Yanchun Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yanchun Liu has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
- Bochen Song
Shandong Luqiao Group Co., Ltd., Jinan 250014, China
2 shared publications - Jiaqi Zhang
Qingdao Haixin Real Estate Co., Ltd., Qingdao 266100, China
2 shared publications - Jijun Miao
School of Civil Engineering, Qingdao University of Technology, Qingdao, China
2 shared publications - Sumeng Song
College of Civil Engineering, Beijing University of Technology, Beijing 100124, China
2 shared publications - Tingting Peng
College of Civil Engineering, Qingdao University of Technology, Qingdao 266033, China
2 shared publications - Xiaoming Guan
School of Civil Engineering, Qingdao University of Technology, Qingdao 266520, China
2 shared publications
Latest Publications
- Open Access
- 20 January 2026
- Published by MDPI AG in Applied Sciences
- Vol. 16 (2) , 1053
Experimental Study on Bonding Performance of Steel Rebar and Grout at Different Positions After Elevated Temperatures
To evaluate the fire safety performance of the joint region in prefabricated buildings, specifically when the grout in the slurry layer is under an unconstrained state. Total 54 pull-out specimens were designed to investigate the effects of elevated temperatures (20 °C, 200 °C, 300 °C, 400 °C, 500 °C, and 600 °C) and steel bar positions (center, mid-side, and corner) on the bond behavior between the grout and steel rebars. The failure modes, bond strength, ultimate displacement, and load–slip curves of the specimens were recorded. The peak load of the specimens with the temperature increasing first rose and then declined, exhibiting a trend consistent with the variation in compressive strength of the grout with temperature. At 600 °C, the ultimate loads of the center, mid-side, and corner specimens decreased by 53.46%, 52.53%, and 51.28%, respectively, compared with those at ambient temperature. At ambient temperature, the bond strength of the mid-side specimen was 11.24% lower than that of the central specimen, but 19.98% higher than that of the corner specimen. At 500 °C, the bond strength of the mid-side and corner specimens decreased by 15.76% and 39.26%, respectively, compared with that of the center specimen. The failure mode changed from steel-rebar fracture to pull-out failure due to the high temperature exposure and the steel rebar position. Finally, based on the post-heating strength test results of grout specimens, a bond strength calculation formula and a bond–slip constitutive model, considering both steel rebar position and temperature, were developed, achieving a correlation coefficient (R2) close to 1.0.
- 20 January 2026
- Published by MDPI AG in Applied Sciences
- Vol. 16 (2) , 1053
Open AccessExperimental Study on Bonding Performance of Steel Rebar and Grout at Different Positions After Elevated Temperatures
To evaluate the fire safety performance of the joint region in prefabricated buildings, specifically when the grout in the slurry layer is under an unconstrained state. Total 54 pull-out specimens were designed to investigate the effects of elevated temperatures (20 °C, 200 °C, 300 °C, 400 °C, 500 °C, and 600 °C) and steel bar positions (center, mid-side, and corner) on the bond behavior between the grout and steel rebars. The failure modes, bond strength, ultimate displacement, and load–slip curves of the specimens were recorded. The peak load of the specimens with the temperature increasing first rose and then declined, exhibiting a trend consistent with the variation in compressive strength of the grout with temperature. At 600 °C, the ultimate loads of the center, mid-side, and corner specimens decreased by 53.46%, 52.53%, and 51.28%, respectively, compared with those at ambient temperature. At ambient temperature, the bond strength of the mid-side specimen was 11.24% lower than that of the central specimen, but 19.98% higher than that of the corner specimen. At 500 °C, the bond strength of the mid-side and corner specimens decreased by 15.76% and 39.26%, respectively, compared with that of the center specimen. The failure mode changed from steel-rebar fracture to pull-out failure due to the high temperature exposure and the steel rebar position. Finally, based on the post-heating strength test results of grout specimens, a bond strength calculation formula and a bond–slip constitutive model, considering both steel rebar position and temperature, were developed, achieving a correlation coefficient (R2) close to 1.0.
- Open Access
Seismic Performance of the Full-Scale Prefabricated Concrete Column Connected in Half-Height: Experimental Study and Numerical Analysis
To improve the seismic performance of prefabricated structures, this study suggested putting grouted sleeves at the half-height of the column (at the point of contraflexure). A quasi-static test under constant axial load was conducted on the full-scale cast-in-place column and the full-scale prefabricated column connected in half-height. The hysteresis loops, skeleton curves, ductility, stiffness degradation, and energy dissipation capacity were compared. The test results indicate that the prefabricated column connected in half-height exhibited reliable seismic performance. Compared with the cast-in-place specimen, the bearing capacity of the prefabricated column decreased by only 1.45%, the energy dissipation decreased by 5.61%, and the initial secant stiffness and ductility coefficient increased by 8.88% and 9.09%, respectively. ABAQUS finite element software was used to establish finite-element models based on the experimental results. The damage pattern and seismic performance indicators of the two types of columns were verified by resolving issues related to the bonding interface model of sleeve-connected columns and the convergence of the multidimensional constitutive model. The formula for calculating the shear bearing capacity was put forward to evaluate the failure pattern. The study provides a basis for further investigation of the seismic performance of sleeve-connected columns with different connection positions under extreme conditions.
Open AccessSeismic Performance of the Full-Scale Prefabricated Concrete Column Connected in Half-Height: Experimental Study and Numerical Analysis
To improve the seismic performance of prefabricated structures, this study suggested putting grouted sleeves at the half-height of the column (at the point of contraflexure). A quasi-static test under constant axial load was conducted on the full-scale cast-in-place column and the full-scale prefabricated column connected in half-height. The hysteresis loops, skeleton curves, ductility, stiffness degradation, and energy dissipation capacity were compared. The test results indicate that the prefabricated column connected in half-height exhibited reliable seismic performance. Compared with the cast-in-place specimen, the bearing capacity of the prefabricated column decreased by only 1.45%, the energy dissipation decreased by 5.61%, and the initial secant stiffness and ductility coefficient increased by 8.88% and 9.09%, respectively. ABAQUS finite element software was used to establish finite-element models based on the experimental results. The damage pattern and seismic performance indicators of the two types of columns were verified by resolving issues related to the bonding interface model of sleeve-connected columns and the convergence of the multidimensional constitutive model. The formula for calculating the shear bearing capacity was put forward to evaluate the failure pattern. The study provides a basis for further investigation of the seismic performance of sleeve-connected columns with different connection positions under extreme conditions.
- Open Access
- 28 July 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (15) , 11699
Mechanical Properties and Influencing Factors of Shield Cutting Existing Station Supporting Piles
Based on the shield-cutting existing station supporting piles project of Zhengzhou metro line 6, the process and mechanism of concrete in the process of pile cutting were analyzed by establishing a three-dimensional model of concrete with a cutter. The magnitude and variation rules of cutting force, penetration force, and tangential force were explored. The variation rules of cutting force with four factors of cutting speed, cutting depth, cutter width, and tool rake angle were explored. The correctness of the numerical model and results were verified by the theoretical analysis method. Finally, the significance of the influencing factors of pile cutting was studied by means of range analysis and variance analysis using the orthogonal test method, and the cutter parameters were optimized. The cutting mechanism is that the front concrete is compressed and crushed to produce a dense core. The cutting force increases rapidly to its maximum value in a short time during the cutting process. The cutting force is always larger than the penetration force and tangential force. The cutter contact force basically remains unchanged with the change in cutting speed; however, it increases with the increase in cutting depth and cutter width. The significant order of the three influencing factors is cutting depth, cutter width, and rake angle. It is suggested that the cutting depth be adjusted preferentially, followed by the cutter width. And the principle of rake angle should be considered last.
- 28 July 2023
- Published by MDPI AG in Sustainability
- Vol. 15 (15) , 11699
Open AccessMechanical Properties and Influencing Factors of Shield Cutting Existing Station Supporting Piles
Based on the shield-cutting existing station supporting piles project of Zhengzhou metro line 6, the process and mechanism of concrete in the process of pile cutting were analyzed by establishing a three-dimensional model of concrete with a cutter. The magnitude and variation rules of cutting force, penetration force, and tangential force were explored. The variation rules of cutting force with four factors of cutting speed, cutting depth, cutter width, and tool rake angle were explored. The correctness of the numerical model and results were verified by the theoretical analysis method. Finally, the significance of the influencing factors of pile cutting was studied by means of range analysis and variance analysis using the orthogonal test method, and the cutter parameters were optimized. The cutting mechanism is that the front concrete is compressed and crushed to produce a dense core. The cutting force increases rapidly to its maximum value in a short time during the cutting process. The cutting force is always larger than the penetration force and tangential force. The cutter contact force basically remains unchanged with the change in cutting speed; however, it increases with the increase in cutting depth and cutter width. The significant order of the three influencing factors is cutting depth, cutter width, and rake angle. It is suggested that the cutting depth be adjusted preferentially, followed by the cutter width. And the principle of rake angle should be considered last.
- Open Access
- 11 January 2023
- Published by MDPI AG in Applied Sciences
- Vol. 13 (2) , 1006
Formation Mechanism and Control Technology of an Excavation Damage Zone in Tunnel-Surrounding Rock
Loosened rock circle is formed around the tunnel when the tunnel is constructed by the drilling and blasting method. The size of the loosened rock circle around the tunnel and the degree of internal rock fragmentation has an important influence on the support parameters, durability, and safety of the tunnel. Firstly, referencing an existing tunnel project, blasting tests using nonelectronic and electronic detonators were carried out to determine the influence of blasting construction on the scope of the rock loose circle and the degree of rock fragmentation. Then, a numerical simulation was used to study the contribution of the blasting impact and surrounding rock stress redistribution on the loosened rock circle around the tunnel. The results showed that the range of the loosened rock circle around the tunnel generated by the normal blasting of nonelectronic detonators was 1.5~2.3 m, and the wave velocity of the rock mass in the loosened rock circle around the tunnel decreased to 23~36%. The size of the loosened rock circle around the tunnel generated by the blasting impact was 0.66 m, accounting for 33% of the range of the loosened rock circle around the tunnel. The range of the loosened rock circle around the tunnel produced by electronic detonator blasting was 0~1.4 m. The wave velocity of the rock mass in the loosened rock circle around the tunnel decreased to 12~17%. The range of the loosened rock circle around the tunnel was approximately 60~76% of that of detonator blasting, and the broken degree of the surrounding rock in the loosened rock circle around the tunnel was small. The research results can provide a reference for the optimization design of preliminary support parameters of tunnels, such as anchors and steel arches in blasting construction.
- 11 January 2023
- Published by MDPI AG in Applied Sciences
- Vol. 13 (2) , 1006
Open AccessFormation Mechanism and Control Technology of an Excavation Damage Zone in Tunnel-Surrounding Rock
Loosened rock circle is formed around the tunnel when the tunnel is constructed by the drilling and blasting method. The size of the loosened rock circle around the tunnel and the degree of internal rock fragmentation has an important influence on the support parameters, durability, and safety of the tunnel. Firstly, referencing an existing tunnel project, blasting tests using nonelectronic and electronic detonators were carried out to determine the influence of blasting construction on the scope of the rock loose circle and the degree of rock fragmentation. Then, a numerical simulation was used to study the contribution of the blasting impact and surrounding rock stress redistribution on the loosened rock circle around the tunnel. The results showed that the range of the loosened rock circle around the tunnel generated by the normal blasting of nonelectronic detonators was 1.5~2.3 m, and the wave velocity of the rock mass in the loosened rock circle around the tunnel decreased to 23~36%. The size of the loosened rock circle around the tunnel generated by the blasting impact was 0.66 m, accounting for 33% of the range of the loosened rock circle around the tunnel. The range of the loosened rock circle around the tunnel produced by electronic detonator blasting was 0~1.4 m. The wave velocity of the rock mass in the loosened rock circle around the tunnel decreased to 12~17%. The range of the loosened rock circle around the tunnel was approximately 60~76% of that of detonator blasting, and the broken degree of the surrounding rock in the loosened rock circle around the tunnel was small. The research results can provide a reference for the optimization design of preliminary support parameters of tunnels, such as anchors and steel arches in blasting construction.