Yue Yang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yue Yang has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
- Zhen Luo
School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China
5 shared publications - Yang Li
Tianjin University
2 shared publications - Yuanbo Bi
School of Materials Science and Engineering, Tianjin University, Tianjin, China
2 shared publications - Bofang Zheng
School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China
1 shared publication - Di Zhang
Central Research Institute of Building and Construction Co., Ltd, MCC, Beijing, People's Republic of China
1 shared publication Jiaqi Sun
School of Materials Science and Engineering Tianjin University Tianjin 300350 China
1 shared publication
Latest Publications
- Open Access
Microstructure and Properties of Resistance Element Welded Joints of DP780 Steel and 6061 Aluminum Alloy
This study developed a metallurgical and mechanical hybrid resistance element welding (REW) method to fabricate lightweight Al/steel joints between 2.0 mm 6061 aluminum alloy and 1.2 mm DP780 steel, addressing critical challenges of interfacial intermetallic compounds (IMC layer thickness: 4.6–8.3 μm) in dissimilar metal welding. In addition, the scanning electron microscope (SEM), electron backscatter diffraction (EBSD), and electron probe microanalysis (EPMA) were used to observe the microstructure characteristics and element distribution. The lath martensite and solidification microstructure were observed in the steel-nugget zone and Al-nugget zone, respectively. Furthermore, the microhardness distribution, volume fraction of the α phase, tensile–shear load, and failure mode of REWed joint were studied. Process optimization demonstrated welding current’s pivotal role in joint performance, achieving a maximum tensile–shear load of 6914.1 N under 10 kA conditions with a button pull-out failure (BPF) mechanism.
Open AccessMicrostructure and Properties of Resistance Element Welded Joints of DP780 Steel and 6061 Aluminum Alloy
This study developed a metallurgical and mechanical hybrid resistance element welding (REW) method to fabricate lightweight Al/steel joints between 2.0 mm 6061 aluminum alloy and 1.2 mm DP780 steel, addressing critical challenges of interfacial intermetallic compounds (IMC layer thickness: 4.6–8.3 μm) in dissimilar metal welding. In addition, the scanning electron microscope (SEM), electron backscatter diffraction (EBSD), and electron probe microanalysis (EPMA) were used to observe the microstructure characteristics and element distribution. The lath martensite and solidification microstructure were observed in the steel-nugget zone and Al-nugget zone, respectively. Furthermore, the microhardness distribution, volume fraction of the α phase, tensile–shear load, and failure mode of REWed joint were studied. Process optimization demonstrated welding current’s pivotal role in joint performance, achieving a maximum tensile–shear load of 6914.1 N under 10 kA conditions with a button pull-out failure (BPF) mechanism.
- Open Access
A Comparative Study on the Performance and Microstructure of 304NG Stainless Steel in Underwater and Air Laser Welding
In order to facilitate the application of underwater laser welding technology in in situ repairs of nuclear power plants, this study conducted comparative experiments between local dry underwater laser welding and laser welding in air on 304NG nitrogen-controlled stainless steel. The aim was to explore its microstructural evolution and mechanical properties in underwater environments. It was found that, near the fusion line of laser welding in air, columnar dendrites gradually evolved into cellular dendrites toward the weld center, eventually disappearing, resulting in a skeletal ferrite and serrated austenite structure. The underwater laser welding joints exhibited similar characteristics yet with more pronounced alternation between columnar and cellular dendrites. Additionally, the size of cellular dendrites decreased significantly, and needle-like ferrite was observed at the weld center. The hardness of underwater laser welded joints was slightly higher than that of in-air laser welded joints. Compared to laser welding in air, the strength of underwater laser welding joints increased from 443 MPa to 471 MPa, and the displacement increased from 2.95 mm to 3.45 mm, both types of welded joints exhibited a mixed mode fracture characterized by plasticity and brittleness.
Open AccessA Comparative Study on the Performance and Microstructure of 304NG Stainless Steel in Underwater and Air Laser Welding
In order to facilitate the application of underwater laser welding technology in in situ repairs of nuclear power plants, this study conducted comparative experiments between local dry underwater laser welding and laser welding in air on 304NG nitrogen-controlled stainless steel. The aim was to explore its microstructural evolution and mechanical properties in underwater environments. It was found that, near the fusion line of laser welding in air, columnar dendrites gradually evolved into cellular dendrites toward the weld center, eventually disappearing, resulting in a skeletal ferrite and serrated austenite structure. The underwater laser welding joints exhibited similar characteristics yet with more pronounced alternation between columnar and cellular dendrites. Additionally, the size of cellular dendrites decreased significantly, and needle-like ferrite was observed at the weld center. The hardness of underwater laser welded joints was slightly higher than that of in-air laser welded joints. Compared to laser welding in air, the strength of underwater laser welding joints increased from 443 MPa to 471 MPa, and the displacement increased from 2.95 mm to 3.45 mm, both types of welded joints exhibited a mixed mode fracture characterized by plasticity and brittleness.
- 10 July 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (15)
Weld Growth Mechanism, Microstructure, and Mechanical Properties of Resistance‐Spot‐Welded Joint of R60702 Zirconium‐Alloy Triple Sheets
In this study, triple sheets of R60702 zirconium (Zr) alloy are joined together using the resistance‐spot‐welding process. The nugget formation mechanism and microstructure of the weld joint in three equal‐thickness sheets of R60702 Zr alloy are studied. In the results, it is revealed that the initial nugget forms at the top of the intermediate sheet, and subsequently expands both radially and axially until a complete nugget is formed. The fusion zone (FZ) exhibits a martensitic microstructure, while the heat‐affected zone (HAZ) consists of two regions: coarse‐grain HAZ and fine‐grain HAZ. The hardness in the FZ is higher than that of the HAZ and the base metal. Furthermore, the tensile‐shear force and fracture mode of the weld nuggets are also studied. The weld joints exhibit a maximum tensile‐shear load of 5.7 kN under the following welding parameters: welding current of 14 kA, welding time of 150 ms, and welding force of 3.6 kN. Three failure modes are identified interface fracture, partial button fracture, and button fracture.
- 10 July 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (15)
Weld Growth Mechanism, Microstructure, and Mechanical Properties of Resistance‐Spot‐Welded Joint of R60702 Zirconium‐Alloy Triple Sheets
In this study, triple sheets of R60702 zirconium (Zr) alloy are joined together using the resistance‐spot‐welding process. The nugget formation mechanism and microstructure of the weld joint in three equal‐thickness sheets of R60702 Zr alloy are studied. In the results, it is revealed that the initial nugget forms at the top of the intermediate sheet, and subsequently expands both radially and axially until a complete nugget is formed. The fusion zone (FZ) exhibits a martensitic microstructure, while the heat‐affected zone (HAZ) consists of two regions: coarse‐grain HAZ and fine‐grain HAZ. The hardness in the FZ is higher than that of the HAZ and the base metal. Furthermore, the tensile‐shear force and fracture mode of the weld nuggets are also studied. The weld joints exhibit a maximum tensile‐shear load of 5.7 kN under the following welding parameters: welding current of 14 kA, welding time of 150 ms, and welding force of 3.6 kN. Three failure modes are identified interface fracture, partial button fracture, and button fracture.
- 11 April 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (11)
Microstructure and Mechanical Properties of Similar/Dissimilar Resistance Spot‐Welded Aluminum Alloys for Aerospace Applications
2195 aluminum–lithium (Al–Li) and 2XXX series aluminum alloys are joined using resistance spot welding for the first time. The macrostructure, microstructure, element distribution, microhardness, and tensile‐shear property of spot‐welded joints are investigated. The microstructure of the fusion zone of 2195/2195, 2195/2219, and 2195/2A14 joints is fine equiaxed spherical grains. It is found that solute segregation of Cu occurs in the grain boundaries in the fusion zone, forming Al2Cu. The microhardness shows that due to the dissolution of strengthening phase T1, the hardness of the fusion zone of the three types of joints is lower than that of the base material. The 2195/2195 joint has the best mechanical performance among the three combinations, with maximum tensile‐shear force and absorbed energy reaching 16893.7 N and 24.9 J, respectively. The fracture surfaces of all three types of joints exhibit mixed ductile‐brittle characteristics.
- 11 April 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (11)
Microstructure and Mechanical Properties of Similar/Dissimilar Resistance Spot‐Welded Aluminum Alloys for Aerospace Applications
2195 aluminum–lithium (Al–Li) and 2XXX series aluminum alloys are joined using resistance spot welding for the first time. The macrostructure, microstructure, element distribution, microhardness, and tensile‐shear property of spot‐welded joints are investigated. The microstructure of the fusion zone of 2195/2195, 2195/2219, and 2195/2A14 joints is fine equiaxed spherical grains. It is found that solute segregation of Cu occurs in the grain boundaries in the fusion zone, forming Al2Cu. The microhardness shows that due to the dissolution of strengthening phase T1, the hardness of the fusion zone of the three types of joints is lower than that of the base material. The 2195/2195 joint has the best mechanical performance among the three combinations, with maximum tensile‐shear force and absorbed energy reaching 16893.7 N and 24.9 J, respectively. The fracture surfaces of all three types of joints exhibit mixed ductile‐brittle characteristics.
- Open Access
Effects of Corner Constraint on the Microstructure and Mechanical Properties of Aluminum Alloy Using the CMT+P Deposition Process
Wire arc additive manufacturing technology with cold metal transfer and pulse welding (CMT+P) is a promising technology for fabricating complex metal structures. In this paper, a lot of basic research was conducted on the corner-constrained and unconstrained zones of 4043 aluminum alloy made using CMT+P. In particular, the microstructure morphology and mechanical properties of the corner-constrained and unconstrained zones of 4043 aluminum alloy made by CMT+P were studied by using a thermal field emission scanning electron microscope, a microhardness tester, etc. The results showed that there were cellular crystals at the top, columnar dendritic crystals in the middle and bottom, and smaller equiaxed crystals in the bottom center. The grain size in the corner-constrained zone was larger than that in the unconstrained zone, and the grain size increased by about 88.34%. Moreover, the microhardness of the unconstrained zone was 50 HV, while the microhardness of the corner-constrained zone was 45 HV. Furthermore, the tensile strength of this material was 148 MPa, the elongation was 31%, the fracture behavior in the middle and top areas was typical of a ductile fracture, and the fracture in the bottom area was a mixed ductile–brittle fracture dominated by the ductile fracture.
Open AccessEffects of Corner Constraint on the Microstructure and Mechanical Properties of Aluminum Alloy Using the CMT+P Deposition Process
Wire arc additive manufacturing technology with cold metal transfer and pulse welding (CMT+P) is a promising technology for fabricating complex metal structures. In this paper, a lot of basic research was conducted on the corner-constrained and unconstrained zones of 4043 aluminum alloy made using CMT+P. In particular, the microstructure morphology and mechanical properties of the corner-constrained and unconstrained zones of 4043 aluminum alloy made by CMT+P were studied by using a thermal field emission scanning electron microscope, a microhardness tester, etc. The results showed that there were cellular crystals at the top, columnar dendritic crystals in the middle and bottom, and smaller equiaxed crystals in the bottom center. The grain size in the corner-constrained zone was larger than that in the unconstrained zone, and the grain size increased by about 88.34%. Moreover, the microhardness of the unconstrained zone was 50 HV, while the microhardness of the corner-constrained zone was 45 HV. Furthermore, the tensile strength of this material was 148 MPa, the elongation was 31%, the fracture behavior in the middle and top areas was typical of a ductile fracture, and the fracture in the bottom area was a mixed ductile–brittle fracture dominated by the ductile fracture.
- Open Access
Narrow Gap Welding of X80 Steel Using Laser-CMT Hybrid Welding with Misaligned Laser and Arc
The feasibility of using laser-cold metal transfer (CMT) misaligned hybrid welding to join an X80 line-pipe steel in a narrow gap configuration was investigated. The laser beam interacted with the sidewall and its bottom at a small angle, while the CMT arc acted on the backside of the laser beam. The influence of the distance parameter between the laser spot and the tip of the welding wire on the formation and defects of the filled weld were investigated. Narrow gap bevel welds were performed, and the joints were tensile and had a satisfactory Charpy impact score. The tensile fracture is located in the base metal, and the impact fracture is a ductile fracture. Under this condition, the heat input could be efficiently reduced, preventing the formation of defects such as lack of fusion and reducing the number of pores. Additionally, welds with a narrow heat affect zone (HAZ) could be obtained. The results reveal that the hybrid process, as a low-heat input method, is suitable for narrow gap welding.
Open AccessNarrow Gap Welding of X80 Steel Using Laser-CMT Hybrid Welding with Misaligned Laser and Arc
The feasibility of using laser-cold metal transfer (CMT) misaligned hybrid welding to join an X80 line-pipe steel in a narrow gap configuration was investigated. The laser beam interacted with the sidewall and its bottom at a small angle, while the CMT arc acted on the backside of the laser beam. The influence of the distance parameter between the laser spot and the tip of the welding wire on the formation and defects of the filled weld were investigated. Narrow gap bevel welds were performed, and the joints were tensile and had a satisfactory Charpy impact score. The tensile fracture is located in the base metal, and the impact fracture is a ductile fracture. Under this condition, the heat input could be efficiently reduced, preventing the formation of defects such as lack of fusion and reducing the number of pores. Additionally, welds with a narrow heat affect zone (HAZ) could be obtained. The results reveal that the hybrid process, as a low-heat input method, is suitable for narrow gap welding.