Kei Hattori
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Kei Hattori has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
Kensuke Demura
Shibaura Mechatronics Corporation, Fine Mechatronics Division, Yokohama, Japan
3 shared publicationsDaisuke Matsushima
Shibaura Mechatronics Corp
2 shared publicationsAtsuo Matsui
Department of Physics, Kōnan University
1 shared publicationF. Sato
Advanced Process Group, Process & Manufacturing Engineering Center, Toshiba Corporation Semiconductor Company, 3500, Matsuoka, Oita City, Oita 870-0197, Japan
1 shared publicationH. Iwai
Frontier Collaborative Research Center, Tokyo Institute of Technology, 4259, Nagatsuta, Midori-ku, Yokohama 226-8502, Japan
1 shared publicationHideaki Terakado
Shibaura Technology International Corp. (United States)
1 shared publication
Latest Publications
- Open Access
- 1 April 2025
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanopatterning, Materials, and Metrology
- Vol. 24 (02) , 024401-13
Rapid freeze-cleaning method for removing nanoparticles
As semiconductor devices become increasingly small and complex,1 – 3 the particles to be removed from photomasks and nanoimprint lithography (NIL) templates become progressively smaller. However, the velocity of the liquid flowing on the substrate surface decreases rapidly at the boundary layer in contact with the substrate and reaches zero at the substrate surface.4 In fluid mechanics, this is a well-known phenomenon that occurs in the boundary layer. Consequently, small particles are challenging to remove. The most typical cleaning methods used in semiconductor device manufacturing to remove nanoparticles smaller than 100 nm are chemical cleaning with chemical solutions and physical cleaning with megasonics or two-fluid sprays. However, these cleaning methods pose a risk of substrate damage. For example, chemical cleaning increases the possibility of optical characteristic variations and critical dimension (CD) shifts in the thin film formed on the substrate surface, whereas physical cleaning increases the risk of pattern collapse. Therefore, conventional cleaning methods involve a trade-off between reducing the size of the particles to be removed and minimizing substrate damage.5 To address this limitation, freeze cleaning—in which water expands in volume as it transitions from liquid to solid, thus weakening the adhesion force linking the particles to the substrate surface—could be a breakthrough cleaning technique for removing nanoparticles while minimizing damage to the substrate. In 2011, by simply freezing water, a particle removal efficiency (PRE) of was achieved for polystyrene latex (PSL) particles 100 nm in size.6- 1 April 2025
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanopatterning, Materials, and Metrology
- Vol. 24 (02) , 024401-13
Open AccessRapid freeze-cleaning method for removing nanoparticles
As semiconductor devices become increasingly small and complex,1 – 3 the particles to be removed from photomasks and nanoimprint lithography (NIL) templates become progressively smaller. However, the velocity of the liquid flowing on the substrate surface decreases rapidly at the boundary layer in contact with the substrate and reaches zero at the substrate surface.4 In fluid mechanics, this is a well-known phenomenon that occurs in the boundary layer. Consequently, small particles are challenging to remove. The most typical cleaning methods used in semiconductor device manufacturing to remove nanoparticles smaller than 100 nm are chemical cleaning with chemical solutions and physical cleaning with megasonics or two-fluid sprays. However, these cleaning methods pose a risk of substrate damage. For example, chemical cleaning increases the possibility of optical characteristic variations and critical dimension (CD) shifts in the thin film formed on the substrate surface, whereas physical cleaning increases the risk of pattern collapse. Therefore, conventional cleaning methods involve a trade-off between reducing the size of the particles to be removed and minimizing substrate damage.5 To address this limitation, freeze cleaning—in which water expands in volume as it transitions from liquid to solid, thus weakening the adhesion force linking the particles to the substrate surface—could be a breakthrough cleaning technique for removing nanoparticles while minimizing damage to the substrate. In 2011, by simply freezing water, a particle removal efficiency (PRE) of was achieved for polystyrene latex (PSL) particles 100 nm in size.6 - Open Access
- 1 October 2020
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanolithography, MEMS, and MOEMS
- Vol. 19 (04) , 044401-17
Particle and pattern discriminant freeze-cleaning method
In recent years, the performance of semiconductor devices has improved owing to improvements such as downscaling, introduction of three-dimensional (3D) structures and new materials, and circuit improvement.1 – 3 For the downscaling process, ArF-immersion (ArF-i) has a resolution limit of , but the minimum critical dimension (CD) of semiconductor devices is already smaller than that in 2012, but the subsequent downscaling of the devices has continued. Extreme ultraviolet (EUV) lithography was recently introduced with a resolution limit of for single patterning. Currently, the minimum size of semiconductor device is thought to be , so even if the EUV lithography technology is used, the minimum CD of the semiconductor devices is smaller than its limit. Downscaling can be realized using patterning techniques such as pattern splitting and self-aligned patterning on a wafer.4,5 Although requirements for a decrease in the photomask dimensions are reduced, fine patterning and cleaning processes exhibit significant performance demands.- 1 October 2020
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanolithography, MEMS, and MOEMS
- Vol. 19 (04) , 044401-17
Open AccessParticle and pattern discriminant freeze-cleaning method
In recent years, the performance of semiconductor devices has improved owing to improvements such as downscaling, introduction of three-dimensional (3D) structures and new materials, and circuit improvement.1 – 3 For the downscaling process, ArF-immersion (ArF-i) has a resolution limit of , but the minimum critical dimension (CD) of semiconductor devices is already smaller than that in 2012, but the subsequent downscaling of the devices has continued. Extreme ultraviolet (EUV) lithography was recently introduced with a resolution limit of for single patterning. Currently, the minimum size of semiconductor device is thought to be , so even if the EUV lithography technology is used, the minimum CD of the semiconductor devices is smaller than its limit. Downscaling can be realized using patterning techniques such as pattern splitting and self-aligned patterning on a wafer.4,5 Although requirements for a decrease in the photomask dimensions are reduced, fine patterning and cleaning processes exhibit significant performance demands. - 23 March 2020
- Published by SPIE-Intl Soc Optical Eng
- Vol. 11326, 23
Unique freeze cleaning technology
In this work, a novel chemical-free technique is proposed to remove adsorbed particles of less than 100 nm from a substrate. More specifically, the small particles buried under the "stagnant layer" were removed using a process that relied on the force generated by volumetric expansion on rapid freezing of supercooled water. In the process, water penetrated into the small (narrow) spaces via the capillary force; it then flowed into the narrow interfacial gap between the substrate and particles, and lifted the particles off the substrate via the volumetric expansion force on ice formation. Because fine patterns have no such gaps, they are not damaged during this process. In other words, unlike conventional cleaning technologies, such as mega sonic cleaning and two-fluid jet cleaning, this cleaning process is able to specifically target the small particles while the fine patterns are unaffected.
- 23 March 2020
- Published by SPIE-Intl Soc Optical Eng
- Vol. 11326, 23
Unique freeze cleaning technology
In this work, a novel chemical-free technique is proposed to remove adsorbed particles of less than 100 nm from a substrate. More specifically, the small particles buried under the "stagnant layer" were removed using a process that relied on the force generated by volumetric expansion on rapid freezing of supercooled water. In the process, water penetrated into the small (narrow) spaces via the capillary force; it then flowed into the narrow interfacial gap between the substrate and particles, and lifted the particles off the substrate via the volumetric expansion force on ice formation. Because fine patterns have no such gaps, they are not damaged during this process. In other words, unlike conventional cleaning technologies, such as mega sonic cleaning and two-fluid jet cleaning, this cleaning process is able to specifically target the small particles while the fine patterns are unaffected.
- 12 June 2018
- Published by SPIE-Intl Soc Optical Eng
- Vol. 10807, 22
Dry etching technologies for Cr film
We have investigated Cr film etching mechanism systematically in order to minimize CDU (CD Uniformity). As a result, employing our dry etching system ARESTM with optimized etch process we achieved an excellent CDU(3σ) (0.5nm with etch contribution). Cr film has been widely used not only for the light-shielding film at Cr Binary Mask but also as a hard mask film at even the leading edge photomasks (Hard Mask-PSM (Phase Shift Mask)). In case of used as a hard-mask, this plays very important role to determine etching process accuracy and to achieve the minimal CDU. As LSI downscaling and complication of their pattern layouts, the current dry etch technology faces technical challenges such as the difficulties in CD control and will be not sufficient to meet requirements. In this study, each behavior of Cr etching process at the various process parameters and various pattern layouts are investigated.
- 12 June 2018
- Published by SPIE-Intl Soc Optical Eng
- Vol. 10807, 22
Dry etching technologies for Cr film
We have investigated Cr film etching mechanism systematically in order to minimize CDU (CD Uniformity). As a result, employing our dry etching system ARESTM with optimized etch process we achieved an excellent CDU(3σ) (0.5nm with etch contribution). Cr film has been widely used not only for the light-shielding film at Cr Binary Mask but also as a hard mask film at even the leading edge photomasks (Hard Mask-PSM (Phase Shift Mask)). In case of used as a hard-mask, this plays very important role to determine etching process accuracy and to achieve the minimal CDU. As LSI downscaling and complication of their pattern layouts, the current dry etch technology faces technical challenges such as the difficulties in CD control and will be not sufficient to meet requirements. In this study, each behavior of Cr etching process at the various process parameters and various pattern layouts are investigated.
- 1 September 2003
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 21 (5) , 2163-2168
Dry etching characteristics of TiN film using Ar/CHF3, Ar/Cl2, and Ar/BCl3 gas chemistries in an inductively coupled plasma
Dry etching characteristics of TiN film have been studied in the case of using Ar/CHF3, Ar/Cl2, and Ar/BCl3 chemistries in an inductively coupled plasma. The TiN film was not etched at all without the addition of CHF3, BCl3, or Cl2 to the Ar gas flow. On the other hand, it was found that the TiN film was etched with one of the earlier additional gases. It was also found that a nontapered profile of etched TiN is obtained by Cl2 addition and a tapered profile by CHF3 or BCl3 addition. Moreover, a lower taper angle is obtained by increasing the amount of additional BCl3. X-ray photoelectron spectroscopy and Auger electron spectroscopy analyses for the etched samples of TiN show that TiF3 exists on the etched surface of TiN in the case of CHF3 addition and that BOxNy exists in the case of BCl3 addition. On the basis of these results, the effect of the gas addition to Ar on the characteristics of TiN reactive ion etching is considered as follows; under the Ar/CHF3 condition, although N in the TiN film is removed by evaporation in the form of NFx, Ti is fluorinated to form TiFx having low vapor pressure, which results in the low etching rate. Under the Ar/Cl2 condition, since NClx and TiClx have high vapor pressures, TiN is easily etched off, resulting in the highest etching rate with a nontapered profile. Under the Ar/BCl3 condition, although Cl plays the same role as it does under the Ar/Cl2 condition, B is likely to form a nonvolatile compound such as BOxNy, resulting in the deposition of the nonvolatile films on both the upper surface and sidewall of the TiN, which leads to a lower etching rate than that in the case of Cl2 addition and a lower taper angle of the etched profile.
- 1 September 2003
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 21 (5) , 2163-2168
Dry etching characteristics of TiN film using Ar/CHF3, Ar/Cl2, and Ar/BCl3 gas chemistries in an inductively coupled plasma
Dry etching characteristics of TiN film have been studied in the case of using Ar/CHF3, Ar/Cl2, and Ar/BCl3 chemistries in an inductively coupled plasma. The TiN film was not etched at all without the addition of CHF3, BCl3, or Cl2 to the Ar gas flow. On the other hand, it was found that the TiN film was etched with one of the earlier additional gases. It was also found that a nontapered profile of etched TiN is obtained by Cl2 addition and a tapered profile by CHF3 or BCl3 addition. Moreover, a lower taper angle is obtained by increasing the amount of additional BCl3. X-ray photoelectron spectroscopy and Auger electron spectroscopy analyses for the etched samples of TiN show that TiF3 exists on the etched surface of TiN in the case of CHF3 addition and that BOxNy exists in the case of BCl3 addition. On the basis of these results, the effect of the gas addition to Ar on the characteristics of TiN reactive ion etching is considered as follows; under the Ar/CHF3 condition, although N in the TiN film is removed by evaporation in the form of NFx, Ti is fluorinated to form TiFx having low vapor pressure, which results in the low etching rate. Under the Ar/Cl2 condition, since NClx and TiClx have high vapor pressures, TiN is easily etched off, resulting in the highest etching rate with a nontapered profile. Under the Ar/BCl3 condition, although Cl plays the same role as it does under the Ar/Cl2 condition, B is likely to form a nonvolatile compound such as BOxNy, resulting in the deposition of the nonvolatile films on both the upper surface and sidewall of the TiN, which leads to a lower etching rate than that in the case of Cl2 addition and a lower taper angle of the etched profile.
- 15 November 1985
- Published by Physical Society of Japan in Journal of the Physical Society of Japan
- Vol. 54 (11) , 4370-4381
Wavelength-Dependent Decay Times and Time-Dependent Spectra of the Singlet-Exciton Luminescence in Anthracene Crystals
- 15 November 1985
- Published by Physical Society of Japan in Journal of the Physical Society of Japan
- Vol. 54 (11) , 4370-4381
Wavelength-Dependent Decay Times and Time-Dependent Spectra of the Singlet-Exciton Luminescence in Anthracene Crystals