Bin Xu
Bin Xu has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Rongfeng Zhou
Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
2 shared publications - Yongkun Li
Faculty of Material Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
2 shared publications - Lingzhi Xie
Faculty of Material Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
1 shared publication - Lingzhi Xie
Faculty of Material Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
1 shared publication - Lingzhi Zhang
Faculty of Material Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
1 shared publication - Lingzhi Zhang
Faculty of Material Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
1 shared publication
Latest Publications
- Open Access
First-Principles Study of the Effect of Sn Content on the Structural, Elastic, and Electronic Properties of Cu–Sn Alloys
In order to explore the mechanism of the influence of Sn contents on the relevant properties of Cu–Sn alloys, the structure, elasticity, electronic, and thermal properties of Cu–Sn alloys doped with different proportions of Sn (3.125 at%, 6.25 at%, and 9.375 at%) were established using the first-principles calculation based on density functional theory. Firstly, their lattice constants and Sn concentration comply with Vegard’s Law. From the mixing enthalpy, it can be seen that Sn atoms can be firmly dissolved in the Cu matrix, and the structure is most stable when the Sn content is 3.125 at%. In addition, the introduction of mismatch strain characterized their solid solution strengthening effect. The elastic and electronic properties showed that when the Sn content is 6.25 at%, the Cu–Sn alloy has the best plasticity and the highest elastic anisotropy; when the Sn content is 3.125 at%, the Cu–Sn alloy is the most stable and has stronger bulk and shear modulus, which was mainly due to a stronger Cu-Cu covalent bond. Finally, the Debye temperature, thermal conductivity, and melting point were calculated. It is estimated that the thermal conductivity of Cu–Sn alloy is relatively good when the Sn content is low.
Open AccessFirst-Principles Study of the Effect of Sn Content on the Structural, Elastic, and Electronic Properties of Cu–Sn Alloys
In order to explore the mechanism of the influence of Sn contents on the relevant properties of Cu–Sn alloys, the structure, elasticity, electronic, and thermal properties of Cu–Sn alloys doped with different proportions of Sn (3.125 at%, 6.25 at%, and 9.375 at%) were established using the first-principles calculation based on density functional theory. Firstly, their lattice constants and Sn concentration comply with Vegard’s Law. From the mixing enthalpy, it can be seen that Sn atoms can be firmly dissolved in the Cu matrix, and the structure is most stable when the Sn content is 3.125 at%. In addition, the introduction of mismatch strain characterized their solid solution strengthening effect. The elastic and electronic properties showed that when the Sn content is 6.25 at%, the Cu–Sn alloy has the best plasticity and the highest elastic anisotropy; when the Sn content is 3.125 at%, the Cu–Sn alloy is the most stable and has stronger bulk and shear modulus, which was mainly due to a stronger Cu-Cu covalent bond. Finally, the Debye temperature, thermal conductivity, and melting point were calculated. It is estimated that the thermal conductivity of Cu–Sn alloy is relatively good when the Sn content is low.
- Open Access
Microstructure and Properties of Semi-Solid 7075 Aluminum Alloy Processed with an Enclosed Cooling Slope Channel
In this study, an enclosed cooling slope channel (ECSC) was used to produce a semi-solid slurry of the 7075 aluminum alloy. The effects of the pouring temperature and the rate of cooling water on the microstructure of the semi-solid slurry were studied. The microstructure, solidification behavior, mechanical properties, and fracture mechanism of rheological squeeze casting (Rheo-SC) and liquid squeeze casting (LSC) samples were compared. The results indicate that lowering the pouring temperature and increasing the rate of cooling water can refine the crystals of the semi-solid slurry. The best process is a pouring temperature of 670 °C and a rate of cooling water of 200 L/h. The microstructure of the LSC samples was made up of coarse dendritic crystals, but the microstructure of the Rheo-SC samples was made up of almost spherical primary α1-Al and refined secondary α2-Al under this method. The ultimate tensile strength, yield strength, and elongation of the Rheo-SC samples were 238 MPa, 151 MPa, and 5.2%, respectively, which were 10%, 10.5%, and 44.4% higher than those of the LSC sample. The key factor contributing to the increased performance of the Rheo-SC samples is the combination of decreased casting flaws, strengthened grain refinement, and improved segregation.
Open AccessMicrostructure and Properties of Semi-Solid 7075 Aluminum Alloy Processed with an Enclosed Cooling Slope Channel
In this study, an enclosed cooling slope channel (ECSC) was used to produce a semi-solid slurry of the 7075 aluminum alloy. The effects of the pouring temperature and the rate of cooling water on the microstructure of the semi-solid slurry were studied. The microstructure, solidification behavior, mechanical properties, and fracture mechanism of rheological squeeze casting (Rheo-SC) and liquid squeeze casting (LSC) samples were compared. The results indicate that lowering the pouring temperature and increasing the rate of cooling water can refine the crystals of the semi-solid slurry. The best process is a pouring temperature of 670 °C and a rate of cooling water of 200 L/h. The microstructure of the LSC samples was made up of coarse dendritic crystals, but the microstructure of the Rheo-SC samples was made up of almost spherical primary α1-Al and refined secondary α2-Al under this method. The ultimate tensile strength, yield strength, and elongation of the Rheo-SC samples were 238 MPa, 151 MPa, and 5.2%, respectively, which were 10%, 10.5%, and 44.4% higher than those of the LSC sample. The key factor contributing to the increased performance of the Rheo-SC samples is the combination of decreased casting flaws, strengthened grain refinement, and improved segregation.