Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Trinuch Eiampongpaiboon has a total of 19 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Effect of various polishing systems on the surface roughness and Streptococcus mutans adhesion of CAD/CAM ceramic materials

    by Anantaya Ekpanithanpong, Trinuch Eiampongpaiboon, Kanda Ngamwuttiwong

    CAD/CAM ceramics provide superior predictability; however, minor adjustments are often required prior to cementation to achieve adequate interdental and oc

  • Open Access

    Layer by layer nanocoating of chlorhexidine-loaded micelles on polymethyl methacrylate denture base

    by Pattarasuda Luanareesatit, Norased Nasongkla, Chuchai Anunmana, Trinuch Eiampongpaiboon

    Denture stomatitis is a prevalent oral infection commonly affecting denture wearers with inadequate oral hygiene cares. This susceptibility stems from the porous and rough nature of denture bases, which readily harbor bacteria and promote plaque accumulation. This study aimed to modify the surface of denture bases with a chlorhexidine (CHX) coating to promote antimicrobial activity against Candida albicans. Denture bases were coated with chlorhexidine-loaded poly(ethylene glycol)-block-poly(ε-caprolactone) micelles (CHX-micelles) using the solvent evaporation method. The surface was coated using a layer-by-layer (LbL) dip coating process involving CHX-micelles and poly(acrylic acid) (PAA). The total number of LbL coating cycles was adjusted, and the coating thickness, drug content, CHX-release, antimicrobial activity, and toxicity of the coated denture base were evaluated. One-way ANOVA and Two-way ANOVA were performed. Statistical significance is defined as p < 0.05. The optimized coated denture base, with 90 layers, achieved a maximum coating thickness of 13.33 ± 2.41 μm and a CHX content of 23.64 ± 4.71 µg/cm2. This coating exhibited sustained CHX release over 14 days. Even with a non-polished side, the coated surface displayed a reduced contact angle, which would decrease fungal adhesion. The adherence of C. albicans to the surface was also significantly reduced by the antifungal activity of CHX-micelles coated denture base, and this activity sustained for 14 days. Whereas free CHX decreased cell viability to less than 80% with 50, 75, and 100% of extracted solution, CHX-micelles contributed more than 85% of cell viability, comparable to non-coated denture base. The development of antimicrobial denture bases using this coating method has shown promising results. The optimized coating effectively prolonged CHX release, inhibited fungal growth, and maintained biocompatibility.

  • Open Access

    Anti-microbial effect of Piper betle crude extract and essential oil incorporated into short-term soft lining material

    by Potsawat Poolkerd, Noppavan Nagaviroj, Ratchapin Laovanitch Srisatjaluk, Trinuch Eiampongpaiboon

    Introduction Using soft lining material to treat denture stomatitis for an extended period of time may result in oral bacterial and fungal accumulations. Several additives, including natural products, have been identified as anti- microbial agents. Objectives The aim of the present study...


  • Open Access

    Grain size, crystalline phase and fracture toughness of the monolithic zirconia

    by Kodchakorn Bocam, Chuchai Anunmana, Trinuch Eiampongpaiboon

    Bocam K, et al. J Adv Prosthodont. 2022 Oct;14(5):285-293. https://doi.org/10.4047/jap.2022.14.5.285


  • Open Access

    Effects of Litsea cubeba Essential Oil Incorporated into Denture Soft Lining Materials

    by Nichakorn Songsang, Chuchai Anunmana, Matsayapan Pudla, Trinuch Eiampongpaiboon

    The antimicrobial properties, cell cytotoxicity and surface hardness of soft lining materials (GC soft liner, Viscogel and Coe comfort) incorporated with various concentrations of Litsea cubeba essential oil (LCEO) were evaluated. The minimum inhibitory concentrations of LCEO against Candida albicans and Streptococcus mutans were 1.25% v/v and 10% v/v, respectively. However, when LCEO was incorporated into the three soft lining materials (GC soft liner, Viscogel and Coe comfort), 10% v/v and 30% v/v of LCEO could inhibit the growth of C. albicans and S. mutans, respectively. The extracts of soft lining materials with 10% and 30% v/v LCEO, 2% chlorhexidine, 30% v/v nystatin and no additive were used for cytotoxicity tests on a human gingival fibroblast cell line. There was no significant difference in cell viability in all groups with additives compared to the no additive group (p > 0.05). Surface hardness increased significantly between 2 h and 7 day incubation times in all groups, including the controls (p < 0.05). A higher LCEO concentration had a dose-dependent effect on the surface hardness of all soft lining materials (p < 0.05). However, the surface hardness of materials with additive remained in accordance with ISO 10139-1. LCEO could be used as a natural product against oral pathogens, without having a negative impact on soft lining materials.


  • Open Access

    Influence of zirconia/glass veneer thickness and implant abutment material on the final shade of implant restorations

    by Trinuch Eiampongpaiboon, Manita Woo, Chuchai Anunmana

    Aim: The aim of this study was to investigate the combined effect of ceramic material, ceramic thickness, and implant abutment background to the final color of restorations. Settings and Design: This was a comparative in vitro study. Materials and Methods: Three different types of monolithic and porcelain-veneered zirconia disc-shaped specimens (Prettau Anterior, VITA YZ ST, and VITA YZ HT) were prepared in A3 shade with two different thicknesses (1 mm and 1.5 mm) (n = 10). Each zirconia material was made of 4-mm thickness as a control specimen of each monolithic zirconia type, and 4-mm thick veneering ceramic (VITA VM9 Base Dentine) was made as a control for veneered zirconia groups. Three simulated implant abutments were fabricated from titanium, white-shaded and yellow-shaded zirconia. The zirconia specimens were placed on different abutment backgrounds, and the color difference (ΔE) between experimental and control specimens was measured. Statistical Analysis Used: The three-way ANOVA and the Scheffé test were used for data analysis (α = 0.05). Results: The mean ΔE values between two thicknesses were significantly different in every background for all zirconia materials. The ΔE values of zirconia specimens on yellow zirconia were lower than those of other abutments. The clinically acceptable ΔE value (ΔE <3) was found in some monolithic zirconia specimens on white-shaded and yellow-shaded abutments, while the ΔE value is approximately 3 or less in all 1.5-mm thick porcelain-veneered zirconia groups. Conclusions: Different zirconia materials on implant abutments affected the final color of restorations. To achieve satisfactory color, the minimum thickness of zirconia restorations should be at least 1.5 mm on yellow zirconia abutment.


  • Open Access

    Effect of Various Retentive Element Materials on Retention of Mandibular Implant-Retained Overdentures

    by Atitiya Chindarungruangrat, Trinuch Eiampongpaiboon, Bundhit Jirajariyavej

    This study aimed to examine the retentive characteristics of each retentive element material and the effects from thermocycling using the two implant-retained mandibular overdenture model. Two stud abutments and three retentive element materials; nylon, polyetheretherketone (PEEK) and polyvinylsiloxane (PVS) were used in this study. Four tested groups, with a total of 40 overdentures, were fabricated, including a Locator® abutment with nylon retention insert (NY), Novaloc® abutment with PEEK retention insert (PK), Locator® abutment with PVS retention insert (RL), and Novaloc® abutment with PVS retention insert (RN). The retentive force (N) was measured before thermocycling, and at 2500, 5000, and 10,000 cycles after thermocycling. Significant changes in the percentage of retention loss were found in the NY and PK groups (p < 0.05) at 6 and 12 months for the RL group (p < 0.05) after artificial aging. The RN group exhibited a constant retentive force (p > 0.05). The tendency of the percentage of retention loss significantly increased for PEEK, nylon, and PVS silicone over time. The results of the present study implied that retentive element materials tend to lose their retentive capability as a result of thermal undulation and water dispersion. Nylon and PEEK, comprising strong polar groups in polymer chains, showed a higher rate of retention loss than polyvinylsiloxane.


  • Effect of Piper betle extract on anti-candidal activity, gelation time, and surface hardness of a short-term soft lining material

    by Juthatip Kumpanich, Trinuch Eiampongpaiboon, Widchaya Kanchanavasita, Somsak Chitmongkolsuk, Jindaporn Puripattanavong

    The purpose of this study was to evaluate anti-candidal activity, gelation time, and surface hardness of a short-term soft lining material incorporated with varying concentrations of Piper betle extract (0.25 to 20% w/w). Agar-diffusion assay was conducted to evaluate an inhibitory effect against Candida albicans. The gelation time was assessed and surface hardness was measured at 2 h and 7 days by Shore AO durometer. A soft liner containing at least 5% w/w of P. betle extract was observed the inhibitory effect against C. albicans. An increasing of P. betle concentrations provided larger inhibition zone. Incorporating 5% w/w of P. betle extract into the soft liner did not significantly alter its gelation time and surface hardness (ANOVA; p>0.05). The optimum composition at 5% w/w of P. betle extract can be used as an additive in the soft liner to provide the anti-candidal activity without significantly affect these two main properties.