Fang Yu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Fang Yu has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Xiangjie Wang
Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang, People’s Republic of China
2 shared publications - Daiyi Chao
Shandong Nanshan Aluminum Co., Ltd., Longkou 265713, China
1 shared publication - Dongfu Song
Guangdong Provincial Key Laboratory of Metal Toughening Technology and Application, Institute of New Materials Guangdong Academy of Sciences, Guangzhou, China
1 shared publication - Guozhong He
Shihezi Zhonghe New Materials Co., Ltd., Shihezi 832000, China
1 shared publication - Lingfei Yang
Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China
1 shared publication - Tongjian Huang
Shandong Nanshan Aluminum Co., Ltd., Longkou 265713, China
1 shared publication
Latest Publications
- Open Access
Research on Hot Deformation Rheological Stress of Al-Mg-Si-Mn-Sc Aluminium Alloy
The hot compression simulation testing machine was utilized to conduct compression experiments on an Al-Mg-Si-Mn alloy containing the rare earth element Sc at a deformation temperature ranging from 450 to 550 °C and a strain rate of 0.01 to 10 s−1. The study focused on the hot deformation behavior of the aluminum alloy, resulting in the determination of the optimal range of deformation process parameters for the alloy. The relationship between material flow stress, deformation temperature, and strain rate was described using the Arrhenius relationship containing thermal activation energy based on the stress-strain curve of hot compression deformation of aluminum alloy. This led to calculations for structural factor A, stress index n, and stress level parameters as well as thermal deformation activation energy to establish a constitutive Formula for hot deformation rheological stress of aluminum alloy and calculate the power dissipation factor η. Through this process, an optimized range for the optimal deformation process parameter for aluminum alloy was determined (deformation temperature: 490~510 °C; strain rate: 0.05 s−1) and verified in combination with mechanical properties and microstructure through hot extrusion deformation trial production.
Open AccessResearch on Hot Deformation Rheological Stress of Al-Mg-Si-Mn-Sc Aluminium Alloy
The hot compression simulation testing machine was utilized to conduct compression experiments on an Al-Mg-Si-Mn alloy containing the rare earth element Sc at a deformation temperature ranging from 450 to 550 °C and a strain rate of 0.01 to 10 s−1. The study focused on the hot deformation behavior of the aluminum alloy, resulting in the determination of the optimal range of deformation process parameters for the alloy. The relationship between material flow stress, deformation temperature, and strain rate was described using the Arrhenius relationship containing thermal activation energy based on the stress-strain curve of hot compression deformation of aluminum alloy. This led to calculations for structural factor A, stress index n, and stress level parameters as well as thermal deformation activation energy to establish a constitutive Formula for hot deformation rheological stress of aluminum alloy and calculate the power dissipation factor η. Through this process, an optimized range for the optimal deformation process parameter for aluminum alloy was determined (deformation temperature: 490~510 °C; strain rate: 0.05 s−1) and verified in combination with mechanical properties and microstructure through hot extrusion deformation trial production.
- Open Access
Effect of Grain Refiner on Fracture Toughness of 7050 Ingot and Plate
In this paper, two types of grain refining alloys, Al-3Ti-0.15C and Al-5Ti-0.2B, were used to cast two types of 7050 rolling ingots. The effect of Al-3Ti-0.15C and Al-5Ti-0.2B grain refiners on fracture toughness in different directions for 7050 ingots after heat treatment and 7050-T7651 plates was investigated using optical electron microscopy (OEM) and scanning electron microscopy (SEM). Mechanical properties testing included both tensile and plane strain fracture toughness (KIC). The grain size was measured from the surface to the center of the 7050 ingots with two different grain refiners. The fracture surface was analyzed by SEM and energy dispersive spectrometer (EDS). The experiments showed the grain size from edge to center was reduced in 7050 ingots with both the TiC and TiB refiners, and the grain size was larger for ingots with the Al-3Ti-0.15C grain refiner at the same position. The tensile properties of 7050 ingots after heat treatment with Al-3Ti-0.15C grain refiner were 1–2 MPa lower than the ingot with the Al-5Ti-0.2B grain refiner. For the 7050-T7651 100 mm thick plate with the Al-3Ti-0.15C grain refiner, for the L direction, the tensile properties were lower by about 10~15 MPa; for the plate with the Al-3Ti-0.15C refiner than plate with Al-5Ti-0.2B refiner, for the LT direction, the tensile properties were lower by about 13–18 MPa; and for the ST direction, they were lower by about 8–10 MPa compared to that of Al-5Ti-0.2B refiner. The fracture toughness of the 7050-T7651 plate produced using the Al-3Ti-0.15C ingot was approximately 2–6 MPa · higher than the plate produced from the Al-5Ti-0.2B ingot. Fractography of the failed fracture toughness specimens revealed that the path of crack propagation of the 7050 ingot after heat treatment produced from the Al-3Ti-0.15C grain refiner was more tortuous than in the ingot produced from the Al-5Ti-0.2B, which resulted in higher fracture toughness.Open AccessEffect of Grain Refiner on Fracture Toughness of 7050 Ingot and Plate
In this paper, two types of grain refining alloys, Al-3Ti-0.15C and Al-5Ti-0.2B, were used to cast two types of 7050 rolling ingots. The effect of Al-3Ti-0.15C and Al-5Ti-0.2B grain refiners on fracture toughness in different directions for 7050 ingots after heat treatment and 7050-T7651 plates was investigated using optical electron microscopy (OEM) and scanning electron microscopy (SEM). Mechanical properties testing included both tensile and plane strain fracture toughness (KIC). The grain size was measured from the surface to the center of the 7050 ingots with two different grain refiners. The fracture surface was analyzed by SEM and energy dispersive spectrometer (EDS). The experiments showed the grain size from edge to center was reduced in 7050 ingots with both the TiC and TiB refiners, and the grain size was larger for ingots with the Al-3Ti-0.15C grain refiner at the same position. The tensile properties of 7050 ingots after heat treatment with Al-3Ti-0.15C grain refiner were 1–2 MPa lower than the ingot with the Al-5Ti-0.2B grain refiner. For the 7050-T7651 100 mm thick plate with the Al-3Ti-0.15C grain refiner, for the L direction, the tensile properties were lower by about 10~15 MPa; for the plate with the Al-3Ti-0.15C refiner than plate with Al-5Ti-0.2B refiner, for the LT direction, the tensile properties were lower by about 13–18 MPa; and for the ST direction, they were lower by about 8–10 MPa compared to that of Al-5Ti-0.2B refiner. The fracture toughness of the 7050-T7651 plate produced using the Al-3Ti-0.15C ingot was approximately 2–6 MPa · higher than the plate produced from the Al-5Ti-0.2B ingot. Fractography of the failed fracture toughness specimens revealed that the path of crack propagation of the 7050 ingot after heat treatment produced from the Al-3Ti-0.15C grain refiner was more tortuous than in the ingot produced from the Al-5Ti-0.2B, which resulted in higher fracture toughness.