MPManuela Cristina Perju

Manuela Cristina Perju

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Manuela Cristina Perju has a total of 9 co-authors. Here are the top co-authors by number of shared publications:

  • Carmen Nejneru

    Faculty of Materials Science and Engineering, Gheorghe Asachi Technical University, 700050 Iasi, Romania

    2 shared publications
  • Costica Bejinariu

    Faculty of Materials Science and Engineering, “Gheorghe Asachi” Technical University of Iasi, 41 Dimitrie Mangeron Blvd., 700050 Iasi, Romania

    2 shared publications
  • Diana-Petronela Burduhos-Nergis

    Department of Materials Engineering and Industrial Safety, Faculty of Materials Science and Engineering, Gheorghe Asachi Technical University of Iasi, 700050 Iasi, Romania

    2 shared publications
  • Mihai Axinte

    Faculty of Materials Science, “Gheorghe Asachi” Technical University of Iași, Blvd. Dimitrie Mangeron 71A, 700050 Iasi, Romania

    2 shared publications
  • Carmen Nejneru

    “Gheorghe Asachi” Technical University of Iași, Faculty of Materials Science and Engineering, Iași, Romania; “Gheorghe Asachi” Technical University of Iași, Faculty of Chemical Engineering and Environmental Protection, Iași, Romania; Academy of Romanian Scientists, Bucharest, Romania

    1 shared publication
  • Elena-Luiza Epure

    “Gheorghe Asachi” Technical University of Iassy, “Cristofor Simionescu” Faculty of Chemical Engineering and Environmental Protection, 700050 Iasi, Prof. Dr. docent D. Mangeron Blvd., Romania

    1 shared publication

Latest Publications

  • Open Access

    Study on the Thermal Fatigue Effect of Carboxymethylcellulose Solution Media Dissolved in Water as a Quenching Cooling Medium

    by Carmen Nejneru, Ramona Cimpoesu, Petrica Vizureanu, Elena-Luiza Epure, Manuela Cristina Perju, Ștefan-Constantin Lupescu

    The degradation of a quenching cooling medium is a particularly important technical aspect in the technology of primary and final thermal treatments. This paper studied the effect of the thermal cycles of heating and cooling on a tempering medium type of 2.5% carboxymethyl cellulose solution in water. The main characteristic of a cooling medium is the absorption of heat from the part, which is influenced by the physico-chemical characteristics of the cooling liquid according to the degree of thermal fatigue. For this, the main properties of the environment are analyzed, such the chemical composition, corrosion capacity, wetting capacity and cooling characteristics. To analyze the change in properties during the operation, we studied the effect of thermal cycles on the physico-chemical characteristics of the quenching medium to determine the optimal period when the quenching medium could function in good parameters without the necessary corrections. For this purpose, cyclic and linear corrosion tests, FTIR compositional analyses and contact angle measurements were conducted.


  • Open Access

    Analysis of the Physical-Mechanical Properties of the Zinc Phosphate Layer Deposited on a Nodular Cast Iron Substrate

    by Carmen Nejneru, Diana-Petronela Burduhos-Nergis, Mihai Axinte, Manuela Cristina Perju, Costica Bejinariu

    The rotors of submersible wastewater pumps, generally made of nodular graphite cast iron, are subjected to complex processes of corrosive erosion during operation. To improve the characteristics of erosion resistance by impact with solid particles in the corrosive environment of wastewater, cast iron was subjected to a chemical phosphating treatment. In the paper, the scratch test behaviour of nodular cast iron and phosphate nodular cast iron is analysed comparatively, studying the behaviour of the deposited layer and its adhesion to the substrate. The nanoindentation characteristics of nodular cast iron and phosphate nodular cast iron were also studied. It was observed that the deposited layer is not compact, but when pressed, it does not crack and does not detach from the substrate; it is impregnated in the substrate in the metal matrix, but not on the area with carbon nodules. The SEM micrographs show that the deposited phosphate layer is relatively porous and can change the behaviour of the liquid flow moving on the surface of the rotor due to its hydrophilic behaviour; this also allows the formation of a boundary layer that adheres to the surface of the rotor and protects it from the impacts of microparticles driven by the liquid stream.


  • Open Access

    Corrosion Behaviour of Nodular Cast Iron Used for Rotor Manufacturing in Different Wastewaters

    by Carmen Nejneru, Diana-Petronela Burduhos-Nergis, Mihai Axinte, Manuela Cristina Perju, Costica Bejinariu

    Submersible drainage sump pumps work in a highly corrosive environment, forming films with corrosive reaction products on the surface. Pump rotors are high-demand parts, so they are made of quality materials with good wear and corrosion resistance properties such as nodular graphite cast iron. This paper analyses the corrosion behaviour of cast iron used in the manufacture of rotors in three types of wastewaters, with variable pH. Nodular graphite cast iron samples were immersed in wastewater for 30, 60, and 90 days and tested by linear polarisation and electrochemical impedance spectroscopy (EIS). Also, the layers of reaction products formed on the surface of the material were analysed by SEM and EDS. The results showed that nodular cast-iron immersed in wastewater with acidic pH showed intense corrosion, the oxide layer formed on its surface is unstable. Also, the final structure of the product layer is that of a tri-layer with cations and anions absorbed from the corrosion media: the double-electric layer directly connected to the metal surface, an internal layer consisting of ferrous compounds and ferric compounds that control the diffusion of oxygen, an outer layer, and a compact crust of ferric compounds. The change in the pH of the wastewater has a major influence on the corrosion rate of the cast iron, which increases from 356.4 µm/year in DWW-1 (6.5 pH) to 1440 µm/year in DWW-2 (3 pH) and 1743 µm/year DWWW-3 (11 pH) respectively. As can be seen, the experimental study covers the problem of the corrosion behaviour of the pump rotor in various types of wastewaters this aspect is particularly important for the good use of wastewater pumps and to predict possible deviations for the operation of the equipment within the treatment plants.