Latest Publications

  • Open Access

    Analysis of the Performances and Optimization of Polyurethane Concrete with a Large Percentage of Fly Ash

    by Tingting Huo, Jiaquan Xue, Zhi’aN Fu

    The properties of polyurethane concrete containing a large amount of fly ash are investigated, and accordingly, a model is introduced to account for the influence of fly ash fineness, water ratio, and loss of ignition (LOI) on its mechanical performances. This research shows that, after optimization, the concrete has a compressive strength of 20.8 MPa, a flexural strength of 3.4 MPa, and a compressive modulus of elasticity of 19.2 GPa. The main factor influencing 28 and 90 d compressive strength is fly ash content, water-binder ratio, and early strength agent content.

  • Open Access

    Comparison between the Influence of Finely Ground Phosphorous Slag and Fly Ash on Frost Resistance, Pore Structures and Fractal Features of Hydraulic Concrete

    by Lei Wang, Yajun Huang, Feng Zhao, Tingting Huo, E Chen, Shengwen Tang

    Hydraulic concrete in cold regions is necessary for good frost resistance. The utilization of finely ground PS (FGPS) in the construction of hydropower projects could solve the pollution issue and the fly ash shortage problem. In this work, the influence of FGPS and fly ash on frost resistance, pore structure and fractal features of hydraulic concretes was investigated and compared. The main results are: (1) The inclusion of 15–45% FGPS reduced the compressive strength of plain cement concretes by about 21–52%, 7–23% and 0.4–8.2% at 3, 28 and 180 days, respectively. (2) The inclusion of FGPS less than 30% contributed to the enhancement of 180-day frost resistance. At the same dosage level, the FGPS concrete presented larger compressive strengths and better frost resistance than fly ash concrete at 28 and 180 days. (3) At 3 days, both the addition of FGPS and fly ash coarsened the pore structures. FGPS has a much stronger pore refinement effect than fly ash at 28 and 180 days. The correlation between frost resistance of hydraulic concrete and pore structure is weak. (4) At 28 days, the incorporation of FGPS and fly ash weakened the air void structure of hydraulic concrete. At 180 days, the presence of FGPS and fly ash was beneficial for refining the air void structure. The optimal dosage for FGPS and fly ash in terms of 180-day air void refinement was 30% and 15%, respectively. The frost resistance of hydraulic concretes is closely correlated with the air void structure. (5) The pore surface fractal dimension (Ds) could characterize and evaluate the pore structure of hydraulic concretes, but it was poorly correlated with the frost resistance.


  • Open Access

    The Influence of Fly Ash Dosages on the Permeability, Pore Structure and Fractal Features of Face Slab Concrete

    by Lei Wang, Shihua Zhou, Yan Shi, Yajun Huang, Feng Zhao, Tingting Huo, Shengwen Tang

    Concrete-face slabs are the primary anti-permeability structures of the concrete-face rockfill dam (CFRD), and the resistance of face slab concrete to permeability is the key factor affecting the operation and safety of CFRDs. Herein, the influences of five fly ash dosages (namely 10%, 20%, 30%, 40% and 50%) on the permeability property of face slab concretes were investigated. Moreover, the difference in the permeability caused by the fly ash dosage variations is revealed in terms of the pore structure and fractal theory. The results illustrate that: (1) The inclusion of 10–50% fly ash lowered the compressive strength of face slab concretes before 28 days of hydration, whereas it contributed to the 180-day strength increment. (2) The incorporation of 10–50% fly ash raised the average water-seepage height (Dm) and the relative permeability coefficient (Kr) of the face slab concrete by about 14–81% and 30–226% at 28 days, respectively. At 180 days, the addition of fly ash improved the 180-day impermeability by less than 30%. (3) The permeability of face slab concretes is closely correlated with their pore structures and Ds. (4) The optimal fly ash dosage in terms of the long-term impermeability and pore refinement of face slab concretes is around 30%. Nevertheless, face slab concretes containing a high dosage of fly ash must be cured for a relatively long period before they can withstand high water pressure.