Jennarong Tungtrongpairoj
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Jennarong Tungtrongpairoj has a total of 29 co-authors. Here are the top co-authors by number of shared publications:
- Boonlom Thavornyutikarn
Biofunctional Materials and Devices Research Group, National Metal and Materials Technology Center Pathum Thani Thailand
3 shared publications - Korbkaroon Doungkeaw
Department of Materials and Production Technology Engineering, Faculty of Engineering, King Mongkut’s University of Technology North Bangkok, Bangkok, Thailand
3 shared publications - Paweena Treewiriyakitja
Department of Materials and Production Technology Engineering, Faculty of Engineering, King Mongkut’s University of Technology North Bangkok, Bang Sue, Thailand
3 shared publications - Penpisuth Thongyoug
Silpakorn University
3 shared publications Boonlom Thavornyutikarn
Biofunctional Materials and Devices Research Group National Metal and Materials Technology Center 114 Thailand Science Park Phahonyothin Road Khlong Nueng Khlong Luang Pathum Thani 12120 Thailand
2 shared publicationsKorbkaroon Doungkeaw
Department of Materials and Production Technology Engineering Faculty of Engineering King Mongkut's University of Technology North Bangkok King Mongkut's University of Technology North Bangkok 10800 Bangkok Thailand
2 shared publications
Latest Publications
- 6 October 2026
- Published by Wiley in Polymer Composites
Experimental and Modeling Investigation of Interfacial Effects on the Mechanical Properties of Iron‐Oxide‐Particle‐Reinforced Acrylonitrile–Butadiene–Styrene Composites for Extrusion‐Based Additive Manufacturing
Waste iron oxide particles generated during steelmaking were proposed as promising reinforcements for enhancing the mechanical properties of acrylonitrile–butadiene–styrene (ABS)‐based composite filaments for extrusion‐based additive manufacturing. The surface chemical states and filler–matrix interfacial bonding in a 1.0 vol% iron oxide/ABS composite were investigated using X‐ray photoelectron spectroscopy. The phase composition and degree of crystallinity of the 3D‐printed composites under different tensile loads were examined using synchrotron wide‐angle X‐ray scattering. Fe 2 O 3 and Fe 3 O 4 phases were detected, and their particles were primarily bonded to the ABS matrix through C–O–H groups. The crystallinity degree of the ABS‐based composite decreased with increasing tensile stress and was accompanied by reduced interfacial bonding. Nanoindentation measurements were performed to determine the interfacial stress around the irregular iron oxide particles. The local stress near the particles was approximately 7% higher than that in the polymer matrix, improving the tensile strength and hardness of the ABS‐based composite. Micromechanical models based on the 3D finite element method were developed to predict stress near the filler particles. The predicted interfacial stresses increased by approximately 20% and 13% when particle size and angularity were doubled, respectively, and high stress concentrations occurred at the iron oxide–matrix interfaces.
- 6 October 2026
- Published by Wiley in Polymer Composites
Experimental and Modeling Investigation of Interfacial Effects on the Mechanical Properties of Iron‐Oxide‐Particle‐Reinforced Acrylonitrile–Butadiene–Styrene Composites for Extrusion‐Based Additive Manufacturing
Waste iron oxide particles generated during steelmaking were proposed as promising reinforcements for enhancing the mechanical properties of acrylonitrile–butadiene–styrene (ABS)‐based composite filaments for extrusion‐based additive manufacturing. The surface chemical states and filler–matrix interfacial bonding in a 1.0 vol% iron oxide/ABS composite were investigated using X‐ray photoelectron spectroscopy. The phase composition and degree of crystallinity of the 3D‐printed composites under different tensile loads were examined using synchrotron wide‐angle X‐ray scattering. Fe 2 O 3 and Fe 3 O 4 phases were detected, and their particles were primarily bonded to the ABS matrix through C–O–H groups. The crystallinity degree of the ABS‐based composite decreased with increasing tensile stress and was accompanied by reduced interfacial bonding. Nanoindentation measurements were performed to determine the interfacial stress around the irregular iron oxide particles. The local stress near the particles was approximately 7% higher than that in the polymer matrix, improving the tensile strength and hardness of the ABS‐based composite. Micromechanical models based on the 3D finite element method were developed to predict stress near the filler particles. The predicted interfacial stresses increased by approximately 20% and 13% when particle size and angularity were doubled, respectively, and high stress concentrations occurred at the iron oxide–matrix interfaces.
- 13 April 2026
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 935, 229-234
Modeling and Investigation of 3D Printing Parameters on the Melt Flow Behavior of Polylactic Acid
3D printing parameters such as printing temperatures and speeds play a vital role in the melt flow and printability of thermoplastic filaments in fused filament fabrication (FFF) technology. Inappropriate print settings mainly induce incomplete and poor printing quality due to melt flow instability. This research work focused on modeling the melt flow behavior of polylactic acid (PLA) at different printing temperatures and speeds using computer fluid dynamics (CFD) method. The shear stress and viscosity of PLA were investigated by a melt flow indexer (MFI) and rheometer in temperature ranges of 200 - 240 °C. A model of a capillary tube in MFI was set up with an initial condition of rheological properties from the experiment to simulate the hot melt extrusion relating to the melt flowability of PLA filaments. The high shear stress and low viscosity presented at the edge of filaments at every printing condition. Additionally, the shear stress and viscosity decreased linearly when the printing temperature increased, while the shear stress increased when the printing speed increased. The increase in shear stress caused high surface roughness of PLA specimens after printing. The findings can guide the optimization of the FFF 3D printing process to improve surface finish quality.
- 13 April 2026
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 935, 229-234
Modeling and Investigation of 3D Printing Parameters on the Melt Flow Behavior of Polylactic Acid
3D printing parameters such as printing temperatures and speeds play a vital role in the melt flow and printability of thermoplastic filaments in fused filament fabrication (FFF) technology. Inappropriate print settings mainly induce incomplete and poor printing quality due to melt flow instability. This research work focused on modeling the melt flow behavior of polylactic acid (PLA) at different printing temperatures and speeds using computer fluid dynamics (CFD) method. The shear stress and viscosity of PLA were investigated by a melt flow indexer (MFI) and rheometer in temperature ranges of 200 - 240 °C. A model of a capillary tube in MFI was set up with an initial condition of rheological properties from the experiment to simulate the hot melt extrusion relating to the melt flowability of PLA filaments. The high shear stress and low viscosity presented at the edge of filaments at every printing condition. Additionally, the shear stress and viscosity decreased linearly when the printing temperature increased, while the shear stress increased when the printing speed increased. The increase in shear stress caused high surface roughness of PLA specimens after printing. The findings can guide the optimization of the FFF 3D printing process to improve surface finish quality.
- 10 February 2024
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 131 (3-4) , 1567-1586
Processing and modeling of 3D-printed mill scale strengthened acrylonitrile butadiene styrene composites
- 10 February 2024
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 131 (3-4) , 1567-1586
Processing and modeling of 3D-printed mill scale strengthened acrylonitrile butadiene styrene composites
- Open Access
- 17 November 2023
- Published by Springer Nature in Research Square
Processing and modeling of mill scale strengthened ABS composites fabricated by fused deposition modeling (FDM): Effects of printing parameters
Mill scale (MS) strengthened acrylonitrile-butadiene-styrene (ABS) composite filaments were fabricated as an optional low-cost and sustainable feedstock material with enhanced strength using fused deposition modeling (FDM) technology. In the present study, the effects of the printing parameters on the mechanical properties of the printed ABS/1.0 vol% MS composites were evaluated. Test specimens of ABS/1.0 vol% MS composites were printed at temperatures of 240–280°C, printing speeds of 10–90 mm s− 1, and infill densities of 25–100%. The average maximum stress and modulus of ABS/1.0 vol% MS samples increased when the printing temperature was raised to 270°C while decreasing the printing speed, with numerous air gaps and pores found in the cross-sectional microstructures after failure at low infill density. High surface roughness of the printed ABS/1.0 vol% MS composites was observed by a 3D laser scanner when printing at high temperatures and speeds due to insufficient cooling. The printed composite microstructures were examined by X-ray micro-computed tomography (µCT), and showed homogeneously dense particle dispersion in the entire printed part. Representative volume element (RVE) based modeling was conducted using real particle geometries from µCT. RVE simulations predicted high local stress distributions around mill scale particles and air gaps in the printed samples.
- 17 November 2023
- Published by Springer Nature in Research Square
Open AccessProcessing and modeling of mill scale strengthened ABS composites fabricated by fused deposition modeling (FDM): Effects of printing parameters
Mill scale (MS) strengthened acrylonitrile-butadiene-styrene (ABS) composite filaments were fabricated as an optional low-cost and sustainable feedstock material with enhanced strength using fused deposition modeling (FDM) technology. In the present study, the effects of the printing parameters on the mechanical properties of the printed ABS/1.0 vol% MS composites were evaluated. Test specimens of ABS/1.0 vol% MS composites were printed at temperatures of 240–280°C, printing speeds of 10–90 mm s− 1, and infill densities of 25–100%. The average maximum stress and modulus of ABS/1.0 vol% MS samples increased when the printing temperature was raised to 270°C while decreasing the printing speed, with numerous air gaps and pores found in the cross-sectional microstructures after failure at low infill density. High surface roughness of the printed ABS/1.0 vol% MS composites was observed by a 3D laser scanner when printing at high temperatures and speeds due to insufficient cooling. The printed composite microstructures were examined by X-ray micro-computed tomography (µCT), and showed homogeneously dense particle dispersion in the entire printed part. Representative volume element (RVE) based modeling was conducted using real particle geometries from µCT. RVE simulations predicted high local stress distributions around mill scale particles and air gaps in the printed samples.
- Open Access
- 27 June 2023
- Published by Metallurgy and Materials Science Research Institute, Chulalongkorn University in Journal of Metals, Materials and Minerals
- Vol. 33 (2) , 156-161
Recycling of iron oxide waste by carbothermic reduction to utilize in FDM 3D printing materials
Iron oxide scale generally forms on low-carbon steel surfaces during the hot rolling processes and produces as solid waste more than 100 thousand tons per year. The utilization of the iron oxide scale is one possible way to reduce the production cost for steel plants and promote environmental protection. Acrylonitrile-Butadiene-Styrol-Copolymer (ABS) is widely used as engineering plastic for automotive parts because of its high strength and wear resistance. The recycling of iron oxide waste as reinforcement particles for enhancing the tensile strength of ABS composite was studied. The iron oxides were recycled by carbon powder at a high temperature between 1150℃ to 1350℃ up to 120 min. After the reduction process, the reduced iron from an optimal condition with the iron-rich fraction was ground to powder. Afterward, the 0.3 vol% to 1.3 vol% powders were mixed with ABS polymer powder and formed as composite filaments for additive manufacturing (FDM 3D printing). The tensile strength of pure ABS filament increased to 37.16 ± 2.37 MPa when added recycled iron powders. The regular distribution and 13.68 ± 9.78 µm of recycled-iron particle sizes on the ABS matrix were investigated and correlated to the mechanical properties.
- 27 June 2023
- Published by Metallurgy and Materials Science Research Institute, Chulalongkorn University in Journal of Metals, Materials and Minerals
- Vol. 33 (2) , 156-161
Open AccessRecycling of iron oxide waste by carbothermic reduction to utilize in FDM 3D printing materials
Iron oxide scale generally forms on low-carbon steel surfaces during the hot rolling processes and produces as solid waste more than 100 thousand tons per year. The utilization of the iron oxide scale is one possible way to reduce the production cost for steel plants and promote environmental protection. Acrylonitrile-Butadiene-Styrol-Copolymer (ABS) is widely used as engineering plastic for automotive parts because of its high strength and wear resistance. The recycling of iron oxide waste as reinforcement particles for enhancing the tensile strength of ABS composite was studied. The iron oxides were recycled by carbon powder at a high temperature between 1150℃ to 1350℃ up to 120 min. After the reduction process, the reduced iron from an optimal condition with the iron-rich fraction was ground to powder. Afterward, the 0.3 vol% to 1.3 vol% powders were mixed with ABS polymer powder and formed as composite filaments for additive manufacturing (FDM 3D printing). The tensile strength of pure ABS filament increased to 37.16 ± 2.37 MPa when added recycled iron powders. The regular distribution and 13.68 ± 9.78 µm of recycled-iron particle sizes on the ABS matrix were investigated and correlated to the mechanical properties.
- Open Access
- 28 March 2023
- Published by Metallurgy and Materials Science Research Institute, Chulalongkorn University in Journal of Metals, Materials and Minerals
- Vol. 33 (1) , 8-13
The high temperature degradation of ferritic stainless steel in solid carbon atmospheres
Stainless steel is widely used for many components and parts in coal-fired thermal power plants. AISI 430 ferritic stainless steel (FSS) is one common grade to combat the degradation at high temperatures in coal combustion atmospheres containing flue gas, coal ash, and soot (impure solid carbon particles). However, the effect of the solid carbon particles on the degradation of FSS needs to be clarified. Graphite powder was used to simulate solid carbon atmospheres for investigating the degradation of AISI 430 at high temperatures of 1150℃ to 1350℃ in coal-fired boilers. After the carbothermic reduction, the mass gain of a pre-oxidized sample at 750℃ was approximately 0.0793 mg⸳cm-2 and increased when increasing the reduction temperature. The peak of Fe2O3 and Cr7C3 were detected by X˗ray diffraction (XRD) after the oxidation and reduction test, respectively. Besides, the degree of sensitivity (%DoS) of the samples was measured by double loop electrochemical potentiokinetic reactivation (DL-EPR) technique and increased around 30 times after heating the pre-oxidized sample to 1150℃.
- 28 March 2023
- Published by Metallurgy and Materials Science Research Institute, Chulalongkorn University in Journal of Metals, Materials and Minerals
- Vol. 33 (1) , 8-13
Open AccessThe high temperature degradation of ferritic stainless steel in solid carbon atmospheres
Stainless steel is widely used for many components and parts in coal-fired thermal power plants. AISI 430 ferritic stainless steel (FSS) is one common grade to combat the degradation at high temperatures in coal combustion atmospheres containing flue gas, coal ash, and soot (impure solid carbon particles). However, the effect of the solid carbon particles on the degradation of FSS needs to be clarified. Graphite powder was used to simulate solid carbon atmospheres for investigating the degradation of AISI 430 at high temperatures of 1150℃ to 1350℃ in coal-fired boilers. After the carbothermic reduction, the mass gain of a pre-oxidized sample at 750℃ was approximately 0.0793 mg⸳cm-2 and increased when increasing the reduction temperature. The peak of Fe2O3 and Cr7C3 were detected by X˗ray diffraction (XRD) after the oxidation and reduction test, respectively. Besides, the degree of sensitivity (%DoS) of the samples was measured by double loop electrochemical potentiokinetic reactivation (DL-EPR) technique and increased around 30 times after heating the pre-oxidized sample to 1150℃.
- 20 February 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (9) , 4165-4183
Mill scale strengthened ABS composite filaments for 3D printing technology
- 20 February 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (9) , 4165-4183
Mill scale strengthened ABS composite filaments for 3D printing technology
- 26 October 2021
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 39 (1) , 1-11
The degradation of oxide layer on Cr-containing steels in simulated atmospheres on carbothermic reduction
High-temperature corrosion has been a critical issue for coal-fired boiler steels, particularly Cr-containing steels SA213-T22, for many decades. Hot combustion gases containing CO2, CO, N2, and unburnt carbon particles play a significant role in the degradation of oxide scale due to reduction reactions. However, carbide precipitation can occur in the oxide layer by carburisation reactions. The effects of reduction and carburisation on the oxide scale of SA213-T22 steel in a simulated combustion atmosphere by carbothermic reduction were investigated and compared with ferritic stainless steels SS430. The two steels were oxidised under an air atmosphere at 750 °C for 48 hours and heated afterwards in graphite powder at 950–1350 °C for 30–60 minutes. After the oxidation test, a thick porous oxide layer of Fe2O3 was found on the SA213-T22 and a thin Fe-Cr-Mn oxide film was found on SS430 as shown by X-ray diffraction analysis. Most oxide scales on SS430 were reduced and destroyed by carbothermic reduction at 1350 °C but the oxide scale on SA213-T22 transformed to compact mixed phases of Fe-C and Fe-C-Cr-O by carburisation and carbon diffusion. The compact oxide layer with heat resistant carbides can increase wear resistance and might withstand corrosive atmospheres in coal-fire boiler plants.
- 26 October 2021
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 39 (1) , 1-11
The degradation of oxide layer on Cr-containing steels in simulated atmospheres on carbothermic reduction
High-temperature corrosion has been a critical issue for coal-fired boiler steels, particularly Cr-containing steels SA213-T22, for many decades. Hot combustion gases containing CO2, CO, N2, and unburnt carbon particles play a significant role in the degradation of oxide scale due to reduction reactions. However, carbide precipitation can occur in the oxide layer by carburisation reactions. The effects of reduction and carburisation on the oxide scale of SA213-T22 steel in a simulated combustion atmosphere by carbothermic reduction were investigated and compared with ferritic stainless steels SS430. The two steels were oxidised under an air atmosphere at 750 °C for 48 hours and heated afterwards in graphite powder at 950–1350 °C for 30–60 minutes. After the oxidation test, a thick porous oxide layer of Fe2O3 was found on the SA213-T22 and a thin Fe-Cr-Mn oxide film was found on SS430 as shown by X-ray diffraction analysis. Most oxide scales on SS430 were reduced and destroyed by carbothermic reduction at 1350 °C but the oxide scale on SA213-T22 transformed to compact mixed phases of Fe-C and Fe-C-Cr-O by carburisation and carbon diffusion. The compact oxide layer with heat resistant carbides can increase wear resistance and might withstand corrosive atmospheres in coal-fire boiler plants.