Lucian Cotet
Research Subjects
Lucian Cotet has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
- Laurentiu Filipescu
Faculty of Applied Chemistry and Materials Science, University Politehnica of Bucharest, 060042 Bucharest, Romania
4 shared publications - Sorin Iliev
Alum Tulcea SA, Isaccei Street, No. 82, 820228 Tulcea, Romania
4 shared publications - Adina Negrea
Department of Applied Chemistry and Environmental Engineering and Inorganic Compounds, Faculty of Industrial Chemistry, Biotechnology and Environmental Engineering, Politehnica University Timisoara, Vasile Parvan 6, 300223 Timisoara, Romania
3 shared publications - Alina Boiangiu
Alum Tulcea SA, Isaccei Street, No. 82, 820228 Tulcea, Romania
3 shared publications - Gheorghe Dobra
Alro Slatina SA, Pitesti Street, No. 116, 230048 Slatina, Romania
3 shared publications - Mihaela Ciopec
Faculty of Chemical Engineering, Biotechnologies and Environmental Protection, Politehnica University Timisoara, Victoriei Square, No. 2, 300006 Timisoara, Romania
3 shared publications
Latest Publications
- Open Access
Research Progress in Lanthanum Extraction from Boehmite
The purpose of this study was to examine the utilization of 0–45 μm aluminum hydrate fraction (gibbsite) manufactured by Alum SA Tulcea, as a precursor in the hydrothermal synthesis process of nanosize boehmite from gibbsite suspensions. Furthermore, the use of the produced material as adsorbent of lanthanum (III) ions was investigated using aqueous solutions. Thermogravimetric analysis (TG), Fourier Transform InfraRed Spectroscopy (FT-IR), Wide-Angle X-Ray Scattering (WAXS), and atomic force microscopy (AFM) were used to demonstrate the preparation of the required material. Additionally, the material point of zero charge (pHpzc) and material specific surface (using BET approach) were evaluated. By conducting adsorption studies, the specific parameters for the lanthanum adsorption process were evaluated. The effects of pH, the ratio of adsorbent material to La(III) quantity from aqueous solution, contact time, and La(III) initial concentration were also assessed. Based on the obtained experimental data, it was proved that the maximum adsorption capacity of 97.7 mg/g was obtained for a solid:liquid ratio = 0.1 g:25 mL, pH between 3 and 6, temperature of 298 K, and contact time of 90 min. The studied adsorption process is most effectively described by the Sips model, suggesting an intricate interaction among the adsorbent material and La (III) ions. The prepared adsorbent exhibited a good desorption capacity (higher than 93%) when 20% HCl was used for desorption.
Open AccessResearch Progress in Lanthanum Extraction from Boehmite
The purpose of this study was to examine the utilization of 0–45 μm aluminum hydrate fraction (gibbsite) manufactured by Alum SA Tulcea, as a precursor in the hydrothermal synthesis process of nanosize boehmite from gibbsite suspensions. Furthermore, the use of the produced material as adsorbent of lanthanum (III) ions was investigated using aqueous solutions. Thermogravimetric analysis (TG), Fourier Transform InfraRed Spectroscopy (FT-IR), Wide-Angle X-Ray Scattering (WAXS), and atomic force microscopy (AFM) were used to demonstrate the preparation of the required material. Additionally, the material point of zero charge (pHpzc) and material specific surface (using BET approach) were evaluated. By conducting adsorption studies, the specific parameters for the lanthanum adsorption process were evaluated. The effects of pH, the ratio of adsorbent material to La(III) quantity from aqueous solution, contact time, and La(III) initial concentration were also assessed. Based on the obtained experimental data, it was proved that the maximum adsorption capacity of 97.7 mg/g was obtained for a solid:liquid ratio = 0.1 g:25 mL, pH between 3 and 6, temperature of 298 K, and contact time of 90 min. The studied adsorption process is most effectively described by the Sips model, suggesting an intricate interaction among the adsorbent material and La (III) ions. The prepared adsorbent exhibited a good desorption capacity (higher than 93%) when 20% HCl was used for desorption.
- Open Access
Adsorption of Scandium Ions by Amberlite XAD7HP Polymeric Adsorbent Loaded with Tri-n-Octylphosphine Oxide
In an actual economic context, the demand for scandium has grown due to its applications in top technologies. However, further development of new technologies will lead to an increase in the market for Sc related to such technologies. The present study aims to improve and upgrade existing technology in terms of efficient scandium recovery, proposing a new material with selective adsorptive properties for scandium recovery. To highlight the impregnation of Amberlite XAD7HP resin with tri-n-octylphosphine oxide extractant by the solvent-impregnated resin method, the obtained adsorbent material was characterized by physico-chemical techniques. Further, the specific surface of the adsorbent and the zero-point charge of the adsorbent surface have been determined. Different parameters, such as initial concentration, adsorbent amount, contact time, or temperature, have been studied. The initial pH effect was investigated when a maximum adsorption capacity of 31.84 mg g−1 was obtained at pH > 3, using 0.1 g of adsorbent and a contact time of 90 min and 298 K. An attempt was made to discuss and provide a clear representation of the studied adsorption process, proposing a specific mechanism for Sc(III) recovery from aqueous solutions through kinetic, thermodynamic, and equilibrium studies. Adsorption/desorption studies reveal that the prepared adsorbent material can be reused five times.
Open AccessAdsorption of Scandium Ions by Amberlite XAD7HP Polymeric Adsorbent Loaded with Tri-n-Octylphosphine Oxide
In an actual economic context, the demand for scandium has grown due to its applications in top technologies. However, further development of new technologies will lead to an increase in the market for Sc related to such technologies. The present study aims to improve and upgrade existing technology in terms of efficient scandium recovery, proposing a new material with selective adsorptive properties for scandium recovery. To highlight the impregnation of Amberlite XAD7HP resin with tri-n-octylphosphine oxide extractant by the solvent-impregnated resin method, the obtained adsorbent material was characterized by physico-chemical techniques. Further, the specific surface of the adsorbent and the zero-point charge of the adsorbent surface have been determined. Different parameters, such as initial concentration, adsorbent amount, contact time, or temperature, have been studied. The initial pH effect was investigated when a maximum adsorption capacity of 31.84 mg g−1 was obtained at pH > 3, using 0.1 g of adsorbent and a contact time of 90 min and 298 K. An attempt was made to discuss and provide a clear representation of the studied adsorption process, proposing a specific mechanism for Sc(III) recovery from aqueous solutions through kinetic, thermodynamic, and equilibrium studies. Adsorption/desorption studies reveal that the prepared adsorbent material can be reused five times.
- Open Access
- 4 September 2022
- Published by MDPI AG in International Journal of Molecular Sciences
- Vol. 23 (17) , 10142
Scandium Recovery from Aqueous Solution by Adsorption Processes in Low-Temperature-Activated Alumina Products
In this paper, we studied the scandium adsorption from aqueous solutions on the surface of low-temperature-activated alumina products (GDAH). The GDAH samples are industrially manufactured, coming from the Bayer production cycle of the Sierra Leone bauxite as aluminium hydroxide, and further, by drying, milling, classifying and thermally treating up to dehydroxilated alumina products at low temperature. All experiments related to hydroxide aluminium activation were conducted at temperature values of 260, 300 and 400 °C on samples having the following particle sizes: <10 µm, 20 µm, <45 µm and <150 µm, respectively. The low-temperature-activated alumina products were characterised, and the results were published in our previous papers. In this paper, we studied the scandium adsorption process on the above materials and related thermodynamic and kinetic studies.
- 4 September 2022
- Published by MDPI AG in International Journal of Molecular Sciences
- Vol. 23 (17) , 10142
Open AccessScandium Recovery from Aqueous Solution by Adsorption Processes in Low-Temperature-Activated Alumina Products
In this paper, we studied the scandium adsorption from aqueous solutions on the surface of low-temperature-activated alumina products (GDAH). The GDAH samples are industrially manufactured, coming from the Bayer production cycle of the Sierra Leone bauxite as aluminium hydroxide, and further, by drying, milling, classifying and thermally treating up to dehydroxilated alumina products at low temperature. All experiments related to hydroxide aluminium activation were conducted at temperature values of 260, 300 and 400 °C on samples having the following particle sizes: <10 µm, 20 µm, <45 µm and <150 µm, respectively. The low-temperature-activated alumina products were characterised, and the results were published in our previous papers. In this paper, we studied the scandium adsorption process on the above materials and related thermodynamic and kinetic studies.
- Open Access
Thermally Activated Al(OH)3 Part II—Effect of Different Thermal Treatments
In this paper, the thermal decomposition of crystalline Al(OH)3 was studied over the temperature range of 260–400 °C for particles with a size between 10 and 150 µm. The weight losses and thermal effects occurring in each of the dehydration process were assessed using thermogravimetry (TG) and differential scanning calorimetry (DSC) thermal analysis. X-ray diffraction (XRD) patterns, refined by the Rietveld method, were used for mineral phase identification, phase composition analysis, and crystallinity degree determination. Moreover, the particle size distributions and their corresponding D10, D50, and D90 numeric values were determined with a laser analyzer. We observed a strong relationship between the calcination temperature, the initial gibbsite grade particle size, and the crystallinity of the resulting powders. Hence, for all endothermic effects identified by DSC, the associated temperature values significantly decreased insofar as the particle dimensions decreased. When the gibbsite was calcined at a low temperature, we identified small amounts of boehmite phase along with amorphous new phases and unconverted gibbsite, while the powders calcined at 400 °C gradually yielded a mixture of boehmite and crystalized γ-Al2O3. The crystallinity % of all phase transition products declined with the increase in particle size or temperature for all the samples.
Open AccessThermally Activated Al(OH)3 Part II—Effect of Different Thermal Treatments
In this paper, the thermal decomposition of crystalline Al(OH)3 was studied over the temperature range of 260–400 °C for particles with a size between 10 and 150 µm. The weight losses and thermal effects occurring in each of the dehydration process were assessed using thermogravimetry (TG) and differential scanning calorimetry (DSC) thermal analysis. X-ray diffraction (XRD) patterns, refined by the Rietveld method, were used for mineral phase identification, phase composition analysis, and crystallinity degree determination. Moreover, the particle size distributions and their corresponding D10, D50, and D90 numeric values were determined with a laser analyzer. We observed a strong relationship between the calcination temperature, the initial gibbsite grade particle size, and the crystallinity of the resulting powders. Hence, for all endothermic effects identified by DSC, the associated temperature values significantly decreased insofar as the particle dimensions decreased. When the gibbsite was calcined at a low temperature, we identified small amounts of boehmite phase along with amorphous new phases and unconverted gibbsite, while the powders calcined at 400 °C gradually yielded a mixture of boehmite and crystalized γ-Al2O3. The crystallinity % of all phase transition products declined with the increase in particle size or temperature for all the samples.
- Open Access
Thermally Activated Al(OH)3: Part I—Morphology and Porosity Evaluation
Aluminum hydroxide is an essential material for the industrial production of ceramics (especially insulators and refractories), desiccants, absorbents, flame retardants, filers for plastics and rubbers, catalysts, and various construction materials. The calcination process of Al(OH)3 first induces dehydration and, finally, results in α-Al2O3 formation. Nevertheless, this process contains various intermediary steps and has been proven to be complicated due to the development of numerous transitional alumina. Each step of the investigation is vital for the entire process because the final properties of materials based on aluminum trihydroxide are determined by their phase composition, morphology, porosity, etc. In this paper, five dried, milled, and size-classified aluminum hydroxide specimens were thermally treated at 260, 300, and 400 °C; then, they were studied in order to identify the effects of temperature on their properties, such as particle morphology, specific surface area, pore size, and pore distribution. The major oxide compounds identified in all samples were characteristic of bauxite—namely, Al2O3 * 3H2O, SiO2, Fe2O3, Na2O, and CaO. Particles with smaller sizes (2/g and their small pore width (3–3.5 nm).
Open AccessThermally Activated Al(OH)3: Part I—Morphology and Porosity Evaluation
Aluminum hydroxide is an essential material for the industrial production of ceramics (especially insulators and refractories), desiccants, absorbents, flame retardants, filers for plastics and rubbers, catalysts, and various construction materials. The calcination process of Al(OH)3 first induces dehydration and, finally, results in α-Al2O3 formation. Nevertheless, this process contains various intermediary steps and has been proven to be complicated due to the development of numerous transitional alumina. Each step of the investigation is vital for the entire process because the final properties of materials based on aluminum trihydroxide are determined by their phase composition, morphology, porosity, etc. In this paper, five dried, milled, and size-classified aluminum hydroxide specimens were thermally treated at 260, 300, and 400 °C; then, they were studied in order to identify the effects of temperature on their properties, such as particle morphology, specific surface area, pore size, and pore distribution. The major oxide compounds identified in all samples were characteristic of bauxite—namely, Al2O3 * 3H2O, SiO2, Fe2O3, Na2O, and CaO. Particles with smaller sizes (2/g and their small pore width (3–3.5 nm).