Rohinikumar Chebolu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Rohinikumar Chebolu has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
Ramanaiah Nallu
Department of Mechanical Engineering, A.U. College of Engineering(A), Andhra University, Visakhapatnam, Andhra Pradesh, India
5 shared publicationsArchana Sharma
Pulsed Power & Electromagnetics Division, Bhabha Atomic Research Centre, Visakhapatnam, Andhra Pradesh, India
3 shared publicationsMahalakshmi Kakarla
Department of Mechanical Engineering, A.U. College of Engineering(A), Andhra University, Visakhapatnam, Andhra Pradesh, India
2 shared publications- Ramesh Rudrapati
Department of Industrial Engineering
2 shared publications Ratnam Chanamala
Dept. of Mechanical Engineering
2 shared publications- Surender Kumar Sharma
Homi Bhabha National Institute Mumbai India
2 shared publications
Latest Publications
- 1 June 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (2) , 025555
Experimental investigation on microstructure, hardness and corrosion resistance of an electromagnetic welded titanium-stainless steel dissimilar materials
The electromagnetic welding (EMW), often known as magnetic pulse welding, is a solid-state welding technology that is used to join two different materials using high-velocity impact. In this study an attempt was made to join the Titanium(Ti)- Stainless Steel(SS 304) materials with the help of multi turn disc coil along with the field shaper. A comparative investigation was conducted on the joint’s microstructure, as well as its mechanical and corrosion properties. Inverted optical microscopy (OM) and x-ray diffraction (XRD) were used to do the microstructural characterization of the joint. The micro-Vickers hardness test was used to analyse the material’s mechanical properties. In addition, electrochemical experiments were run on the Ti-SS 304 EMW junction as well as the component materials to establish how resistant they were to corrosion. Using an electrochemical impedance analyzer, the levels of corrosion that were caused by the structures were measured while they were submerged in a solution of nitric acid at room temperature. The microstructural pictures revealed a wave-like pattern at the material’s interface, which is evidence of strong adhesion between the components. The micro vickers hardness of the joints was within the permitted range, as was the corrosion rate.
- 1 June 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (2) , 025555
Experimental investigation on microstructure, hardness and corrosion resistance of an electromagnetic welded titanium-stainless steel dissimilar materials
The electromagnetic welding (EMW), often known as magnetic pulse welding, is a solid-state welding technology that is used to join two different materials using high-velocity impact. In this study an attempt was made to join the Titanium(Ti)- Stainless Steel(SS 304) materials with the help of multi turn disc coil along with the field shaper. A comparative investigation was conducted on the joint’s microstructure, as well as its mechanical and corrosion properties. Inverted optical microscopy (OM) and x-ray diffraction (XRD) were used to do the microstructural characterization of the joint. The micro-Vickers hardness test was used to analyse the material’s mechanical properties. In addition, electrochemical experiments were run on the Ti-SS 304 EMW junction as well as the component materials to establish how resistant they were to corrosion. Using an electrochemical impedance analyzer, the levels of corrosion that were caused by the structures were measured while they were submerged in a solution of nitric acid at room temperature. The microstructural pictures revealed a wave-like pattern at the material’s interface, which is evidence of strong adhesion between the components. The micro vickers hardness of the joints was within the permitted range, as was the corrosion rate.
- 28 March 2024
- Published by Springer Nature in Acta Mechanica
- Vol. 235 (6) , 3687-3697
Effect of interlayer materials on microstructure, hardness and corrosion resistance of an electromagnetic welded titanium–stainless steel interface
- 28 March 2024
- Published by Springer Nature in Acta Mechanica
- Vol. 235 (6) , 3687-3697
Effect of interlayer materials on microstructure, hardness and corrosion resistance of an electromagnetic welded titanium–stainless steel interface
- Open Access
- 14 April 2023
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2023, 1-7
Experimental Studies on Mechanical Behavior of TIG and Friction Stir Welded AA5083 -AA7075 Dissimilar Aluminum Alloys
Welding is a suitable and better process to manufacture complex objects for aerospace, naval, and automotive structures. Service conditions and complexity in load acting force the manufactures to make joints between dissimilar materials. Thus, there is a need for efficient welding techniques to form sound joints and an understanding of imperfections and their effects. In this study an attempt has been made to study the joining feasibility of dissimilar aluminum alloys by two different welding techniques, namely, tungsten inert gas welding (TIG) and friction stir welding (FSW). Dissimilar AA5083-O and AA7075-T651 aluminum alloys successfully joined by considered welding techniques. Metallurgical and mechanical characteristics of fabricated weld joints are studied at different weld currents (80–120 amp) for TIG and various rotational speeds (800, 1000, 1100, 1200, and 1400 rpm) with constant traverse speed for FSW. Weld joints made by FSW exhibit superior tensile strength, whereas the joint line microhardness of TIG samples is higher than the FSW ones.
- 14 April 2023
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2023, 1-7
Open AccessExperimental Studies on Mechanical Behavior of TIG and Friction Stir Welded AA5083 -AA7075 Dissimilar Aluminum Alloys
Welding is a suitable and better process to manufacture complex objects for aerospace, naval, and automotive structures. Service conditions and complexity in load acting force the manufactures to make joints between dissimilar materials. Thus, there is a need for efficient welding techniques to form sound joints and an understanding of imperfections and their effects. In this study an attempt has been made to study the joining feasibility of dissimilar aluminum alloys by two different welding techniques, namely, tungsten inert gas welding (TIG) and friction stir welding (FSW). Dissimilar AA5083-O and AA7075-T651 aluminum alloys successfully joined by considered welding techniques. Metallurgical and mechanical characteristics of fabricated weld joints are studied at different weld currents (80–120 amp) for TIG and various rotational speeds (800, 1000, 1100, 1200, and 1400 rpm) with constant traverse speed for FSW. Weld joints made by FSW exhibit superior tensile strength, whereas the joint line microhardness of TIG samples is higher than the FSW ones.
- 1 March 2023
- Published by IOP Publishing in Engineering Research Express
- Vol. 5 (1) , 015055
Experimental investigations on magnetic pulse crimping of copper lug
One of the most complicated issues in the production of electronic circuit boards, vehicles, aircraft, satellite, and communication components is the crimping of electrical wires to produce a secure connection. Furthermore, terminal crimping is crucial to the safe transmission of electricity; improper crimping causes difficulties like overheating of the plug, power loss, arcing, and mechanical connection failure. Magnetic pulse crimping has the ability to effectively address these difficulties. Magnetic pulse crimping is a non-contact technique creating a uniform pressure without any tool marks on lugs. This technique has better compression of conducting metal wires strands inside the lug and also has less voids compared to conventional mechanical crimping techniques. In this technique the pulsed magnetic field is generated inside the electromagnetic coil by the discharge of capacitor bank current. This magnetic field applies uniform pressure across the circumference of lug and crimp it with cable. 120 sq mm copper lug is magnetic pulse crimped with copper wire at 20 T. Significant improvements in leak rate in magnetically crimped lugs is seem compared to mechanically crimped 120 sq mm copper lugs. This technique also reduces the contact resistance and ultimately the temperature during operation in electrical system.
- 1 March 2023
- Published by IOP Publishing in Engineering Research Express
- Vol. 5 (1) , 015055
Experimental investigations on magnetic pulse crimping of copper lug
One of the most complicated issues in the production of electronic circuit boards, vehicles, aircraft, satellite, and communication components is the crimping of electrical wires to produce a secure connection. Furthermore, terminal crimping is crucial to the safe transmission of electricity; improper crimping causes difficulties like overheating of the plug, power loss, arcing, and mechanical connection failure. Magnetic pulse crimping has the ability to effectively address these difficulties. Magnetic pulse crimping is a non-contact technique creating a uniform pressure without any tool marks on lugs. This technique has better compression of conducting metal wires strands inside the lug and also has less voids compared to conventional mechanical crimping techniques. In this technique the pulsed magnetic field is generated inside the electromagnetic coil by the discharge of capacitor bank current. This magnetic field applies uniform pressure across the circumference of lug and crimp it with cable. 120 sq mm copper lug is magnetic pulse crimped with copper wire at 20 T. Significant improvements in leak rate in magnetically crimped lugs is seem compared to mechanically crimped 120 sq mm copper lugs. This technique also reduces the contact resistance and ultimately the temperature during operation in electrical system.
- Open Access
- 17 August 2022
- Published by Wiley in Journal of Engineering
- Vol. 2022, 1-5
Influence of SiC/TiB2 Particles Addition on Corrosion Behavior of As-Cast Zn-Al-Cu Alloy Hybrid Composites
In this work, the silicon carbide (SiC) and titanium diboride (TiB2) reinforced as-cast Zn-Al-Cu alloy-based hybrid composites were produced with ultrasonic-assisted stir casting. The corrosion behavior of as-cast Zn-Al-Cu/TiB2/SiC hybrid composites with varying 0, 5, 10, and 15 weight percent of SiC+TiB2 particulates in Zn-Al-Cu matrix alloy was investigated in this study, The effect of additional reinforcements content on the corrosion behavior of hybrid composites with respect to Zn-Al-Cu alloy was investigated. The corrosion rate of hybrid composites was taken by using potentiodynamic polarization equipment (with 3.5 wt. NaCl solution). The potentiodynamic polarization test findings showed that the hybrid composites uniform and localized corrosion resistances were enhanced by the addition of dual reinforcements. As the weight fraction of the SiC/TiB2 reinforcement increases, weak microgalvanic cells that form between the constituent phases of the fabricated as-cast Zn-Al-Cu hybrid composites weaken, improving their resistance to uniform and localized corrosion. The results revealed that the corrosion rate values were reduced to 28.88 at 15 of reinforcement when compared to the base alloy.
- 17 August 2022
- Published by Wiley in Journal of Engineering
- Vol. 2022, 1-5
Open AccessInfluence of SiC/TiB2 Particles Addition on Corrosion Behavior of As-Cast Zn-Al-Cu Alloy Hybrid Composites
In this work, the silicon carbide (SiC) and titanium diboride (TiB2) reinforced as-cast Zn-Al-Cu alloy-based hybrid composites were produced with ultrasonic-assisted stir casting. The corrosion behavior of as-cast Zn-Al-Cu/TiB2/SiC hybrid composites with varying 0, 5, 10, and 15 weight percent of SiC+TiB2 particulates in Zn-Al-Cu matrix alloy was investigated in this study, The effect of additional reinforcements content on the corrosion behavior of hybrid composites with respect to Zn-Al-Cu alloy was investigated. The corrosion rate of hybrid composites was taken by using potentiodynamic polarization equipment (with 3.5 wt. NaCl solution). The potentiodynamic polarization test findings showed that the hybrid composites uniform and localized corrosion resistances were enhanced by the addition of dual reinforcements. As the weight fraction of the SiC/TiB2 reinforcement increases, weak microgalvanic cells that form between the constituent phases of the fabricated as-cast Zn-Al-Cu hybrid composites weaken, improving their resistance to uniform and localized corrosion. The results revealed that the corrosion rate values were reduced to 28.88 at 15 of reinforcement when compared to the base alloy.
- 1 June 2022
- Published by IOP Publishing in Engineering Research Express
- Vol. 4 (2) , 025040
Experimental investigation on mechanical behavior of as cast Zn-Al-Cu/SiC/TiB2 hybrid metal matrix composite by ultrasonic assisted stir casting technique
Now a days, the Zn-Al-Cu alloy-based composites have great impact on modern trends for bearing applications because of its reliable mechanical performance. In this paper the mechanical characteristics of as cast Zn-Al-Cu alloy-based hybrid metal matrix composites have been investigated, as well as the influence of reinforcements Silicon Carbide (SiC) and Titanium Diboride (TiB2) on the composite. The ultrasonic assisted stir casting technique has been adopted for fabricating the composites with the addition of dual reinforcements like 5 wt% of SiC as constant and by varying the wt% of TiB2 as 0 wt%, 5 wt% and 10 wt%. The ceramic particles SiC and TiB2 are taken with 20 and 30 microns in size. The ASTM standards were used to conduct the different tests, and the findings demonstrate the significance of adding reinforcements to alloy and also noticeable increase in mechanical performance in terms of hardness, tensile strength, young’s modulus and impact strength. As cast Zn-Al-Cu/5 wt.% of SiC/10 wt.% of TiB2 hybrid composite gives the minimum density as 4.79 g cc−1 and maximum hardness as 156Hv.
- 1 June 2022
- Published by IOP Publishing in Engineering Research Express
- Vol. 4 (2) , 025040
Experimental investigation on mechanical behavior of as cast Zn-Al-Cu/SiC/TiB2 hybrid metal matrix composite by ultrasonic assisted stir casting technique
Now a days, the Zn-Al-Cu alloy-based composites have great impact on modern trends for bearing applications because of its reliable mechanical performance. In this paper the mechanical characteristics of as cast Zn-Al-Cu alloy-based hybrid metal matrix composites have been investigated, as well as the influence of reinforcements Silicon Carbide (SiC) and Titanium Diboride (TiB2) on the composite. The ultrasonic assisted stir casting technique has been adopted for fabricating the composites with the addition of dual reinforcements like 5 wt% of SiC as constant and by varying the wt% of TiB2 as 0 wt%, 5 wt% and 10 wt%. The ceramic particles SiC and TiB2 are taken with 20 and 30 microns in size. The ASTM standards were used to conduct the different tests, and the findings demonstrate the significance of adding reinforcements to alloy and also noticeable increase in mechanical performance in terms of hardness, tensile strength, young’s modulus and impact strength. As cast Zn-Al-Cu/5 wt.% of SiC/10 wt.% of TiB2 hybrid composite gives the minimum density as 4.79 g cc−1 and maximum hardness as 156Hv.