  • Open Access

    Fractal Characterization of Cavitation Erosion in Glycerol-Water Mixtures: Role of Viscosity in Aluminum Surface Failure

    by Osman Omran Osman, A. Abouel-Kasem, M. Heshmat, B. Saleh, S. M. Ahmed

    This study investigates how fluid viscosity modulates cavitation erosion in Al-99.92 aluminum surfaces by employing fractal analysis to quantify degradation patterns in water and glycerol-water mixtures (10–40 cSt). Fractal dimensions, calculated from power spectral density (PSD) slopes of SEM-derived surface topographies, correlate strongly with traditional erosion metrics (mean depth penetration, MDP). Both fractal dimension and MDP exhibit a viscosity-dependent decline, revealing reduced cavitation intensity in high-viscosity fluids. Critically, fractal trends remain scale-invariant across magnifications, confirming that viscosity governs surface texture complexity independently of imaging resolution. Detached particle morphology and surface features (cracks, plastic deformation) identify fatigue failure as the dominant erosion mechanism, with liquid viscosity exerting secondary influence. By bridging fractal metrics to mechanical erosion outcomes, this work establishes fractal analysis as a robust tool for predicting viscosity-dependent cavitation damage in aluminum alloys, offering insights for material selection in high-viscosity hydraulic systems.

  • Shock Waves as Dominant Mechanism for Cavitation Damage

    by O. O. Osman, A. Abouel-Kasem, S. M. Ahmed

    In this paper, the mechanism of energy transfer from cavitation bubbles to solids is demonstrated as shock waves. To identify this mechanism, cavitation bubble structures, the corresponding damaged surface, and the wear particles in vibratory erosion tests on pure aluminum Al-99.999 using high-speed and scanning electron microscope photography were observed. The eroded surface morphology was in the form of large swellings (hundreds of micrometers), which embodies the plastic flow. Results indicate that large swelling regions formed in a few seconds are caused by shock pressure waves and not by a microjet only several micrometers in size. The observed surface erosion and falling particles make it clear that the mechanism of cavitation wear is fatigue failure.


  • The Limited Role of Pit Formed by Microjet in Evolution of Cavitation Erosion in the Incubation Period

    by A. Abouel-Kasem, Osman Omar Osman, S. A. Karrab, Shemy Mohamed Ahmed

    Stepwise cavitation erosion is used to study pits formed by microjets. The aim is to determine the role of the pit in the development of cavitation erosion damage, including geometrical features of the pitted area and pit counting. The study also identified the dominant feature in the development of cavitation damage. We used a vibratory cavitation apparatus to perform cavitation erosion damage on a stainless steel, SUS 304, in tap water with scanning electron microscopy (SEM) at 5-min intervals from t = 0 min to t = 45 min. We then analyzed and characterized the pits formed by impacting the surface with a microjet. These results showed that individual pits and clusters of pits are characterized by a black spot surrounded by plastic deformation, and both are irregular in shape. This suggests that the microjet is hitting the wear surface in an oblique direction. Over the course of the test time, neither the shape nor the size of the microjet pits and their clusters change; pit diameters approximately 2 μm or less. The area of pits and their clusters does not exceed 1% of the worn surface. All these features demonstrate that the pit and its clusters do not impact the evolution of cavitation damage. Our results also indicated that slip bands were caused by a shock wave. Slip bands are large (>10 μm) and account for about 30% of the wear surface. This confirms that slip bands are predominantly responsible for the development of cavitation; the predominant cavitation mechanism is fatigue due to multiple shock waves.