Julia Magalhães Costa Lima
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Julia Magalhães Costa Lima has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Marco Antonio Bottino
Department of Cariology, Restorative Sciences, and Endodontics, School of Dentistry, University of Michigan, Ann Arbor, MI 48109, USA
2 shared publications - Renata Marques de Melo
Department of Dental Materials and Prosthodontics, Institute of Science and Technology, Sao Paulo State University (UNESP), Sao Jose dos Campos, Brazil
2 shared publications - Rodrigo Othavio de Assuncao E Souza
Department of Dentistry Federal University of Rio Grande do Norte (UFRN) Natal Brazil
2 shared publications - Alexandre Luiz Souto Borges
Department of Dental Materials and Prosthodontics, Institute of Science and Technology, São Paulo State University (UNESP), São José dos Campos 12245-000, SP, Brazil
1 shared publication - Anna Karina Figueiredo Costa
São Paulo State University, Brazil
1 shared publication - Elen G. Lima
São Paulo State University, Brazil
1 shared publication
Latest Publications
- Open Access
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e245917
Effect of cementation protocols on the fracture load of bilayer ceramic crowns manufactured by the Rapid Layer Technology
To evaluate the fracture load of bilayer ceramic crowns manufactured by Rapid Layer Technology (RLT) after different cementation protocols of the veneering ceramic to the zirconia infrastructures. Sixty epoxy resin preparations simulating a molar tooth were obtained and 60 zirconia infrastructures and feldspathic crowns were manufactured by RLT and divided into 6 groups according to the cementation protocol at the interface to veneering ceramic (n=10): Ctr- control: conventional resin cement; Al- Al2O3 sandblasting 50µm + conventional resin cement; Al/MDP- Al2O3 sandblasting (50µm) + resin cement with MDP; Sil- silicatization 30µm + conventional resin cement; Gl/HF- glaze + hydrofluoridric acid (5%,60s) + silane + conventional resin cement; Gl- glazing as bonding agent. The feldspathic ceramic internal surface was etched with fluoridric acid (5%) + silane followed by cementation according to respective protocols. All samples were mechanically cycled (200N and 4.5x105 Pa, 37°C, 2x106 cycles, 3.4Hz) and submitted to axial compressing fracture load test (10kN, 0.5mm/min). The results(N) were submitted to descriptive and analytical statistical analysis with 1-way ANOVA, Weibull, and the Tukey test (α=0.05). ANOVA revealed that there was a significant difference among the tested groups (p<0.0001). The group Al/MDP presented the higher resistance to fracture (1972.46A N), followed by the Ctr group (1584.41B N). The characteristic strength(σ0) was significantly different (p=0.000). The crack and chipping were the predominant failures. The air-abrasion at the external surface of zirconia with Al2O3 followed by cementation with MDP resin cement, should be selected to Rapid Layer Technique when felspathic ceramic is used as veneer ceramic.
- 1 January 2024
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 35, e245917
Open AccessEffect of cementation protocols on the fracture load of bilayer ceramic crowns manufactured by the Rapid Layer Technology
To evaluate the fracture load of bilayer ceramic crowns manufactured by Rapid Layer Technology (RLT) after different cementation protocols of the veneering ceramic to the zirconia infrastructures. Sixty epoxy resin preparations simulating a molar tooth were obtained and 60 zirconia infrastructures and feldspathic crowns were manufactured by RLT and divided into 6 groups according to the cementation protocol at the interface to veneering ceramic (n=10): Ctr- control: conventional resin cement; Al- Al2O3 sandblasting 50µm + conventional resin cement; Al/MDP- Al2O3 sandblasting (50µm) + resin cement with MDP; Sil- silicatization 30µm + conventional resin cement; Gl/HF- glaze + hydrofluoridric acid (5%,60s) + silane + conventional resin cement; Gl- glazing as bonding agent. The feldspathic ceramic internal surface was etched with fluoridric acid (5%) + silane followed by cementation according to respective protocols. All samples were mechanically cycled (200N and 4.5x105 Pa, 37°C, 2x106 cycles, 3.4Hz) and submitted to axial compressing fracture load test (10kN, 0.5mm/min). The results(N) were submitted to descriptive and analytical statistical analysis with 1-way ANOVA, Weibull, and the Tukey test (α=0.05). ANOVA revealed that there was a significant difference among the tested groups (p<0.0001). The group Al/MDP presented the higher resistance to fracture (1972.46A N), followed by the Ctr group (1584.41B N). The characteristic strength(σ0) was significantly different (p=0.000). The crack and chipping were the predominant failures. The air-abrasion at the external surface of zirconia with Al2O3 followed by cementation with MDP resin cement, should be selected to Rapid Layer Technique when felspathic ceramic is used as veneer ceramic.
- Open Access
- 1 June 2021
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 32 (3) , 44-55
CAD-FEA modeling and fracture resistance of bilayer zirconia crowns manufactured by the rapid layer technology
In the RLT (Rapid Layer Technology), veneering ceramic and framework are fabricated by computer-aided design/computer-aided manufacturing (CAD/CAM) and then cemented to obtain the restoration. This study aimed to evaluate the effect of the thickness of veneering ceramic manufactured by the RLT technique on the fracture resistance (FR) of bilayer crowns with zirconia frameworks. Twenty zirconia frameworks and twenty feldspathic posterior crowns with two different veneering ceramic occlusal thicknesses (1mm=TF1; 2mm=TF2) were manufactured using CAD/CAM system. The specimens were luted to an epoxy resin abutment with resin cement and mechanically cycled (200N and 4.5×105 Pa, 37°C, 2×106 cycles, 3Hz). The FR test was performed (10kN, 0.5mm/min), and the specimens were analyzed in a stereomicroscope. For the stress analysis (finite element analysis, FEA), a 10kN load was equal to the in vitro test, and the principal stress was evaluated. The FR data were analyzed by Student’s t-test and Weibull's analysis. The thickness influenced the FR of bilayer crowns. The FR was higher in the TF2 than in the TF1 group. The TF2 group presented the highest characteristic strength compared to the group TF1. The predominant type of failure was delamination. The FEA showed higher stress concentrations below the loading application point at the veneering cement interface in the 1-mm-thick model. The bilayer crowns manufactured using the approach of 2mm of veneering ceramic promoted higher FR compared to the group with 1mm veneering ceramic. Also, the FEA showed that the veneer ceramic thickness has an effect on stress distribution in zirconia-based bilayer crowns.
- 1 June 2021
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 32 (3) , 44-55
Open AccessCAD-FEA modeling and fracture resistance of bilayer zirconia crowns manufactured by the rapid layer technology
In the RLT (Rapid Layer Technology), veneering ceramic and framework are fabricated by computer-aided design/computer-aided manufacturing (CAD/CAM) and then cemented to obtain the restoration. This study aimed to evaluate the effect of the thickness of veneering ceramic manufactured by the RLT technique on the fracture resistance (FR) of bilayer crowns with zirconia frameworks. Twenty zirconia frameworks and twenty feldspathic posterior crowns with two different veneering ceramic occlusal thicknesses (1mm=TF1; 2mm=TF2) were manufactured using CAD/CAM system. The specimens were luted to an epoxy resin abutment with resin cement and mechanically cycled (200N and 4.5×105 Pa, 37°C, 2×106 cycles, 3Hz). The FR test was performed (10kN, 0.5mm/min), and the specimens were analyzed in a stereomicroscope. For the stress analysis (finite element analysis, FEA), a 10kN load was equal to the in vitro test, and the principal stress was evaluated. The FR data were analyzed by Student’s t-test and Weibull's analysis. The thickness influenced the FR of bilayer crowns. The FR was higher in the TF2 than in the TF1 group. The TF2 group presented the highest characteristic strength compared to the group TF1. The predominant type of failure was delamination. The FEA showed higher stress concentrations below the loading application point at the veneering cement interface in the 1-mm-thick model. The bilayer crowns manufactured using the approach of 2mm of veneering ceramic promoted higher FR compared to the group with 1mm veneering ceramic. Also, the FEA showed that the veneer ceramic thickness has an effect on stress distribution in zirconia-based bilayer crowns.