JQJisen Qiao

Jisen Qiao

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Jisen Qiao has a total of 22 co-authors. Here are the top co-authors by number of shared publications:

  • Qilun Li

    School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China

    3 shared publications
  • Han Zhang

    School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China

    2 shared publications
  • Junqiang Ren

    State Key Laboratory of Advanced Processing and Recycling of Non-Ferrous Metals, School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China

    2 shared publications
  • Qilun Li

    State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metal, Department of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China

    2 shared publications
  • Qing Gao

    State Key Laboratory of Advanced Processing and Recycling of Non-Ferrous Metal, School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, P. R. China

    2 shared publications
  • Tiandong Xia

    School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China

    2 shared publications

Latest Publications

  • Open Access

    Microstructure Evolution and Plastic Deformation Mechanism of Cold Rolling Deformation of Micro/Nano Pure Electrolytic Nickel

    by Han Zhang, Jisen Qiao, Hao Yang, Yangtao Xu, Tiandong Xia

    This paper investigates the cold rolling (CR) deformation behavior of electrolytic nickel at room temperature. While the microstructural evolution across deformation levels ranging from 5% to 98% is systematically characterized. The deposited electrolytic nickel exhibits numerous growth twins of various lengths and thicknesses, accounting for over 70% of the microstructure. The average grain size is 0.56 μm, and the grain size distribution is relatively broad. The plastic deformation of electrolytic nickel in the early stage is governed by the interaction between high-density dislocations and abundant twins. The primary mechanism accommodating deformation is detwinning. At 70% deformation, under high strain, complete detwinning occurs. When the CR reaches 90%, the average short-axis grain size is refined to 113 nm, indicating the deformation-induced refinement limit of electrolytic nickel. The microstructure at this stage exhibits a typical lamellar morphology. At 98% deformation, the average microhardness peaks at 240.3 HV, representing a cumulative increase of 46.88%. Dynamic recovery and recrystallization are observed at both 70% and 98% deformation levels, accompanied by the formation of Σ3 {120} type incoherent twins within recrystallized grains. Under large strain, the dominant cold plastic deformation mechanism transitions to a synergistic effect of dislocation slip and stratification.

  • Atomic-Scale Study on the Dislocation Evolution Mechanism of Al/Cu-Layered Materials Under Nanoindentation

    by Qing Gao, Junqiang Ren, Qilun Li, Xuefeng Lu, Jisen Qiao

    Al/Cu-layered metal materials, a kind of material with a highly ordered structure and excellent comprehensive performance, are widely used in the fields of automobile, aerospace and shipbuilding. The molecular dynamics method was adopted to simulate the mechanical behavior and dislocation evolution mechanism of Al/Cu-layered materials at different indentation velocities; the results indicating the uniquely periodic dislocation network formed during deformation at the interface can prevent further dislocation slip and relieve stress concentration, leading to the improvement of the strength and hardness. The interface dislocation can be activated when the indentation depth is sufficient, along with the location and slip system, depending on the symmetry of the crystal structure and the Schmidt factor. Moreover, the plastic deformation begins with the nucleation and movement of Shockley partial dislocations and is dominated by the dislocation slip. With the increase of indentation velocity, the movement and reaction of dislocations are promoted, which have an emergence of immobile dislocations, complex dislocation loops, many dislocation tangles and limited dislocation cross-slip, greatly accelerating the work hardening and delaying the deformation. Particularly, there are two main steps in the formation of independent prismatic dislocation loops. First, multiple “u”-type dislocation loops nucleate and then slip. Second, the screw dislocation fragments of the shear dislocation loop cross-slip on the intersecting [ ] slip plane. The research results open a window in manufacturing nanoprecision devices, analyzing the service performance and carrying out reliability evaluation.

  • Open Access

    Research on the Mechanism of Oxygen-Induced Embrittlement Fracturing in Industrial Electrolytic Nickel

    by Han Zhang, Chen Sang, Chengpeng Miao, Yangtao Xu, Jisen Qiao, Tiandong Xia

    In this study, severe cracking occurred during an investigation of the direct hot rolling of industrial electrolytic nickel plates. To determine the cause of hot-rolling cracking, the microstructure phase composition was analyzed through the utilization of various techniques, including optical microscopy, scanning electron microscopy, electron backscattering diffraction, transmission electron microscopy (TEM), energy-dispersive X-ray spectroscopy (EDS) and electron probe micro-analysis. The comparative microstructural analysis took place between specimens heat treated in atmospheric and vacuum environments. The characterization and analysis of the hot-rolled plates considered the crack microstructure and fracture morphology. It was shown that holes appeared along the large angular grain boundaries after annealing at 1100 °C for 8 h. Possible reason: In a high-temperature environment, the decomposition of residual additives in the electrolytic nickel releases oxidizing gases, which oxidizes the grain boundaries. The reaction with carbon diffused into the grain boundaries and produced carbon monoxide gas, which induced holes and severely reduced the grain boundary plasticity. The heat treatment time did not need to be very long for severe grain boundary degradation to occur. After severe cavitation, the electrolytic nickel was severely cracked at grain boundaries cracks due to a shear force, and brittle fractures occurred along grains with very low plasticity.


  • Open Access

    Effect of Multistage Solution Aging Heat Treatment on Mechanical Properties and Precipitated Phase Characteristics of High-Strength Toughened 7055 Alloy

    by Qilun Li, Xiaobo Zhang, Ce Guo, Jisen Qiao

    In this paper, a one-step hot extrusion dual-stage solution treatment method is employed to fabricate high-strength and tough T-shaped complex cross-section 7055 (Al-Zn-Mg-Cu-Zr) alloy profiles, and a detailed investigation is conducted on the microstructure and mechanical properties. The results indicate that the comprehensive mechanical properties of the 7055 aluminum extruded alloy using the two-stage solution aging treatment are excellent. This is particularly evident in the balance between strength and ductility, where outstanding strength is accompanied by a plasticity that is maintained at 13.2%. During the extrusion process, the deformation textures are mainly composed of brass and copper, forming a 15.1% recrystallization texture Cube. In addition, the equilibrium phase η(MgZn2) precipitated in the grain is the main strengthening phase, and there are large discontinuous grain boundary precipitates at the grain boundary, which hinders the grain boundary dislocation movement and has great influence on the mechanical properties of alloy materials.


  • Dislocation-based mechanical responses and deformation mechanisms of Al/Cu heterointerfaces: A computational study via molecular dynamics simulations

    by Qing Gao, Wei Li, Junqiang Ren, Xin Guo, Qilun Li, Xuefeng Lu, Jisen Qiao

    Layered metal composites have been widely used in various industries fields because of their excellent properties and are responsible for mechanical behavior of materials. This paper focuses on analyzing the deformation mechanism of the (110) interface under different loading states by MD. The results show that there are two yield points in the stress–strain curve under both Z- and Y-axis loading states. The first yield is the nucleation of dislocations at the interface, meantime the slip of dislocations and the extension of stacking faults begin at the Al layer. The second one, the dislocation passes through the interface, nucleates and emits toward the Cu layer at the interface, leading to a stress mutation. It is worth noting that during the stable rheological stage, the deformation mechanisms vary under different loading directions. Under Y-axis tensile loading, the phase transformation of FCC–HCP is present due to the interaction of dislocation movement and stacking fault. On the contrary, there are two twin paths A and B, improving the strength, during Z-axis compression loading. For other loading modes, there are three zones, namely the elastic stage, the release of energy, and strain hardening and dynamic softening. The interface plays the role of nucleation, annihilation and penetration of dislocations, and this interface-dislocation mechanism is reflected in the whole stage of plastic deformation. The results have an insight into the design and control in heterointerface.


  • Open Access

    The Effect of Extrusion and Heat Treatment on the Microstructure and Tensile Properties of 2024 Aluminum Alloy

    by Qilun Li, Xiaobo Zhang, Lei Wang, Jisen Qiao

    Hot extrusion forming is one of the best cost-effective processing methods to obtain high-strength aluminum alloys. In order to obtain high performance 2024 aluminum alloy for the aero and automobile industries, this research comprehensively uses heat treatment and reverse isothermal extrusion technology to prepare 2024 alloy. The effects of homogenization, extrusion and post-extrusion annealing treatment on the microstructure and mechanical properties of 2024 aluminum alloy were discussed in detail. The results indicate that the grain refinement of the extruded alloy material is significant. The coarse eutectic microstructure at the grain boundaries was refined, and these grains tended to be uniformly distributed after the annealing treatment. Extruded 2024 aluminum alloy material mainly has S (Al2CuMg) and Al7Cu2Fe second phases. The appearance of a large number of S phases led to a significant improvement in the properties of the alloy with an increase in tensile strength and elongation of 176% and 547%, respectively. In addition, EBSD analysis showed a significant meritocratic growth in the extrusion direction with the appearance of Copper {112} rolling weaving, which led to process hardening and the strength improvement of the alloy.