MYMinglong Yang

Minglong Yang

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Minglong Yang has a total of 24 co-authors. Here are the top co-authors by number of shared publications:

  • Haitao Liu

    Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha 410073, China

    3 shared publications
  • Yadan Wu

    Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha 410073, China

    3 shared publications
  • Xun Sun

    Science and Technology on Advanced Ceramic Fibers and Composites Laboratory College of Aerospace Science and Engineering National University of Defense Technology Changsha China

    2 shared publications
  • Chaocan Cai

    1 shared publication
  • Di Lan

    School of Automotive Materials Hubei University of Automotive Technology Shiyan 442002 China

    1 shared publication
  • Dongyi Lei

    School of Civil Engineering, Qingdao University of Technology, Qingdao 266520, China

    1 shared publication

Latest Publications

  • Open Access

    Investigation on the Degradation Mechanisms and Mechanical Property Evolution of 3D-SiO2-Fiber-Reinforced Polyimide Composites After Thermal Aging

    by Minglong Yang, Yadan Wu, Jiahao He, Qiujin Gu, Haitao Liu

    Understanding the thermal aging behavior of SiO2f/PI composites is crucial for ensuring their reliability and longevity in high-temperature aerospace applications. In this study, the thermal aging behavior of three-dimensional quartz-fiber-reinforced polyimide (3D-SiO2f/PI) composites was investigated. The composites were fabricated through a modified prepreg compression molding (PCM) method, including a vacuum-assisted impregnation process followed by thermal compression molding. Long-term thermal aging was carried out to evaluate the high-temperature aging resistance. The flexural properties were tested with a three-point bending test method. The micromechanical characterization was performed though nanoindentation. Interfacial properties were evaluated through single-fiber push-in tests, and the interfacial shear strength (IFSS) was calculated. The thermal aging experiment results revealed that the composites maintained excellent long-term thermal stability. The PI matrix showed no detectable oxidation or thermal degradation of after 100 h aging at 350 °C, yet no significant porosity or cracks were observed for the composite. However, further prolonged thermal exposure led to significant mechanical property degradation. The flexural strength retention rates dropped to below 15% after 300 h at 350 °C or 100 h at 400 °C aging. On the other hand, 350 °C isothermal aging for 300 h led to a progressive decrease in IFSS from 128.6 MPa to near-zero. The degradation mechanism was primarily attributed to two factors: increased porosity due to thermal decomposition of the PI matrix and significant deterioration of fiber–matrix interfacial bonding strength. These findings provide critical insights into the durability prediction and failure mechanisms of 3D-SiO2f/PI composites in high-temperature usage environments.

  • Top Cited Papers

    Construction of cotton derived carbon fiber@FeNi nanoparticle/porous carbon sponge for boosting electromagnetic wave absorption

    by Ying Li, Yu‐Hao Lu, Zhen‐Xin Liu, Dong‐Yi Lei, Ming‐Long Yang, Dong‐Lei Yang, Yi‐Han Jin, Jia‐Xin Liu, Di Lan

    Carbon‐based sponge materials have attracted massive attention as electromagnetic wave (EMW) absorber candidates due to their lightweight and excellent electromagnetic (EM) attenuation capability. However, the high cost, complex fabrication process and limited EMW absorption bandwidth restrict their application. Herein, a hierarchical three‐dimensional (3D) cotton derived carbon fibers coated with core–shell structure FeNi nanoparticle@porous carbon (CCF/FeNi@PC) from MOF precursor were successfully constructed by coprecipitation and one‐step pyrolysis methods. By regulating carbonization temperature, optimizing the electromagnetic parameters, outstanding electromagnetic absorption (EMA) performance was achieved. The CCF@FeNi/PC synthesized at 900 °C demonstrates a −64.5 dB minimum reflection loss (RL min ) at 15.39 GHz, and the effective absorption bandwidth (EAB) is 5.08 GHz when the thickness is only 1.9 mm. Notably, the maximum EAB (EAB max ) was extended 8.18 GHz at 2.96 mm for FeNi‐800. The excellent microwave absorption performance is attributed to the synergistic effect of enhanced dielectric loss and magnetic loss, good impedance matching as well as hierarchical multiple scattering and reflection of EMWs. The obtained CCF@FeNi/PC composites provide a novel and promising strategy for constructing lightweight low‐cost efficient microwave absorption materials.


  • Open Access

    Study on Thermal Oxygen Aging Characteristics and Degradation Kinetics of PMR350 Resin

    by Yadan Wu, Wenchen Zhao, Yang Liu, Haitao Liu, Minglong Yang, Xun Sun

    The thermal stability and aging kinetics of polyimides have garnered significant research attention. As a newly developed class of high thermal stability polyimide, the thermal aging characteristics and degradation kinetics of phenylene-capped polyimide prepolymer (PMR350) have not yet been reported. In this article, the thermo-oxidative stability of PMR350 was investigated systematically. The thermal degradation kinetics of PMR350 resin under different atmospheres were also analyzed using the Flynn–Wall–Ozawa method, the Kissinger–Akahira–Sunose method, and the Friedman method. Thermogravimetric analysis (TGA) results revealed that the 5% thermal decomposition temperature (Td5%) of PMR350 in a nitrogen atmosphere was 29 °C higher than that in air, and the maximum thermal degradation rate was 0.0025%/°C, which is only one-seventh of that observed in air. Isothermal oxidative aging results indicated that the weight loss rate of PMR350 and the time-dependence relationship follow a first-order exponential growth function. PMR350 resin thermal decomposition reaction under air atmosphere includes one stage, with a degradation activation energy of approximately 57 kJ/mol. The reaction model g(α) fits the F2 model, and the integral form is given by g(α) = 1/(1 − α). In contrast, the thermal decomposition reaction under a nitrogen atmosphere consists of two stages, with degradation activation energies of 240 kJ/mol and 200 kJ/mol, respectively. The reaction models g(α) correspond to the A2 and D3 models, with the integral forms represented as g(α) = [−ln(1 − α)]2 and g(α) = [1 − (1 − α)1/3]2 due to the oxygen accelerating thermal degradation from multiple perspectives. Moreover, PMR350 resin maintained high hardness and modulus even after thermal aging at 350 °C for 300 h. The results indicate that the resin exhibits excellent resistance to thermal and oxygen aging. This study represents the first systematic analysis of the thermal stability characteristics of PMR350 resin, offering essential theoretical insights and data support for understanding the mechanisms of thermal stability modification in PMR350 and its engineering applications.


  • Curved and straight combined cross-section structure for energy absorption

    by Xin Wang, Weilong Yin, Liuxiao Zou, Chaocan Cai, Peng Li, Huiran Zou, MingLong Yang, Jianjun Li, Yibin Li