Guoling Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Guoling Zhang has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Guogang Yang
Marine engineering college, Dalian Maritime University, Dalian 116000, China
4 shared publications - Hao Wang
Marine Engineering College, Dalian Maritime University, Dalian 116026, China
4 shared publications - Qiuwan Shen
Marine Engineering College, Dalian Maritime University, Dalian, China
4 shared publications - Shian Li
Marine Engineering College, Dalian Maritime University, Dalian, China
4 shared publications - Jiadong Liao
Marine Engineering College, Dalian Maritime University, Dalian 116026, China
3 shared publications - Zheng Li
Marine Engineering College, Dalian Maritime University, Dalian 116026, China
3 shared publications
Latest Publications
- Open Access
Pore-Scale Investigation of Mass Transport in Compressed Cathode Gas Diffusion Layer of Proton Exchange Membrane Fuel Cells
Proton exchange membrane fuel cells (PEMFCs) are considered a promising energy source in the field of transport and distributed power generation. Fundamental research into their key components is needed to improve PEMFC performance and accelerate commercialization. Binder addition and compression induced by assembly pressure can significantly change the microstructure of the gas diffusion layer and affect mass transport. A two-dimensional multicomponent lattice Boltzmann (LB) model considering the cathode electrochemical reaction was developed, and a GDL was reconstructed numerically and considering a binder structure. The effects of the binder and compression on mass transport and electrochemical performance within the GDL were investigated. The results showed that an increase in binder volume fraction led to more chain-like structures and closed pores that were unfavorable for mass transport. Compression increased the mass transfer resistance of the GDL in the region under the rib, leading to a decrease in oxygen concentration and local current density.
Open AccessPore-Scale Investigation of Mass Transport in Compressed Cathode Gas Diffusion Layer of Proton Exchange Membrane Fuel Cells
Proton exchange membrane fuel cells (PEMFCs) are considered a promising energy source in the field of transport and distributed power generation. Fundamental research into their key components is needed to improve PEMFC performance and accelerate commercialization. Binder addition and compression induced by assembly pressure can significantly change the microstructure of the gas diffusion layer and affect mass transport. A two-dimensional multicomponent lattice Boltzmann (LB) model considering the cathode electrochemical reaction was developed, and a GDL was reconstructed numerically and considering a binder structure. The effects of the binder and compression on mass transport and electrochemical performance within the GDL were investigated. The results showed that an increase in binder volume fraction led to more chain-like structures and closed pores that were unfavorable for mass transport. Compression increased the mass transfer resistance of the GDL in the region under the rib, leading to a decrease in oxygen concentration and local current density.
- Open Access
Effects of Compression and Porosity Gradients on Two-Phase Behavior in Gas Diffusion Layer of Proton Exchange Membrane Fuel Cells
Water management within the gas diffusion layer (GDL) plays an important role in the performance of the proton exchange membrane fuel cell (PEMFC) and its reliability. The compression of the gas diffusion layer during fabrication and assembly has a significant impact on the mass transport, and the porosity gradient design of the gas diffusion layer is an essential way to improve water management. In this paper, the two-dimensional lattice Boltzmann method (LBM) is applied to investigate the two-phase behavior in gas diffusion layers with different porosity gradients under compression. Compression results in an increase in flow resistance below the ribs, prompting the appearance of the flow path of liquid water below the channel, and liquid water breaks through to the channel more quickly. GDLs with linear, multilayer, and inverted V-shaped porosity distributions with an overall porosity of 0.78 are generated to evaluate the effect of porosity gradients on the liquid water transport. The liquid water saturation values within the linear and multilayer GDLs are significantly reduced compared to that of the GDL with uniform porosity, but the liquid water within the inverted V-shaped GDL accumulates in the middle region and is more likely to cause flooding.
Open AccessEffects of Compression and Porosity Gradients on Two-Phase Behavior in Gas Diffusion Layer of Proton Exchange Membrane Fuel Cells
Water management within the gas diffusion layer (GDL) plays an important role in the performance of the proton exchange membrane fuel cell (PEMFC) and its reliability. The compression of the gas diffusion layer during fabrication and assembly has a significant impact on the mass transport, and the porosity gradient design of the gas diffusion layer is an essential way to improve water management. In this paper, the two-dimensional lattice Boltzmann method (LBM) is applied to investigate the two-phase behavior in gas diffusion layers with different porosity gradients under compression. Compression results in an increase in flow resistance below the ribs, prompting the appearance of the flow path of liquid water below the channel, and liquid water breaks through to the channel more quickly. GDLs with linear, multilayer, and inverted V-shaped porosity distributions with an overall porosity of 0.78 are generated to evaluate the effect of porosity gradients on the liquid water transport. The liquid water saturation values within the linear and multilayer GDLs are significantly reduced compared to that of the GDL with uniform porosity, but the liquid water within the inverted V-shaped GDL accumulates in the middle region and is more likely to cause flooding.
- Open Access
Transient Multi-Physics Modeling and Performance Degradation Evaluation of Direct Internal Reforming Solid Oxide Fuel Cell Focusing on Carbon Deposition Effect
The performance degradation issue caused by carbon deposition has limited the commercial application of natural-gas-fueled solid oxide fuel cells. Most previous corresponding studies are based on thermodynamic equilibrium analyses, while long-term transient evaluation work is lacking. Therefore, a transient multi-physics numerical model is developed in present work. The corresponding long-term performance degradation evaluation is then conducted. The results show that, for a direct internal reforming solid oxide fuel cell, the increase in carbon deposition and deterioration of performance degradation were concentrated in the first 180 days of steady−state operation and slowed down at the later stage. The electrode inlet rapidly developed a high concentration of carbon deposition after 180 days of steady−state operation. The deposited carbon deteriorated the gas transport and decayed reaction activity within the porous electrode, eventually inducing a deactivation zone with 0 current density at the inlet. Key measures to inhibit carbon deposition should be implemented within the first 180 days of operation, and the pre-reformed operation of natural gas is encouraged for natural-gas-fueled solid oxide fuel cells.
Open AccessTransient Multi-Physics Modeling and Performance Degradation Evaluation of Direct Internal Reforming Solid Oxide Fuel Cell Focusing on Carbon Deposition Effect
The performance degradation issue caused by carbon deposition has limited the commercial application of natural-gas-fueled solid oxide fuel cells. Most previous corresponding studies are based on thermodynamic equilibrium analyses, while long-term transient evaluation work is lacking. Therefore, a transient multi-physics numerical model is developed in present work. The corresponding long-term performance degradation evaluation is then conducted. The results show that, for a direct internal reforming solid oxide fuel cell, the increase in carbon deposition and deterioration of performance degradation were concentrated in the first 180 days of steady−state operation and slowed down at the later stage. The electrode inlet rapidly developed a high concentration of carbon deposition after 180 days of steady−state operation. The deposited carbon deteriorated the gas transport and decayed reaction activity within the porous electrode, eventually inducing a deactivation zone with 0 current density at the inlet. Key measures to inhibit carbon deposition should be implemented within the first 180 days of operation, and the pre-reformed operation of natural gas is encouraged for natural-gas-fueled solid oxide fuel cells.
- Open Access
Effects of Hydration and Temperature on the Microstructure and Transport Properties of Nafion Polyelectrolyte Membrane: A Molecular Dynamics Simulation
To investigate the effects of temperature and hydration on the microstructure of polymer electrolyte membrane and the transport of water molecules and hydronium ions, molecular dynamics simulations are performed on Nafion 117 for a series of water contents at different temperatures. The interactions among the sulfonate groups, hydronium ions, and water molecules are studied according to the analysis of radial distribution functions and coordination numbers. The sizes and connectivity of water clusters are also discussed, and it is found that the hydration level plays a key role in the phase separation of the membrane. However, the effect of the temperature is slight. When the water content increases from 3.5 to 16, the size of water clusters in the membrane increases, and the clusters connect to each other to form continuous channels for diffusion of water molecules and hydronium ions. The diffusion coefficients are estimated by studying the mean square displacements. The results show that the diffusion of water molecules and hydronium ions are both enhanced by the increase of the temperature and hydration level. Furthermore, the diffusion coefficient of water molecules is always much larger than that of hydronium ions. However, the ratio of the diffusion coefficient of water molecules to that of hydronium ions decreases with the increase of water content.
Open AccessEffects of Hydration and Temperature on the Microstructure and Transport Properties of Nafion Polyelectrolyte Membrane: A Molecular Dynamics Simulation
To investigate the effects of temperature and hydration on the microstructure of polymer electrolyte membrane and the transport of water molecules and hydronium ions, molecular dynamics simulations are performed on Nafion 117 for a series of water contents at different temperatures. The interactions among the sulfonate groups, hydronium ions, and water molecules are studied according to the analysis of radial distribution functions and coordination numbers. The sizes and connectivity of water clusters are also discussed, and it is found that the hydration level plays a key role in the phase separation of the membrane. However, the effect of the temperature is slight. When the water content increases from 3.5 to 16, the size of water clusters in the membrane increases, and the clusters connect to each other to form continuous channels for diffusion of water molecules and hydronium ions. The diffusion coefficients are estimated by studying the mean square displacements. The results show that the diffusion of water molecules and hydronium ions are both enhanced by the increase of the temperature and hydration level. Furthermore, the diffusion coefficient of water molecules is always much larger than that of hydronium ions. However, the ratio of the diffusion coefficient of water molecules to that of hydronium ions decreases with the increase of water content.