Selem Alvarenga Vilela
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Interests
Selem Alvarenga Vilela has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Aline Batista Gonçalves Franco
Faculdade São Leopoldo Mandic
2 shared publications - Caio Marques Martins
Faculdade São Leopoldo Mandic
2 shared publications - Elimario Venturin Ramos
Faculdade São Leopoldo Mandic
2 shared publications - Fabiano Perez
Faculdade São Leopoldo Mandic
2 shared publications - Francisco Fernando Massola Filho
Faculdade São Leopoldo Mandic
2 shared publications - Geraldo Alberto Pinheiro de Carvalho
Faculdade São Leopoldo Mandic
2 shared publications
Latest Publications
- Open Access
- 9 March 2022
- Published by Research, Society and Development in Research, Society and Development
- Vol. 11 (4)
Influence of surface treatment on the shear strength of Ultra Translucent Multi Layered Zirconia Katana
The aim of this study is to assess how shear strength of Ultra Translucent Multi Layered Zirconia Katana (UTML) is affected by the conditioning with 10% hydrofluoric acid combined with the current surface treatment protocol: air, primer containing 10-MDP, and cement. Samples of UTML Zirconia Katana were machined to measure 5x5x10 units of measurement, attached, and divided into two groups. In the control group, samples were treated with 27 um aluminum oxide blasting at 4 bars, application of Zr primer containing 10-MDP and, finally, cement Panávia V5. In the experimental group, samples were also treated with 10% hydrofluoric acid following blasting and prior to the primer application. The test specimens were submitted to shear mechanical strength test on a universal testing machine EMIC DL2000 (EMIC, São Paulo, Brazil), surface analysis with Scanning Electron Microscope (SEM) (Sputter Coaster Emitech, K450) and surface roughness. Results showed that the bond strength of specimens conditioned with acid was 41% higher (p = 0.031). Student’s t test showed that the samples conditioned with acid were rougher than those without conditioning (p = 0.045). Microscopic analysis showed surface alterations on samples conditioned with acid. It is possible to conclude that the group conditioned with hydrofluoric acid showed better adhesive behavior.
- 9 March 2022
- Published by Research, Society and Development in Research, Society and Development
- Vol. 11 (4)
Open AccessInfluence of surface treatment on the shear strength of Ultra Translucent Multi Layered Zirconia Katana
The aim of this study is to assess how shear strength of Ultra Translucent Multi Layered Zirconia Katana (UTML) is affected by the conditioning with 10% hydrofluoric acid combined with the current surface treatment protocol: air, primer containing 10-MDP, and cement. Samples of UTML Zirconia Katana were machined to measure 5x5x10 units of measurement, attached, and divided into two groups. In the control group, samples were treated with 27 um aluminum oxide blasting at 4 bars, application of Zr primer containing 10-MDP and, finally, cement Panávia V5. In the experimental group, samples were also treated with 10% hydrofluoric acid following blasting and prior to the primer application. The test specimens were submitted to shear mechanical strength test on a universal testing machine EMIC DL2000 (EMIC, São Paulo, Brazil), surface analysis with Scanning Electron Microscope (SEM) (Sputter Coaster Emitech, K450) and surface roughness. Results showed that the bond strength of specimens conditioned with acid was 41% higher (p = 0.031). Student’s t test showed that the samples conditioned with acid were rougher than those without conditioning (p = 0.045). Microscopic analysis showed surface alterations on samples conditioned with acid. It is possible to conclude that the group conditioned with hydrofluoric acid showed better adhesive behavior.
- Open Access
- 6 February 2022
- Published by Research, Society and Development in Research, Society and Development
- Vol. 11 (3)
Analysis of compressive strength of occlusal splints manufactured with three liquid resins at three angles of orientation on 3D printer
The aim of this study is to analyze the compressive strength of occlusal splints manufactured with three different liquid resins in a 3D printer and in three angles of orientation. The resins used here are (n=12): Resilab Clear (Wilcos do Brasil, Petrópolis, RJ, Brazil), Prizma Smart Print Bio (Makertech Labs, Tatuí, SP, Brazil), and Cosmos Splint (Yller Biomateriais, Pelotas, RS, Brazil); each resin group are divided into three subgroups according to orientation of manufacture: 0, 45 and 90 degrees. A dental manikin was scanned and the file was used to manufacture a steel hemiarch model. This model was used to design the occlusal splints and as a basis for the tests. The splints were designed with flat occlusal surface and minimum thickness of 2 mm. The compressive test was performed with constant force of 200N, velocity of 0.5 mm/min, along the entire occlusal surface until fracture. Results show no difference between the resins, regardless of orientation of manufacture. The orientation showed no intragroup effect for resins Prizma Smart Print Bio and Resilab Clear; the resin Cosmos showed larger compressive strength for the samples manufactured at 45 degrees than at 0 degree. The 90-degree samples were intermediary and showed no difference from other angles. This study shows that the three resins had similar behavior in terms of compressive strength, except for the intragroup effect of orientation of Cosmos Splint resin, where plates manufactured at 0 degree performed worse than those at 45 degrees.
- 6 February 2022
- Published by Research, Society and Development in Research, Society and Development
- Vol. 11 (3)
Open AccessAnalysis of compressive strength of occlusal splints manufactured with three liquid resins at three angles of orientation on 3D printer
The aim of this study is to analyze the compressive strength of occlusal splints manufactured with three different liquid resins in a 3D printer and in three angles of orientation. The resins used here are (n=12): Resilab Clear (Wilcos do Brasil, Petrópolis, RJ, Brazil), Prizma Smart Print Bio (Makertech Labs, Tatuí, SP, Brazil), and Cosmos Splint (Yller Biomateriais, Pelotas, RS, Brazil); each resin group are divided into three subgroups according to orientation of manufacture: 0, 45 and 90 degrees. A dental manikin was scanned and the file was used to manufacture a steel hemiarch model. This model was used to design the occlusal splints and as a basis for the tests. The splints were designed with flat occlusal surface and minimum thickness of 2 mm. The compressive test was performed with constant force of 200N, velocity of 0.5 mm/min, along the entire occlusal surface until fracture. Results show no difference between the resins, regardless of orientation of manufacture. The orientation showed no intragroup effect for resins Prizma Smart Print Bio and Resilab Clear; the resin Cosmos showed larger compressive strength for the samples manufactured at 45 degrees than at 0 degree. The 90-degree samples were intermediary and showed no difference from other angles. This study shows that the three resins had similar behavior in terms of compressive strength, except for the intragroup effect of orientation of Cosmos Splint resin, where plates manufactured at 0 degree performed worse than those at 45 degrees.