Xun Sun
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Xun Sun has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Haitao Liu
Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha 410073, China
4 shared publications - Minglong Yang
Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha 410073, China
2 shared publications - Yadan Wu
Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha 410073, China
2 shared publications - Yang Liu
Science and Technology on Advanced Ceramic Fibers and Composites Laboratory College of Aerospace Science and Engineering National University of Defense Technology Changsha China
2 shared publications Jian Ma
1 shared publicationRu Jiang
School of Physics and Electronic Science Hunan University of Science and Technology Xiangtan China
1 shared publication
Latest Publications
- 22 February 2025
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Impact of heat treatment on microstructure and tensile strength of monofilaments and bundles of aluminosilicate fibers
Continuous alumina fiber serves as the reinforcement phase within the Al2O3/oxide composite system, and its behavior at elevated temperatures significantly influences the mechanical properties of the composite. This study focuses on a novel type of continuous aluminosilicate fiber (AF18) to investigate the effects of heat treatment temperature (ranging from 1100°C to 1400°C) and duration (2/4/8 h) on the microstructure and mechanical properties of the monofilament. Acknowledging that fibers typically exist in bundles within the composite material, the study further examines the changes in tensile strength of these bundles following heat treatment at various temperatures. The findings indicate that both the heat treatment temperature and duration contribute to an increase in grain size and an enhancement in the surface roughness of the fiber, with the temperature having a more pronounced effect than the duration. The tensile strength of the original fiber monofilament is measured at 2.08 GPa, while the tensile strength of the tow exhibits a reduction of approximately 10% compared to the monofilament, with the degree of attenuation correlating with the heat treatment conditions. Notably, with 8 h of heat treatment at 1200°C, the fiber retains approximately 70% of its tensile strength, demonstrating its capacity for long‐term temperature resistance.
- 22 February 2025
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Impact of heat treatment on microstructure and tensile strength of monofilaments and bundles of aluminosilicate fibers
Continuous alumina fiber serves as the reinforcement phase within the Al2O3/oxide composite system, and its behavior at elevated temperatures significantly influences the mechanical properties of the composite. This study focuses on a novel type of continuous aluminosilicate fiber (AF18) to investigate the effects of heat treatment temperature (ranging from 1100°C to 1400°C) and duration (2/4/8 h) on the microstructure and mechanical properties of the monofilament. Acknowledging that fibers typically exist in bundles within the composite material, the study further examines the changes in tensile strength of these bundles following heat treatment at various temperatures. The findings indicate that both the heat treatment temperature and duration contribute to an increase in grain size and an enhancement in the surface roughness of the fiber, with the temperature having a more pronounced effect than the duration. The tensile strength of the original fiber monofilament is measured at 2.08 GPa, while the tensile strength of the tow exhibits a reduction of approximately 10% compared to the monofilament, with the degree of attenuation correlating with the heat treatment conditions. Notably, with 8 h of heat treatment at 1200°C, the fiber retains approximately 70% of its tensile strength, demonstrating its capacity for long‐term temperature resistance.
- Open Access
Study on Thermal Oxygen Aging Characteristics and Degradation Kinetics of PMR350 Resin
The thermal stability and aging kinetics of polyimides have garnered significant research attention. As a newly developed class of high thermal stability polyimide, the thermal aging characteristics and degradation kinetics of phenylene-capped polyimide prepolymer (PMR350) have not yet been reported. In this article, the thermo-oxidative stability of PMR350 was investigated systematically. The thermal degradation kinetics of PMR350 resin under different atmospheres were also analyzed using the Flynn–Wall–Ozawa method, the Kissinger–Akahira–Sunose method, and the Friedman method. Thermogravimetric analysis (TGA) results revealed that the 5% thermal decomposition temperature (Td5%) of PMR350 in a nitrogen atmosphere was 29 °C higher than that in air, and the maximum thermal degradation rate was 0.0025%/°C, which is only one-seventh of that observed in air. Isothermal oxidative aging results indicated that the weight loss rate of PMR350 and the time-dependence relationship follow a first-order exponential growth function. PMR350 resin thermal decomposition reaction under air atmosphere includes one stage, with a degradation activation energy of approximately 57 kJ/mol. The reaction model g(α) fits the F2 model, and the integral form is given by g(α) = 1/(1 − α). In contrast, the thermal decomposition reaction under a nitrogen atmosphere consists of two stages, with degradation activation energies of 240 kJ/mol and 200 kJ/mol, respectively. The reaction models g(α) correspond to the A2 and D3 models, with the integral forms represented as g(α) = [−ln(1 − α)]2 and g(α) = [1 − (1 − α)1/3]2 due to the oxygen accelerating thermal degradation from multiple perspectives. Moreover, PMR350 resin maintained high hardness and modulus even after thermal aging at 350 °C for 300 h. The results indicate that the resin exhibits excellent resistance to thermal and oxygen aging. This study represents the first systematic analysis of the thermal stability characteristics of PMR350 resin, offering essential theoretical insights and data support for understanding the mechanisms of thermal stability modification in PMR350 and its engineering applications.
Open AccessStudy on Thermal Oxygen Aging Characteristics and Degradation Kinetics of PMR350 Resin
The thermal stability and aging kinetics of polyimides have garnered significant research attention. As a newly developed class of high thermal stability polyimide, the thermal aging characteristics and degradation kinetics of phenylene-capped polyimide prepolymer (PMR350) have not yet been reported. In this article, the thermo-oxidative stability of PMR350 was investigated systematically. The thermal degradation kinetics of PMR350 resin under different atmospheres were also analyzed using the Flynn–Wall–Ozawa method, the Kissinger–Akahira–Sunose method, and the Friedman method. Thermogravimetric analysis (TGA) results revealed that the 5% thermal decomposition temperature (Td5%) of PMR350 in a nitrogen atmosphere was 29 °C higher than that in air, and the maximum thermal degradation rate was 0.0025%/°C, which is only one-seventh of that observed in air. Isothermal oxidative aging results indicated that the weight loss rate of PMR350 and the time-dependence relationship follow a first-order exponential growth function. PMR350 resin thermal decomposition reaction under air atmosphere includes one stage, with a degradation activation energy of approximately 57 kJ/mol. The reaction model g(α) fits the F2 model, and the integral form is given by g(α) = 1/(1 − α). In contrast, the thermal decomposition reaction under a nitrogen atmosphere consists of two stages, with degradation activation energies of 240 kJ/mol and 200 kJ/mol, respectively. The reaction models g(α) correspond to the A2 and D3 models, with the integral forms represented as g(α) = [−ln(1 − α)]2 and g(α) = [1 − (1 − α)1/3]2 due to the oxygen accelerating thermal degradation from multiple perspectives. Moreover, PMR350 resin maintained high hardness and modulus even after thermal aging at 350 °C for 300 h. The results indicate that the resin exhibits excellent resistance to thermal and oxygen aging. This study represents the first systematic analysis of the thermal stability characteristics of PMR350 resin, offering essential theoretical insights and data support for understanding the mechanisms of thermal stability modification in PMR350 and its engineering applications.
- Open Access
- 20 April 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 30, 5677-5684
Effect of high temperature annealing on microstructure and mechanical properties of Morlion735 alumina fiber
- 20 April 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 30, 5677-5684
Open AccessEffect of high temperature annealing on microstructure and mechanical properties of Morlion735 alumina fiber
- 4 November 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (2) , 655-663
Slurry infiltration and sintering cycle‐dependent mechanical properties of 3D oxide/oxide ceramic matrix composites
In this study, oxide/oxide ceramic matrix composites reinforced with three‐dimensional fiber preform were fabricated by a slurry infiltration and sintering (SIS) process. The influence of the SIS cycle on microstructures and mechanical properties of the 3D oxide/oxide composite was investigated. Results showed that the porous matrix was densified due to the SIS effect. The elastic modulus of the weak matrix and interfacial shear strength increased with the increasing SIS cycle. This led to an obvious improvement in flexural strength and interlaminar shear strength of the composite. The fracture toughness and work of fracture of the composite slightly decreased. A good balance between fracture strength and damage tolerance was achieved on the sixth SIS fabricated oxide/oxide composite, which had a high flexural strength of 295.1 ± 14.9 MPa, a high interlaminar shear strength of 18.2 ± .5 MPa, and a high fracture 11.5 ± .8 MPa m 1/2 . The SIS process is a promising way to fabricate the 3D oxide/oxide composite.
- 4 November 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (2) , 655-663
Slurry infiltration and sintering cycle‐dependent mechanical properties of 3D oxide/oxide ceramic matrix composites
In this study, oxide/oxide ceramic matrix composites reinforced with three‐dimensional fiber preform were fabricated by a slurry infiltration and sintering (SIS) process. The influence of the SIS cycle on microstructures and mechanical properties of the 3D oxide/oxide composite was investigated. Results showed that the porous matrix was densified due to the SIS effect. The elastic modulus of the weak matrix and interfacial shear strength increased with the increasing SIS cycle. This led to an obvious improvement in flexural strength and interlaminar shear strength of the composite. The fracture toughness and work of fracture of the composite slightly decreased. A good balance between fracture strength and damage tolerance was achieved on the sixth SIS fabricated oxide/oxide composite, which had a high flexural strength of 295.1 ± 14.9 MPa, a high interlaminar shear strength of 18.2 ± .5 MPa, and a high fracture 11.5 ± .8 MPa m 1/2 . The SIS process is a promising way to fabricate the 3D oxide/oxide composite.