Tong Zhao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Interests
Tong Zhao has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
Haimei Gong
Shanghai Institute of Technical Physics , Shanghai , China
3 shared publicationsXue Li
Shanghai Institute of Technical Physics , Shanghai , China
3 shared publications- Defeng Mo
National Key Laboratory of Infrared Detector, Shanghai Institute of Technical Physics, Chinese Academy of Sciences, Shanghai 200083, China
2 shared publications Xinmin Shi
National Key Laboratory of Infrared Detection Technologies Shanghai Institute of Technical Physics Chinese Academy of Sciences Shanghai 200083 China
2 shared publicationsH W Liu
Nanoscale Physics and Devices Laboratory, Institute of Physics,#N#Chinese Academy of Sciences, Beijing 100080, People?s Republic of China
1 shared publication- Hong-Jun Gao
Chinese Academy of Sciences
1 shared publication
Latest Publications
- 11 January 2024
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 66 (2) , 207-214
Interfacial microstructure and mechanical properties of Si3N4/Invar joints using Ag–Cu–In–Ti with Cu foil as an interlayer
Si3N4 and Invar alloy brazed joints were achieved using two types of Ag-based interlayers: a Ag–Cu–In–Ti foil and a Ag–Cu–In–Ti/Cu/Ag–Cu multi-interlayer. The results showed that when only using a single Ag–Cu–In–Ti filler, the wave-shaped Fe2Ti + Ni3Ti intermetallic compounds are concentrated in the middle of the brazing seam. When adding Cu as the interlayer, the dissolution of the Cu interlayer formed a large number of Cu(s,s) blocks of different sizes in the brazing seam, which hindered the concentrated distribution of Fe2Ti + Ni3Ti intermetallic compounds in the brazing seam. As a result, Fe2Ti and Ni3Ti were dispersedly distributed in the brazing seam, increasing the shear strength of the brazed joint. The shear strength of brazed joints was increased by 82 % compared to joints brazed with a single Ag–Cu–In–Ti filler when the Cu interlayer was added.
- 11 January 2024
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 66 (2) , 207-214
Interfacial microstructure and mechanical properties of Si3N4/Invar joints using Ag–Cu–In–Ti with Cu foil as an interlayer
Si3N4 and Invar alloy brazed joints were achieved using two types of Ag-based interlayers: a Ag–Cu–In–Ti foil and a Ag–Cu–In–Ti/Cu/Ag–Cu multi-interlayer. The results showed that when only using a single Ag–Cu–In–Ti filler, the wave-shaped Fe2Ti + Ni3Ti intermetallic compounds are concentrated in the middle of the brazing seam. When adding Cu as the interlayer, the dissolution of the Cu interlayer formed a large number of Cu(s,s) blocks of different sizes in the brazing seam, which hindered the concentrated distribution of Fe2Ti + Ni3Ti intermetallic compounds in the brazing seam. As a result, Fe2Ti and Ni3Ti were dispersedly distributed in the brazing seam, increasing the shear strength of the brazed joint. The shear strength of brazed joints was increased by 82 % compared to joints brazed with a single Ag–Cu–In–Ti filler when the Cu interlayer was added.
- 15 September 2023
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (21)
Microstructure and Mechanical Properties of the Joint between Si3N4 and Mo Brazed by Near‐Eutectic Ag–Cu–In–Ti Filler Alloy
The joining of Si3N4 and Mo using Ag–Cu–In–Ti active filler alloy with the brazing temperature ranging from 720 to 860 °C for 10 min is investigated in this article. The correlation between the joint strength and the microstructures of the brazed joints is discussed. In the results, it is shown that the activity of Ti is different at different temperatures, and thus the degree of diffusion of Ti to the interface is different. The activity of Ti gradually increases as the brazing temperature increases, and more Ti atoms diffuse into both sides of the base materials, resulting in a progressively thicker TiN + Ti5Si3 reaction layer on the Si3N4 ceramic side. Between 720 and 860 °C, the shear strength of the joint first increases and then decreases with brazing temperature. The maximum shear strength (223 MPa) is obtained at 830 °C.
- 15 September 2023
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (21)
Microstructure and Mechanical Properties of the Joint between Si3N4 and Mo Brazed by Near‐Eutectic Ag–Cu–In–Ti Filler Alloy
The joining of Si3N4 and Mo using Ag–Cu–In–Ti active filler alloy with the brazing temperature ranging from 720 to 860 °C for 10 min is investigated in this article. The correlation between the joint strength and the microstructures of the brazed joints is discussed. In the results, it is shown that the activity of Ti is different at different temperatures, and thus the degree of diffusion of Ti to the interface is different. The activity of Ti gradually increases as the brazing temperature increases, and more Ti atoms diffuse into both sides of the base materials, resulting in a progressively thicker TiN + Ti5Si3 reaction layer on the Si3N4 ceramic side. Between 720 and 860 °C, the shear strength of the joint first increases and then decreases with brazing temperature. The maximum shear strength (223 MPa) is obtained at 830 °C.
- 29 November 2022
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 64 (12) , 1765-1772
Effects of silver interlayer thickness on the microstructure and properties of electron beam welded joints of TC4 titanium and 4J29 Kovar alloys
Electron beam welding of TC4 titanium alloy and 4J29 Kovar alloy was performed by using different thicknesses of silver interlayers. The microstructure and the composition of welded joints were characterized by scanning electron microscopy, X-ray diffraction, and energy-dipersive spectrometry. The mechanical properties of welded joints were evaluated by tensile strength tests. The results indicated that Ag thickness has great effects on the weld appearance, microstructure, and mechanical properties of electron beam-welded joints. In case of 0.3 and 0.4 mm thickness of Ag interlayers, a considerable part of 4J29 and TC4 melts and a large amount of Fe, Ti, and Ni elements diffuse into the molten pool forming intermetallic compounds (IMCs) such as TiFe2, NiTi, and FeTi. In case of 0.6 mm thickness of Ag interlayer, the welded joint exhibits brazing characteristics with little IMCs near the fusion line of 4J29 Kovar alloy side. When the thickness of the Ag interlayer increases to 0.8 mm, the diffusion of Ti and Fe elements is completely inhibited by Ag. As the thickness of the Ag interlayer increases from 0.3 to 0.8 mm, the tensile strength of the welded sample shows a phenomenon that first rises and then falls, and the largest tensile strength is 243 MPa.
- 29 November 2022
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 64 (12) , 1765-1772
Effects of silver interlayer thickness on the microstructure and properties of electron beam welded joints of TC4 titanium and 4J29 Kovar alloys
Electron beam welding of TC4 titanium alloy and 4J29 Kovar alloy was performed by using different thicknesses of silver interlayers. The microstructure and the composition of welded joints were characterized by scanning electron microscopy, X-ray diffraction, and energy-dipersive spectrometry. The mechanical properties of welded joints were evaluated by tensile strength tests. The results indicated that Ag thickness has great effects on the weld appearance, microstructure, and mechanical properties of electron beam-welded joints. In case of 0.3 and 0.4 mm thickness of Ag interlayers, a considerable part of 4J29 and TC4 melts and a large amount of Fe, Ti, and Ni elements diffuse into the molten pool forming intermetallic compounds (IMCs) such as TiFe2, NiTi, and FeTi. In case of 0.6 mm thickness of Ag interlayer, the welded joint exhibits brazing characteristics with little IMCs near the fusion line of 4J29 Kovar alloy side. When the thickness of the Ag interlayer increases to 0.8 mm, the diffusion of Ti and Fe elements is completely inhibited by Ag. As the thickness of the Ag interlayer increases from 0.3 to 0.8 mm, the tensile strength of the welded sample shows a phenomenon that first rises and then falls, and the largest tensile strength is 243 MPa.
- 8 November 2002
- Published by IOP Publishing in Nanotechnology
- Vol. 13 (6) , 733-735
Ultrahigh-density data storage on a novel organic thin film achieved using a scanning tunnelling microscope
- 8 November 2002
- Published by IOP Publishing in Nanotechnology
- Vol. 13 (6) , 733-735
Ultrahigh-density data storage on a novel organic thin film achieved using a scanning tunnelling microscope