Jirat Srihatajati
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Jirat Srihatajati has a total of 1 co-authors. Here are the top co-authors by number of shared publications:
- Pattarawadee Krassanairawiwong
Prosthodontics Department, College of Dental Medicine, Rangsit University, Mueang, Pathum Thani, Thailand, rsu.ac.th
1 shared publication
Latest Publications
- Open Access
- 1 January 2026
- Published by Wiley in International Journal of Dentistry
- Vol. 2026 (1)
Evaluation of Shear Bond Strength and Surface Morphology (via SEM) of Different Provisional Crowns and Surface Treatments to PMMA
Purpose of the Study: To compare the shear bond strengths (SBSs) of different provisional crown materials with various surface treatments when relined with autopolymerizing polymethyl methacrylate (PMMA). Materials and Methods: Part 1: Seventy‐five specimens were divided into five groups: PMAC (autopolymerizing PMMA), PMAM (CAD/CAM system PMMA), PMAD (3D‐printed PMMA), PLAI (injectable polylactic acid [PLA]), and PLAD (3D‐printed PLA). All specimens were surface‐treated by sandblasting followed by 180 s of MMA application, then relined with autopolymerizing PMMA. Part 2: Forty‐five PLAD specimens were divided into three groups: PLAD (control), PLAD MC (methylene chloride treatment), and PLAD AT (acetone treatment), then relined with autopolymerizing PMMA. All samples underwent thermocycling before being evaluated for SBS with a universal testing machine (Shimadzu, Japan). Statistical analysis was performed using one‐way ANOVA and Tukey’s HSD at a significance level of p ≤ 0.05. Failure modes were examined using a stereomicroscope, and surface morphology was evaluated by scanning electron microscopy (SEM). Result: In Part 1, the mean SBS values in MPa were: PMAC (26.85 ± 1.31), PMAM (22.92 ± 1.20), PMAD (13.98 ± 1.20), PLAI (10.19 ± 1.59), and PLAD (8.44 ± 1.14). Significant differences were found between all groups ( p ≤ 0.05). In Part 2, the mean SBS values in MPa were: PLAD (8.44 ± 1.14), PLAD MC (8.35 ± 0.84), and PLAD AT (7.83 ± 1.13). No significant differences were found between the three groups ( p > 0.05). PMAC, PMAM, and PMAD exhibited mixed failure modes in 87.5%, 80%, and 73.3% at the fractured surfaces of the specimens, respectively. In contrast, PLAD and PLAI displayed 100% adhesive failure. PLAD, PLAD MC, and PLAD AT also showed 100% adhesive failure at fractured surfaces. Conclusion: The PMAC group achieved the highest SBS among all tested materials. Surface treatment of PLAD with methylene chloride or acetone did not significantly improve SBS compared to the untreated control.
- 1 January 2026
- Published by Wiley in International Journal of Dentistry
- Vol. 2026 (1)
Open AccessEvaluation of Shear Bond Strength and Surface Morphology (via SEM) of Different Provisional Crowns and Surface Treatments to PMMA
Purpose of the Study: To compare the shear bond strengths (SBSs) of different provisional crown materials with various surface treatments when relined with autopolymerizing polymethyl methacrylate (PMMA). Materials and Methods: Part 1: Seventy‐five specimens were divided into five groups: PMAC (autopolymerizing PMMA), PMAM (CAD/CAM system PMMA), PMAD (3D‐printed PMMA), PLAI (injectable polylactic acid [PLA]), and PLAD (3D‐printed PLA). All specimens were surface‐treated by sandblasting followed by 180 s of MMA application, then relined with autopolymerizing PMMA. Part 2: Forty‐five PLAD specimens were divided into three groups: PLAD (control), PLAD MC (methylene chloride treatment), and PLAD AT (acetone treatment), then relined with autopolymerizing PMMA. All samples underwent thermocycling before being evaluated for SBS with a universal testing machine (Shimadzu, Japan). Statistical analysis was performed using one‐way ANOVA and Tukey’s HSD at a significance level of p ≤ 0.05. Failure modes were examined using a stereomicroscope, and surface morphology was evaluated by scanning electron microscopy (SEM). Result: In Part 1, the mean SBS values in MPa were: PMAC (26.85 ± 1.31), PMAM (22.92 ± 1.20), PMAD (13.98 ± 1.20), PLAI (10.19 ± 1.59), and PLAD (8.44 ± 1.14). Significant differences were found between all groups ( p ≤ 0.05). In Part 2, the mean SBS values in MPa were: PLAD (8.44 ± 1.14), PLAD MC (8.35 ± 0.84), and PLAD AT (7.83 ± 1.13). No significant differences were found between the three groups ( p > 0.05). PMAC, PMAM, and PMAD exhibited mixed failure modes in 87.5%, 80%, and 73.3% at the fractured surfaces of the specimens, respectively. In contrast, PLAD and PLAI displayed 100% adhesive failure. PLAD, PLAD MC, and PLAD AT also showed 100% adhesive failure at fractured surfaces. Conclusion: The PMAC group achieved the highest SBS among all tested materials. Surface treatment of PLAD with methylene chloride or acetone did not significantly improve SBS compared to the untreated control.