Lama Osman
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Lama Osman has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Abdelrahman Zkria
Department of Applied Science for Electronics and Materials, Kyushu University
4 shared publications - Hiroshi Naragino
Department of Advanced Energy Science and Engineering Kyushu University Kasuga‐Koen Kasuga Fukuoka 816‐8580 Japan
4 shared publications - Tsuyoshi Yoshitake
Department of Applied Science for Electronics and Materials, Kyushu University
4 shared publications - Ali Mohamed Ali
Department of Applied Science for Electronics and Materials, Kyushu University, Fukuoka 816-8580, Japan
3 shared publications Hiroki Hashiguchi
Interdisciplinary Graduate School of Engineering Sciences, Kyushu University
1 shared publication- Mohamed Ragab Diab
Department of Mechanical Engineering, Kafrelsheikh University, Kafrelsheikh 33516, Egypt
1 shared publication
Latest Publications
- Open Access
- 23 October 2024
- Published by Taylor & Francis in Functional Diamond
- Vol. 4 (1)
Fabrication of nitrogen-doped quenched-produced diamond electrodes on titanium substrates by coaxial arc plasma deposition
- 23 October 2024
- Published by Taylor & Francis in Functional Diamond
- Vol. 4 (1)
Open AccessFabrication of nitrogen-doped quenched-produced diamond electrodes on titanium substrates by coaxial arc plasma deposition
- 1 July 2023
- Published by IOP Publishing in Applied Physics Express
- Vol. 16 (7) , 075501
Synergistic effects of optimal negative bias-enhanced growth of quenched-produced diamond films on titanium substrates
We report on negative bias-enhanced growth of quenched-produced diamond films on titanium using hybrid coaxial arc plasma deposition at room temperature. Optimizing the bias voltage to −40 V resulted in a spontaneous formation of a titanium carbide interfacial layer, which caused a significant increase in the adhesion strength from 16 to 48 N. Selective etching of undesired sp 2–C bonded atoms and ultrafast quenching of the energetic carbon ions (C+) promoted the growth of dense sp 3–C bonded atoms, achieving a superhardness of 96 GPa, comparable to natural diamond. These pioneering findings have the potential to revolutionize multifunctional materials for biomedical applications.
- 1 July 2023
- Published by IOP Publishing in Applied Physics Express
- Vol. 16 (7) , 075501
Synergistic effects of optimal negative bias-enhanced growth of quenched-produced diamond films on titanium substrates
We report on negative bias-enhanced growth of quenched-produced diamond films on titanium using hybrid coaxial arc plasma deposition at room temperature. Optimizing the bias voltage to −40 V resulted in a spontaneous formation of a titanium carbide interfacial layer, which caused a significant increase in the adhesion strength from 16 to 48 N. Selective etching of undesired sp 2–C bonded atoms and ultrafast quenching of the energetic carbon ions (C+) promoted the growth of dense sp 3–C bonded atoms, achieving a superhardness of 96 GPa, comparable to natural diamond. These pioneering findings have the potential to revolutionize multifunctional materials for biomedical applications.
- Open Access
- 1 June 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (6) , 066401
Influence of different pretreatments on the adhesion of nanodiamond composite films on Ti substrates via coaxial arc plasma deposition
In this study, we report on the novel growth of nanodiamond composite (NDC) films on titanium (Ti) substrates using the coaxial arc plasma deposition (CAPD) at room temperature, which offers several advantages over conventional growth techniques. CAPD employs a unique coaxial arc plasma gun structure that provides a supersaturated condition of highly energetic carbon ions (C+) for ultrafast quenching on the substrate, promoting the growth of nanodiamond grains. This allows for NDC films’ growth on diverse substrates without the need for initial seeding or substrate heating. However, the growth of NDC films on Ti substrates at room temperature is challenging due to the native oxide layer (TiO2). Here, we grew NDC films on Ti substrates using three different pretreatments: (i) hydrofluoric acid (HF) etching, (ii) insertion of a titanium carbide (TiC) intermediate layer, and (iii) in situ Ar+ plasma etching. The morphology and structure of the grown NDC films were examined by 3D laser, high-resolution scanning electron microscopies (HR-SEM), Raman, and x-ray photoelectron (XPS) spectroscopies. Our results demonstrate that in situ Ar+ plasma etching is the most effective pretreatment method for completely removing the native TiO2 layer compared to the other two ex situ pretreatments, in which re-oxidation is more likely to occur after these pretreatments. Furthermore, NDC films grown using the hybrid Ar+ ion etching gun (IG) and CAPD exhibit the highest sp 3 content (63%) and adhesion strength (16 N).
- 1 June 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (6) , 066401
Open AccessInfluence of different pretreatments on the adhesion of nanodiamond composite films on Ti substrates via coaxial arc plasma deposition
In this study, we report on the novel growth of nanodiamond composite (NDC) films on titanium (Ti) substrates using the coaxial arc plasma deposition (CAPD) at room temperature, which offers several advantages over conventional growth techniques. CAPD employs a unique coaxial arc plasma gun structure that provides a supersaturated condition of highly energetic carbon ions (C+) for ultrafast quenching on the substrate, promoting the growth of nanodiamond grains. This allows for NDC films’ growth on diverse substrates without the need for initial seeding or substrate heating. However, the growth of NDC films on Ti substrates at room temperature is challenging due to the native oxide layer (TiO2). Here, we grew NDC films on Ti substrates using three different pretreatments: (i) hydrofluoric acid (HF) etching, (ii) insertion of a titanium carbide (TiC) intermediate layer, and (iii) in situ Ar+ plasma etching. The morphology and structure of the grown NDC films were examined by 3D laser, high-resolution scanning electron microscopies (HR-SEM), Raman, and x-ray photoelectron (XPS) spectroscopies. Our results demonstrate that in situ Ar+ plasma etching is the most effective pretreatment method for completely removing the native TiO2 layer compared to the other two ex situ pretreatments, in which re-oxidation is more likely to occur after these pretreatments. Furthermore, NDC films grown using the hybrid Ar+ ion etching gun (IG) and CAPD exhibit the highest sp 3 content (63%) and adhesion strength (16 N).
- 31 October 2022
- Published by IOP Publishing in Applied Physics Express
- Vol. 15 (11) , 115004
Adhesion of nanodiamond composite films on Ti substrates at room temperature via hybrid ion etching gun and coaxial arc plasma deposition
It has been extremely difficult for nanodiamond composite (NDC) films to be deposited on Ti due to a large thermal expansion coefficient difference. The native oxide layer on Ti is another problem preventing the appropriate adhesion of NDC films and subsequent delamination. In this work, innovative room temperature adhesion of 3 μm NDC films with 54 GPa hardness on Ti substrates was accomplished via a hybrid system of ion etching gun and coaxial arc plasma deposition (CAPD). Ar+ plasma etching is capable to terminate the superficial TiO2 layer and manipulates substrate morphology during CAPD provides instantaneous deposition of NDC films at room temperature.
- 31 October 2022
- Published by IOP Publishing in Applied Physics Express
- Vol. 15 (11) , 115004
Adhesion of nanodiamond composite films on Ti substrates at room temperature via hybrid ion etching gun and coaxial arc plasma deposition
It has been extremely difficult for nanodiamond composite (NDC) films to be deposited on Ti due to a large thermal expansion coefficient difference. The native oxide layer on Ti is another problem preventing the appropriate adhesion of NDC films and subsequent delamination. In this work, innovative room temperature adhesion of 3 μm NDC films with 54 GPa hardness on Ti substrates was accomplished via a hybrid system of ion etching gun and coaxial arc plasma deposition (CAPD). Ar+ plasma etching is capable to terminate the superficial TiO2 layer and manipulates substrate morphology during CAPD provides instantaneous deposition of NDC films at room temperature.