Ming Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Ming Zhang has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Hui Wang
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
3 shared publications - Yidi Li
State Key Lab for Powder Metallurgy, Central South University, Changsha 410083, China
3 shared publications - Yunping Li
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
3 shared publications - Biaobiao Yang
IMDEA Materials Institute, c/Eric Kandel 2, Getafe, 28906 Madrid, Spain
2 shared publications - Ruilin Lai
Research Institute of Light Alloy, Central South University, Changsha, China
2 shared publications - Kuo Ma
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
1 shared publication
Latest Publications
- 15 February 2025
- Published by Springer Nature in Progress in Additive Manufacturing
- Vol. 10 (9) , 6769-6783
Influence of protrusion geometry on the microstructure and mechanical properties of AA2219 fabricated by additive friction stir deposition
- 15 February 2025
- Published by Springer Nature in Progress in Additive Manufacturing
- Vol. 10 (9) , 6769-6783
Influence of protrusion geometry on the microstructure and mechanical properties of AA2219 fabricated by additive friction stir deposition
- Open Access
Effect of Heat Treatment States of Feedstock on the Microstructure and Mechanical Properties of AA2219 Layers Deposited by Additive Friction Stir Deposition
This study is the first to research the microstructure and mechanical properties of the workpiece after additive friction stir deposition (AFSD) of the feedstock at different heat treatment stages. AA2219 aluminum alloys with three different heat treatment stages were selected as the feedstock, and alloys with dense structure were successfully prepared by the additive friction stir deposition AFSD process. Experimental results show that AFSD exhibits an excellent ability to refine grains and improve the uniform distribution of precipitates in the second phase, thereby improving the plasticity of AA2219 alloy after the AFSD process. Because of the continuous dynamic recrystallization (CDRX) in the AA2219 alloy during AFSD, the grain size after the AFSD process is independent of the initial feedstock grain size for three samples. The equilibrium phase (θ) size is genetically related to the initial size of the second-phase particles in the feedstock. Due to grain refinement and dislocation strengthening, the yield strength of AA2219-casting increased significantly from 79.8 MPa to 124.1 MPa after AFSD. The yield strength of the AA2219-T4 decreases slightly from 151.8 MPa to 140.4 MPa after AFSD. The precipitation of the second phase leads to a decrease in solid solution strengthening and dislocation strengthening. However, grain refinement strengthening partially offsets this reduction. The yield strength of AA2219-T87 decreased from 398.5 MPa to 147.2 MPa after AFSD. As such, grain refinement strengthening and solid solution strengthening by the AFSD process are much smaller than the yield strength lost by precipitation strengthening and dislocation strengthening.
Open AccessEffect of Heat Treatment States of Feedstock on the Microstructure and Mechanical Properties of AA2219 Layers Deposited by Additive Friction Stir Deposition
This study is the first to research the microstructure and mechanical properties of the workpiece after additive friction stir deposition (AFSD) of the feedstock at different heat treatment stages. AA2219 aluminum alloys with three different heat treatment stages were selected as the feedstock, and alloys with dense structure were successfully prepared by the additive friction stir deposition AFSD process. Experimental results show that AFSD exhibits an excellent ability to refine grains and improve the uniform distribution of precipitates in the second phase, thereby improving the plasticity of AA2219 alloy after the AFSD process. Because of the continuous dynamic recrystallization (CDRX) in the AA2219 alloy during AFSD, the grain size after the AFSD process is independent of the initial feedstock grain size for three samples. The equilibrium phase (θ) size is genetically related to the initial size of the second-phase particles in the feedstock. Due to grain refinement and dislocation strengthening, the yield strength of AA2219-casting increased significantly from 79.8 MPa to 124.1 MPa after AFSD. The yield strength of the AA2219-T4 decreases slightly from 151.8 MPa to 140.4 MPa after AFSD. The precipitation of the second phase leads to a decrease in solid solution strengthening and dislocation strengthening. However, grain refinement strengthening partially offsets this reduction. The yield strength of AA2219-T87 decreased from 398.5 MPa to 147.2 MPa after AFSD. As such, grain refinement strengthening and solid solution strengthening by the AFSD process are much smaller than the yield strength lost by precipitation strengthening and dislocation strengthening.
- Open Access
Influence of Preheating Temperature on the Microstructure and Mechanical Properties of 6061/TA1 Composite Plates Fabricated by AFSD
In this study, composite plates of 6061/TA1 were successfully manufactured using additive friction stir deposition (AFSD). The impact of preheating temperatures (room temperature, 100 °C, 200 °C) on the interfacial microstructure and interface mechanical properties at various deposition zones was studied. The results showed that as the preheating temperature increased or when the deposit zone shifted from the boundary to the center, the diffusion width of Al and Ti increased, accompanied by an increase in bonding shear strength. Moreover, in the boundary zone of the sample preheated at room temperature (P-RT), only mechanical bonding was observed, resulting in the lowest bonding shear strength. Conversely, the other samples exhibited a combination of mechanical and metallurgical bonding. Under the preheating temperature of 200 °C, interfacial intermetallic compounds were observed near the center zone, which exhibited the highest bonding shear strength.
Open AccessInfluence of Preheating Temperature on the Microstructure and Mechanical Properties of 6061/TA1 Composite Plates Fabricated by AFSD
In this study, composite plates of 6061/TA1 were successfully manufactured using additive friction stir deposition (AFSD). The impact of preheating temperatures (room temperature, 100 °C, 200 °C) on the interfacial microstructure and interface mechanical properties at various deposition zones was studied. The results showed that as the preheating temperature increased or when the deposit zone shifted from the boundary to the center, the diffusion width of Al and Ti increased, accompanied by an increase in bonding shear strength. Moreover, in the boundary zone of the sample preheated at room temperature (P-RT), only mechanical bonding was observed, resulting in the lowest bonding shear strength. Conversely, the other samples exhibited a combination of mechanical and metallurgical bonding. Under the preheating temperature of 200 °C, interfacial intermetallic compounds were observed near the center zone, which exhibited the highest bonding shear strength.