Siska Prifiharni
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Siska Prifiharni has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
Gadang Priyotomo
National Research and Innovation Agency, Research Center of Metallurgy, Tangerang Selatan, Indonesia
3 shared publicationsArini Nikitasari
National Research and Innovation Agency, Research Center of Metallurgy, Tangerang Selatan, Indonesia
2 shared publications- Gadang Priyotomo
National Research and Innovation Agency
2 shared publications Rahayu Kusumastuti
National Research and Innovation Agency, Research Center of Metallurgy, Tangerang Selatan, Indonesia
2 shared publicationsSiti Musabikha
National Research and Innovation Agency, Research Center of Metallurgy, Tangerang Selatan, Indonesia
2 shared publicationsAga Ridhova
1 shared publication
Latest Publications
- Open Access
- 15 March 2024
- Published by Engineering Society of Corrosion in Zastita materijala
- Vol. 65 (1) , 35-44
Electrochemical analysis of corrosion inhibition shallot leaf (Allium cepa) extract on mild steel in acidic medium at different immersion times
Plant derivatives as eco-friendly corrosion inhibitors are currently greatly interested in much research. Shallot leaf (Allium cepa) was utilized in 0.1M HCl as a corrosion inhibitor of mild steel. The functional groups present in the macerated extract were subsequently identified using an FTIR test. Electrochemical tests such as tafel polarization and EIS were carried out to determine the corrosion inhibition performance of shallot leaf extract on the SS400 steel. The results of the electrochemical analysis show that shallot leaf extract can inhibit mild steel up to 94% at a concentration of 500 ppm. Furthermore, the addition of SLE reduces surface damage of mild steel, which can be seen by SEM.
- 15 March 2024
- Published by Engineering Society of Corrosion in Zastita materijala
- Vol. 65 (1) , 35-44
Open AccessElectrochemical analysis of corrosion inhibition shallot leaf (Allium cepa) extract on mild steel in acidic medium at different immersion times
Plant derivatives as eco-friendly corrosion inhibitors are currently greatly interested in much research. Shallot leaf (Allium cepa) was utilized in 0.1M HCl as a corrosion inhibitor of mild steel. The functional groups present in the macerated extract were subsequently identified using an FTIR test. Electrochemical tests such as tafel polarization and EIS were carried out to determine the corrosion inhibition performance of shallot leaf extract on the SS400 steel. The results of the electrochemical analysis show that shallot leaf extract can inhibit mild steel up to 94% at a concentration of 500 ppm. Furthermore, the addition of SLE reduces surface damage of mild steel, which can be seen by SEM.
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3003 (1) , 020053
Seaweed (Sargassum polycystum) extract as eco-friendly corrosion inhibitor for mild steel in CO2-saturated 3.5% NaCl solution
In the petroleum industry, sweet corrosion is the most severe corrosion concern for steel-based crude oil transportation pipelines. It is a type of severe local
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3003 (1) , 020053
Seaweed (Sargassum polycystum) extract as eco-friendly corrosion inhibitor for mild steel in CO2-saturated 3.5% NaCl solution
In the petroleum industry, sweet corrosion is the most severe corrosion concern for steel-based crude oil transportation pipelines. It is a type of severe local
- Open Access
- 31 December 2022
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 6 (6 (120)) , 30-41
Effect of syzygium cumini leaf extract as a green corrosion inhibitor on API 5l carbon steel in 1M HCL
Corrosion in API 5L steel under 1M HCl is a common issue; hence, creating a more effective and naturally-based inhibitor is critical. In this research, Syzygium Cumini leaf extract (SCLE) was used as a new green corrosion inhibitor under acidic conditions. The inhibition properties of the novel cumini extract were thoroughly characterized using potentiodynamic polarization (PDP), electrochemical impedance spectroscopy (EIS), Fourier-transform infrared spectroscopy (FTIR), and atomic force microscope (AFM). The results show that the cumini inhibitor has excellent corrosion inhibition with 93 % inhibition efficiency. The adsorption behavior of the inhibitor follows the Langmuir Adsorption Isotherm due to the nearness of R2 to unity. The potentiodynamic and electrochemical measurements demonstrate the mixed type of corrosion inhibitor. Thermodynamic calculation of ΔGads is – 18.41 kJ mol-1 showing the physical adsorption process between the inhibitor and metals. Further inspection of ΔHads at ‒58.93 kJ mol-1 considers releasing energy during adsorption. The FTIR results agree with the increased growth of passive layers due to the adsorption of polyphenol and flavonoids on metals. Remarkably, the adsorption peak at 3266.59 cm-1 corresponds to the adsorption of –OH. The peak at 1612.56 and 1698.4 cm-1 is attributed to C=C and C=O functional groups. The above functional groups serve as adsorption centers to reduce the corrosion effect. The surface treatment of AFM indicated a good relationship with the functional group characterization and confirmed the significant corrosion rate reduction. This work can be used as a benchmark to develop a natural plant as a corrosion inhibitor.
- 31 December 2022
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 6 (6 (120)) , 30-41
Open AccessEffect of syzygium cumini leaf extract as a green corrosion inhibitor on API 5l carbon steel in 1M HCL
Corrosion in API 5L steel under 1M HCl is a common issue; hence, creating a more effective and naturally-based inhibitor is critical. In this research, Syzygium Cumini leaf extract (SCLE) was used as a new green corrosion inhibitor under acidic conditions. The inhibition properties of the novel cumini extract were thoroughly characterized using potentiodynamic polarization (PDP), electrochemical impedance spectroscopy (EIS), Fourier-transform infrared spectroscopy (FTIR), and atomic force microscope (AFM). The results show that the cumini inhibitor has excellent corrosion inhibition with 93 % inhibition efficiency. The adsorption behavior of the inhibitor follows the Langmuir Adsorption Isotherm due to the nearness of R2 to unity. The potentiodynamic and electrochemical measurements demonstrate the mixed type of corrosion inhibitor. Thermodynamic calculation of ΔGads is – 18.41 kJ mol-1 showing the physical adsorption process between the inhibitor and metals. Further inspection of ΔHads at ‒58.93 kJ mol-1 considers releasing energy during adsorption. The FTIR results agree with the increased growth of passive layers due to the adsorption of polyphenol and flavonoids on metals. Remarkably, the adsorption peak at 3266.59 cm-1 corresponds to the adsorption of –OH. The peak at 1612.56 and 1698.4 cm-1 is attributed to C=C and C=O functional groups. The above functional groups serve as adsorption centers to reduce the corrosion effect. The surface treatment of AFM indicated a good relationship with the functional group characterization and confirmed the significant corrosion rate reduction. This work can be used as a benchmark to develop a natural plant as a corrosion inhibitor.
- 13 May 2022
- Published by Elsevier in Journal of the Indian Chemical Society
- Vol. 99 (7)
Extract sarampa wood (Xylocarpus Moluccensis) as an eco-friendly corrosion inhibitor for mild steel in HCl 1M
- 13 May 2022
- Published by Elsevier in Journal of the Indian Chemical Society
- Vol. 99 (7)
Extract sarampa wood (Xylocarpus Moluccensis) as an eco-friendly corrosion inhibitor for mild steel in HCl 1M
- Open Access
- 27 August 2021
- Published by College of Graduate Studies, Walailak University in Walailak Journal of Science and Technology (WJST)
- Vol. 18 (17)
A Field Study of Atmospheric Corrosion of Carbon Steel after Short Exposure in Pelabuhan Ratu, West Java Province, Indonesia
The investigation of atmospheric corrosion of mild carbon steel as representative of offshore infrastructure has been carried out in the marine tropical of Pelabuhan Ratu, West Java, Indonesia. They are exposed up to 76 days of periods, and their corrosion rates are determined according to ASTM G1-03. The surface morphology, the elemental compositions and compounds were observed using a scanning electron microscope (SEM), energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD), respectively. The environmental parameters of the test site are monitored during exposure, such as air temperature, relative humidity (RH), airborne salinity and dew temperature. Based on the results, the corrosion rates of steels were 2.79 and 2.8 mpy within the 27 and 76 days exposures, respectively. The presence of chloride deposition on the surface of steel can increase the severity of corrosion. Moreover, the detrimental effect of chloride was observed in rust product, which was covered by an oxygen element. The main phases of rust products present were magnetite (Fe3O4) and hematite (α-Fe2O3.H2O). Several cracks were observed in the rust layer, which tended to exfoliate and lose adherence and protectiveness from further corrosion attack. HIGHLIGHTS GRAPHICAL ABSTRACT
- 27 August 2021
- Published by College of Graduate Studies, Walailak University in Walailak Journal of Science and Technology (WJST)
- Vol. 18 (17)
Open AccessA Field Study of Atmospheric Corrosion of Carbon Steel after Short Exposure in Pelabuhan Ratu, West Java Province, Indonesia
The investigation of atmospheric corrosion of mild carbon steel as representative of offshore infrastructure has been carried out in the marine tropical of Pelabuhan Ratu, West Java, Indonesia. They are exposed up to 76 days of periods, and their corrosion rates are determined according to ASTM G1-03. The surface morphology, the elemental compositions and compounds were observed using a scanning electron microscope (SEM), energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD), respectively. The environmental parameters of the test site are monitored during exposure, such as air temperature, relative humidity (RH), airborne salinity and dew temperature. Based on the results, the corrosion rates of steels were 2.79 and 2.8 mpy within the 27 and 76 days exposures, respectively. The presence of chloride deposition on the surface of steel can increase the severity of corrosion. Moreover, the detrimental effect of chloride was observed in rust product, which was covered by an oxygen element. The main phases of rust products present were magnetite (Fe3O4) and hematite (α-Fe2O3.H2O). Several cracks were observed in the rust layer, which tended to exfoliate and lose adherence and protectiveness from further corrosion attack. HIGHLIGHTS GRAPHICAL ABSTRACT
- Open Access
- 1 January 2016
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 1725 (1) , 020005
The effect of tempering temperature on pitting corrosion resistance of 420 stainless steels
The AISI Type 420 stainless steels are commonly used to steam generators, mixer blades, etc. These stainless steels are most prone to pitting in dissolved Cl− containing environments. In this paper, the effect of tempering temperature on pitting corrosion resistance of AISI Type 420 stainless steels was studied. The AISI Type 420 stainless steels specimens were heat treated at the temperature of 1050°C for 1 hour to reach austenite stabilization and then quench in the oil. After that, the specimens were tempered at the temperature of 150, 250, 350 and 450°C for 30 minutes and then air cooled to the room temperature. The electrochemical potentiodynamic polarization test was conducted at 3.5% sodium chloride solution to evaluate corrosion rate and pitting corrosion behaviour. The Scanning Electron Microscope (SEM), Energy Dispersive X-Ray Spectroscopy (EDS) were used to evaluate the pitting corrosion product. The result have shown that highest pitting potential was found in the sample tempered at 250°C and corrosion pits were found to initiate preferentially around chromium carbides.
- 1 January 2016
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 1725 (1) , 020005
Open AccessThe effect of tempering temperature on pitting corrosion resistance of 420 stainless steels
The AISI Type 420 stainless steels are commonly used to steam generators, mixer blades, etc. These stainless steels are most prone to pitting in dissolved Cl− containing environments. In this paper, the effect of tempering temperature on pitting corrosion resistance of AISI Type 420 stainless steels was studied. The AISI Type 420 stainless steels specimens were heat treated at the temperature of 1050°C for 1 hour to reach austenite stabilization and then quench in the oil. After that, the specimens were tempered at the temperature of 150, 250, 350 and 450°C for 30 minutes and then air cooled to the room temperature. The electrochemical potentiodynamic polarization test was conducted at 3.5% sodium chloride solution to evaluate corrosion rate and pitting corrosion behaviour. The Scanning Electron Microscope (SEM), Energy Dispersive X-Ray Spectroscopy (EDS) were used to evaluate the pitting corrosion product. The result have shown that highest pitting potential was found in the sample tempered at 250°C and corrosion pits were found to initiate preferentially around chromium carbides.