Kejun Xu
Kejun Xu has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Haiqin Qin
Qingdao Campus, Naval Aviation University, Qingdao 266041, China
2 shared publications - Mingming Jia
Qingdao Campus, Naval Aviation University, Qingdao 266041, China
2 shared publications - Pengcheng Ji
Qingdao Campus, Naval Aviation University, Qingdao 266041, China
2 shared publications - Zhenbo Xie
Qingdao Campus, Naval Aviation University, Qingdao 266041, China
2 shared publications - Zhengguang Li
Qingdao Campus, Naval Aviation University, Qingdao 266041, China
2 shared publications
Latest Publications
- Open Access
Study on High-Temperature Low-Cycle Fatigue Behavior of the FGH96 Superalloy Based on Internal Stress Division
In order to deeply explore the high-temperature cyclic characteristics of the FGH96 superalloy under different strain amplitudes, the high-temperature low-cycle fatigue behavior of the FGH96 superalloy was analyzed from the perspective of internal stress evolution. Four sets of strain amplitude (0.5%, 0.6%, 0.8%, and 1.2%) controlled high-temperature low-cycle fatigue tests were carried out on the FGH96 superalloy at 550 °C, and the internal stress was divided into back stress and effective stress through the cyclic stress-strain curves. The results show that the cyclic softening/hardening characteristics of the FGH96 superalloy under different strain amplitudes are closely related to the evolution of internal stress. The strain amplitude has a significant effect on the back stress of the FGH96 superalloy but has little effect on effective stress. At low strain amplitudes (0.5% and 0.6%), the back stress evolution rate of the FGH96 superalloy is lower than effective stress, and the material mainly exhibits cyclic softening. At high strain amplitudes (0.8% and 1.2%), the back stress evolution rate of the FGH96 superalloy is significantly higher than effective stress, and the material exhibits cyclic hardening. The combined effect of back stress and effective stress is the main reason for the different low-cycle fatigue behaviors of the FGH96 superalloy under different strain amplitudes.
Open AccessStudy on High-Temperature Low-Cycle Fatigue Behavior of the FGH96 Superalloy Based on Internal Stress Division
In order to deeply explore the high-temperature cyclic characteristics of the FGH96 superalloy under different strain amplitudes, the high-temperature low-cycle fatigue behavior of the FGH96 superalloy was analyzed from the perspective of internal stress evolution. Four sets of strain amplitude (0.5%, 0.6%, 0.8%, and 1.2%) controlled high-temperature low-cycle fatigue tests were carried out on the FGH96 superalloy at 550 °C, and the internal stress was divided into back stress and effective stress through the cyclic stress-strain curves. The results show that the cyclic softening/hardening characteristics of the FGH96 superalloy under different strain amplitudes are closely related to the evolution of internal stress. The strain amplitude has a significant effect on the back stress of the FGH96 superalloy but has little effect on effective stress. At low strain amplitudes (0.5% and 0.6%), the back stress evolution rate of the FGH96 superalloy is lower than effective stress, and the material mainly exhibits cyclic softening. At high strain amplitudes (0.8% and 1.2%), the back stress evolution rate of the FGH96 superalloy is significantly higher than effective stress, and the material exhibits cyclic hardening. The combined effect of back stress and effective stress is the main reason for the different low-cycle fatigue behaviors of the FGH96 superalloy under different strain amplitudes.
- Open Access
Fatigue Behavior of the FGH96 Superalloy under High-Temperature Cyclic Loading
Strain-controlled low-cycle fatigue (LCF) tests and stress-controlled creep-fatigue interaction (CFI) tests on the FGH96 superalloy were carried out at 550 °C to obtain the cyclic softening/hardening characteristics at different strain amplitudes and ratcheting strain characteristics under different hold time. The failure mechanism of the FGH96 superalloy under different loading conditions was analyzed through fracture observations. The results show that the FGH96 superalloy exhibits different cyclic softening/hardening characteristics at different strain amplitudes, and the introduction of the hold time at peak stress exacerbates the ratcheting strain of the FGH96 superalloy under asymmetric stress cycles. Fracture observations show that the magnitude of the strain amplitude, high-temperature oxidation, and the introduction of the hold time will affect the mechanical properties of the FGH96 superalloy and change its fracture mode.
Open AccessFatigue Behavior of the FGH96 Superalloy under High-Temperature Cyclic Loading
Strain-controlled low-cycle fatigue (LCF) tests and stress-controlled creep-fatigue interaction (CFI) tests on the FGH96 superalloy were carried out at 550 °C to obtain the cyclic softening/hardening characteristics at different strain amplitudes and ratcheting strain characteristics under different hold time. The failure mechanism of the FGH96 superalloy under different loading conditions was analyzed through fracture observations. The results show that the FGH96 superalloy exhibits different cyclic softening/hardening characteristics at different strain amplitudes, and the introduction of the hold time at peak stress exacerbates the ratcheting strain of the FGH96 superalloy under asymmetric stress cycles. Fracture observations show that the magnitude of the strain amplitude, high-temperature oxidation, and the introduction of the hold time will affect the mechanical properties of the FGH96 superalloy and change its fracture mode.