Ziming Zeng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Ziming Zeng has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Biaobiao Yang
IMDEA Materials Institute, c/Eric Kandel 2, Getafe, 28906 Madrid, Spain
3 shared publications - Yunping Li
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
3 shared publications - Hui Wang
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
2 shared publications - Kuo Ma
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
2 shared publications - Yidi Li
State Key Lab for Powder Metallurgy, Central South University, Changsha 410083, China
2 shared publications - Chao Li
State Key Laboratory for Powder Metallurgy, Central South University, Changsha 410083, China
1 shared publication
Latest Publications
- Open Access
Oxidation Behavior of Aluminide Coatings on Cobalt-Based Superalloys by a Vapor Phase Aluminizing Process
In this work, the oxidation behavior of an aluminide coating at 900, 1000, and 1100 °C was investigated. The aluminide coating was prepared on a cobalt-based superalloy using a vapor phase aluminizing process, which is composed of a β-(Co,Ni)Al phase outer layer and a Cr-rich phase diffusion layer. The experimental results showed that the oxidation of the coating at 900–1100 °C all obey the parabolic law. The oxidation rate constants of the coating were between 2.19 × 10−7 and 47.56 × 10−7 mg2·cm−4·s−1. The coating produced metastable θ-Al2O3 at 900 °C and stable α-Al2O3 at 1000 and 1100 °C. As the oxidation temperature increases, the formation of Al2O3 is promoted, consuming large amount of Al in the coating, resulting in the transformation from β-(Co,Ni)Al phase to α-(Co,Ni,Cr) phase. And the decrease in the β phase in the coating led to the dissolution of the diffusion layer.
Open AccessOxidation Behavior of Aluminide Coatings on Cobalt-Based Superalloys by a Vapor Phase Aluminizing Process
In this work, the oxidation behavior of an aluminide coating at 900, 1000, and 1100 °C was investigated. The aluminide coating was prepared on a cobalt-based superalloy using a vapor phase aluminizing process, which is composed of a β-(Co,Ni)Al phase outer layer and a Cr-rich phase diffusion layer. The experimental results showed that the oxidation of the coating at 900–1100 °C all obey the parabolic law. The oxidation rate constants of the coating were between 2.19 × 10−7 and 47.56 × 10−7 mg2·cm−4·s−1. The coating produced metastable θ-Al2O3 at 900 °C and stable α-Al2O3 at 1000 and 1100 °C. As the oxidation temperature increases, the formation of Al2O3 is promoted, consuming large amount of Al in the coating, resulting in the transformation from β-(Co,Ni)Al phase to α-(Co,Ni,Cr) phase. And the decrease in the β phase in the coating led to the dissolution of the diffusion layer.
- Open Access
Tribocorrosion Behavior of NiCoCrMoCu Alloys Containing Different Carbides in Acidic Media at Various Applied Loads and Sliding Speeds
In this study, the ball-on-disk sliding wear and tribocorrosion behavior in the H2SO4 and HCl solution of NiCoCrMoCu alloys with carbon additions of 0.2, 1, 1.5, and 2 wt.% with the Al2O3 ball as a counterpart was investigated systematically. Obvious tribocorrosion antagonistic effects were found after wear in both aqueous solutions. Compared with dry sliding wear conditions, the lubrication effect of the aqueous solution significantly reduces the wear rate of the alloy, and the reduction effect in the H2SO4 aqueous solution was more obvious than that in HCl. The antagonistic effects of the 0.2C and 1C alloys decrease with the load and sliding rate, while those of the 1.5C and 2C alloys increase. The (coefficient of friction) COF and wear rate under different loads and sliding rates were analyzed using the response surface analysis (RSM) method. It was found that the COF mainly showed dependence on the sliding rate, while the wear rate showed dependence on load and sliding speed.
Open AccessTribocorrosion Behavior of NiCoCrMoCu Alloys Containing Different Carbides in Acidic Media at Various Applied Loads and Sliding Speeds
In this study, the ball-on-disk sliding wear and tribocorrosion behavior in the H2SO4 and HCl solution of NiCoCrMoCu alloys with carbon additions of 0.2, 1, 1.5, and 2 wt.% with the Al2O3 ball as a counterpart was investigated systematically. Obvious tribocorrosion antagonistic effects were found after wear in both aqueous solutions. Compared with dry sliding wear conditions, the lubrication effect of the aqueous solution significantly reduces the wear rate of the alloy, and the reduction effect in the H2SO4 aqueous solution was more obvious than that in HCl. The antagonistic effects of the 0.2C and 1C alloys decrease with the load and sliding rate, while those of the 1.5C and 2C alloys increase. The (coefficient of friction) COF and wear rate under different loads and sliding rates were analyzed using the response surface analysis (RSM) method. It was found that the COF mainly showed dependence on the sliding rate, while the wear rate showed dependence on load and sliding speed.
- Open Access
Influence of Preheating Temperature on the Microstructure and Mechanical Properties of 6061/TA1 Composite Plates Fabricated by AFSD
In this study, composite plates of 6061/TA1 were successfully manufactured using additive friction stir deposition (AFSD). The impact of preheating temperatures (room temperature, 100 °C, 200 °C) on the interfacial microstructure and interface mechanical properties at various deposition zones was studied. The results showed that as the preheating temperature increased or when the deposit zone shifted from the boundary to the center, the diffusion width of Al and Ti increased, accompanied by an increase in bonding shear strength. Moreover, in the boundary zone of the sample preheated at room temperature (P-RT), only mechanical bonding was observed, resulting in the lowest bonding shear strength. Conversely, the other samples exhibited a combination of mechanical and metallurgical bonding. Under the preheating temperature of 200 °C, interfacial intermetallic compounds were observed near the center zone, which exhibited the highest bonding shear strength.
Open AccessInfluence of Preheating Temperature on the Microstructure and Mechanical Properties of 6061/TA1 Composite Plates Fabricated by AFSD
In this study, composite plates of 6061/TA1 were successfully manufactured using additive friction stir deposition (AFSD). The impact of preheating temperatures (room temperature, 100 °C, 200 °C) on the interfacial microstructure and interface mechanical properties at various deposition zones was studied. The results showed that as the preheating temperature increased or when the deposit zone shifted from the boundary to the center, the diffusion width of Al and Ti increased, accompanied by an increase in bonding shear strength. Moreover, in the boundary zone of the sample preheated at room temperature (P-RT), only mechanical bonding was observed, resulting in the lowest bonding shear strength. Conversely, the other samples exhibited a combination of mechanical and metallurgical bonding. Under the preheating temperature of 200 °C, interfacial intermetallic compounds were observed near the center zone, which exhibited the highest bonding shear strength.