Xiuyuan He
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Xiuyuan He has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Wen Liu
Department of Electrical and Electronic Engineering, School of Advanced Technology, Xian Jiaotong-Liverpool University, Suzhou, China
2 shared publications Yinchao Zhao
School of Chips, Entrepreneur College (Taicang), Xian Jiaotong-Liverpool University, Suzhou, China
2 shared publications- Yuanlei Zhang
Department of Electrical and Electronic Engineering, School of Advanced Technology, Xian Jiaotong-Liverpool University, Suzhou, China
2 shared publications - Huiqing Wen
Xian Jiaotong-Liverpool University, Suzhou, China
1 shared publication Jingqun Zhang
School of Advanced Technology, Xian Jiaotong-Liverpool University, Suzhou, China
1 shared publication- Joseph D. Yan
University of Liverpool
1 shared publication
Latest Publications
- 14 March 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 71 (5) , 2914-2919
Dynamic RON Degradation in AlGaN/GaNMIS-HEMTs With Si3N4 or Si3N4/ZrO2Passivation Layer
The dynamic ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation in AlGaN/GaN metal-insulator-semiconductor high electron mobility transistors (MIS-HEMTs) with different passivation layers (SiSi3N4 or Si3N4/ZrO2 stack) under off-, semi-on, and ON-state stress have been investigated in this work. Under the OFF-state stress of 40 V, a 20% reduction in the maximum drain current has been observed in devices passivated with Si{3}N{4}, along with a degraded ${R}_{ \mathrm{\scriptscriptstyle ON}}$ that is 1.42 times higher than the initial ${R}_{ \mathrm{\scriptscriptstyle ON}}$ . In contrast, devices passivated with Si3N4 or Si3N4/ZrO2 stack have only shown a 2% reduction, and the ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation is only 1.03 times higher than the initial ${R}_{ \mathrm{\scriptscriptstyle ON}}$ . This can be attributed to the different interface states present in the two devices. According to the multifrequency $\vphantom {_{\int _{\text {a}}}}~{C}$ – ${V}$ curves, the Si3N4/GaN-cap interface trap density is in the range of $2\times 10^{{13}}$ – $5.5\times 10^{{13}}$ from ${E}_{C}-{0.47}$ to ${E}_{C}-{0.37}$ eV, and ZrO2/GaN-cap interface trap density is in the range of $2.7\times 10^{{12}}$ – $1.2\times 10^{{13}}$ from ${E}_{C}-{0.47}$ to ${E}_{C}-{0.31}$ eV. Under the semi-on state stress, the dynamic ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation exhibits a “bell-shaped” behavior in the Si3N4 or Si3N4/ZrO2 stack passivated sample. Arrenhius plots indicate that the sample passivated by Si3N4 has an activation energy of 0.06 eV, while the sample passivated by Si3N4 or Si3N4/ZrO2 stack has an activation energy of 0.16 eV, which means a deeper trap distribution. The ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation under semi-on/ ON-state stress in Si3N4 or Si3N4/ZrO2 passivated devices can be attributed to the hot-electron-related injection mechanism. Device designers must consider the trade-off between the high breakdown voltage (BV) and the ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation in Si3N4 or Si3N4/ZrO2 passivated devices.
- 14 March 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 71 (5) , 2914-2919
Dynamic RON Degradation in AlGaN/GaNMIS-HEMTs With Si3N4 or Si3N4/ZrO2Passivation Layer
The dynamic ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation in AlGaN/GaN metal-insulator-semiconductor high electron mobility transistors (MIS-HEMTs) with different passivation layers (SiSi3N4 or Si3N4/ZrO2 stack) under off-, semi-on, and ON-state stress have been investigated in this work. Under the OFF-state stress of 40 V, a 20% reduction in the maximum drain current has been observed in devices passivated with Si{3}N{4}, along with a degraded ${R}_{ \mathrm{\scriptscriptstyle ON}}$ that is 1.42 times higher than the initial ${R}_{ \mathrm{\scriptscriptstyle ON}}$ . In contrast, devices passivated with Si3N4 or Si3N4/ZrO2 stack have only shown a 2% reduction, and the ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation is only 1.03 times higher than the initial ${R}_{ \mathrm{\scriptscriptstyle ON}}$ . This can be attributed to the different interface states present in the two devices. According to the multifrequency $\vphantom {_{\int _{\text {a}}}}~{C}$ – ${V}$ curves, the Si3N4/GaN-cap interface trap density is in the range of $2\times 10^{{13}}$ – $5.5\times 10^{{13}}$ from ${E}_{C}-{0.47}$ to ${E}_{C}-{0.37}$ eV, and ZrO2/GaN-cap interface trap density is in the range of $2.7\times 10^{{12}}$ – $1.2\times 10^{{13}}$ from ${E}_{C}-{0.47}$ to ${E}_{C}-{0.31}$ eV. Under the semi-on state stress, the dynamic ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation exhibits a “bell-shaped” behavior in the Si3N4 or Si3N4/ZrO2 stack passivated sample. Arrenhius plots indicate that the sample passivated by Si3N4 has an activation energy of 0.06 eV, while the sample passivated by Si3N4 or Si3N4/ZrO2 stack has an activation energy of 0.16 eV, which means a deeper trap distribution. The ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation under semi-on/ ON-state stress in Si3N4 or Si3N4/ZrO2 passivated devices can be attributed to the hot-electron-related injection mechanism. Device designers must consider the trade-off between the high breakdown voltage (BV) and the ${R}_{ \mathrm{\scriptscriptstyle ON}}$ degradation in Si3N4 or Si3N4/ZrO2 passivated devices.
- Open Access
- 10 October 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of the Electron Devices Society
- Vol. 10, 920-926
Characterization of Oxide Trapping in SiC MOSFETs Under Positive Gate Bias
SiC MOSFETs devices with double-trench dominate the market due to their low on-resistance. However, studies on its temperature-dependent properties are not comprehensive. This work uses fast I-V and static I-V techniques to explore the location of electrons trapped in the device under moderate gate stress. Threshold voltage instability ( ${\mathrm {V}}_{\mathrm {TH}}$ hysteresis and $\Delta{\mathrm {V}}_{\mathrm {TH}}$ ) and on-resistance degradation ( $\Delta{\mathrm {R}}_{\mathrm {ON}}$ ) are used to characterize oxide trapping. Although the observation method is different, it can be found that the ${\mathrm {V}}_{\mathrm {TH}}$ instability and ${\mathrm {R}}_{\mathrm {ON}}$ degradation increase linearly with logarithmic time over a wide time range from $100~\mu{\mathrm {s}}$ to 104 s, suggesting that the direct tunneling mechanism dominates the electrons trapping in the oxide near the SiO2/SiC interface. The interface trap density is $3.8\times 10^{12}$ cm−2 $\cdot$ eV−1. In addition, a negative temperature dependence is shown in the test, and the fitting parameter $\gamma$ from 0.16 to 0.18 indicated that these traps are concentrated in the oxide layer. These traps’ energy level at 0.68 eV below the conduction band was obtained in the recovery phase through the Arrhenius plot.
- 10 October 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of the Electron Devices Society
- Vol. 10, 920-926
Open AccessCharacterization of Oxide Trapping in SiC MOSFETs Under Positive Gate Bias
SiC MOSFETs devices with double-trench dominate the market due to their low on-resistance. However, studies on its temperature-dependent properties are not comprehensive. This work uses fast I-V and static I-V techniques to explore the location of electrons trapped in the device under moderate gate stress. Threshold voltage instability ( ${\mathrm {V}}_{\mathrm {TH}}$ hysteresis and $\Delta{\mathrm {V}}_{\mathrm {TH}}$ ) and on-resistance degradation ( $\Delta{\mathrm {R}}_{\mathrm {ON}}$ ) are used to characterize oxide trapping. Although the observation method is different, it can be found that the ${\mathrm {V}}_{\mathrm {TH}}$ instability and ${\mathrm {R}}_{\mathrm {ON}}$ degradation increase linearly with logarithmic time over a wide time range from $100~\mu{\mathrm {s}}$ to 104 s, suggesting that the direct tunneling mechanism dominates the electrons trapping in the oxide near the SiO2/SiC interface. The interface trap density is $3.8\times 10^{12}$ cm−2 $\cdot$ eV−1. In addition, a negative temperature dependence is shown in the test, and the fitting parameter $\gamma$ from 0.16 to 0.18 indicated that these traps are concentrated in the oxide layer. These traps’ energy level at 0.68 eV below the conduction band was obtained in the recovery phase through the Arrhenius plot.