Pattarawadee Krassanairawiwong
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Pattarawadee Krassanairawiwong has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Atima Kurjirattikan
College of Dental Medicine, Rangsit University, Pathum Thani 12000, Thailand
1 shared publication - Chanidapa Sangkanchanavanich
College of Dental Medicine, Rangsit University, Pathum Thani 12000, Thailand
1 shared publication Jirat Srihatajati
1 shared publication- Jirat Srihatajati
Prosthodontics Department, College of Dental Medicine, Rangsit University, Mueang, Pathum Thani, Thailand, rsu.ac.th
1 shared publication - Kanyarak Kunyawatyuwapong
College of Dental Medicine, Rangsit University, Pathum Thani 12000, Thailand
1 shared publication - Natlada Tantivasin
College of Dental Medicine, Rangsit University, Pathum Thani 12000, Thailand
1 shared publication
Latest Publications
- Open Access
- 1 January 2026
- Published by Wiley in International Journal of Dentistry
- Vol. 2026 (1)
Evaluation of Shear Bond Strength and Surface Morphology (via SEM) of Different Provisional Crowns and Surface Treatments to PMMA
Purpose of the Study: To compare the shear bond strengths (SBSs) of different provisional crown materials with various surface treatments when relined with autopolymerizing polymethyl methacrylate (PMMA). Materials and Methods: Part 1: Seventy‐five specimens were divided into five groups: PMAC (autopolymerizing PMMA), PMAM (CAD/CAM system PMMA), PMAD (3D‐printed PMMA), PLAI (injectable polylactic acid [PLA]), and PLAD (3D‐printed PLA). All specimens were surface‐treated by sandblasting followed by 180 s of MMA application, then relined with autopolymerizing PMMA. Part 2: Forty‐five PLAD specimens were divided into three groups: PLAD (control), PLAD MC (methylene chloride treatment), and PLAD AT (acetone treatment), then relined with autopolymerizing PMMA. All samples underwent thermocycling before being evaluated for SBS with a universal testing machine (Shimadzu, Japan). Statistical analysis was performed using one‐way ANOVA and Tukey’s HSD at a significance level of p ≤ 0.05. Failure modes were examined using a stereomicroscope, and surface morphology was evaluated by scanning electron microscopy (SEM). Result: In Part 1, the mean SBS values in MPa were: PMAC (26.85 ± 1.31), PMAM (22.92 ± 1.20), PMAD (13.98 ± 1.20), PLAI (10.19 ± 1.59), and PLAD (8.44 ± 1.14). Significant differences were found between all groups ( p ≤ 0.05). In Part 2, the mean SBS values in MPa were: PLAD (8.44 ± 1.14), PLAD MC (8.35 ± 0.84), and PLAD AT (7.83 ± 1.13). No significant differences were found between the three groups ( p > 0.05). PMAC, PMAM, and PMAD exhibited mixed failure modes in 87.5%, 80%, and 73.3% at the fractured surfaces of the specimens, respectively. In contrast, PLAD and PLAI displayed 100% adhesive failure. PLAD, PLAD MC, and PLAD AT also showed 100% adhesive failure at fractured surfaces. Conclusion: The PMAC group achieved the highest SBS among all tested materials. Surface treatment of PLAD with methylene chloride or acetone did not significantly improve SBS compared to the untreated control.
- 1 January 2026
- Published by Wiley in International Journal of Dentistry
- Vol. 2026 (1)
Open AccessEvaluation of Shear Bond Strength and Surface Morphology (via SEM) of Different Provisional Crowns and Surface Treatments to PMMA
Purpose of the Study: To compare the shear bond strengths (SBSs) of different provisional crown materials with various surface treatments when relined with autopolymerizing polymethyl methacrylate (PMMA). Materials and Methods: Part 1: Seventy‐five specimens were divided into five groups: PMAC (autopolymerizing PMMA), PMAM (CAD/CAM system PMMA), PMAD (3D‐printed PMMA), PLAI (injectable polylactic acid [PLA]), and PLAD (3D‐printed PLA). All specimens were surface‐treated by sandblasting followed by 180 s of MMA application, then relined with autopolymerizing PMMA. Part 2: Forty‐five PLAD specimens were divided into three groups: PLAD (control), PLAD MC (methylene chloride treatment), and PLAD AT (acetone treatment), then relined with autopolymerizing PMMA. All samples underwent thermocycling before being evaluated for SBS with a universal testing machine (Shimadzu, Japan). Statistical analysis was performed using one‐way ANOVA and Tukey’s HSD at a significance level of p ≤ 0.05. Failure modes were examined using a stereomicroscope, and surface morphology was evaluated by scanning electron microscopy (SEM). Result: In Part 1, the mean SBS values in MPa were: PMAC (26.85 ± 1.31), PMAM (22.92 ± 1.20), PMAD (13.98 ± 1.20), PLAI (10.19 ± 1.59), and PLAD (8.44 ± 1.14). Significant differences were found between all groups ( p ≤ 0.05). In Part 2, the mean SBS values in MPa were: PLAD (8.44 ± 1.14), PLAD MC (8.35 ± 0.84), and PLAD AT (7.83 ± 1.13). No significant differences were found between the three groups ( p > 0.05). PMAC, PMAM, and PMAD exhibited mixed failure modes in 87.5%, 80%, and 73.3% at the fractured surfaces of the specimens, respectively. In contrast, PLAD and PLAI displayed 100% adhesive failure. PLAD, PLAD MC, and PLAD AT also showed 100% adhesive failure at fractured surfaces. Conclusion: The PMAC group achieved the highest SBS among all tested materials. Surface treatment of PLAD with methylene chloride or acetone did not significantly improve SBS compared to the untreated control.
- 21 January 2022
- Published by Chiang Mai University in Chiang Mai University Journal of Natural Sciences
- Vol. 21 (1)
Effect of Different Resin Cements on Shear Bond Strength between Acrylic Denture Teeth and Resin Composite
The purpose of this study was to evaluate the effect of different bonding agents and resin cements on shear bond strength (SBS) between acrylic resin teeth and resin composite. Thirty acrylic teeth were cut along the long axis and embedded in cold-cure acrylic resin. The specimens were randomly divided into 3 groups (n = 10) according to the types of luting agents: Group C (OptiBond FL), Group P (Panavia F2.0), and Group S (Superbond C&B). SBS was measured using the Shimadzu EZ-S Universal Testing Machine. The collected data were analyzed using a one-way ANOVA to determine significant differences with P-value < 0.05. Multiple comparisons of SBS were calculated using the Tukey HSD test at a 95% confidence level. The average SBS values in MPa were 5.78 ± 0.97 for Group C, 13.60 ± 1.20 for Group P, and 17.93 ± 1.24 for Group S. The SBS value for Group S was significantly higher compared to the other groups, while the value for Group C was significantly lower. Group C was categorized as an adhesive failure, while Group S was accounted as a cohesive failure and Group P was shown to be a mixed failure. In conclusion, different resin cements significantly affected the SBS between acrylic resin teeth and resin composite. Keywords: Acrylic denture tooth, Bonding agent, Resin cement, Resin composite, Shear bond strength Funding: The authors are grateful for the research funding provided by the College of Dental Medicine, Rangsit University, Thailand. Citation: Srihatajati, J. and Krassanairawiwong, P. 2021. Effect of different resin cements on shear bond strength between acrylic denture teeth and resin composite. CMU J. Nat. Sci. 21(1): e2022011.
- 21 January 2022
- Published by Chiang Mai University in Chiang Mai University Journal of Natural Sciences
- Vol. 21 (1)
Effect of Different Resin Cements on Shear Bond Strength between Acrylic Denture Teeth and Resin Composite
The purpose of this study was to evaluate the effect of different bonding agents and resin cements on shear bond strength (SBS) between acrylic resin teeth and resin composite. Thirty acrylic teeth were cut along the long axis and embedded in cold-cure acrylic resin. The specimens were randomly divided into 3 groups (n = 10) according to the types of luting agents: Group C (OptiBond FL), Group P (Panavia F2.0), and Group S (Superbond C&B). SBS was measured using the Shimadzu EZ-S Universal Testing Machine. The collected data were analyzed using a one-way ANOVA to determine significant differences with P-value < 0.05. Multiple comparisons of SBS were calculated using the Tukey HSD test at a 95% confidence level. The average SBS values in MPa were 5.78 ± 0.97 for Group C, 13.60 ± 1.20 for Group P, and 17.93 ± 1.24 for Group S. The SBS value for Group S was significantly higher compared to the other groups, while the value for Group C was significantly lower. Group C was categorized as an adhesive failure, while Group S was accounted as a cohesive failure and Group P was shown to be a mixed failure. In conclusion, different resin cements significantly affected the SBS between acrylic resin teeth and resin composite. Keywords: Acrylic denture tooth, Bonding agent, Resin cement, Resin composite, Shear bond strength Funding: The authors are grateful for the research funding provided by the College of Dental Medicine, Rangsit University, Thailand. Citation: Srihatajati, J. and Krassanairawiwong, P. 2021. Effect of different resin cements on shear bond strength between acrylic denture teeth and resin composite. CMU J. Nat. Sci. 21(1): e2022011.
- Open Access
- 10 August 2021
- Published by Wiley in International Journal of Dentistry
- Vol. 2021, 1-9
The Influence of Different Surface Cleansing Agents on Shear Bond Strength of Contaminated Lithium Disilicate Ceramic: An In Vitro Study
Background and Purpose. Contamination of the lithium disilicate (LDS) during the try-in procedure is unavoidable and may weaken the bond strength of restoration. The purpose of this study was to investigate the efficacy of different surface cleansing agents on the shear bond strength (SBS) of contaminated LDS. Materials and Methods. Seventy LDS specimens were randomly divided into seven groups. The first group was noncontaminated surface (PC). The six other groups were contaminated with the saliva and silicone disclosing medium and treated with no surface cleansing agent (NC); phosphoric acid (PO); Ivoclean (IV); sodium hydroxide solution (NA); Restorative Cleansing Agent (RC); and hydrofluoric acid (HF). Then, LDS specimens were cementated with Panavia V5 to resin composite rod. Each specimen was subjected to an SBS test. The modes of failure was inspected under light microscope. The surface element of each group was examined by SEM-EDS. Results. The results were analyzed with one-way ANOVA and Tamhane’s T2. The mean SBS value of NC was significantly lower than others ( ), and HF was significantly higher than others ( ). However, PC, PO, IV, NA, and RC were not significantly different from each other ( ). The mode of failure was mostly adhesive failure in every group. The surface showed similar amount of elements in every group. Conclusions. The SBS of LDS was reduced by saliva and silicone disclosing medium contamination which can be restored using acid- and alkaline-based surface cleansing agents before the cementation procedure.
- 10 August 2021
- Published by Wiley in International Journal of Dentistry
- Vol. 2021, 1-9
Open AccessThe Influence of Different Surface Cleansing Agents on Shear Bond Strength of Contaminated Lithium Disilicate Ceramic: An In Vitro Study
Background and Purpose. Contamination of the lithium disilicate (LDS) during the try-in procedure is unavoidable and may weaken the bond strength of restoration. The purpose of this study was to investigate the efficacy of different surface cleansing agents on the shear bond strength (SBS) of contaminated LDS. Materials and Methods. Seventy LDS specimens were randomly divided into seven groups. The first group was noncontaminated surface (PC). The six other groups were contaminated with the saliva and silicone disclosing medium and treated with no surface cleansing agent (NC); phosphoric acid (PO); Ivoclean (IV); sodium hydroxide solution (NA); Restorative Cleansing Agent (RC); and hydrofluoric acid (HF). Then, LDS specimens were cementated with Panavia V5 to resin composite rod. Each specimen was subjected to an SBS test. The modes of failure was inspected under light microscope. The surface element of each group was examined by SEM-EDS. Results. The results were analyzed with one-way ANOVA and Tamhane’s T2. The mean SBS value of NC was significantly lower than others ( ), and HF was significantly higher than others ( ). However, PC, PO, IV, NA, and RC were not significantly different from each other ( ). The mode of failure was mostly adhesive failure in every group. The surface showed similar amount of elements in every group. Conclusions. The SBS of LDS was reduced by saliva and silicone disclosing medium contamination which can be restored using acid- and alkaline-based surface cleansing agents before the cementation procedure.