Margono Margono
Research Subjects
Margono Margono has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Bambang Hari Priyambodo
Mechanical Engineering Department, Vocational College, Universitas Gadjah Mada
2 shared publications - Edy Suryono
Sekolah Tinggi Teknologi Warga Surakarta
1 shared publication - Farit Ardiyanto
Department of Electrical Engineering, Sekolah Tinggi Teknologi Warga Surakarta, Surakarta, Indonesia
1 shared publication - Haikal Haikal
Sekolah Tinggi Teknologi "Warga" Surakarta
1 shared publication - Moch. Chamim
Sekolah Tinggi Teknologi Warga Surakarta
1 shared publication - Nugroho Tri Atmoko
Sekolah Tinggi Teknologi Warga Surakarta
1 shared publication
Latest Publications
- Open Access
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3145 (1) , 050003
Improvement of hardness and micro structure of Cu-Zn as a propeller material by shot peening method
Brass metal is widely used as a supporting equipment material, one of which is a propeller. The propeller itself is one component of the boat that rotates and p Brass metal is widely used as a supporting equipment material, one of which is a propeller. The propeller itself is one component of the boat that rotates and p
- 1 January 2024
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 3145 (1) , 050003
Open AccessImprovement of hardness and micro structure of Cu-Zn as a propeller material by shot peening method
Brass metal is widely used as a supporting equipment material, one of which is a propeller. The propeller itself is one component of the boat that rotates and p Brass metal is widely used as a supporting equipment material, one of which is a propeller. The propeller itself is one component of the boat that rotates and p
- Open Access
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2689 (1) , 070019
The heat treatment effect of cast iron on mechanical properties and microstructure
Cast iron is used as the raw material in the automotive and manufacturing industries and requirements contained in cast iron material to produce an excellent quality product, one of which is having a sufficient lifetime. Research works aim to analyze the effect of the heat treatment process of Cast Iron on mechanical properties and microstructure. Three various heat treatment methods were used in this research, namely annealing, normalizing, and quenching. After the quenching process, the specimen cooled rapidly using cooling fluid as pure water, oil, and cold water. The chemical composition test is used to determine the type of cast iron material while analyzing the structure and mechanical properties using the microstructure test and micro-Vickers hardness. The result of this works showed that the specimen is grey cast iron type ASTM A48, whereas hardness will increase by 11.52% when the heat treatment process uses the normalizing method. When the method used is annealing, the hardness will be decreased by 20.33% compared with raw material. The hardness of the cast iron material increased after quenching using pure water oil, and cold water, where the surface hardness of the cast iron material increased 45.4% - 50.0%. The highest hardness was obtained when the cooling medium was cold water which produced an average hardness of 566.6HV or increased by 62.01%. Annealing method on cast iron specimen has little effect on morphology and distribution of graphite. Still, it will decrease the pearlite phase and improve the ferrite content in the metrics when the normalizing method used material structure shows less excess ferrite or cementite and the pearlite is finer. On quenching, the structure of the material looks different; especially the grain size becomes small. It is also seen that the structure of the ferrite and pearlite material is increasing, spreading evenly overall material surfaces.
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2689 (1) , 070019
Open AccessThe heat treatment effect of cast iron on mechanical properties and microstructure
Cast iron is used as the raw material in the automotive and manufacturing industries and requirements contained in cast iron material to produce an excellent quality product, one of which is having a sufficient lifetime. Research works aim to analyze the effect of the heat treatment process of Cast Iron on mechanical properties and microstructure. Three various heat treatment methods were used in this research, namely annealing, normalizing, and quenching. After the quenching process, the specimen cooled rapidly using cooling fluid as pure water, oil, and cold water. The chemical composition test is used to determine the type of cast iron material while analyzing the structure and mechanical properties using the microstructure test and micro-Vickers hardness. The result of this works showed that the specimen is grey cast iron type ASTM A48, whereas hardness will increase by 11.52% when the heat treatment process uses the normalizing method. When the method used is annealing, the hardness will be decreased by 20.33% compared with raw material. The hardness of the cast iron material increased after quenching using pure water oil, and cold water, where the surface hardness of the cast iron material increased 45.4% - 50.0%. The highest hardness was obtained when the cooling medium was cold water which produced an average hardness of 566.6HV or increased by 62.01%. Annealing method on cast iron specimen has little effect on morphology and distribution of graphite. Still, it will decrease the pearlite phase and improve the ferrite content in the metrics when the normalizing method used material structure shows less excess ferrite or cementite and the pearlite is finer. On quenching, the structure of the material looks different; especially the grain size becomes small. It is also seen that the structure of the ferrite and pearlite material is increasing, spreading evenly overall material surfaces.
- Open Access
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2706 (1) , 020017
Characteristic stress corrosion cracking of GTAW stainless steel grade 304 in corrosion environment
This paper deals with experimental investigation of stress corrosion cracking of stainless-steel grade 304 after GTAW welded under simulated environment corrosion. Specimens welded in 60 and 65 Ampere used 5 and 10 L/mnt of Argon shielding gas. Constant tensile load test 4000N and immersed specimen were conducted for 24 hours in Hcl+Aquades solution result variety crack characteristics. After testing, an orange-colored layer of corrosion was seen covering the entire surface. This layer causes corrosion resistance for a certain period of time so that the corrosion process stops. The parameter ampere and shielding gas flow rate affected the crack that occurs. The results of the photo of the microstructure show cracks with the model trans granular at surface and intergranular after crack insert to grains boundaries. Vickers Hardness and Microstructure used to evaluate of welding area. The Lowest ampere of welded result maximum rough crack from surface and The Highest ampere result smooth crack on all of surface.
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2706 (1) , 020017
Open AccessCharacteristic stress corrosion cracking of GTAW stainless steel grade 304 in corrosion environment
This paper deals with experimental investigation of stress corrosion cracking of stainless-steel grade 304 after GTAW welded under simulated environment corrosion. Specimens welded in 60 and 65 Ampere used 5 and 10 L/mnt of Argon shielding gas. Constant tensile load test 4000N and immersed specimen were conducted for 24 hours in Hcl+Aquades solution result variety crack characteristics. After testing, an orange-colored layer of corrosion was seen covering the entire surface. This layer causes corrosion resistance for a certain period of time so that the corrosion process stops. The parameter ampere and shielding gas flow rate affected the crack that occurs. The results of the photo of the microstructure show cracks with the model trans granular at surface and intergranular after crack insert to grains boundaries. Vickers Hardness and Microstructure used to evaluate of welding area. The Lowest ampere of welded result maximum rough crack from surface and The Highest ampere result smooth crack on all of surface.