Yi Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Yi Liu has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Weihong Chen
College of Civil Engineering, Fuzhou University, Fuzhou 350116, China
2 shared publications - Chunhui Han
College of Civil Engineering, Fuzhou University, Fuzhou 350116, China
1 shared publication - Fanghao Liu
College of Civil Engineering, Fuzhou University, Fuzhou 350116, China
1 shared publication - Hui Qian
School of Civil Engineering, Zhengzhou University, Zhengzhou 450000, People’s Republic of China
1 shared publication - Kai Feng
College of Civil Engineering, Fuzhou University, Fuzhou 350116, China
1 shared publication - Peng Wu
School of Civil Engineering, Zhengzhou University, Zhengzhou 450001, China
1 shared publication
Latest Publications
- Open Access
Experimental Investigation of Cumulative Damage and Self-Healing Properties of Smart Cementitious Composite under Continuous Compression Load
This study investigated the effect of sustained loading on the cumulative damage of a newly developed smart cement-based self-healing composite material (SMA-ECC). SMA-ECC is composed of engineered cementitious composite (ECC) and shape memory alloy (SMA) fibers. A uniaxial compressive test with five predefined loading levels (0%, 30%, 40%, 50%, and 60% of compressive strength) was conducted on SMA-ECC hollow-cylindrical specimens and ECC control hollow-cylindrical specimens. The cumulative damage was mainly determined by changes in the total water absorption of different groups of specimens during three different periods (not loaded, at a predefined loading level, and after unloading). A normalized water content index was proposed to couple the effects of self-healing, sustained loading, and cumulative damage. The test results indicate that the cumulative water absorption of SMA-ECC was 35% lower than that of ECC, which may indicate less irreparable damage. In addition, the self-healing ability of SMA-ECC specimens under different compression load levels was evaluated through normalized water content analysis. SMA-ECC exhibited a 100% repair rate at load levels of 30% and 40%. At a higher load level of 60%, the repair rate of SMA-ECC was 76%. These results collectively emphasize the significant impermeability and self-healing performance of SMA-ECC after unloading.
Open AccessExperimental Investigation of Cumulative Damage and Self-Healing Properties of Smart Cementitious Composite under Continuous Compression Load
This study investigated the effect of sustained loading on the cumulative damage of a newly developed smart cement-based self-healing composite material (SMA-ECC). SMA-ECC is composed of engineered cementitious composite (ECC) and shape memory alloy (SMA) fibers. A uniaxial compressive test with five predefined loading levels (0%, 30%, 40%, 50%, and 60% of compressive strength) was conducted on SMA-ECC hollow-cylindrical specimens and ECC control hollow-cylindrical specimens. The cumulative damage was mainly determined by changes in the total water absorption of different groups of specimens during three different periods (not loaded, at a predefined loading level, and after unloading). A normalized water content index was proposed to couple the effects of self-healing, sustained loading, and cumulative damage. The test results indicate that the cumulative water absorption of SMA-ECC was 35% lower than that of ECC, which may indicate less irreparable damage. In addition, the self-healing ability of SMA-ECC specimens under different compression load levels was evaluated through normalized water content analysis. SMA-ECC exhibited a 100% repair rate at load levels of 30% and 40%. At a higher load level of 60%, the repair rate of SMA-ECC was 76%. These results collectively emphasize the significant impermeability and self-healing performance of SMA-ECC after unloading.
- Open Access
Chloride Ion Corrosion Resistance of Innovative Self-Healing SMA Fiber-Reinforced Engineering Cementitious Composites under Dry-Wet Cycles for Ocean Structures
To evaluate the chloride ion corrosion resistance of proposed innovative self-healing concrete based on shape memory alloys (SMA) and engineering cementitious composites (ECC), a total of 2 kinds of 22 specimens were prepared. Chloride ion corrosion tests of self-healing SMA-ECC concrete under dry-wet cycles were carried out. It was found that the chloride ion erosion depths of SMA-ECC were significantly smaller than that of MC, and the growth rate of erosion depth of SMA-ECC was obviously smaller than that of MC after 15 dry-wet (dry and wet) corrosion cycles. The chloride ion content of SMA-ECC vanished at the erosion depth more than 10 mm, which was consistent with the test result of AgNO3 solution color-rendering test. Test results indicate that, compared to marine concrete (MC), SMA-ECC has a better chloride ion corrosion resistance behavior. Moreover, the chloride ion concentration of SMA-ECC at a chloride ion erosion depth of less than 10 mm decreased more significantly than that of MC, indicating that almost all chloride salt solution reacted in the outer layer of SMA-ECC, which is consistent with the conclusions of 4.1 and 4.2. Finally, based on the erosion distribution of chloride ions and Fick’s second law, a calculation model describing the relationship between the apparent chloride ion diffusion coefficient and the boundary condition of the chloride ion content was proposed.
Open AccessChloride Ion Corrosion Resistance of Innovative Self-Healing SMA Fiber-Reinforced Engineering Cementitious Composites under Dry-Wet Cycles for Ocean Structures
To evaluate the chloride ion corrosion resistance of proposed innovative self-healing concrete based on shape memory alloys (SMA) and engineering cementitious composites (ECC), a total of 2 kinds of 22 specimens were prepared. Chloride ion corrosion tests of self-healing SMA-ECC concrete under dry-wet cycles were carried out. It was found that the chloride ion erosion depths of SMA-ECC were significantly smaller than that of MC, and the growth rate of erosion depth of SMA-ECC was obviously smaller than that of MC after 15 dry-wet (dry and wet) corrosion cycles. The chloride ion content of SMA-ECC vanished at the erosion depth more than 10 mm, which was consistent with the test result of AgNO3 solution color-rendering test. Test results indicate that, compared to marine concrete (MC), SMA-ECC has a better chloride ion corrosion resistance behavior. Moreover, the chloride ion concentration of SMA-ECC at a chloride ion erosion depth of less than 10 mm decreased more significantly than that of MC, indicating that almost all chloride salt solution reacted in the outer layer of SMA-ECC, which is consistent with the conclusions of 4.1 and 4.2. Finally, based on the erosion distribution of chloride ions and Fick’s second law, a calculation model describing the relationship between the apparent chloride ion diffusion coefficient and the boundary condition of the chloride ion content was proposed.