Koravith Tiprak
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Koravith Tiprak has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Chanachai Thongchom
Department of Civil Engineering, Faculty of Engineering, Thammasat School of Engineering, Thammasat University, Pathumthani 12120, Thailand
4 shared publications Kittipat Prathyajuta
2 shared publications- Nitipong Praphaphankul
Architectural Intelligence (A.I.) Research Group, Faculty of Architecture, Chulalongkorn University
2 shared publications - Akhrawat Lenwari
Chulalongkorn Univ
1 shared publication Cherdsak Suksiripattanapong
1 shared publication- Cherdsak Suksiripattanapong
Department of Civil Engineering, Faculty of Engineering and Technology, Rajamangala University of Technology Isan, Nakhon Ratchasima 30000, Thailand
1 shared publication
Latest Publications
- Open Access
- 6 August 2026
- Published by Elsevier in Results in Engineering
- Vol. 32
Confinement interaction in Concrete-Filled GFRP Tubes: Effects of reinforcement morphology
- 6 August 2026
- Published by Elsevier in Results in Engineering
- Vol. 32
Open AccessConfinement interaction in Concrete-Filled GFRP Tubes: Effects of reinforcement morphology
- 9 July 2026
- Published by Elsevier in Structures
- Vol. 91
Axial behavior of hollow concrete columns with GFRP and hybrid reinforcement: An integrated experimental and numerical study
- 9 July 2026
- Published by Elsevier in Structures
- Vol. 91
Axial behavior of hollow concrete columns with GFRP and hybrid reinforcement: An integrated experimental and numerical study
- Open Access
- 16 February 2026
- Published by Elsevier in SSRN Electronic Journal
Confinement Synergy in Concrete-Filled GFRP Tubes: Effects of Reinforcement Morphology
The Concrete-Filled GFRP Tube (CFGT) system offers a high-performance, corrosion-resistant alternative to conventional reinforced concrete, yet the synergistic mechanics between external passive confinement and internal reinforcement morphology remain under-characterized. This study experimentally investigates the monotonic axial compression behavior of 16 full-scale CFGT short columns to systematically decouple the effects of external tube geometry, 3, 5, and 7 mm wall thickness and internal reinforcement configurations, discrete ties vs. continuous spirals; steel with GFRP; varying diameters. Experimental results reveal that while the external tube serves as the primary governor of ultimate capacity exhibiting a linear strength enhancement with wall thickness the efficiency of the internal reinforcement is strictly dictated by geometric compatibility rather than volumetric ratio. A critical confinement stiffness mismatch was identified: contrary to standard design assumptions, maximizing the internal steel spiral diameter to 12 mm reduced confinement efficiency. The excessive flexural rigidity of these large-diameter bars prevented intimate contact with the concrete core, causing a lag in confinement activation compared to flexible 6 mm spirals, which facilitated immediate composite engagement. Furthermore, increasing the tube thickness shifted the failure mode from catastrophic mixed-mode rupture to a ductile, energy-dissipating axial splitting mechanism. These findings challenge existing volumetric-based design paradigms, suggesting that optimal hybrid column performance requires a stiffness-balanced approach to reinforcement detailing.
- 16 February 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessConfinement Synergy in Concrete-Filled GFRP Tubes: Effects of Reinforcement Morphology
The Concrete-Filled GFRP Tube (CFGT) system offers a high-performance, corrosion-resistant alternative to conventional reinforced concrete, yet the synergistic mechanics between external passive confinement and internal reinforcement morphology remain under-characterized. This study experimentally investigates the monotonic axial compression behavior of 16 full-scale CFGT short columns to systematically decouple the effects of external tube geometry, 3, 5, and 7 mm wall thickness and internal reinforcement configurations, discrete ties vs. continuous spirals; steel with GFRP; varying diameters. Experimental results reveal that while the external tube serves as the primary governor of ultimate capacity exhibiting a linear strength enhancement with wall thickness the efficiency of the internal reinforcement is strictly dictated by geometric compatibility rather than volumetric ratio. A critical confinement stiffness mismatch was identified: contrary to standard design assumptions, maximizing the internal steel spiral diameter to 12 mm reduced confinement efficiency. The excessive flexural rigidity of these large-diameter bars prevented intimate contact with the concrete core, causing a lag in confinement activation compared to flexible 6 mm spirals, which facilitated immediate composite engagement. Furthermore, increasing the tube thickness shifted the failure mode from catastrophic mixed-mode rupture to a ductile, energy-dissipating axial splitting mechanism. These findings challenge existing volumetric-based design paradigms, suggesting that optimal hybrid column performance requires a stiffness-balanced approach to reinforcement detailing.
- Open Access
Experimental Investigation on Post-Fire Mechanical Properties of Glass Fiber-Reinforced Polymer Rebars
Glass fiber-reinforced polymer (GFRP) rebars are commonly used as an alternative to conventional steel reinforcement in a variety of structural applications due to their superior low cost, strength-to-weight ratio, and durability. However, their mechanical properties after exposure to elevated temperatures, particularly in fire-prone environments, remain a significant concern. To address this concern, the present study focuses on investigating the residual tensile behavior, specifically the tensile strength and elastic modulus, of GFRP rebars exposed to high temperatures that are realistically encountered during fire incidents. The temperature range considered in this analysis spans from 100 °C to 400 °C, with a heating rate of 20 °C/min. The fire duration of 1 h is used. This comprehensive analysis is essential for enhancing our understanding of the performance and applicability of GFRP rebars in fire-prone environments. Based on their actual application in the construction industry, five specimens of three different rebar sizes (16, 20, and 25 mm) were examined for the effect of rebar size on tensile behavior after fire exposure. In addition, the effects were investigated of air- and water-cooling methods on residual tensile behavior. The nominal tensile strength, elastic modulus, and ultimate strain of GFRP rebars at ambient temperature are 930 MPa, 50.2 GPa and 1.85%, respectively. The test results indicated that as the temperature increased to 400 °C, the ultimate tensile strength of the GFRP bars decreased by up to 55%, while the ultimate strain increased by up to 44%, regardless of the cooling method. In addition, when rebars of sizes 16–25 mm were subjected to a 400 °C fire treatment, the smaller the rebar, the greater the percentage of ultimate tensile and strain reduction. These findings hold great significance for the utilization of GFRP bars within the construction industry. This study offers valuable insights into the design of fire-resilient structures, emphasizing the importance of considering rebar size and cooling methods due to their impact on the post-fire tensile strength and strain of GFRP rebars.
Open AccessExperimental Investigation on Post-Fire Mechanical Properties of Glass Fiber-Reinforced Polymer Rebars
Glass fiber-reinforced polymer (GFRP) rebars are commonly used as an alternative to conventional steel reinforcement in a variety of structural applications due to their superior low cost, strength-to-weight ratio, and durability. However, their mechanical properties after exposure to elevated temperatures, particularly in fire-prone environments, remain a significant concern. To address this concern, the present study focuses on investigating the residual tensile behavior, specifically the tensile strength and elastic modulus, of GFRP rebars exposed to high temperatures that are realistically encountered during fire incidents. The temperature range considered in this analysis spans from 100 °C to 400 °C, with a heating rate of 20 °C/min. The fire duration of 1 h is used. This comprehensive analysis is essential for enhancing our understanding of the performance and applicability of GFRP rebars in fire-prone environments. Based on their actual application in the construction industry, five specimens of three different rebar sizes (16, 20, and 25 mm) were examined for the effect of rebar size on tensile behavior after fire exposure. In addition, the effects were investigated of air- and water-cooling methods on residual tensile behavior. The nominal tensile strength, elastic modulus, and ultimate strain of GFRP rebars at ambient temperature are 930 MPa, 50.2 GPa and 1.85%, respectively. The test results indicated that as the temperature increased to 400 °C, the ultimate tensile strength of the GFRP bars decreased by up to 55%, while the ultimate strain increased by up to 44%, regardless of the cooling method. In addition, when rebars of sizes 16–25 mm were subjected to a 400 °C fire treatment, the smaller the rebar, the greater the percentage of ultimate tensile and strain reduction. These findings hold great significance for the utilization of GFRP bars within the construction industry. This study offers valuable insights into the design of fire-resilient structures, emphasizing the importance of considering rebar size and cooling methods due to their impact on the post-fire tensile strength and strain of GFRP rebars.