OYOmar Yadak

Omar Yadak

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Omar Yadak has a total of 16 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Flexural Performance of Pre-Cracked UHPC with Varying Fiber Contents and Fiber Types Exposed to Freeze–Thaw Cycles

    by Dip Banik, Omar Yadak, Royce Floyd

    Ultra-high-performance concrete (UHPC) is an advanced cementitious composite material with high durability and the strength properties exceeding those of conventional concrete. This paper presents the results of experimental testing assessing the freeze–thaw durability of UHPC specimens with varying fiber types (13 mm straight microfibers and 30 mm hooked-end fibers) and fiber percentages, as well as pre-existing cracks. The performance of all specimens was evaluated by measuring resonant frequency at intervals during testing and residual flexural strength after the completion of 350 freeze–thaw cycles. All specimens showed no degradation of resonant frequency over time. However, the pre-cracked specimens showed an increase in resonant frequency over the course of testing. The uncracked straight fibers specimens exposed to freeze–thaw cycles had the highest flexural strength, but the flexural resistance of the pre-cracked straight fibers specimens increased compared to the control specimens after 350 freeze–thaw cycles. The pre-cracked hooked fiber specimens showed higher first cracking strength and similar ultimate strength to the uncracked specimens after freeze–thaw exposure.

  • Open Access

    Scanning Electron Microscopy of Carbon Nanotube–Epoxy Interfaces: Correlating Morphology to Sulfate Exposure

    by Sijan Adhikari, Braiden M. Myers, Bryce L. Tuck, Courtney Dawson, Joey R. Cipriano, Jules F. Ahlert, Menziwokuhle Thwala, Mia A. Griffin, Omar Yadak, Osama A. Alfailakawi, et al.

    Epoxy resins are widely used as protective coatings in civil infrastructure, yet sulfate-rich environments accelerate their deterioration. This study evaluates the effectiveness of multi-walled carbon nanotubes (MWCNTs) in enhancing the sulfate resistance of epoxy resins. Neat and MWCNT-reinforced epoxy specimens (0.25 wt.% and 0.5 wt.%) were fabricated, heat cured at 100 °C and exposed to a solution of sulfuric acid and sodium chloride maintaining a pH of less than 3 for 0, 30, and 60 days. Analytical techniques, including scanning electron microscopy (SEM) and energy-dispersive spectroscopy (EDS), revealed distinct degradation patterns: the neat epoxy exhibited puncture damage and extensive salt deposition, while the MWCNT-reinforced specimens showed crack propagation mitigated by nanotube bridging. Heat curing introduced micro-voids that exacerbated sulfate ingress. The salt deposition surged to 200 times for the MWCNT-reinforced specimens compared to the neat ones, whereas crack width was higher in the MWCNT reinforced specimen compared to their neat counterparts, given that crack-bridging was observed. These findings highlight the potential of MWCNTs to improve epoxy durability in sulfate-prone environments, though the optimization of curing conditions and dispersion methods is critical.


  • Open Access

    Flexural Resistance of Ultra-High Performance-Concrete Subjected to Freeze-Thaw Cycles

    by Omar Yadak, Dip Banik, Royce W. Floyd

    Ultra-High Performance-Concrete (UHPC) is an advanced cementitious composite material with high durability and strength properties exceeding those of conventional concrete. This paper presents the flexural resistance of UHPC and the effect of fiber percentages by volume on flexural strength of UHPC subjected to freeze-thaw cycles. Freeze-thaw testing was performed on uncracked and pre-cracked 3-in. by 3-in. by 12-in. (75-mm by 75-mm by 300-mm) prisms of nonproprietary UHPC developed at the University of Oklahoma with 2% steel fibers by volume. Freeze-thaw testing was also performed on a series of 4-in. by 4-in. by 15-in. (100-mm by 100mm by 380-mm) prisms with no fibers, 1%, 2%, 4%, and 6% fibers by volume. Performance of all specimens was evaluated by measuring resonant frequency after every 36 or fewer cycles and residual flexural strength after the completion of 350 freeze-thaw cycles. All specimens showed no degradation of resonant frequency over time. The 3-in. by 3-in. pre-cracked specimens showed an increase in resonant frequency over the course of freeze-thaw testing while the uncracked specimens did not show a significant change in resonant frequency. The uncracked specimens exposed to freeze-thaw cycles achieved higher flexural capacity compared to the pre-cracked and no degradation compared to the control specimens. The 4-in. by 4-in. specimens with 2% and 4% fiber content exposed to freeze-thaw showed similar flexural behavior to the uncracked specimens. However, the flexural resistance of the pre-cracked, no-fibers, 1%, and 6% specimens had reduced compared to their respective control specimens.