Uttam Kumar Tarai
Research Subjects
Research Interests
Uttam Kumar Tarai has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Suyog Jhavar
Department of Mechanical Engineering, VIT-AP University, Amravathi, India
3 shared publications - Swagat Dwibedi
Indian Institute of Technology Guwahati
3 shared publications - Alok Ranjan Biswal
Department of Mechanical Engineering,National Institute of Technology Rourkela, 769008, India
2 shared publications - Deepak Ranjan Biswal
DRIEMS University, Department of Mechanical Engineering, Cuttack 754022, India
2 shared publications Sukhomay Pal
Department of Mechanical Engineering, Indian Institute of Technology, Guwahati, India
2 shared publications- Devnath Chatterjee1 shared publication
Latest Publications
- 10 February 2026
- Published by Springer Nature
- p. 269-281
Modelling and Analysis of a Two-Phalange Robotic Manipulator for Dexterous Grasping
- 10 February 2026
- Published by Springer Nature
- p. 269-281
Modelling and Analysis of a Two-Phalange Robotic Manipulator for Dexterous Grasping
- Open Access
- 25 June 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 973-981
Influence of Process Parameters on the Microstructural and Mechanical Characteristics of TLP Bonded IN718
Study explores the role of process parameters in joining IN718 with the TLP bonding process is explored. Microstructure evolution and mechanical performance of the bond are investigated using scanning electron microscopy, tensile test, and micro-hardness test. The bond metallurgy showed three distinct zones: the base material zone, the diffusion-affected zone containing a large number of boride precipitates, and the isothermal solidification zone. Further investigation reveals that the ISZ contains a few brittle intermetallic particles, which reduce the mechanical properties of the bond. The results demonstrates that higher bonding temperature, time, optimal interlayer thickness, and pressure enhance the mechanical and microstructural properties of the bond. The bond formed at 1423 K bonding temperature, 1.5 h holding time, 80 μm interlayer thickness, and 12.5 kg load demonstrates the highest strength of 625 MPa.
- 25 June 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 973-981
Open AccessInfluence of Process Parameters on the Microstructural and Mechanical Characteristics of TLP Bonded IN718
Study explores the role of process parameters in joining IN718 with the TLP bonding process is explored. Microstructure evolution and mechanical performance of the bond are investigated using scanning electron microscopy, tensile test, and micro-hardness test. The bond metallurgy showed three distinct zones: the base material zone, the diffusion-affected zone containing a large number of boride precipitates, and the isothermal solidification zone. Further investigation reveals that the ISZ contains a few brittle intermetallic particles, which reduce the mechanical properties of the bond. The results demonstrates that higher bonding temperature, time, optimal interlayer thickness, and pressure enhance the mechanical and microstructural properties of the bond. The bond formed at 1423 K bonding temperature, 1.5 h holding time, 80 μm interlayer thickness, and 12.5 kg load demonstrates the highest strength of 625 MPa.
- 28 January 2025
- Published by Springer Nature
- p. 233-244
Influence of Post Bond Heat Treatment on IN718 Joints: An Experimental Study
- 28 January 2025
- Published by Springer Nature
- p. 233-244
Influence of Post Bond Heat Treatment on IN718 Joints: An Experimental Study
- 28 January 2025
- Published by Springer Nature
- p. 103-112
Calculation of Ni–Cu, Ni–Ag, and Cu–Ag Phase Diagram Using CALPHAD Method
- 28 January 2025
- Published by Springer Nature
- p. 103-112
Calculation of Ni–Cu, Ni–Ag, and Cu–Ag Phase Diagram Using CALPHAD Method
- 30 September 2023
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 129 (3-4) , 1425-1442
Reduction of ASZ size and enhancement of mechanical properties of TLP bonded IN718 joint using post bond heat treatment process
- 30 September 2023
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 129 (3-4) , 1425-1442
Reduction of ASZ size and enhancement of mechanical properties of TLP bonded IN718 joint using post bond heat treatment process
- Open Access
- 27 April 2023
- Published by Springer Nature in Research Square
Reduction of ASZ size and enhancement of mechanical properties of TLP bonded IN718 joint using post bond heat treatment process
Transient liquid phase (TLP) bonding can be used to join Inconel 718 superalloy because the bond properties are similar to the parent material properties and little melting of base material. Presence of centerline eutectic and boride precipitates in the microstructure of the TLP bonded Inconel 718 joints affects mechanical properties of the joints. The eutectics and borides should be minimized to enhance the mechanical properties of the bond. This can be achieved to a great extent by prolonged isothermal holding. However, it can induce adverse effects by modifying the microstructure of the base material. Post bond heat treatment (PBHT) processes can be implemented to improve the mechanical properties without inducing any harmful effect of prolonged heating. In the present work, the effect of PBHT technique (i.e. solution treatment and double aging) on the microstructural evolution and improvement in mechanical properties were investigated. The ultimate tensile strength (UTS) and microhardness of TLP bond before and after the PBHT were analyzed and compared with the as-received workpiece. FESEM, FETEM and XRD analysis were used to quantify different precipitates formed during PBHT of TLP bond. The results showed that the PBHT improved the microstructure and mechanical properties of the bonded samples. After the solution treatment and double aging, a maximum UTS of 1210 MPa was obtained, which correspond to a 113.5% increase. The improvement of bond strength was attributed to increase volume fraction of γ' and γ" type strengthening phases during double aging and a decrease in the fraction of Nb-Mo type borides in the diffusion affected zone.
- 27 April 2023
- Published by Springer Nature in Research Square
Open AccessReduction of ASZ size and enhancement of mechanical properties of TLP bonded IN718 joint using post bond heat treatment process
Transient liquid phase (TLP) bonding can be used to join Inconel 718 superalloy because the bond properties are similar to the parent material properties and little melting of base material. Presence of centerline eutectic and boride precipitates in the microstructure of the TLP bonded Inconel 718 joints affects mechanical properties of the joints. The eutectics and borides should be minimized to enhance the mechanical properties of the bond. This can be achieved to a great extent by prolonged isothermal holding. However, it can induce adverse effects by modifying the microstructure of the base material. Post bond heat treatment (PBHT) processes can be implemented to improve the mechanical properties without inducing any harmful effect of prolonged heating. In the present work, the effect of PBHT technique (i.e. solution treatment and double aging) on the microstructural evolution and improvement in mechanical properties were investigated. The ultimate tensile strength (UTS) and microhardness of TLP bond before and after the PBHT were analyzed and compared with the as-received workpiece. FESEM, FETEM and XRD analysis were used to quantify different precipitates formed during PBHT of TLP bond. The results showed that the PBHT improved the microstructure and mechanical properties of the bonded samples. After the solution treatment and double aging, a maximum UTS of 1210 MPa was obtained, which correspond to a 113.5% increase. The improvement of bond strength was attributed to increase volume fraction of γ' and γ" type strengthening phases during double aging and a decrease in the fraction of Nb-Mo type borides in the diffusion affected zone.