Konstantin V. Knyaz’KOv
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Konstantin V. Knyaz’KOv has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Aleksandr N. Smirnov
T.F. Gorbachev Kuzbass State Technical University
4 shared publications - Nikolay V. Ababkov
T.F. Gorbachev Kuzbass State Technical University
4 shared publications - Elena L. Nikonenko
Tomsk State University of Architecture and Building
3 shared publications - Natal'YA A. Popova
Tomsk State University of Architecture and Building, Tomsk, Russia
3 shared publications - E. E. Levashova
T.F. Gorbachev Kuzbass State Technical University, Kemerovo, Russia
2 shared publications - Maxim V. Pimonov
T.F. Gorbachev Kuzbass State Technical University
1 shared publication
Latest Publications
- Open Access
- 27 August 2026
- Published by T.F. Gorbachev Kuzbass State Technicak University in Vestnik of Kuzbass State Technical University
- No. 3
INFLUENCE OF THE WELDING METHOD OF CORROSION-RESISTANT AUSTENITIC 0.12C-18Cr-10Ni-Ti STEEL ON THE STRUCTURAL STATE
This paper presents the results of a study of welded joints made from 0.12C-18Cr-10Ni-Ti steel blanks in the fusion line zone on both the base metal side and the weld metal side (deposited metal) after manual arc welding (MMA) using standard technology, after semiautomatic argon welding, and after laser welding. Under real-world operating conditions, most welded joints made from corrosion-resistant austenitic steels operate in aggressive environments and under increased loads, which can lead to damage accumulation and elastic-plastic deformation. Furthermore, welded joints of technical devices of hazardous industrial facilities (TDHF) after installation (repair), according to Rostekhnadzor guidelines, must undergo hydraulic testing with elevated pressure or loads exceeding the design load by up to 25% before being put into operation. Corrosion-resistant steels are readily weldable, but specific grades require the development of specialized technologies. The thermal cycle of welding results in complex physical and chemical processes associated with phase transformations and localized structural changes in the metal's heat-affected zone (HAZ). These processes often lead to undesirable effects, such as grain growth, alloying element segregation, intermetallic formation, and, consequently, reduced performance. Based on studies of welded joint samples produced by various methods, it can be concluded that the most advanced joints are produced using both manual arc welding and semiautomatic argon-arc welding with a consumable electrode. Laser welding offers potential for achieving satisfactory performance characteristics in welded joints, but careful selection of the welding mode is necessary.
- 27 August 2026
- Published by T.F. Gorbachev Kuzbass State Technicak University in Vestnik of Kuzbass State Technical University
- No. 3
Open AccessINFLUENCE OF THE WELDING METHOD OF CORROSION-RESISTANT AUSTENITIC 0.12C-18Cr-10Ni-Ti STEEL ON THE STRUCTURAL STATE
This paper presents the results of a study of welded joints made from 0.12C-18Cr-10Ni-Ti steel blanks in the fusion line zone on both the base metal side and the weld metal side (deposited metal) after manual arc welding (MMA) using standard technology, after semiautomatic argon welding, and after laser welding. Under real-world operating conditions, most welded joints made from corrosion-resistant austenitic steels operate in aggressive environments and under increased loads, which can lead to damage accumulation and elastic-plastic deformation. Furthermore, welded joints of technical devices of hazardous industrial facilities (TDHF) after installation (repair), according to Rostekhnadzor guidelines, must undergo hydraulic testing with elevated pressure or loads exceeding the design load by up to 25% before being put into operation. Corrosion-resistant steels are readily weldable, but specific grades require the development of specialized technologies. The thermal cycle of welding results in complex physical and chemical processes associated with phase transformations and localized structural changes in the metal's heat-affected zone (HAZ). These processes often lead to undesirable effects, such as grain growth, alloying element segregation, intermetallic formation, and, consequently, reduced performance. Based on studies of welded joint samples produced by various methods, it can be concluded that the most advanced joints are produced using both manual arc welding and semiautomatic argon-arc welding with a consumable electrode. Laser welding offers potential for achieving satisfactory performance characteristics in welded joints, but careful selection of the welding mode is necessary.
- 1 November 2025
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 70 (11) , 544-551
Influence of Cladding with Flux-Cored Wire on the Structural–Phase State of Steel 20
Using transmission diffraction electron microscopy methods on thin foils, the influence of the metal of surfacing with welding wire of type 0.35С–5Cr–1Mn–1V–1Ni–1W–1Mo–Fe on the structure of the substrate made of steel 20 has been investigated. A quantitative analysis of changes in the fine structure of the substrate and surfacing materials at different distances (0.5 and 3.0 mm) from the fusion line has been performed. The morphological components of the structure, their volume fraction and phase composition have been determined. It has been established that in the initial state, steel 20 is represented by lamellar pearlite and ferrite. Surfacing with welding wire has led to significant destruction of lamellar pearlite, complete fragmentation of ferrite, release of small cementite particles at the boundaries and joints of ferrite fragments, creation of an elastically stressed state of the steel matrix, and strengthening of the substrate by 1.5 times.
- 1 November 2025
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 70 (11) , 544-551
Influence of Cladding with Flux-Cored Wire on the Structural–Phase State of Steel 20
Using transmission diffraction electron microscopy methods on thin foils, the influence of the metal of surfacing with welding wire of type 0.35С–5Cr–1Mn–1V–1Ni–1W–1Mo–Fe on the structure of the substrate made of steel 20 has been investigated. A quantitative analysis of changes in the fine structure of the substrate and surfacing materials at different distances (0.5 and 3.0 mm) from the fusion line has been performed. The morphological components of the structure, their volume fraction and phase composition have been determined. It has been established that in the initial state, steel 20 is represented by lamellar pearlite and ferrite. Surfacing with welding wire has led to significant destruction of lamellar pearlite, complete fragmentation of ferrite, release of small cementite particles at the boundaries and joints of ferrite fragments, creation of an elastically stressed state of the steel matrix, and strengthening of the substrate by 1.5 times.
- Open Access
- 30 September 2024
- Published by Altai State Technical University in Фундаментальные проблемы современного материаловедения
- Vol. 21 (3) , 345-356
ВЛИЯНИЕ НАПЛАВКИ ПОРОШКОВОЙ ПРОВОЛОКОЙ НА СТРУКТУРНО-ФАЗОВОЕ СОСТОЯНИЕ СТАЛИ 20
Методами просвечивающей дифракционной электронной микроскопии на тонких фольгах проведены исследования влияния металла наплавки, выполненной сварочной проволокой типа 35Х5ГФНВМ, на структуру подложки из стали 20. Выполнен количественный анализ изменения тонкой структуры материалов подложки и наплавки на различном расстоянии (0,5 и 3,0 мм) от линии сплавления. Определены морфологические составляющие структуры, их объемная доля и фазовый состав. Установлено, что в исходном состоянии сталь 20 представлена пластинчатым перлитом и ферритом. Наплавка сварочной проволокой привела к существенному разрушению пластинчатого перлита, полной фрагментации феррита, выделению мелких частиц цементита на границах и в стыках фрагментов феррита, созданию упруго-напряженного состояния матрицы стали и упрочнению подложки в 1,5 раза.
- 30 September 2024
- Published by Altai State Technical University in Фундаментальные проблемы современного материаловедения
- Vol. 21 (3) , 345-356
Open AccessВЛИЯНИЕ НАПЛАВКИ ПОРОШКОВОЙ ПРОВОЛОКОЙ НА СТРУКТУРНО-ФАЗОВОЕ СОСТОЯНИЕ СТАЛИ 20
Методами просвечивающей дифракционной электронной микроскопии на тонких фольгах проведены исследования влияния металла наплавки, выполненной сварочной проволокой типа 35Х5ГФНВМ, на структуру подложки из стали 20. Выполнен количественный анализ изменения тонкой структуры материалов подложки и наплавки на различном расстоянии (0,5 и 3,0 мм) от линии сплавления. Определены морфологические составляющие структуры, их объемная доля и фазовый состав. Установлено, что в исходном состоянии сталь 20 представлена пластинчатым перлитом и ферритом. Наплавка сварочной проволокой привела к существенному разрушению пластинчатого перлита, полной фрагментации феррита, выделению мелких частиц цементита на границах и в стыках фрагментов феррита, созданию упруго-напряженного состояния матрицы стали и упрочнению подложки в 1,5 раза.
- Open Access
- 2 September 2021
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 64 (8) , 572-580
Influence of deformation degree of austenitic steels welded joints on structural state and internal stresses felds in weld line zone
Nowadays initial assessment of welding quality is performed by testing equipment with increased loads (high pressure) at technical devices of hazardous production facilities. Test requirements are regulated by standardized documents of the Federal Service for Environmental, Technological and Nuclear Oversight of Russia (Rostekhnadzor). Recently, along with traditional tests, a “stress test” was used – the essence of which is to load pipeline section to the yield point, followed by leak test. However, in scientifc publications there is practically no information about physical processes occurring in the base metal and in welded joints during such tests. In addition, effect of preload (deformation) on the parameters of substructure and internal stresses feld in welded joints of austenitic steels and, consequently, on the further troublefree operation of the tested equipment was not evaluated. The paper analyzes changes in structural state and values of internal stresses in the samples of austenitic steel under the action of high loads. It substantiates the use of modulated current welding with automatic control of heat input process in molten weld pool. The admissible limits values of plastic deformation are argued when testing technical devices with high pressure for this type of steel. In order to reduce the risk of damage to austenitic steels welded joints of technical devices of hazardous industrial facilities, performed by pulsed welding with smalldrop transfer, and to exclude formation of microdefects in them, high pressure tests (stress test) can be performed under loads that create deformations in metal, not exceeding 5 %. For joints welded by manual arc welding, deformations should be less than 5 %. Welded joints made by pulsed welding with largedrop transfer (with and without defects) are not recommended to be tested with high pressure.
- 2 September 2021
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 64 (8) , 572-580
Open AccessInfluence of deformation degree of austenitic steels welded joints on structural state and internal stresses felds in weld line zone
Nowadays initial assessment of welding quality is performed by testing equipment with increased loads (high pressure) at technical devices of hazardous production facilities. Test requirements are regulated by standardized documents of the Federal Service for Environmental, Technological and Nuclear Oversight of Russia (Rostekhnadzor). Recently, along with traditional tests, a “stress test” was used – the essence of which is to load pipeline section to the yield point, followed by leak test. However, in scientifc publications there is practically no information about physical processes occurring in the base metal and in welded joints during such tests. In addition, effect of preload (deformation) on the parameters of substructure and internal stresses feld in welded joints of austenitic steels and, consequently, on the further troublefree operation of the tested equipment was not evaluated. The paper analyzes changes in structural state and values of internal stresses in the samples of austenitic steel under the action of high loads. It substantiates the use of modulated current welding with automatic control of heat input process in molten weld pool. The admissible limits values of plastic deformation are argued when testing technical devices with high pressure for this type of steel. In order to reduce the risk of damage to austenitic steels welded joints of technical devices of hazardous industrial facilities, performed by pulsed welding with smalldrop transfer, and to exclude formation of microdefects in them, high pressure tests (stress test) can be performed under loads that create deformations in metal, not exceeding 5 %. For joints welded by manual arc welding, deformations should be less than 5 %. Welded joints made by pulsed welding with largedrop transfer (with and without defects) are not recommended to be tested with high pressure.