Bo Zhao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Bo Zhao has a total of 32 co-authors. Here are the top co-authors by number of shared publications:
- Yanxin Chen
College of Materials Science and Engineering, Xi’an University of Architecture and Technology, Xi’an, China
5 shared publications - Shaowu Jiu
School of Materials and Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
4 shared publications - Chang Chen
College of Materials Science and Engineering, Xi’an University of Architecture and Technology, Xi’an, China
2 shared publications - Chao Yang
College of Materials Science and Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
2 shared publications - Feng Cheng
School of Materials and Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
2 shared publications - Hongbo Zhang
School of Materials and Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
2 shared publications
Latest Publications
- Open Access
Self-Sustaining Calcination of Coal Gangue Coupled with Cement Production: An Industrial-Scale Evaluation of Material Performance and Energy Balance
The accumulation of coal gangue has caused environmental issues, including spontaneous combustion, dust emissions, and leaching of hazardous elements. Using coal gangue as a supplementary cementitious material offers a promising approach to solid-waste valorization and carbon emission reduction in the cement industry. In this study, a coupled process integrating coal gangue calcination with cement production was established and validated on an industrial demonstration line with a designed annual output of approximately 100,000 tons of calcined coal gangue. At 800 °C and a feed rate of 20 t/h, the system operated without external fuel and relied solely on the inherent calorific value of coal gangue. Waste heat recovery fully covered the total electricity consumption. Calcination temperature exhibited a nonmonotonic effect on product performance: carbon content decreased with increasing temperature, whereas the strength activity index reached its maximum of 100% at 800 °C. Considering carbon content, strength activity index, and energy consumption, 800–825 °C was identified as the optimal temperature window for the industrial suspension reactor, which differs from static calcination conditions. A thermodynamic boundary equation was established, revealing that calcite content exerted ~3.24 times greater influence on the calorific value threshold than kaolinite. The self-sustaining boundary covered a broad compositional range of 40–98% kaolinite and 0–10% calcite, corresponding to calorific value thresholds of 527–1056 kcal/kg. At a 40% replacement level, the prepared low-carbon cementitious material achieved a 28-day compressive strength of 47.2 MPa, meeting the 42.5-grade cement requirement. Compared with P.O 42.5 cement, the clinker content was reduced by ~29 percentage points; this corresponded to an energy saving of 23.35 kgce/t, an energy saving rate of 27.8%, and a carbon emission reduction of 9.9%. The main novelty lies in the industrial-scale process integration, on-site energy balance, self-sustaining operating boundary, and validated material performance. This coupled process provides a viable technical pathway for the low-carbon utilization of coal gangue in the cement industry.
Open AccessSelf-Sustaining Calcination of Coal Gangue Coupled with Cement Production: An Industrial-Scale Evaluation of Material Performance and Energy Balance
The accumulation of coal gangue has caused environmental issues, including spontaneous combustion, dust emissions, and leaching of hazardous elements. Using coal gangue as a supplementary cementitious material offers a promising approach to solid-waste valorization and carbon emission reduction in the cement industry. In this study, a coupled process integrating coal gangue calcination with cement production was established and validated on an industrial demonstration line with a designed annual output of approximately 100,000 tons of calcined coal gangue. At 800 °C and a feed rate of 20 t/h, the system operated without external fuel and relied solely on the inherent calorific value of coal gangue. Waste heat recovery fully covered the total electricity consumption. Calcination temperature exhibited a nonmonotonic effect on product performance: carbon content decreased with increasing temperature, whereas the strength activity index reached its maximum of 100% at 800 °C. Considering carbon content, strength activity index, and energy consumption, 800–825 °C was identified as the optimal temperature window for the industrial suspension reactor, which differs from static calcination conditions. A thermodynamic boundary equation was established, revealing that calcite content exerted ~3.24 times greater influence on the calorific value threshold than kaolinite. The self-sustaining boundary covered a broad compositional range of 40–98% kaolinite and 0–10% calcite, corresponding to calorific value thresholds of 527–1056 kcal/kg. At a 40% replacement level, the prepared low-carbon cementitious material achieved a 28-day compressive strength of 47.2 MPa, meeting the 42.5-grade cement requirement. Compared with P.O 42.5 cement, the clinker content was reduced by ~29 percentage points; this corresponded to an energy saving of 23.35 kgce/t, an energy saving rate of 27.8%, and a carbon emission reduction of 9.9%. The main novelty lies in the industrial-scale process integration, on-site energy balance, self-sustaining operating boundary, and validated material performance. This coupled process provides a viable technical pathway for the low-carbon utilization of coal gangue in the cement industry.
- Open Access
Numerical Simulation of a Novel Secondary Separation Cyclone
The low separation efficiency of conventional cyclone separators for sub-10 μm particles remains a critical challenge in Na2S production processes. Previous optimization attempts have failed to reconcile economic feasibility with effective fine particle capture requirements. To address this industrial bottleneck, we propose an innovative secondary separation cyclone design tailored for next-generation Na2S manufacturing systems. Our methodology synergizes computational fluid dynamics (CFD) simulations with experimental validation, achieving cost-effective development while ensuring numerical model reliability. Comparative analyses reveal significant improvements: under varying gas velocities, the novel design demonstrates 5.67–9.77% and 7.03–10.14% enhancements in 1–10 μm particle collection efficiency compared to standard and volute-type cyclones, respectively. Mechanistic investigations through flow field characterization elucidate the relationship between vortex dynamics and separation performance. This work provides a structurally optimized cyclone configuration with industrial applicability, as well as a validated hybrid experimental–computational framework that could inform solutions for fine particle separation across chemical processing industries.
Open AccessNumerical Simulation of a Novel Secondary Separation Cyclone
The low separation efficiency of conventional cyclone separators for sub-10 μm particles remains a critical challenge in Na2S production processes. Previous optimization attempts have failed to reconcile economic feasibility with effective fine particle capture requirements. To address this industrial bottleneck, we propose an innovative secondary separation cyclone design tailored for next-generation Na2S manufacturing systems. Our methodology synergizes computational fluid dynamics (CFD) simulations with experimental validation, achieving cost-effective development while ensuring numerical model reliability. Comparative analyses reveal significant improvements: under varying gas velocities, the novel design demonstrates 5.67–9.77% and 7.03–10.14% enhancements in 1–10 μm particle collection efficiency compared to standard and volute-type cyclones, respectively. Mechanistic investigations through flow field characterization elucidate the relationship between vortex dynamics and separation performance. This work provides a structurally optimized cyclone configuration with industrial applicability, as well as a validated hybrid experimental–computational framework that could inform solutions for fine particle separation across chemical processing industries.
- Open Access
Characteristics of Solid Mineral Phase Transitions During Sulfuric Acid Production from Gaseous-Sulphur-Reduced Gypsum
The acid co-production of cement is a prominent research focus for the large-scale, high-value utilization of phosphogypsum in the context of dual-carbon strategies. This paper builds on extensive research conducted by its authors on the co-production of sulphoaluminate cement clinker through acid production from gaseous-sulphur-reduced phosphogypsum. The solid mineral phase transformations occurring in the kiln during this process are systematically studied, and the effects of various calcination regimes (temperature, time, and atmosphere) on the evolution of clinker mineral phases are elucidated. This paper provides basic data support for the gas-sulfur-reduced phosphogypsum-acid cogeneration of sulfoaluminate cement clinker processes, and promotes the realization of the large-scale high-value utilization of phosphogypsum resources. The generation of the clinker mineral phase anhydrous calcium sulphoaluminate (C4A3S̅) begins at 1100 °C. Increasing the calcination temperature and extending the calcination time promote C4A3S̅ formation. However, when the calcination temperature exceeds 1350 °C, C4A3S̅ decomposes, leading to the formation of low-activity C2AS. In a CO atmosphere, the main mineral phases in the clinker transform into C2AS and 12CaO·7Al2O3, owing to the decomposition of CaSO4, which inhibits C4A3S̅ formation. At calcination temperatures exceeding 1300 °C, a significant amount of C2AS appears in the calcined material, and 12CaO·7Al2O3 begins to form.
Open AccessCharacteristics of Solid Mineral Phase Transitions During Sulfuric Acid Production from Gaseous-Sulphur-Reduced Gypsum
The acid co-production of cement is a prominent research focus for the large-scale, high-value utilization of phosphogypsum in the context of dual-carbon strategies. This paper builds on extensive research conducted by its authors on the co-production of sulphoaluminate cement clinker through acid production from gaseous-sulphur-reduced phosphogypsum. The solid mineral phase transformations occurring in the kiln during this process are systematically studied, and the effects of various calcination regimes (temperature, time, and atmosphere) on the evolution of clinker mineral phases are elucidated. This paper provides basic data support for the gas-sulfur-reduced phosphogypsum-acid cogeneration of sulfoaluminate cement clinker processes, and promotes the realization of the large-scale high-value utilization of phosphogypsum resources. The generation of the clinker mineral phase anhydrous calcium sulphoaluminate (C4A3S̅) begins at 1100 °C. Increasing the calcination temperature and extending the calcination time promote C4A3S̅ formation. However, when the calcination temperature exceeds 1350 °C, C4A3S̅ decomposes, leading to the formation of low-activity C2AS. In a CO atmosphere, the main mineral phases in the clinker transform into C2AS and 12CaO·7Al2O3, owing to the decomposition of CaSO4, which inhibits C4A3S̅ formation. At calcination temperatures exceeding 1300 °C, a significant amount of C2AS appears in the calcined material, and 12CaO·7Al2O3 begins to form.
- Open Access
H2 Reduction of Na2SO4 to Na2S Based on Dilute-Phase Fluidization
Sodium sulfate (Na2SO4) is used in the ecofriendly production of sodium sulfide (Na2S) through H2 reduction, thereby facilitating the valorization of Na2SO4. However, studies on this technique remain at the laboratory stage. This paper proposes a novel process involving the external circulation of Na2S in a dilute-phase fluidized system to address the low-temperature eutectic formation between Na2S and Na2SO4 during the H2 reduction of Na2SO4 to Na2S. The process aims to increase the reaction temperature of the Na2SO4 while reducing the volume of the liquid phase formed to prevent sintering blockages and enhance the reduction rate. In a proprietary experimental setup, the H2 reduction process in a dilute-phase fluidized system was investigated. The Na2S/Na2SO4 ratio and reaction temperature were determined to be critical factors influencing the Na2SO4 reduction rate. The melting point of the system increased and the amount of liquid phase produced decreased as the Na2S content was increased to more than 60%. The Na2S–Na2SO4 mixture (mass ratio of 80:20) existed as a solid at the reaction temperature of 740 °C. After roasting for 10 s, the Na2SO4 reduction rate reached 93.7% and the Na2S content in the mixture increased to 98.74%.
Open AccessH2 Reduction of Na2SO4 to Na2S Based on Dilute-Phase Fluidization
Sodium sulfate (Na2SO4) is used in the ecofriendly production of sodium sulfide (Na2S) through H2 reduction, thereby facilitating the valorization of Na2SO4. However, studies on this technique remain at the laboratory stage. This paper proposes a novel process involving the external circulation of Na2S in a dilute-phase fluidized system to address the low-temperature eutectic formation between Na2S and Na2SO4 during the H2 reduction of Na2SO4 to Na2S. The process aims to increase the reaction temperature of the Na2SO4 while reducing the volume of the liquid phase formed to prevent sintering blockages and enhance the reduction rate. In a proprietary experimental setup, the H2 reduction process in a dilute-phase fluidized system was investigated. The Na2S/Na2SO4 ratio and reaction temperature were determined to be critical factors influencing the Na2SO4 reduction rate. The melting point of the system increased and the amount of liquid phase produced decreased as the Na2S content was increased to more than 60%. The Na2S–Na2SO4 mixture (mass ratio of 80:20) existed as a solid at the reaction temperature of 740 °C. After roasting for 10 s, the Na2SO4 reduction rate reached 93.7% and the Na2S content in the mixture increased to 98.74%.
- Open Access
Activation of Low-Quality Coal Gangue Using Suspension Calcination for the Preparation of High-Performance Low-Carbon Cementitious Materials: A Pilot Study
Although the calcination-based activation of coal gangue is important for its valorization in the form of cementitious materials, the related works mainly focus on high-quality coal gangue, neglecting its low-quality counterpart. To bridge this gap, we herein conducted the pilot-scale suspension calcination of low-quality coal gangue; explored the effects of calcination temperature, particle size, and O2 content on the phase composition of the calcined product, kaolinite decomposition, decarbonization, and silica/alumina dissolution; and evaluated calcination-product-based cementitious materials. Under optimal conditions (temperature = 875–900 °C; particle size = 39.71–46.84 μm; and O2 content = 12–14%), the carbon content of the calcined product equaled 1.24–1.87 wt%, and the dissolution rates of activated alumina and silica were 77.6–79.5% and 49.4–51.1%, respectively. The 28 d compressive strength (50.8–55.7 MPa) and true activity index (98.8–108.4%) of the cementitious material prepared at a calcination product dosage of 30–38 wt% met the standard of 42.5 grade cement. This study demonstrated the suitability of suspension calcination for the preparation of high-performance low-carbon cementitious materials from low-quality coal gangue, thus providing a basis for further industrialization and technological development.
Open AccessActivation of Low-Quality Coal Gangue Using Suspension Calcination for the Preparation of High-Performance Low-Carbon Cementitious Materials: A Pilot Study
Although the calcination-based activation of coal gangue is important for its valorization in the form of cementitious materials, the related works mainly focus on high-quality coal gangue, neglecting its low-quality counterpart. To bridge this gap, we herein conducted the pilot-scale suspension calcination of low-quality coal gangue; explored the effects of calcination temperature, particle size, and O2 content on the phase composition of the calcined product, kaolinite decomposition, decarbonization, and silica/alumina dissolution; and evaluated calcination-product-based cementitious materials. Under optimal conditions (temperature = 875–900 °C; particle size = 39.71–46.84 μm; and O2 content = 12–14%), the carbon content of the calcined product equaled 1.24–1.87 wt%, and the dissolution rates of activated alumina and silica were 77.6–79.5% and 49.4–51.1%, respectively. The 28 d compressive strength (50.8–55.7 MPa) and true activity index (98.8–108.4%) of the cementitious material prepared at a calcination product dosage of 30–38 wt% met the standard of 42.5 grade cement. This study demonstrated the suitability of suspension calcination for the preparation of high-performance low-carbon cementitious materials from low-quality coal gangue, thus providing a basis for further industrialization and technological development.
- Open Access
Pilot Study on a New Conveyor Bed Magnetization Roasting Process for Efficient Iron Extraction from Low-Grade Siderite
Realizing the large-scale development and utilization of siderite, a difficult iron ore reserve, has great practical significance in ensuring the supply of iron ore resources. Therefore, a new in-house conveyor bed magnetization roasting–dry cooling process was pilot-tested using low-grade siderite from the Daxigou iron ore mine. A two-stage weak magnetic separation method was used for a beneficiation test to investigate the influence of temperature and CO content on the magnetization of siderite. At 600 °C and 800 °C under suspension, iron minerals were converted into magnetite with an effective 3–5 s residence time. Furthermore, at 600 °C and 750 °C, increasing the calcination temperature increased the iron grade and the concentrate recovery rate. However, calcination at temperatures >750 °C resulted in a slight decrease in the iron grade and recovery rate of the concentrate. 61.50% Fe grade and 80.30% concentrate recovery rate were obtained under 750 °C from magnetization roasting. Magnetization roasting in a reducing atmosphere provides mainly magnetite as the roasted ore, and increased CO content can efficiently promote this effect. At 700–780 °C and when the CO content was increased to more than 3 wt.%, the improvement of the roasting effect was very limited. Rapid cooling of the roasted ore using a mixture of circulating exhaust gas and air could prevent considerable oxidation of the magnetic ferrous material. Therefore, the preferred process conditions are 700–780 °C with a CO content range of 1–3%. It provided a concentrate iron grade of 59.27–61.50% and a recovery rate of 78.32–80.30%. The results of this study provide a reference for the development of conveyor bed magnetization technology, process design, and production control.
Open AccessPilot Study on a New Conveyor Bed Magnetization Roasting Process for Efficient Iron Extraction from Low-Grade Siderite
Realizing the large-scale development and utilization of siderite, a difficult iron ore reserve, has great practical significance in ensuring the supply of iron ore resources. Therefore, a new in-house conveyor bed magnetization roasting–dry cooling process was pilot-tested using low-grade siderite from the Daxigou iron ore mine. A two-stage weak magnetic separation method was used for a beneficiation test to investigate the influence of temperature and CO content on the magnetization of siderite. At 600 °C and 800 °C under suspension, iron minerals were converted into magnetite with an effective 3–5 s residence time. Furthermore, at 600 °C and 750 °C, increasing the calcination temperature increased the iron grade and the concentrate recovery rate. However, calcination at temperatures >750 °C resulted in a slight decrease in the iron grade and recovery rate of the concentrate. 61.50% Fe grade and 80.30% concentrate recovery rate were obtained under 750 °C from magnetization roasting. Magnetization roasting in a reducing atmosphere provides mainly magnetite as the roasted ore, and increased CO content can efficiently promote this effect. At 700–780 °C and when the CO content was increased to more than 3 wt.%, the improvement of the roasting effect was very limited. Rapid cooling of the roasted ore using a mixture of circulating exhaust gas and air could prevent considerable oxidation of the magnetic ferrous material. Therefore, the preferred process conditions are 700–780 °C with a CO content range of 1–3%. It provided a concentrate iron grade of 59.27–61.50% and a recovery rate of 78.32–80.30%. The results of this study provide a reference for the development of conveyor bed magnetization technology, process design, and production control.
- Open Access
High-Efficiency Iron Extraction from Low-Grade Siderite via a Conveyor Bed Magnetization Roasting–Magnetic Separation Process: Kinetics Research and Applications
Upgrading and utilizing low-grade iron ore is of great practical importance to improve the strategic security of the iron ore resource supply. In this study, a thermal analysis–infrared (IR) analysis–in-situ IR method was used to investigate the reaction mechanism and kinetics of Daxigou siderite. Experiments were conducted using a conveyor bed magnetization roasting process (CBMRP) to investigate the magnetization of siderite. Multi-stage magnetic separation processes were adopted to extract magnetite. The results show that simultaneously the iron carbonate in siderite decomposes, and magnetite is formed between 364 °C and 590 °C under both inert and reducing atmospheres. The activation energy of the magnetization roasting reaction is 106.1 kJ/mol, consistent with a random nucleation and growth reaction mechanism. Magnetization roasting at 750–780 °C for approximately 3.5 s in the CBMRP results in a magnetic conversion rate of >0.99 of the iron minerals in the siderite. A beneficiation process of one roughing, one sweeping, and three cleaning processes was adopted. A dissociation particle size of −400 mesh accounting for 94.78%, a concentrate iron grade of 62.8 wt.%, and a recovery of 68.83% can be obtained. Overall, a theoretical and experimental basis is presented for the comprehensive utilization of low-grade siderite.
Open AccessHigh-Efficiency Iron Extraction from Low-Grade Siderite via a Conveyor Bed Magnetization Roasting–Magnetic Separation Process: Kinetics Research and Applications
Upgrading and utilizing low-grade iron ore is of great practical importance to improve the strategic security of the iron ore resource supply. In this study, a thermal analysis–infrared (IR) analysis–in-situ IR method was used to investigate the reaction mechanism and kinetics of Daxigou siderite. Experiments were conducted using a conveyor bed magnetization roasting process (CBMRP) to investigate the magnetization of siderite. Multi-stage magnetic separation processes were adopted to extract magnetite. The results show that simultaneously the iron carbonate in siderite decomposes, and magnetite is formed between 364 °C and 590 °C under both inert and reducing atmospheres. The activation energy of the magnetization roasting reaction is 106.1 kJ/mol, consistent with a random nucleation and growth reaction mechanism. Magnetization roasting at 750–780 °C for approximately 3.5 s in the CBMRP results in a magnetic conversion rate of >0.99 of the iron minerals in the siderite. A beneficiation process of one roughing, one sweeping, and three cleaning processes was adopted. A dissociation particle size of −400 mesh accounting for 94.78%, a concentrate iron grade of 62.8 wt.%, and a recovery of 68.83% can be obtained. Overall, a theoretical and experimental basis is presented for the comprehensive utilization of low-grade siderite.