Yutaka Kobayashi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Yutaka Kobayashi has a total of 69 co-authors. Here are the top co-authors by number of shared publications:
- Hiroshi Ito
Department of Organic Materials Science, Graduate School of Organic Materials Science, Yamagata University, 4-3-16 Jonan, Yonezawa 992-8510, Yamagata, Japan
11 shared publications - Akira Ishigami
Graduate School of Organic Materials Science, Yamagata University, 4-3-16 Jonan, Yonezawa, Yamagata 992-8510, Japan
7 shared publications - Supaphorn Thumsorn
Research Center for GREEN Materials and Advanced Processing, Yamagata University, 4-3-16 Jonan, Yonezawa 992-8510, Yamagata, Japan
3 shared publications Atsushi Takahara
2 shared publications- Dai-Ichiro Kato
Kagoshima University
2 shared publications Hiroshi Ito
Yamagata University
2 shared publications
Latest Publications
- Open Access
- 1 September 2026
- Published by Elsevier in SSRN Electronic Journal
UV-Stable Polyamide 6/Clay Nanocomposites with Enhanced Marine Biodegradation
Biodegradable plastics offer a promising strategy to mitigate mismanaged waste plastic pollution, yet balancing mechanical integrity during service with rapid post-disposal degradation remains challenging. This study reports a facile approach to fabricating polyamide 6/layered silicate nanocomposites (PA6/clay) that achieve an excellent balance between durability and environmental degradability. The resulting composites exhibit thermal properties comparable to those of neat PA6 while delivering significantly enhanced mechanical performance; specifically, the Young's modulus and yield strength increased by 139% and 31%, respectively, compared to neat PA6. Crucially, the PA6/clay composites exhibit superior photostability; even after extended UV exposure, they retain mechanical properties comparable to those of unexposed PA6 films. Furthermore, the incorporation of nanoclay enhances the marine biodegradability of the matrix, as demonstrated by the higher degree of biodegradation. Consequently, this work establishes a viable materials-design strategy for engineering polymers that maintain high weathering resistance during active use but undergo accelerated biodegradation upon disposal.
- 1 September 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessUV-Stable Polyamide 6/Clay Nanocomposites with Enhanced Marine Biodegradation
Biodegradable plastics offer a promising strategy to mitigate mismanaged waste plastic pollution, yet balancing mechanical integrity during service with rapid post-disposal degradation remains challenging. This study reports a facile approach to fabricating polyamide 6/layered silicate nanocomposites (PA6/clay) that achieve an excellent balance between durability and environmental degradability. The resulting composites exhibit thermal properties comparable to those of neat PA6 while delivering significantly enhanced mechanical performance; specifically, the Young's modulus and yield strength increased by 139% and 31%, respectively, compared to neat PA6. Crucially, the PA6/clay composites exhibit superior photostability; even after extended UV exposure, they retain mechanical properties comparable to those of unexposed PA6 films. Furthermore, the incorporation of nanoclay enhances the marine biodegradability of the matrix, as demonstrated by the higher degree of biodegradation. Consequently, this work establishes a viable materials-design strategy for engineering polymers that maintain high weathering resistance during active use but undergo accelerated biodegradation upon disposal.
- Open Access
- 18 August 2026
- Published by Springer Nature in Research Square
Marine biodegradation of otherwise persistent engineering nylons
Engineering nylons are generally considered persistent in the environment, including the marine environment. However, some commercially available nylon fishing lines, composed of mass-produced engineering nylon copolymers, unexpectedly exhibit biodegradation in natural seawater, and the mechanisms underlying this behaviour remain unclear. Here, we systematically examined the effect of the composition and structural state of nylon filaments on their marine biodegradation. Accelerated marine biological oxygen demand (BOD) tests revealed substantial marine biodegradation even in highly crystalline, oriented nylon filaments, with structural disruption further enhancing the process. Long-term in situ seafloor exposure experiments under negligible ultraviolet irradiation revealed progressive surface erosion and mechanical deterioration, suggesting degradation under environmentally relevant marine conditions. Additionally, nylon filament biodegradability strongly correlated with water uptake across compositions and structural states, highlighting hydration-mediated accessibility as a key factor linking polymer structure with microbial biodegradation. Molecular and microbiological analyses further confirmed microbial chain scission and high-molecular-weight nylon assimilation, with a newly isolated Dasania species contributing to this process. Therefore, environmental persistence in engineering plastics is not solely determined by polymer chemistry, but also by structure-dependent microbial accessibility, providing new insights into the environmental fate of ghost fishing gear, marine debris, and secondary microplastics.
- 18 August 2026
- Published by Springer Nature in Research Square
Open AccessMarine biodegradation of otherwise persistent engineering nylons
Engineering nylons are generally considered persistent in the environment, including the marine environment. However, some commercially available nylon fishing lines, composed of mass-produced engineering nylon copolymers, unexpectedly exhibit biodegradation in natural seawater, and the mechanisms underlying this behaviour remain unclear. Here, we systematically examined the effect of the composition and structural state of nylon filaments on their marine biodegradation. Accelerated marine biological oxygen demand (BOD) tests revealed substantial marine biodegradation even in highly crystalline, oriented nylon filaments, with structural disruption further enhancing the process. Long-term in situ seafloor exposure experiments under negligible ultraviolet irradiation revealed progressive surface erosion and mechanical deterioration, suggesting degradation under environmentally relevant marine conditions. Additionally, nylon filament biodegradability strongly correlated with water uptake across compositions and structural states, highlighting hydration-mediated accessibility as a key factor linking polymer structure with microbial biodegradation. Molecular and microbiological analyses further confirmed microbial chain scission and high-molecular-weight nylon assimilation, with a newly isolated Dasania species contributing to this process. Therefore, environmental persistence in engineering plastics is not solely determined by polymer chemistry, but also by structure-dependent microbial accessibility, providing new insights into the environmental fate of ghost fishing gear, marine debris, and secondary microplastics.
- Open Access
Molecular Orientation and Mechanical Properties of Biomass-Derived Aliphatic Polyamide (PA11) by High-Pressure Compression Molding
This study investigates the effects of high-pressure compression molding on the molecular orientation and mechanical properties of biomass-derived aliphatic polyamide (PA11). Tensile fracture strength exhibited a significant increase—up to 2.4 times that of untreated samples—under conditions of 1000 kN and 140 °C. Differential Scanning Calorimetry (DSC) and Wide-Angle X-ray Scattering (WAXS) analyses revealed a temperature- and pressure-dependent shift in crystalline phases, suggesting a transition from α’ to phase. The δ’ phase, formed by high-pressure compression molding, is retained even after cooling to room temperature (i.e., Brill transition was not observed). In addition, polarized optical microscopy (POM) observations further supported the presence of changes in molecular orientation. This enhancement (under conditions of 1000 kN and 140 °C) is primarily attributed to the molecular orientation. However, it is also noteworthy that the formation of the δ’ phase is accompanied by an increase in the degree of crystallinity, and that this δ’ phase is retained even after cooling to room temperature without undergoing a Brill transition. In contrast, at 180 °C, although the degree of crystallinity increased, molecular orientation decreased, resulting in reduced tensile strength. These findings indicate that the mechanical properties of PA11 are governed by a complex interplay among phase transitions, molecular orientation, and crystallization, all of which are strongly influenced by temperature and pressure conditions. These findings demonstrate that high-pressure compression molding is an effective method for enhancing the mechanical properties of PA11 through controlled phase transition and orientation
Open AccessMolecular Orientation and Mechanical Properties of Biomass-Derived Aliphatic Polyamide (PA11) by High-Pressure Compression Molding
This study investigates the effects of high-pressure compression molding on the molecular orientation and mechanical properties of biomass-derived aliphatic polyamide (PA11). Tensile fracture strength exhibited a significant increase—up to 2.4 times that of untreated samples—under conditions of 1000 kN and 140 °C. Differential Scanning Calorimetry (DSC) and Wide-Angle X-ray Scattering (WAXS) analyses revealed a temperature- and pressure-dependent shift in crystalline phases, suggesting a transition from α’ to phase. The δ’ phase, formed by high-pressure compression molding, is retained even after cooling to room temperature (i.e., Brill transition was not observed). In addition, polarized optical microscopy (POM) observations further supported the presence of changes in molecular orientation. This enhancement (under conditions of 1000 kN and 140 °C) is primarily attributed to the molecular orientation. However, it is also noteworthy that the formation of the δ’ phase is accompanied by an increase in the degree of crystallinity, and that this δ’ phase is retained even after cooling to room temperature without undergoing a Brill transition. In contrast, at 180 °C, although the degree of crystallinity increased, molecular orientation decreased, resulting in reduced tensile strength. These findings indicate that the mechanical properties of PA11 are governed by a complex interplay among phase transitions, molecular orientation, and crystallization, all of which are strongly influenced by temperature and pressure conditions. These findings demonstrate that high-pressure compression molding is an effective method for enhancing the mechanical properties of PA11 through controlled phase transition and orientation
- Open Access
Synthesis of High-Performance and Biodegradable Polymer Blends Based on Poly(butylene succinate) and Grafted Polyrotaxane via Controlled Reactive Processing
In this study, novel, high-strength polymer blends were synthesized using poly(butylene succinate) (PBS) modified with grafted polyrotaxane (GPR). Then, their mechanical properties and morphologies were evaluated. A unique, two-step, reactive kneading method was developed to substantially improve the mechanical properties of PBS, which promoted transesterification reaction using an organo-titanium catalyst (Ti) in the first step and a urethanization reaction using hexamethylene diisocyanate (HDI) in the second step. The optimized blend material, [PBS/GPR10/Ti]-HDI, achieved remarkable toughening, and its Izod impact strength increased approximately seven-fold compared with that of unmodified PBS. Scanning electron microscopy (SEM) of the fracture surfaces confirmed a transition from brittle to ductile fracture, attributed to the controlled reaction sequence. First, strong chemical bonds formed at the PBS/GPR interface via Ti-catalyzed transesterification. Then, HDI induced simultaneous internal crosslinking (gelation) of the GPR domains and chain extension of the PBS matrix. This modification strategy maintained the excellent inherent soil biodegradability of PBS while improving its degradability in marine environments. This study presents a new guideline for designing materials that can considerably enhance the mechanical properties of biodegradable plastics.
Open AccessSynthesis of High-Performance and Biodegradable Polymer Blends Based on Poly(butylene succinate) and Grafted Polyrotaxane via Controlled Reactive Processing
In this study, novel, high-strength polymer blends were synthesized using poly(butylene succinate) (PBS) modified with grafted polyrotaxane (GPR). Then, their mechanical properties and morphologies were evaluated. A unique, two-step, reactive kneading method was developed to substantially improve the mechanical properties of PBS, which promoted transesterification reaction using an organo-titanium catalyst (Ti) in the first step and a urethanization reaction using hexamethylene diisocyanate (HDI) in the second step. The optimized blend material, [PBS/GPR10/Ti]-HDI, achieved remarkable toughening, and its Izod impact strength increased approximately seven-fold compared with that of unmodified PBS. Scanning electron microscopy (SEM) of the fracture surfaces confirmed a transition from brittle to ductile fracture, attributed to the controlled reaction sequence. First, strong chemical bonds formed at the PBS/GPR interface via Ti-catalyzed transesterification. Then, HDI induced simultaneous internal crosslinking (gelation) of the GPR domains and chain extension of the PBS matrix. This modification strategy maintained the excellent inherent soil biodegradability of PBS while improving its degradability in marine environments. This study presents a new guideline for designing materials that can considerably enhance the mechanical properties of biodegradable plastics.
- Open Access
Analyzing the Tensile Creep Behavior of Different Types of Polypropylenes Using a Simple Fractional Differential Viscoelastic Model
Fractional differential viscoelastic calculus was used to develop a model for predicting the primary to tertiary creep in the tensile creep deformation of various polypropylenes (PPs). The primary and secondary creep were described via simple fractional differential viscoelasticity with an empirical formula for the stress and temperature dependence of the fractional differential order. Tertiary creep was treated as a pure viscous body with damage. The temperature dependence is treated simply, and Arrhenius’s law is applied. As for stress dependence, the Eyring law of the sinh function was applied to the primary and secondary creep processes, while the WLF-type shift function was adopted for tertiary creep. The primary and secondary creep behaviors of each model material showed creep growth rates according to the rigidity of each material. As for the tertiary creep, the homo PP showed a little damage progression with a damage index of 0.17, while the impact-resistant PP showed faster damage progression with a damage index of around 0.5. The three types of post-consumer recycled PPs showed intermediate properties between these virgin PPs, and no peculiarities were confirmed in the static creep behaviors. It was confirmed that the creep experimental results for all model materials fell on the same Monkman–Grant law. The presented creep model can predict the creep strain transition and minimum strain rate well and is effective in predicting the creep characteristics of PPs.
Open AccessAnalyzing the Tensile Creep Behavior of Different Types of Polypropylenes Using a Simple Fractional Differential Viscoelastic Model
Fractional differential viscoelastic calculus was used to develop a model for predicting the primary to tertiary creep in the tensile creep deformation of various polypropylenes (PPs). The primary and secondary creep were described via simple fractional differential viscoelasticity with an empirical formula for the stress and temperature dependence of the fractional differential order. Tertiary creep was treated as a pure viscous body with damage. The temperature dependence is treated simply, and Arrhenius’s law is applied. As for stress dependence, the Eyring law of the sinh function was applied to the primary and secondary creep processes, while the WLF-type shift function was adopted for tertiary creep. The primary and secondary creep behaviors of each model material showed creep growth rates according to the rigidity of each material. As for the tertiary creep, the homo PP showed a little damage progression with a damage index of 0.17, while the impact-resistant PP showed faster damage progression with a damage index of around 0.5. The three types of post-consumer recycled PPs showed intermediate properties between these virgin PPs, and no peculiarities were confirmed in the static creep behaviors. It was confirmed that the creep experimental results for all model materials fell on the same Monkman–Grant law. The presented creep model can predict the creep strain transition and minimum strain rate well and is effective in predicting the creep characteristics of PPs.
- Open Access
Enhanced Marine Biodegradation of Polycaprolactone through Incorporation of Mucus Bubble Powder from Violet Sea Snail as Protein Fillers
Microplastics’ spreading in the ocean is currently causing significant damage to organisms and ecosystems around the world. To address this oceanic issue, there is a current focus on marine degradable plastics. Polycaprolactone (PCL) is a marine degradable plastic that is attracting attention. To further improve the biodegradability of PCL, we selected a completely new protein that has not been used before as a functional filler to incorporate it into PCL, aiming to develop an environmentally friendly biocomposite material. This novel protein is derived from the mucus bubbles of the violet sea snail (VSS, Janthina globosa), which is a strong bio-derived material that is 100% degradable in the sea environment by microorganisms. Two types of PCL/bubble composites, PCL/b1 and PCL/b5, were prepared with mass ratios of PCL to bubble powder of 99:1 and 95:5, respectively. We investigated the thermal properties, mechanical properties, biodegradability, surface structure, and crystal structure of the developed PCL/bubble composites. The maximum biochemical oxygen demand (BOD) degradation for PCL/b5 reached 96%, 1.74 times that of pure PCL (≈55%), clearly indicating that the addition of protein fillers significantly enhanced the biodegradability of PCL. The surface morphology observation results through scanning electron microscopy (SEM) definitely confirmed the occurrence of degradation, and it was found that PCL/b5 underwent more significant degradation compared to pure PCL. The water contact angle measurement results exhibited that all sheets were hydrophobic (water contact angle > 90°) before the BOD test and showed the changes in surface structure after the BOD test due to the newly generated indentations on the surface, which led to an increase in surface toughness and, consequently, an increase in surface hydrophobility. A crystal structure analysis by wide-angle X-ray scattering (WAXS) discovered that the amorphous regions were decomposed first during the BOD test, and more amorphous regions were decomposed in PCL/b5 than in PCL, owing to the addition of the bubble protein fillers from the VSS. The differential scanning calorimeter (DSC) and thermal gravimetric analysis (TGA) results suggested that the addition of mucus bubble protein fillers had only a slight impact on the thermal properties of PCL. In terms of mechanical properties, compared to pure PCL, the mucus-bubble-filler-added composites PCL/b1 and PCL/b5 exhibited slightly decreased values. Although the biodegradability of PCL was significantly improved by adding the protein fillers from mucus bubbles of the VSS, enhancing the mechanical properties at the same time poses the next challenging issue.
Open AccessEnhanced Marine Biodegradation of Polycaprolactone through Incorporation of Mucus Bubble Powder from Violet Sea Snail as Protein Fillers
Microplastics’ spreading in the ocean is currently causing significant damage to organisms and ecosystems around the world. To address this oceanic issue, there is a current focus on marine degradable plastics. Polycaprolactone (PCL) is a marine degradable plastic that is attracting attention. To further improve the biodegradability of PCL, we selected a completely new protein that has not been used before as a functional filler to incorporate it into PCL, aiming to develop an environmentally friendly biocomposite material. This novel protein is derived from the mucus bubbles of the violet sea snail (VSS, Janthina globosa), which is a strong bio-derived material that is 100% degradable in the sea environment by microorganisms. Two types of PCL/bubble composites, PCL/b1 and PCL/b5, were prepared with mass ratios of PCL to bubble powder of 99:1 and 95:5, respectively. We investigated the thermal properties, mechanical properties, biodegradability, surface structure, and crystal structure of the developed PCL/bubble composites. The maximum biochemical oxygen demand (BOD) degradation for PCL/b5 reached 96%, 1.74 times that of pure PCL (≈55%), clearly indicating that the addition of protein fillers significantly enhanced the biodegradability of PCL. The surface morphology observation results through scanning electron microscopy (SEM) definitely confirmed the occurrence of degradation, and it was found that PCL/b5 underwent more significant degradation compared to pure PCL. The water contact angle measurement results exhibited that all sheets were hydrophobic (water contact angle > 90°) before the BOD test and showed the changes in surface structure after the BOD test due to the newly generated indentations on the surface, which led to an increase in surface toughness and, consequently, an increase in surface hydrophobility. A crystal structure analysis by wide-angle X-ray scattering (WAXS) discovered that the amorphous regions were decomposed first during the BOD test, and more amorphous regions were decomposed in PCL/b5 than in PCL, owing to the addition of the bubble protein fillers from the VSS. The differential scanning calorimeter (DSC) and thermal gravimetric analysis (TGA) results suggested that the addition of mucus bubble protein fillers had only a slight impact on the thermal properties of PCL. In terms of mechanical properties, compared to pure PCL, the mucus-bubble-filler-added composites PCL/b1 and PCL/b5 exhibited slightly decreased values. Although the biodegradability of PCL was significantly improved by adding the protein fillers from mucus bubbles of the VSS, enhancing the mechanical properties at the same time poses the next challenging issue.
- 19 October 2023
- Published by Springer Nature in Cellulose
- Vol. 30 (17) , 10983-10998
Surface replication and characterization of ultrahigh-pressure homogenizer treated cellulose nanofiber-reinforced polyvinyl alcohol composites by thermal imprinting
- 19 October 2023
- Published by Springer Nature in Cellulose
- Vol. 30 (17) , 10983-10998
Surface replication and characterization of ultrahigh-pressure homogenizer treated cellulose nanofiber-reinforced polyvinyl alcohol composites by thermal imprinting
- Open Access
- 8 February 2023
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 7 (1) , 44
Influence of Ambient Temperature and Crystalline Structure on Fracture Toughness and Production of Thermoplastic by Enclosure FDM 3D Printer
Fused deposition modeling (FDM) 3D printing has printed thermoplastic materials layer-by-layer to form three dimensional products whereby interlayer adhesion must be well controlled to obtain high mechanical performance and product integrity. This research studied the effects of ambient temperatures and crystalline structure on the interlayer adhesion and properties of thermoplastic FDM 3D printing. Five kinds of poly(lactic acid) (PLA) filaments, both commercially available and the laboratory-made, were printed using the enclosure FDM 3D printer. The ambient temperatures were set by the temperature-controlled chamber from room temperature to 75 °C with and without a cooling fan. The interlayer adhesion was characterized by the degree of entanglement density, morphology, and fracture toughness. In addition, PLA filament with high crystallinity has induced heat resistance, which could prevent filament clogging and successfully print at higher chamber temperatures. The ambient temperature increased with increased chamber temperature and significantly increased when printed without a cooling fan, resulting in improved interlayer bonding. The crystalline structure and dynamic mechanical properties of the 3D printed products were promoted when the chamber temperature was increased without a cooling fan, especially in PLA composites and PLA containing a high content of L-isomer. However, although the additives in the PLA composite improved crystallinity and the degree of entanglement density in the 3D-printed products, they induced an anisotropic characteristic that resulted in the declination of the interlayer bonding in the transverse orientation products. The increasing of chamber temperatures over 40 °C improved the interlayer bonding in pristine PLA products, which was informed by the increased fracture toughness. Further, it can be noted that the amorphous nature of PLA promotes molecular entanglement, especially when printed at higher chamber temperatures with and without a cooling fan.
- 8 February 2023
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 7 (1) , 44
Open AccessInfluence of Ambient Temperature and Crystalline Structure on Fracture Toughness and Production of Thermoplastic by Enclosure FDM 3D Printer
Fused deposition modeling (FDM) 3D printing has printed thermoplastic materials layer-by-layer to form three dimensional products whereby interlayer adhesion must be well controlled to obtain high mechanical performance and product integrity. This research studied the effects of ambient temperatures and crystalline structure on the interlayer adhesion and properties of thermoplastic FDM 3D printing. Five kinds of poly(lactic acid) (PLA) filaments, both commercially available and the laboratory-made, were printed using the enclosure FDM 3D printer. The ambient temperatures were set by the temperature-controlled chamber from room temperature to 75 °C with and without a cooling fan. The interlayer adhesion was characterized by the degree of entanglement density, morphology, and fracture toughness. In addition, PLA filament with high crystallinity has induced heat resistance, which could prevent filament clogging and successfully print at higher chamber temperatures. The ambient temperature increased with increased chamber temperature and significantly increased when printed without a cooling fan, resulting in improved interlayer bonding. The crystalline structure and dynamic mechanical properties of the 3D printed products were promoted when the chamber temperature was increased without a cooling fan, especially in PLA composites and PLA containing a high content of L-isomer. However, although the additives in the PLA composite improved crystallinity and the degree of entanglement density in the 3D-printed products, they induced an anisotropic characteristic that resulted in the declination of the interlayer bonding in the transverse orientation products. The increasing of chamber temperatures over 40 °C improved the interlayer bonding in pristine PLA products, which was informed by the increased fracture toughness. Further, it can be noted that the amorphous nature of PLA promotes molecular entanglement, especially when printed at higher chamber temperatures with and without a cooling fan.
- Open Access
Rheological Behavior and Dynamic Mechanical Properties for Interpretation of Layer Adhesion in FDM 3D Printing
Commercial filaments of poly(lactic acid) (PLA) composites with particulate filler, carbon fiber, and copper powder with different contents were fabricated by FDM 3D printing in XZ-direction at bed temperatures of 45 °C and 60 °C. The effects of additives and bed temperatures on layer adhesion, fracture behavior, and mechanical performance of the PLA composites 3D printing were evaluated. Rheological properties informed viscous nature of all filaments and interface bonding in the PLA composites, which improved printability and dimensional stability of the 3D printing. Crystallinity of the PLA composites 3D printing increased with increasing bed temperature resulting in an improvement of storage modulus, tensile, and flexural properties. On the contrary, the ductility of the 3D printing was raised when printed at low bed temperature. Dynamic mechanical properties, the degree of entanglement, the adhesion factor, the effectiveness coefficient, the reinforcing efficiency factor, and the Cole–Cole analysis were used to understand the layer adhesion, and the interfacial interaction of the composites as compared to the compression molded sheets. SEM images revealed good adhesion between the additives and the PLA matrix. However, the additives induced faster solidification and showed larger voids in the 3D printing, which indicated lower layer adhesion as compared to neat PLA. It can be noted that the combination of the additives and the optimized 3D printing conditions would be obtain superior mechanical performance even layer adhesion has been restricted.
Open AccessRheological Behavior and Dynamic Mechanical Properties for Interpretation of Layer Adhesion in FDM 3D Printing
Commercial filaments of poly(lactic acid) (PLA) composites with particulate filler, carbon fiber, and copper powder with different contents were fabricated by FDM 3D printing in XZ-direction at bed temperatures of 45 °C and 60 °C. The effects of additives and bed temperatures on layer adhesion, fracture behavior, and mechanical performance of the PLA composites 3D printing were evaluated. Rheological properties informed viscous nature of all filaments and interface bonding in the PLA composites, which improved printability and dimensional stability of the 3D printing. Crystallinity of the PLA composites 3D printing increased with increasing bed temperature resulting in an improvement of storage modulus, tensile, and flexural properties. On the contrary, the ductility of the 3D printing was raised when printed at low bed temperature. Dynamic mechanical properties, the degree of entanglement, the adhesion factor, the effectiveness coefficient, the reinforcing efficiency factor, and the Cole–Cole analysis were used to understand the layer adhesion, and the interfacial interaction of the composites as compared to the compression molded sheets. SEM images revealed good adhesion between the additives and the PLA matrix. However, the additives induced faster solidification and showed larger voids in the 3D printing, which indicated lower layer adhesion as compared to neat PLA. It can be noted that the combination of the additives and the optimized 3D printing conditions would be obtain superior mechanical performance even layer adhesion has been restricted.