Shahram Amirifar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shahram Amirifar has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Elham Ahmadi
Department of Restorative Dentistry, Dental School, Tehran University of Medical Sciences, Tehran, Iran
2 shared publications - Elmira Najafrad
Department of restorative Dentistry, School of Dentistry, Tehran University of Medical Sciences, Tehran, Iran
1 shared publication - Fatemeh Farshad
Dental Research Center, Dentistry Research Institute, Tehran University of Medical Sciences (TUMS), Tehran, Iran
1 shared publication - Mahdi Abbasi
Department of Restorative Dentistry, Dental School, Tehran University of Medical Sciences, Tehran, Iran
1 shared publication - Niyousha Rafeie
Dental Research Center, Dentistry Research Institute, School of Dentistry, Tehran University of Medical Sciences, Tehran, Iran
1 shared publication - Saba Tohidkhah
Minnesota Dental Research Center for Biomaterials and Biomechanics, School of Dentistry of University of Minnesota, Minneapolis, Minnesota, USA
1 shared publication
Latest Publications
- Open Access
- 1 January 2025
- Published by Wiley in BioMed Research International
- Vol. 2025 (1) , 1496726
Effect of Universal Adhesive Etching Mode on Shear Bond Strength of Pulp Capping Materials to Deep Dentin
Objective: This study was aimed at investigating the shear bond strength (SBS) of composite to deep dentin with universal adhesive in total‐etch (TE) and self‐etch (SE) mode using different pulp capping materials. Methods: One hundred twelve sound human third molars were divided according to universal adhesives (All‐Bond Universal and G‐Premio Bond), etching modes (TE and SE), and pulp capping materials (TheraCal PT, TheraCal LC, and Lime‐Lite). After sectioning the tooth 2 mm above and 3 mm below the CEJ, the liner, adhesive, and composite were applied. Specimens were tested for SBS using the universal testing machine at a crosshead speed of 1 mm/min after restoring with composite. Data were analyzed with three‐way ANOVA ( α = 0.05). Results: The highest and lowest SBS value was related to G‐Premio bonding adhesive in SE mode using Lime‐Lite (11.91 ± 0.77) and G‐Premio bonding adhesive in SE mode using TheraCal PT (4.48 ± 0.83), respectively. Although the type of adhesive material did not have a significant impact on SBS values ( p = 0.58), the mode of acid etching ( p = 0.001) and the type of liner ( p = 0.001) used were found to have a significant effect. Moreover, TE mode was associated with higher SBS values than SE mode. Conclusions: Using TE mode increased the SBS; in contrast, liners reduced the SBS of the composite to deep dentin. Moreover, other generations of adhesives and comparison with universal bonding should be done in future studies.
- 1 January 2025
- Published by Wiley in BioMed Research International
- Vol. 2025 (1) , 1496726
Open AccessEffect of Universal Adhesive Etching Mode on Shear Bond Strength of Pulp Capping Materials to Deep Dentin
Objective: This study was aimed at investigating the shear bond strength (SBS) of composite to deep dentin with universal adhesive in total‐etch (TE) and self‐etch (SE) mode using different pulp capping materials. Methods: One hundred twelve sound human third molars were divided according to universal adhesives (All‐Bond Universal and G‐Premio Bond), etching modes (TE and SE), and pulp capping materials (TheraCal PT, TheraCal LC, and Lime‐Lite). After sectioning the tooth 2 mm above and 3 mm below the CEJ, the liner, adhesive, and composite were applied. Specimens were tested for SBS using the universal testing machine at a crosshead speed of 1 mm/min after restoring with composite. Data were analyzed with three‐way ANOVA ( α = 0.05). Results: The highest and lowest SBS value was related to G‐Premio bonding adhesive in SE mode using Lime‐Lite (11.91 ± 0.77) and G‐Premio bonding adhesive in SE mode using TheraCal PT (4.48 ± 0.83), respectively. Although the type of adhesive material did not have a significant impact on SBS values ( p = 0.58), the mode of acid etching ( p = 0.001) and the type of liner ( p = 0.001) used were found to have a significant effect. Moreover, TE mode was associated with higher SBS values than SE mode. Conclusions: Using TE mode increased the SBS; in contrast, liners reduced the SBS of the composite to deep dentin. Moreover, other generations of adhesives and comparison with universal bonding should be done in future studies.
- Open Access
- 23 November 2022
- Published by Wiley in International Journal of Dentistry
- Vol. 2022 (1) , 3399120
Combined Minimally Invasive Treatment of Teeth Discoloration Caused by Occupational Exposure to Bronze Alloy
Recently, dental bleaching has been frequently sought by patients to improve the appearance and color of the teeth. Among various treatment options, in‐office bleaching is commonly preferred by patients with severely discolored teeth due to its fast aesthetic results. In addition, other pretreatment methods, such as air‐powder polishing, have been reported to increase the efficacy of bleaching treatment. Compared to other causes of tooth discoloration, occupational tooth discoloration caused by bronze alloy and further treatment have not been sufficiently documented in the literature. In the present case report, we explain a case of tooth discoloration following exposure to a bronze alloy and a conservative clinical approach used for the management of tooth discoloration. A 15‐year‐old male patient who worked in a foundry was presented with tooth discoloration. At the first session, a rubber‐cap prophylaxis was performed. After one week, air‐powder polishing was used to remove the remaining stains. Finally, at the third session, two cycles of bleaching were performed using hydrogen peroxide gel 35%, each for 20 minutes. Photographs were taken at the end of each session and used for visual evaluation. The final result was aesthetically satisfactory.
- 23 November 2022
- Published by Wiley in International Journal of Dentistry
- Vol. 2022 (1) , 3399120
Open AccessCombined Minimally Invasive Treatment of Teeth Discoloration Caused by Occupational Exposure to Bronze Alloy
Recently, dental bleaching has been frequently sought by patients to improve the appearance and color of the teeth. Among various treatment options, in‐office bleaching is commonly preferred by patients with severely discolored teeth due to its fast aesthetic results. In addition, other pretreatment methods, such as air‐powder polishing, have been reported to increase the efficacy of bleaching treatment. Compared to other causes of tooth discoloration, occupational tooth discoloration caused by bronze alloy and further treatment have not been sufficiently documented in the literature. In the present case report, we explain a case of tooth discoloration following exposure to a bronze alloy and a conservative clinical approach used for the management of tooth discoloration. A 15‐year‐old male patient who worked in a foundry was presented with tooth discoloration. At the first session, a rubber‐cap prophylaxis was performed. After one week, air‐powder polishing was used to remove the remaining stains. Finally, at the third session, two cycles of bleaching were performed using hydrogen peroxide gel 35%, each for 20 minutes. Photographs were taken at the end of each session and used for visual evaluation. The final result was aesthetically satisfactory.