Yangtao Xu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Yangtao Xu has a total of 26 co-authors. Here are the top co-authors by number of shared publications:
- Tiandong Xia
School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China
3 shared publications - Han Zhang
School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China
2 shared publications Huai Li
School of Materials Science and Engineering, LanZhou University of Technology, GanSu, China
2 shared publications- Jisen Qiao
School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China
2 shared publications - Chen Sang
School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China
1 shared publication - Chengpeng Miao
Jinchuan Group Nickel Alloy Co., Ltd., Jinchang 737100, China
1 shared publication
Latest Publications
- Open Access
Microstructure Evolution and Plastic Deformation Mechanism of Cold Rolling Deformation of Micro/Nano Pure Electrolytic Nickel
This paper investigates the cold rolling (CR) deformation behavior of electrolytic nickel at room temperature. While the microstructural evolution across deformation levels ranging from 5% to 98% is systematically characterized. The deposited electrolytic nickel exhibits numerous growth twins of various lengths and thicknesses, accounting for over 70% of the microstructure. The average grain size is 0.56 μm, and the grain size distribution is relatively broad. The plastic deformation of electrolytic nickel in the early stage is governed by the interaction between high-density dislocations and abundant twins. The primary mechanism accommodating deformation is detwinning. At 70% deformation, under high strain, complete detwinning occurs. When the CR reaches 90%, the average short-axis grain size is refined to 113 nm, indicating the deformation-induced refinement limit of electrolytic nickel. The microstructure at this stage exhibits a typical lamellar morphology. At 98% deformation, the average microhardness peaks at 240.3 HV, representing a cumulative increase of 46.88%. Dynamic recovery and recrystallization are observed at both 70% and 98% deformation levels, accompanied by the formation of Σ3 {120} type incoherent twins within recrystallized grains. Under large strain, the dominant cold plastic deformation mechanism transitions to a synergistic effect of dislocation slip and stratification.
Open AccessMicrostructure Evolution and Plastic Deformation Mechanism of Cold Rolling Deformation of Micro/Nano Pure Electrolytic Nickel
This paper investigates the cold rolling (CR) deformation behavior of electrolytic nickel at room temperature. While the microstructural evolution across deformation levels ranging from 5% to 98% is systematically characterized. The deposited electrolytic nickel exhibits numerous growth twins of various lengths and thicknesses, accounting for over 70% of the microstructure. The average grain size is 0.56 μm, and the grain size distribution is relatively broad. The plastic deformation of electrolytic nickel in the early stage is governed by the interaction between high-density dislocations and abundant twins. The primary mechanism accommodating deformation is detwinning. At 70% deformation, under high strain, complete detwinning occurs. When the CR reaches 90%, the average short-axis grain size is refined to 113 nm, indicating the deformation-induced refinement limit of electrolytic nickel. The microstructure at this stage exhibits a typical lamellar morphology. At 98% deformation, the average microhardness peaks at 240.3 HV, representing a cumulative increase of 46.88%. Dynamic recovery and recrystallization are observed at both 70% and 98% deformation levels, accompanied by the formation of Σ3 {120} type incoherent twins within recrystallized grains. Under large strain, the dominant cold plastic deformation mechanism transitions to a synergistic effect of dislocation slip and stratification.
- 12 December 2025
- Published by Springer Nature in Korean Journal of Chemical Engineering
- Vol. 43 (3) , 775-788
Selenium Control in the Electrolyte of Electrowinning Nickel System: Speciation, Electrochemical Analysis and Removal Strategies
- 12 December 2025
- Published by Springer Nature in Korean Journal of Chemical Engineering
- Vol. 43 (3) , 775-788
Selenium Control in the Electrolyte of Electrowinning Nickel System: Speciation, Electrochemical Analysis and Removal Strategies
- Open Access
Rapid Determination of Thiourea Concentration in Copper Electrolyte
Due to the characteristics of high salt and high acidity of the electrolyte and the chemical reaction between thiourea (Tu) and metal ions, it is still a problem to quickly and accurately detect Tu concentration in copper electrolyte. An improved spectrophotometric method has been proposed by simplifying the extraction steps of the traditional extraction–spectrophotometry and reducing the dosage of extractant and buffer. The improved method, with a favorable R2 of 0.9991, great precision of 1.67% and excellent spiked recovery of 102.19%, was not affected by the presence of gelatin and copper ions. Moreover, based on the spectrophotometry, a colorimetric method for rapid detection of Tu concentration in copper electrolyte was proposed. Using the standard color card produced enabled the expeditious determination of the concentration range of Tu in copper electrolyte. Since the gray value of the standard color card is linearly related to the Tu concentration, it is feasible to determine the Tu concentration by measuring the gray value of the test strip, and its accuracy was verified by spectrophotometry. The colorimetric method has satisfactory results in industrial practice. This study provides a novel approach for the rapid detection of Tu concentration in the copper electrolysis industry.
Open AccessRapid Determination of Thiourea Concentration in Copper Electrolyte
Due to the characteristics of high salt and high acidity of the electrolyte and the chemical reaction between thiourea (Tu) and metal ions, it is still a problem to quickly and accurately detect Tu concentration in copper electrolyte. An improved spectrophotometric method has been proposed by simplifying the extraction steps of the traditional extraction–spectrophotometry and reducing the dosage of extractant and buffer. The improved method, with a favorable R2 of 0.9991, great precision of 1.67% and excellent spiked recovery of 102.19%, was not affected by the presence of gelatin and copper ions. Moreover, based on the spectrophotometry, a colorimetric method for rapid detection of Tu concentration in copper electrolyte was proposed. Using the standard color card produced enabled the expeditious determination of the concentration range of Tu in copper electrolyte. Since the gray value of the standard color card is linearly related to the Tu concentration, it is feasible to determine the Tu concentration by measuring the gray value of the test strip, and its accuracy was verified by spectrophotometry. The colorimetric method has satisfactory results in industrial practice. This study provides a novel approach for the rapid detection of Tu concentration in the copper electrolysis industry.
- Open Access
Research on the Mechanism of Oxygen-Induced Embrittlement Fracturing in Industrial Electrolytic Nickel
In this study, severe cracking occurred during an investigation of the direct hot rolling of industrial electrolytic nickel plates. To determine the cause of hot-rolling cracking, the microstructure phase composition was analyzed through the utilization of various techniques, including optical microscopy, scanning electron microscopy, electron backscattering diffraction, transmission electron microscopy (TEM), energy-dispersive X-ray spectroscopy (EDS) and electron probe micro-analysis. The comparative microstructural analysis took place between specimens heat treated in atmospheric and vacuum environments. The characterization and analysis of the hot-rolled plates considered the crack microstructure and fracture morphology. It was shown that holes appeared along the large angular grain boundaries after annealing at 1100 °C for 8 h. Possible reason: In a high-temperature environment, the decomposition of residual additives in the electrolytic nickel releases oxidizing gases, which oxidizes the grain boundaries. The reaction with carbon diffused into the grain boundaries and produced carbon monoxide gas, which induced holes and severely reduced the grain boundary plasticity. The heat treatment time did not need to be very long for severe grain boundary degradation to occur. After severe cavitation, the electrolytic nickel was severely cracked at grain boundaries cracks due to a shear force, and brittle fractures occurred along grains with very low plasticity.
Open AccessResearch on the Mechanism of Oxygen-Induced Embrittlement Fracturing in Industrial Electrolytic Nickel
In this study, severe cracking occurred during an investigation of the direct hot rolling of industrial electrolytic nickel plates. To determine the cause of hot-rolling cracking, the microstructure phase composition was analyzed through the utilization of various techniques, including optical microscopy, scanning electron microscopy, electron backscattering diffraction, transmission electron microscopy (TEM), energy-dispersive X-ray spectroscopy (EDS) and electron probe micro-analysis. The comparative microstructural analysis took place between specimens heat treated in atmospheric and vacuum environments. The characterization and analysis of the hot-rolled plates considered the crack microstructure and fracture morphology. It was shown that holes appeared along the large angular grain boundaries after annealing at 1100 °C for 8 h. Possible reason: In a high-temperature environment, the decomposition of residual additives in the electrolytic nickel releases oxidizing gases, which oxidizes the grain boundaries. The reaction with carbon diffused into the grain boundaries and produced carbon monoxide gas, which induced holes and severely reduced the grain boundary plasticity. The heat treatment time did not need to be very long for severe grain boundary degradation to occur. After severe cavitation, the electrolytic nickel was severely cracked at grain boundaries cracks due to a shear force, and brittle fractures occurred along grains with very low plasticity.
- 26 October 2023
- Published by Springer Nature in Journal of Applied Electrochemistry
- Vol. 54 (3) , 597-609
Effect of cerium chloride on electric crystallization behavior and grain refinement of electrodeposited copper
- 26 October 2023
- Published by Springer Nature in Journal of Applied Electrochemistry
- Vol. 54 (3) , 597-609
Effect of cerium chloride on electric crystallization behavior and grain refinement of electrodeposited copper
- Open Access
- 22 August 2023
- Published by Springer Nature in Research Square
The effect of lanthanum chloride on the electrocrystallization behavior of cobalt and grain refinement in deposition layers
This study investigates the effect of different concentrations of lanthanum chloride (LaCl3) on the grain refinement of cobalt deposition layers during the electrochemical deposition process in industrial electrolytes. The impact of different LaCl3 concentrations on cobalt electrodeposition behavior was analyzed using the Liner sweep voltammetry curve (LSV), Cyclic voltammetry curve (CV), and Chronoamperometry curve (CA). The microstructure morphology and grain size of the deposition layers were analyzed using scanning electron microscopy and atomic force microscopy and the preferred orientation and crystal structure were analyzed using X-ray diffraction. The results show that the addition of different concentrations of LaCl3 to the industrial electrolyte leads to a negative shift in the starting deposition potential of cobalt, an increase in cathode polarization degree, an increase in overpotential, a shortened nucleation relaxation time tm and an accelerated nucleation rate during cobalt electrodeposition, resulting in grain refinement of the deposition layers. However, the addition of LaCl3 does not change the cobalt electrocrystallization mechanism, nor does it alter the crystal structure of the cobalt deposition layers, which remain in a close-packed hexagonal structure (HCP). When 0.2 g/L LaCl3 is added, the grain growth orientation changes from the (11\(\stackrel{\text{-}}{\text{2}}\)0) plane to the (11\(\stackrel{\text{-}}{\text{2}}\)0) and (10\(\stackrel{\text{-}}{\text{1}}\)0) planes, resulting in a uniform distribution of grain size and obvious grain refinement of the deposition layers.- 22 August 2023
- Published by Springer Nature in Research Square
Open AccessThe effect of lanthanum chloride on the electrocrystallization behavior of cobalt and grain refinement in deposition layers
This study investigates the effect of different concentrations of lanthanum chloride (LaCl3) on the grain refinement of cobalt deposition layers during the electrochemical deposition process in industrial electrolytes. The impact of different LaCl3 concentrations on cobalt electrodeposition behavior was analyzed using the Liner sweep voltammetry curve (LSV), Cyclic voltammetry curve (CV), and Chronoamperometry curve (CA). The microstructure morphology and grain size of the deposition layers were analyzed using scanning electron microscopy and atomic force microscopy and the preferred orientation and crystal structure were analyzed using X-ray diffraction. The results show that the addition of different concentrations of LaCl3 to the industrial electrolyte leads to a negative shift in the starting deposition potential of cobalt, an increase in cathode polarization degree, an increase in overpotential, a shortened nucleation relaxation time tm and an accelerated nucleation rate during cobalt electrodeposition, resulting in grain refinement of the deposition layers. However, the addition of LaCl3 does not change the cobalt electrocrystallization mechanism, nor does it alter the crystal structure of the cobalt deposition layers, which remain in a close-packed hexagonal structure (HCP). When 0.2 g/L LaCl3 is added, the grain growth orientation changes from the (11\(\stackrel{\text{-}}{\text{2}}\)0) plane to the (11\(\stackrel{\text{-}}{\text{2}}\)0) and (10\(\stackrel{\text{-}}{\text{1}}\)0) planes, resulting in a uniform distribution of grain size and obvious grain refinement of the deposition layers. - 19 December 2022
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 32 (7) , 1-9
Effect of Rare Earth Nd on the Microstructure and Compression Behavior of Co-8.8Al-9.8 W Alloy
- 19 December 2022
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 32 (7) , 1-9
Effect of Rare Earth Nd on the Microstructure and Compression Behavior of Co-8.8Al-9.8 W Alloy