 1 January 2025
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications)
- p. 217-218
Influence of SiC Quality on the Mechanical Properties and Oxidation Resistance of Ultra-High Temperature Composites Based on HfB₂–Si Cobtained by Hot Pressing
The effect of SiC content and powder characteristics on HfB₂–SiC composites was studied. The best composite (HfB₂ + 30 wt.% SiC, 5-10 μm) showed high density (6.54 g/cm3), hardness (Hv = 38.6 GPa), fracture toughness (K1с = 7.7 MPa·m⁰·⁵), and Young’s modulus (510 GPa). Ablation tests revealed superior thermal stability compared to pure HfB₂ and composites with finer or differently shaped SiC powders. Enhanced performance is due to optimal SiC morphology, solid solution formation, and uniform phase distribution.
- 1 January 2025
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications)
- p. 217-218
Influence of SiC Quality on the Mechanical Properties and Oxidation Resistance of Ultra-High Temperature Composites Based on HfB₂–Si Cobtained by Hot Pressing
The effect of SiC content and powder characteristics on HfB₂–SiC composites was studied. The best composite (HfB₂ + 30 wt.% SiC, 5-10 μm) showed high density (6.54 g/cm3), hardness (Hv = 38.6 GPa), fracture toughness (K1с = 7.7 MPa·m⁰·⁵), and Young’s modulus (510 GPa). Ablation tests revealed superior thermal stability compared to pure HfB₂ and composites with finer or differently shaped SiC powders. Enhanced performance is due to optimal SiC morphology, solid solution formation, and uniform phase distribution.
- Open Access
- 30 April 2021
- Published by Private Company Technology Center in Technology audit and production reserves
- Vol. 2 (1(58)) , 21-25
Influence of heating to high temperatures on mechanical properties of boride-based refractory materials
The object of research is HfB2, ZrB2 and ceramics composition HfB2-30 % SiC and ZrB2-20 % SiC, ZrB2-20 % SiC-4 % Si3N4 obtained under high pressure, their mechanical characteristics before and after heating to high temperatures and temperatures of beginning of melting. The research was conducted in order to create new effective refractory materials for use in the aerospace industry. Therefore, the melting temperatures of sintered materials and the effect of heating on their mechanical properties were also studied. Additives (ZrB2-20 % SiC and HfB2-30 % SiC) although led to a decrease in specific gravity. But increased hardness (by 17 % and 46 % in the case of ZrB2 and HfB2, respectively) and fracture toughness (by 40 % and 21 % in the case of ZrB2 and HfB2, respectively). However, significantly reduced the onset of melting temperature in vacuum to 2150–2160 °C. Materials sintered from ZrB2 and HfB2 was not melted after heating to 2970 °C. After heating to a melting point of 2150–2160 °C (in the case of materials with additives) and to temperatures of 2970 °C (in the case of materials sintered with ZrB2 or HfB2), the hardness and fracture toughness decreased. Thus, the hardness of the material prepared from ZrB2 decreased by 19 % and its fracture toughness – by 18 %, and of that prepared from ZrB2–20 % SiC – by 46 % and 32 %, respectively. The hardness of the material prepared from HfB2 decreased by 46 %, its fracture toughness – by 55 %, and of that prepared from HfB2-30 % SiC, after heating decreased by 40 %, but its fracture toughness increased by 15 %. The sintered HfB2 (with a density of 10.4 g/cm3) before heating showed a hardness of HV(9.8 N)=21.27±0.84 GPa, HV(49 N)=19.29±1.34 and HV(98 N)=19.17±0.5, and fracture toughness K1C(9.8 N)=0.47 MH·m0.5, and ZrB2 with a density of 6.2 g/cm3 was characterized by HV(9.8 N)=17.66±0.60 GPa, HV(49 N)=15.25±1.22 GPa and HV(98 N)=15.32±0.36 GPa, K1C(9.8 N)=4.3 MH·m0.5. Material sintered with HfB2-30 % SiC (density 6.21 g/cm3) had Hv(9.8 N)=38.1±1.4 GPa, HV(49 N)=27.7±2.8 GPa, and K1C(9.8 N)=8.1 MH·m0.5, K1C(49 H)=6.8 MH·m0.5. The sintered with ZrB2-20 % SiC material had density of 5.04 g/cm3, HV(9.8 N)=24.2±1.9 GPa, HV(49 N)=16.7±2.8 GPa, K1C(49 H)=7.1 MH·m0.5. The SiC addition to the initial mixture significantly reduces the elasticity of the materials.
- 30 April 2021
- Published by Private Company Technology Center in Technology audit and production reserves
- Vol. 2 (1(58)) , 21-25
Open AccessInfluence of heating to high temperatures on mechanical properties of boride-based refractory materials
The object of research is HfB2, ZrB2 and ceramics composition HfB2-30 % SiC and ZrB2-20 % SiC, ZrB2-20 % SiC-4 % Si3N4 obtained under high pressure, their mechanical characteristics before and after heating to high temperatures and temperatures of beginning of melting. The research was conducted in order to create new effective refractory materials for use in the aerospace industry. Therefore, the melting temperatures of sintered materials and the effect of heating on their mechanical properties were also studied. Additives (ZrB2-20 % SiC and HfB2-30 % SiC) although led to a decrease in specific gravity. But increased hardness (by 17 % and 46 % in the case of ZrB2 and HfB2, respectively) and fracture toughness (by 40 % and 21 % in the case of ZrB2 and HfB2, respectively). However, significantly reduced the onset of melting temperature in vacuum to 2150–2160 °C. Materials sintered from ZrB2 and HfB2 was not melted after heating to 2970 °C. After heating to a melting point of 2150–2160 °C (in the case of materials with additives) and to temperatures of 2970 °C (in the case of materials sintered with ZrB2 or HfB2), the hardness and fracture toughness decreased. Thus, the hardness of the material prepared from ZrB2 decreased by 19 % and its fracture toughness – by 18 %, and of that prepared from ZrB2–20 % SiC – by 46 % and 32 %, respectively. The hardness of the material prepared from HfB2 decreased by 46 %, its fracture toughness – by 55 %, and of that prepared from HfB2-30 % SiC, after heating decreased by 40 %, but its fracture toughness increased by 15 %. The sintered HfB2 (with a density of 10.4 g/cm3) before heating showed a hardness of HV(9.8 N)=21.27±0.84 GPa, HV(49 N)=19.29±1.34 and HV(98 N)=19.17±0.5, and fracture toughness K1C(9.8 N)=0.47 MH·m0.5, and ZrB2 with a density of 6.2 g/cm3 was characterized by HV(9.8 N)=17.66±0.60 GPa, HV(49 N)=15.25±1.22 GPa and HV(98 N)=15.32±0.36 GPa, K1C(9.8 N)=4.3 MH·m0.5. Material sintered with HfB2-30 % SiC (density 6.21 g/cm3) had Hv(9.8 N)=38.1±1.4 GPa, HV(49 N)=27.7±2.8 GPa, and K1C(9.8 N)=8.1 MH·m0.5, K1C(49 H)=6.8 MH·m0.5. The sintered with ZrB2-20 % SiC material had density of 5.04 g/cm3, HV(9.8 N)=24.2±1.9 GPa, HV(49 N)=16.7±2.8 GPa, K1C(49 H)=7.1 MH·m0.5. The SiC addition to the initial mixture significantly reduces the elasticity of the materials.
- 1 May 2019
- Published by Elsevier in Ceramics International
- Vol. 45 (7) , 9580-9588
Lightweight ceramics based on aluminum dodecaboride, boron carbide and self-bonded silicon carbide
- 1 May 2019
- Published by Elsevier in Ceramics International
- Vol. 45 (7) , 9580-9588
Lightweight ceramics based on aluminum dodecaboride, boron carbide and self-bonded silicon carbide