Penpisuth Thongyoug
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Penpisuth Thongyoug has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Jennarong Tungtrongpairoj
Department of Materials and Production Technology Engineering, Faculty of Engineering King Mongkut's University of Technology North Bangkok Bangkok Thailand
3 shared publications Jennarong Tungtrongpairoj
King Mongkut’s University of Technology North Bangkok
2 shared publicationsChayada Teanchaie
Research Center, Faculty of Dentistry Mahidol University, 6 Yothi Alley, Thung Phaya Thai, Ratchathewi, Bangkok 10400, Thailand
1 shared publication- Jennarong Tungtrongpairoj
Faculty of Engineering, King Mongkut’s University of Technology North Bangkok
1 shared publication Krongthong Kamonsuangkasem
Synchrotron Light Research Institute (Public Organization)
1 shared publication- Mack Boonpensina
High Temperature Corrosion Research Centre, Department of Materials and Production Technology Engineering, King Mongkut’s University of Technology North Bangkok, 1518, Pracharat 1 Road, Bangsue, Bangkok, 10800, Thailand
1 shared publication
Latest Publications
- 29 October 2025
- Published by Trans Tech Publications, Ltd. in Solid State Phenomena
- Vol. 378, 39-44
High Temperature Oxidation of Fe-18Cr-Nano Al2O3 ODS Steel in Humidified Atmospheres
One candidate material for boiler components in supercritical water gasification (SCWG) processes is oxide dispersion-strengthened steels (ODS), which can resist aggressive humidified atmospheres under high pressures and temperatures. The high-temperature oxidation resistance of ODS steel can be improved by adding nanooxide particles such as Al 2 O 3 . In this study, the corrosion resistance of Fe-18Cr ferritic ODS steel reinforced with different nanoAl 2 O 3 between 0.5-3.0 wt% in a humidified atmosphere containing 80% H 2 O at 800 °C was investigated. The lump phase of chromium and nanoAl 2 O 3 particles were dispersed on iron matrixes after sintering. Several pores occurred in the Fe-18Cr ODS matrix due to air entrainment during forming processes, but they decreased after reinforcing with the nanoAl 2 O 3 . Adding 0.5 wt% nanoAl 2 O 3 decreased the porosity of the ODS steel by around 1.8 times. After the oxidation test for 10 hours, the mass gain of the ferritic ODS steel decreased by about 9 % when the nanooxide was added. Fe-Al-rich oxides were found with hematite and Fe-Cr spinel oxide layers, which increased the oxidation resistance of the ODS steel.
- 29 October 2025
- Published by Trans Tech Publications, Ltd. in Solid State Phenomena
- Vol. 378, 39-44
High Temperature Oxidation of Fe-18Cr-Nano Al2O3 ODS Steel in Humidified Atmospheres
One candidate material for boiler components in supercritical water gasification (SCWG) processes is oxide dispersion-strengthened steels (ODS), which can resist aggressive humidified atmospheres under high pressures and temperatures. The high-temperature oxidation resistance of ODS steel can be improved by adding nanooxide particles such as Al 2 O 3 . In this study, the corrosion resistance of Fe-18Cr ferritic ODS steel reinforced with different nanoAl 2 O 3 between 0.5-3.0 wt% in a humidified atmosphere containing 80% H 2 O at 800 °C was investigated. The lump phase of chromium and nanoAl 2 O 3 particles were dispersed on iron matrixes after sintering. Several pores occurred in the Fe-18Cr ODS matrix due to air entrainment during forming processes, but they decreased after reinforcing with the nanoAl 2 O 3 . Adding 0.5 wt% nanoAl 2 O 3 decreased the porosity of the ODS steel by around 1.8 times. After the oxidation test for 10 hours, the mass gain of the ferritic ODS steel decreased by about 9 % when the nanooxide was added. Fe-Al-rich oxides were found with hematite and Fe-Cr spinel oxide layers, which increased the oxidation resistance of the ODS steel.
- 23 September 2024
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 1125, 11-17
Influence of Reinforcing nano-Al2O3 Particles on Microstructure and Hardness Properties of HVOF Sprayed 80Ni20Cr Coatings
80Ni20Cr coatings produced by high-velocity oxygen fuel (HVOF) thermal spray technique are novel and widely used to improve the corrosion and wear resistance of metal and steel components in many applications, especially in coal-fired power plants. The present study investigated the effects of nano-Al2O3 at 0.5 wt.% on the microstructure of HVOF-sprayed 80Ni20Cr coating deposited on AISI 304L steels corresponding to its coating hardness. The coating was successfully sprayed with a thickness of 150 – 180 µm. The microstructure and phase formed by the coating were analyzed by a field emission electron microscope (FE-SEM) and an X-ray diffractometer (XRD). Synchrotron X-ray fluorescence spectroscopy (SRXRF) was used to confirm the Cr solid solution in the Ni-based coating. The presence of the nano-Al2O3 phase in the 80Ni20Cr coating was characterized by electron backscattered diffraction (EBSD). The nano-Al2O3 particles were homogenously distributed in the coating layers. The incorporation of nano-Al2O3 into 80Ni20Cr enhanced coating characteristics by decreasing surface roughness by 23% and increasing coating hardness by around 4%.
- 23 September 2024
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 1125, 11-17
Influence of Reinforcing nano-Al2O3 Particles on Microstructure and Hardness Properties of HVOF Sprayed 80Ni20Cr Coatings
80Ni20Cr coatings produced by high-velocity oxygen fuel (HVOF) thermal spray technique are novel and widely used to improve the corrosion and wear resistance of metal and steel components in many applications, especially in coal-fired power plants. The present study investigated the effects of nano-Al2O3 at 0.5 wt.% on the microstructure of HVOF-sprayed 80Ni20Cr coating deposited on AISI 304L steels corresponding to its coating hardness. The coating was successfully sprayed with a thickness of 150 – 180 µm. The microstructure and phase formed by the coating were analyzed by a field emission electron microscope (FE-SEM) and an X-ray diffractometer (XRD). Synchrotron X-ray fluorescence spectroscopy (SRXRF) was used to confirm the Cr solid solution in the Ni-based coating. The presence of the nano-Al2O3 phase in the 80Ni20Cr coating was characterized by electron backscattered diffraction (EBSD). The nano-Al2O3 particles were homogenously distributed in the coating layers. The incorporation of nano-Al2O3 into 80Ni20Cr enhanced coating characteristics by decreasing surface roughness by 23% and increasing coating hardness by around 4%.
- Open Access
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2984 (1) , 040002
Effect of impact angles and velocity on solid particle erosion behavior of boiler steel at room temperature
The objective of this research is to study the effect of impact angles and particle velocities on the solid particle erosion behavior of boiler steel (Fe-23Cr-8
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2984 (1) , 040002
Open AccessEffect of impact angles and velocity on solid particle erosion behavior of boiler steel at room temperature
The objective of this research is to study the effect of impact angles and particle velocities on the solid particle erosion behavior of boiler steel (Fe-23Cr-8
- 26 October 2021
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 39 (1) , 1-11
The degradation of oxide layer on Cr-containing steels in simulated atmospheres on carbothermic reduction
High-temperature corrosion has been a critical issue for coal-fired boiler steels, particularly Cr-containing steels SA213-T22, for many decades. Hot combustion gases containing CO2, CO, N2, and unburnt carbon particles play a significant role in the degradation of oxide scale due to reduction reactions. However, carbide precipitation can occur in the oxide layer by carburisation reactions. The effects of reduction and carburisation on the oxide scale of SA213-T22 steel in a simulated combustion atmosphere by carbothermic reduction were investigated and compared with ferritic stainless steels SS430. The two steels were oxidised under an air atmosphere at 750 °C for 48 hours and heated afterwards in graphite powder at 950–1350 °C for 30–60 minutes. After the oxidation test, a thick porous oxide layer of Fe2O3 was found on the SA213-T22 and a thin Fe-Cr-Mn oxide film was found on SS430 as shown by X-ray diffraction analysis. Most oxide scales on SS430 were reduced and destroyed by carbothermic reduction at 1350 °C but the oxide scale on SA213-T22 transformed to compact mixed phases of Fe-C and Fe-C-Cr-O by carburisation and carbon diffusion. The compact oxide layer with heat resistant carbides can increase wear resistance and might withstand corrosive atmospheres in coal-fire boiler plants.
- 26 October 2021
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 39 (1) , 1-11
The degradation of oxide layer on Cr-containing steels in simulated atmospheres on carbothermic reduction
High-temperature corrosion has been a critical issue for coal-fired boiler steels, particularly Cr-containing steels SA213-T22, for many decades. Hot combustion gases containing CO2, CO, N2, and unburnt carbon particles play a significant role in the degradation of oxide scale due to reduction reactions. However, carbide precipitation can occur in the oxide layer by carburisation reactions. The effects of reduction and carburisation on the oxide scale of SA213-T22 steel in a simulated combustion atmosphere by carbothermic reduction were investigated and compared with ferritic stainless steels SS430. The two steels were oxidised under an air atmosphere at 750 °C for 48 hours and heated afterwards in graphite powder at 950–1350 °C for 30–60 minutes. After the oxidation test, a thick porous oxide layer of Fe2O3 was found on the SA213-T22 and a thin Fe-Cr-Mn oxide film was found on SS430 as shown by X-ray diffraction analysis. Most oxide scales on SS430 were reduced and destroyed by carbothermic reduction at 1350 °C but the oxide scale on SA213-T22 transformed to compact mixed phases of Fe-C and Fe-C-Cr-O by carburisation and carbon diffusion. The compact oxide layer with heat resistant carbides can increase wear resistance and might withstand corrosive atmospheres in coal-fire boiler plants.
- Open Access
- 1 August 2021
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1163 (1) , 012023
The Degradation of SA213-T22 steels Coated with Ni-based Alloy Containing WC-Co in Simulated Molten Salt Atmospheres
This work reveals the high-temperature oxidation resistance of WC-Co coated on SA213-T22 by High-Velocity Oxy-Fuel (HVOF) technique in simulated molten salt atmospheres and compare that with the uncoated Cr-containing steel. The corrosion behaviors of SA213-T22 coated and uncoated with WC-Co alloys were studied by immersion test under simulated molten salt atmospheres at 600 °C for 3 hours and investigated their corrosion current densities by electrochemical test. Scanning electron microscope equipped with EDS technique and X-ray diffraction were used to evaluate the surface morphology and phase constitution. The oxidation rate of the coated and uncoated steels was observed under simulated atmospheres at 750 °C for 120 hours before the immersion test. The mass gain scale increase with increasing the oxidation time and the oxidation rate of scale are limited by the WC-Co alloys coating layer, which acted as a protective layer. The low corrosion current density of the WC-Co self-fluxing coated steel after oxidation was shown 5 – 10 μA/cm 2 after the corrosion test in molten salt for 3 hours. After the immersion, the scale layer on the uncoated specimen was disappeared, but one-half of the oxidized coating layer on the coated specimen has remained.
- 1 August 2021
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1163 (1) , 012023
Open AccessThe Degradation of SA213-T22 steels Coated with Ni-based Alloy Containing WC-Co in Simulated Molten Salt Atmospheres
This work reveals the high-temperature oxidation resistance of WC-Co coated on SA213-T22 by High-Velocity Oxy-Fuel (HVOF) technique in simulated molten salt atmospheres and compare that with the uncoated Cr-containing steel. The corrosion behaviors of SA213-T22 coated and uncoated with WC-Co alloys were studied by immersion test under simulated molten salt atmospheres at 600 °C for 3 hours and investigated their corrosion current densities by electrochemical test. Scanning electron microscope equipped with EDS technique and X-ray diffraction were used to evaluate the surface morphology and phase constitution. The oxidation rate of the coated and uncoated steels was observed under simulated atmospheres at 750 °C for 120 hours before the immersion test. The mass gain scale increase with increasing the oxidation time and the oxidation rate of scale are limited by the WC-Co alloys coating layer, which acted as a protective layer. The low corrosion current density of the WC-Co self-fluxing coated steel after oxidation was shown 5 – 10 μA/cm 2 after the corrosion test in molten salt for 3 hours. After the immersion, the scale layer on the uncoated specimen was disappeared, but one-half of the oxidized coating layer on the coated specimen has remained.
- Open Access
- 1 November 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 965 (1) , 012024
Carbothermic Reduction of the Waste Chromium Oxide Rods from Thermal Spray Processes
The waste chromium-oxide rods from thermal spray processes contained the valuable components of high chromium. The carbothermic reduction with graphite powders can be used to recover the chromium from the chromium-oxide rod. The waste rods were prepared into small pieces with a half-dimensions of 6.3 mm diameter and 5 mm length, and heated under the reducing atmosphere at 1150 – 1350 °C. Besides, the effect of different types and sizes of reducing agent on the reduction was observed. During the heating and cooling period, argon gas was fed into the atmosphere. Chromium carbide formation was promoted when the temperature and time were increased. Cr-O and Cr-O-Al-Si were observed in the microstructures before and after the reduction. The outermost part of the waste rod can be reduced to chromium because of the interphase zone. Consequently, the carbothermic reduction is one possible recycling method for utilizing ceramic rod wastes from the thermal spray process.
- 1 November 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 965 (1) , 012024
Open AccessCarbothermic Reduction of the Waste Chromium Oxide Rods from Thermal Spray Processes
The waste chromium-oxide rods from thermal spray processes contained the valuable components of high chromium. The carbothermic reduction with graphite powders can be used to recover the chromium from the chromium-oxide rod. The waste rods were prepared into small pieces with a half-dimensions of 6.3 mm diameter and 5 mm length, and heated under the reducing atmosphere at 1150 – 1350 °C. Besides, the effect of different types and sizes of reducing agent on the reduction was observed. During the heating and cooling period, argon gas was fed into the atmosphere. Chromium carbide formation was promoted when the temperature and time were increased. Cr-O and Cr-O-Al-Si were observed in the microstructures before and after the reduction. The outermost part of the waste rod can be reduced to chromium because of the interphase zone. Consequently, the carbothermic reduction is one possible recycling method for utilizing ceramic rod wastes from the thermal spray process.
- 3 August 2020
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 856, 21-28
High Temperature Degradation of Thermal Oxides on AISI 304 Stainless Steels by Carbon
AISI 304 austenitic stainless steel specimens are oxidised in laboratory air at 750 °C for 48 h. They are further subjected to the reduction test in carbon at 1350 °C for 30 and 60 min. The results show that the mass gain of the oxidised AISI 304 slighter increases to be 0.08 mg cm–2 after the reduction for 30 min and is unchanged at the longer reduction period up to 60 min. The oxide on AISI 304 is deteriorated after the reduction but its morphology tends to be unchanged when the reduction period is longer from 30 to 60 min. The results then indicate the superior performance of the AISI 304 to combat the corrosion under carbon at this high temperature.
- 3 August 2020
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 856, 21-28
High Temperature Degradation of Thermal Oxides on AISI 304 Stainless Steels by Carbon
AISI 304 austenitic stainless steel specimens are oxidised in laboratory air at 750 °C for 48 h. They are further subjected to the reduction test in carbon at 1350 °C for 30 and 60 min. The results show that the mass gain of the oxidised AISI 304 slighter increases to be 0.08 mg cm–2 after the reduction for 30 min and is unchanged at the longer reduction period up to 60 min. The oxide on AISI 304 is deteriorated after the reduction but its morphology tends to be unchanged when the reduction period is longer from 30 to 60 min. The results then indicate the superior performance of the AISI 304 to combat the corrosion under carbon at this high temperature.